| HS Code | 877805 |
| Polymertype | Polypropylene (PP) |
| Reinforcement | Glass fiber |
| Glassfibercontent | 25% by weight |
| Flameretardanttype | Halogen-free flame retardant |
| Halogenfree | Yes |
| Flameretardancyrating | UL94 V-0 (typical; thickness-dependent) |
| Density | Approx. 1.3 g/cm³ |
| Tensilestrength | Approx. 70–85 MPa |
| Flexuralmodulus | Approx. 5,000–6,500 MPa |
| Notchedizodimpactstrength | Approx. 6–12 kJ/m² |
| Heatdeflectiontemperature | Approx. 140–155 °C at 1.8 MPa |
| Processingmethod | Injection molding |
| Moldingshrinkage | Typical low shrinkage; glass-fiber dependent |
| Waterabsorption | Low |
| Electricalinsulation | Typical insulating behavior for PP-based compounds |
As an accredited Kingfa PP-NPG25,Halogen-Free FR PP-GF25 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-resistant bags, 40 bags per pallet (1,000 kg net). |
| Container Loading (20′ FCL) | Kingfa PP-NPG25 Halogen-Free FR PP-GF25 loaded in a 20′ FCL, palletized, shrink-wrapped, and secured for safe ocean transport. |
| Shipping | Shipping description: Kingfa PP-NPG25 (Halogen-Free FR PP-GF25), non-hazardous polypropylene glass-fiber compound pellets. Not regulated for transport; no UN number, hazard class, or packing group. Typically shipped in 25 kg moisture-barrier bags on pallets or in bulk; keep dry, cool, and away from sunlight and ignition sources. |
| Storage | Store Kingfa PP-NPG25 (Halogen-Free FR PP-GF25) in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and ignition sources. Keep original containers sealed and palletized to prevent moisture pickup, contamination, and bag damage. Avoid prolonged UV exposure and excessive temperature fluctuations. Use first-in, first-out rotation; maintain good housekeeping and control dust. Consult the SDS/TDS for specific storage limits. |
| Shelf Life | Kingfa PP-NPG25 typically has a 24-month shelf life when stored sealed, dry, and protected from sunlight at ambient temperature. |
Low-voltage distribution board and miniature circuit breaker subcomponents processed from Kingfa PP-NPG25 are run on reciprocating single-screw injection-moulding machines with screw L/D of 20:1 to 25:1, compression ratio 2.2:1–2.8:1, and clamp force from 1,200 kN to 4,500 kN depending on projected part area. The primary process conflict is thermal residence time: barrel temperature from hopper to nozzle is set at 170°C, 190°C, 210°C, 220°C, and nozzle at 215°C–230°C. Melt temperature above 240°C for more than 6 min degrades the halogen-free flame-retardant package, producing splay, yellowing, and localised loss of glow-wire resistance. Back pressure is held at 0.5–1.2 MPa and screw speed at 50–80 rpm to limit glass-fibre attrition; melt fibre length below 250 µm is associated with lower unnotched Charpy impact when tested under ISO 179-1/1eU. Mould temperature is controlled to 35°C–50°C with turbulent water flow in drilled cooling channels. Cooling time for 2.5 mm wall sections ranges from 14 s to 22 s. Compliance anchors include UL 94 V-0 at 1.5 mm and 3.0 mm under the supplier’s Yellow Card, IEC 60695-2-11 GWFI of 960°C at 2.0 mm, IEC 61439-1:2020 for low-voltage switchgear assemblies, and Directive 2011/65/EU RoHS recast Annex II. Formula addition ratio: the compound is not diluted with unreinforced PP; closed-loop regrind from clean sprues and runners is added at 15–20 wt% to 80–85 wt% virgin Kingfa PP-NPG25 only after the regrind lot shows melt mass-flow rate drift no greater than ±2 g/10 min at 230°C/2.16 kg. Terminal product types are MCB bases, busbar supports, distribution board covers, and DIN-rail insulation carriers.
Observed production-floor failure modes in this application include gate blush when injection velocity exceeds 100 mm/s through narrow fan gates, and warpage across a 300 mm distribution-board cover exceeding 0.4 mm where differential shrinkage develops between glass-rich and polymer-rich surface layers. Tooling for such covers therefore uses end-of-fill overflow tabs and valve-gate sequencing rather than single direct sprue gating. On clamping units below 1,500 kN, flash appears at the parting line when cavity pressure exceeds 45 MPa, which limits the usable hold-pressure window. Batch-to-batch variance in regrind-derived ash content is checked by thermogravimetric analysis after 2 h at 600°C; ash deviation greater than ±1.5 wt% relative to virgin material triggers rejection from the low-voltage enclosure run.
In automotive underbonnet electrical distribution, production-scale trials with Kingfa PP-NPG25 are launched on multicavity hot-runner tools with 2 or 4 pneumatic valve gates to avoid knit lines at fuse-slot partitions; the hot-runner manifold is set 5–10°C above nozzle temperature. Compliance is governed by FMVSS 302 where interior materials are in scope, SAE J369 where specified by OEM material standards, and IEC 60068-2-30 for damp-heat cyclic exposure at 55°C/95% RH on engine-side electrical housings. Continuous operating temperature in the nominated mounting location is kept below 90°C; heat deflection temperature under ISO 75-2/A at 1.8 MPa is in the range of 130°C–150°C for this compound, but underhood locations exceeding 105°C are excluded from this material specification. The material is pre-dried at 80°C for 2–4 h when open storage RH exceeds 60% because surface moisture produces silver streaks at gate locations and reduces dry-as-moulded tracking performance. Injection speed is staged from 30–40 mm/s through the gate to 70–100 mm/s across the periphery of the box, with switchover to holding pressure at a cavity pressure of 35–45 MPa. Formula addition ratio: the compound is processed as supplied; regrind from the same hot-runner material stream is limited to 20 wt% because higher regrind fractions can reduce comparative tracking index below 600 V when verified by IEC 60112. Terminal products are automotive fuse boxes, relay boxes, E-box brackets, and electrical distribution covers.
Washing machine motor supports and dishwasher control-panel brackets are moulded from Kingfa PP-NPG25 under IEC 60335-1:2016 Clause 30.2, which for insulated material supporting live parts at current above 0.2 A requires glow-wire testing at 750°C or 850°C depending on part position. Moulded parts are validated against IEC 60695-2-11 for GWFI at 850°C/2.0 mm and IEC 60695-2-13 for GWIT at 775°C/1.5 mm. Field data from a 4,000 kN clamping unit with 55 mm screw diameter show that barrel temperatures must be shifted to 200°C–220°C to avoid local fibre accumulation behind hot-runner needle shut-offs; when screw rotational speed exceeds 70 rpm, shear heating at the check ring raises melt temperature by 8°C–12°C, increasing flash tendency at the parting line. Insert moulding of M5 brass threaded inserts is performed with insert preheat at 120°C; insert-to-wall distance is not less than 2.5 mm to prevent hoop stress cracking during thermal cycling from −25°C to 85°C. Formula addition ratio for insert-bearing parts: 100% Kingfa PP-NPG25, with organic pigment masterbatch at 1.5–2.0 wt% only if the masterbatch carrier is PP-g-MAH and has a UL 94 V-0 rating at 1.5 mm; carbon black masterbatch above 2.5 wt% tends to lower CTI and is avoided in terminal-block geometry. Compliance includes EN 60335-1, EN 60695-2-11, EN 60695-2-13, Directive 2011/65/EU, and REACH Annex XVII entry 50 for restricted PAH in consumer articles. Terminal product types are washing machine motor brackets, dishwasher control-panel frames, tumble dryer door bases, and terminal block supports.
Because AC charging system exterior shells for IEC 62196-2 infrastructure demand both halogen-free flame retardance and dimensional stability after thermal shock, processors select Kingfa PP-NPG25 for charge-port brackets and non-current-carrying coupler housings rather than for direct contact interfaces. The injection-moulding process uses a three-plate cold-runner mould with 2 point gates on a deep draw; gate lands are polished to a 0.02 mm radius to reduce delamination at the glass-rich skin. Melt temperature is capped at 225°C, and hot-runner nozzles are individually controlled within ±2°C; holding pressure is maintained until the gate seals, monitored by cavity-pressure sensors at 45 MPa peak. The material must satisfy UL 94 V-0 at 1.5 mm and 3.0 mm, IEC 60695-2-11 GWFI 960°C at 2.0 mm, IEC 60112 CTI ≥ 600 V, and REACH Article 33 SVHC absence below 0.1 wt%. Production-scale experience shows that regrind levels above 25 wt% produce unmelted glass bundles at thin ribs, visible as white specks and lower notched Charpy impact when tested per ISO 179-1/1eA. Formula addition ratio is therefore maintained at 80–100 wt% virgin compound, with closed-loop regrind limited to 0–20 wt% and excluded from the visible surface unless black masterbatch at 1 wt% is used. Terminal product types are AC charging coupler shells, charge-port mounting brackets, and internal insulation separators.
Polymeric junction box lower shells in photovoltaic modules are subject to wet leakage current tests and flammability classification, but Kingfa PP-NPG25 is specified only where continuous service temperature inside the junction box remains below 85°C and where UV radiation is attenuated by cover glass or adjacent framing; published data for this specific configuration as a direct UV-exposed enclosure is limited. Binding standards are IEC 62790:2014 for PV junction boxes, IEC 60695-11-10 for flammability classification, UL 746C for polymeric materials used as outdoor electrical enclosures where f1 outdoor suitability is required, and Directive 2011/65/EU. Flame classification is UL 94 V-0 at 1.5 mm, and glow-wire GWFI at 2.0 mm is 960°C when tested per IEC 60695-2-11. Because thermoset potting compound injected into the lower shell can reach exothermic cure temperatures of 100°C–120°C, moulded wall thickness below 2.0 mm is avoided to prevent creep under load at 85°C. The lower shell is moulded on a 2,800 kN machine with a cold-runner tab gate into a flat base; mould temperature is held at 45°C. Melt temperature is set at 210°C–225°C, screw speed 50–60 rpm, back pressure 0.3–0.5 MPa. Formula addition ratio: 100% compound as supplied, with no regrind because potting compound adhesion to glass-rich surfaces changes after multiple heat histories and reprocessed material is not qualified for this outdoor electrical assembly. Terminal product types are photovoltaic junction box lower shells, combiner box terminal brackets, and DC disconnect insulating bases.
Within industrial control panel assembly, the material is used for terminal block bases and circuit-board mounting boards that must survive high current faults without becoming an ignition source. Compliance is anchored to UL 1059 for terminal blocks, IEC 60947-7-1:2009 for terminal blocks in low-voltage switchgear, and UL 94 V-0 at 0.8 mm and 1.5 mm where specified. The grade is injection moulded on high-cavitation tools with 8–16 cavities, using a cold runner system with a heated sprue bush; runner diameter is not reduced below 4.0 mm because glass-fibre filled melt freezes rapidly and thinner runners generate imbalanced pressure drops across cavities. Clamp force is estimated at 0.3–0.4 kN per cm² of projected area; a 120 mm × 80 mm plate with 8 cavities uses 1,200–1,500 kN. Decompression is set at 3–5 mm after screw retraction to prevent drooling at the open nozzle; decompression beyond 7 mm introduces air bubbles in the melt. Formula addition ratio: 90 wt% virgin Kingfa PP-NPG25 and 10 wt% closed-loop regrind, only if regrind is produced from sprues and runners and has an apparent density change of ±0.03 g/cm³ relative to virgin compound. Terminal product types are terminal block bases, relay sockets, and industrial control board insulating mounts.
Cable management components in concealed building routes, when replacing PPO/PS blends with Kingfa PP-NPG25, are constrained by lower melt stiffness and by the requirement that halogen content remain below 0.2% by mass when tested per IEC 60754-2. The relevant standards are IEC 61386-1:2008/AC:2010 and IEC 61386-21:2008 for rigid conduit systems, UL 514C for thermoplastic conduit fittings, UL 94 V-0 at 1.5 mm, and IEC 60695-2-11 GWFI 850°C/2.0 mm. On production scale, threaded adapters and cable glands are moulded in tools with mechanical unscrewing cores driven by hydraulic rotary actuators; the unscrewing core is maintained at 40°C to prevent PP shrinkage seizure. Melt temperature is 215°C–225°C, injection velocity is 40–60 mm/s, and holding pressure is 50–70 MPa. Because flame-retardant polypropylene is notch-sensitive at threaded roots, thread root radius is designed at 0.2 mm minimum and the gate is placed at the flange rather than at the thread root. Formula addition ratio: 100% Kingfa PP-NPG25; regrind is avoided where IEC 60754-2 halogen content after processing is required, because multiple heat histories can increase surface organic residue. Terminal product types are rigid conduit adapters, cable glands, inspection box bases, and conduit junction fittings.
Competitive Kingfa PP-NPG25,Halogen-Free FR PP-GF25 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-NPG25 is a halogen-free flame-retardant polypropylene compound reinforced with nominal 25 wt% glass fiber. The grade designation couples the NPG series prefix to the numeral 25, which identifies the glass fiber mass fraction after ash testing per ISO 3451-1; the flame-retardant package is based on phosphorus–nitrogen intumescent chemistry rather than brominated flame retardants with antimony trioxide synergism. Published data for this specific configuration is limited in openly accessible literature, and the following treatment should be read as a framework for lot-specific verification rather than a replacement for the manufacturer’s certificate of analysis.
Because the material contains 25 wt% glass fiber, its mechanical response differs from unfilled halogen-free FR PP in three primary ways: higher tensile and flexural modulus, reduced mold shrinkage, and lower elongation at break. Tensile properties are evaluated by ISO 527-1/-2 on specimens molded in accordance with ISO 294-1; flexural properties by ISO 178; and notched impact by ISO 179-1 or ISO 180. Exact values are lot-dependent and must be read from the certificate of analysis, but the glass fiber phase generally compresses the strain-to-failure envelope and increases anisotropy between flow and cross-flow directions.
Thermal decomposition of the phosphorus–nitrogen FR package defines an upper operating boundary. Ammonium polyphosphate-based intumescent systems begin to release bound water and ammonia at temperatures approaching 240 °C to 250 °C; therefore barrel and nozzle setpoints for PP-NPG25 are typically limited to 180 °C to 230 °C, with a hard avoidance of melt temperatures above 240 °C unless specifically validated on a lot basis. Lower melt temperatures reduce flash and minimize thermal degradation of the flame-retardant synergist, but they also increase melt viscosity because the glass fiber filler raises the elastic component of the melt. Molding trials on general-purpose injection machines should begin with a flat to slightly rising rear-to-front barrel profile, a screw back pressure below 0.7 MPa, and injection speeds that avoid shear heating above 230 °C at the nozzle.
Pre-drying is required when storage relative humidity exceeds 60% or when silo or bag exposure exceeds 24 h. Desiccant dryer settings of 80 °C to 100 °C for 2 h to 4 h with a dew point of -20 °C or lower are typical for halogen-free FR PP-GF compounds; grade-specific instructions may differ. Inlet moisture above 0.05% can generate splay, reduce UL 94 performance, and accelerate hydrolysis of the FR package during processing.
On twin-screw compounding lines, glass fiber is typically introduced through side stuffing after the polymer is fully molten, while the heat-sensitive intumescent flame-retardant package may be fed downstream to limit thermal history. A co-rotating twin-screw extruder with an L/D between 32:1 and 44:1 is standard for this compound class; barrel tempering zones are segmented to apply high dispersive mixing in the glass incorporation zone and low-shear distribution in downstream FR incorporation. Glass fiber attrition must be controlled by using low-shear conveying elements after the side feeder, because severe fiber breakage lowers tensile modulus and tensile strength below the values expected for 25 wt% fiber content.
Lot release data for glass fiber content via ISO 3451-1 ash analysis and melt flow rate via ISO 1133-1:2022 at 230 °C/2.16 kg are standard incoming inspection points. If ash content deviates below nominal 25 wt% fiber loading by more than the manufacturer’s tolerance, mechanical stiffness and flammability can shift; if MFR is outside the specified window, filling pressure and weld-line strength may depart from mold trials.
| Characteristic | Halogen-free FR PP-GF25 (PP-NPG25 class) | Brominated FR PP-GF25 |
|---|---|---|
| Flame-retardant mechanism | Intumescent char formation and fuel dilution | Gas-phase radical quenching with bromine/antimony synergism |
| Smoke density under ISO 5659-2 | Typically lower smoke release than brominated systems | Can show higher smoke and soot depending on formulation |
| Combustion gas corrosivity | Lower halogen acid potential | Higher potential for HBr and antimony halide release |
| Density | Generally lower than brominated FR PP-GF25 | Generally higher due to brominated/antimony additive loading |
| Processing thermal stability | Upper melt limit near 240 °C due to FR package decomposition | Often wider but still limited by PP oxidative degradation |
| Color and plate-out | May require venting and mold surface maintenance due to intumescent additives | May show antimony/bromine deposit and occasional yellowing |
Compared with unfilled halogen-free FR PP, the 25 wt% glass fiber phase increases flexural modulus under ISO 178 and reduces linear mold shrinkage measured by ISO 294-4. The property shift is not uniform; weld-line regions in glass-filled parts can retain only a fraction of the bulk tensile strength, and design allowable stress at weld lines should be established by instrumented impact or tensile testing of welded specimens. Published data for PP-NPG25 specific weld-line behavior is limited.
Halogen-free status is generally evaluated against IEC 61249-2-21, which limits bromine to 900 ppm, chlorine to 900 ppm, and total halogens to 1500 ppm. Compliance with RoHS Directive 2011/65/EU Annex II and REACH Candidate List obligations should be confirmed from the material declaration; the absence of PBDE and PBB substances is a baseline expectation but not a substitute for full substance-of-concern screening. Electrical appliance components may additionally require glow-wire verification under IEC 60695-2-12 at 750 °C or 850 °C, and flammability classification under UL 94 / IEC 60695-11-10 is thickness-dependent. Lot certification for thin-wall sections below 1.5 mm must be requested specifically because halogen-free intumescent systems can exhibit a thickness-dependent UL 94 transition.
| Standard test method | Property | Purpose in grade qualification |
|---|---|---|
| ISO 1183-1 | Density | Part weight and filler-level cross-check |
| ISO 3451-1 | Glass fiber content | Verify nominal 25 wt% loading |
| ISO 1133-1:2022 | Melt mass-flow rate | Lot-to-lot flow consistency at 230 °C/2.16 kg |
| ISO 527-1/-2 | Tensile modulus, tensile strength, elongation | Structural design values |
| ISO 178 | Flexural modulus, flexural strength | Stiffness for enclosures and supports |
| ISO 179-1 / ISO 180 | Charpy/Izod impact | Fracture resistance after FR addition |
| UL 94 / IEC 60695-11-10 | Vertical burn classification | Flammability compliance at required thickness |
| IEC 60695-2-12 | Glow-wire flammability index | Appliance end-product safety testing |
| IEC 61249-2-21 | Halogen content | Halogen-free verification |
Because 25 wt% glass fiber orients in the flow direction during mold filling, the resulting part has anisotropic tensile properties and shrinkage behavior. In injection molded plaques, flow-direction tensile modulus can exceed cross-flow tensile modulus by more than 20% in glass-reinforced PP; exact shift for PP-NPG25 should be measured from plaques molded per ISO 294-5 rather than extrapolated from generic composites. Gate placement should move weld lines away from structural load paths and current-carrying areas.
For living-hinge features, halogen-free FR PP-GF25 is generally unsuitable because glass fibers and intumescent fillers reduce flexural endurance and hinge life compared with unfilled PP; molders requiring hinge functionality should select an unfilled FR PP grade. Component wall thickness below 1.0 mm may require fast injection speeds and elevated mold temperatures near 60 °C to 90 °C to preserve surface fill and reduce fiber read-through, but the mold temperature must remain compatible with the grade’s shrinkage targets and cycle-time constraints.
Short shots in thin-wall sections often arise from poor flow because glass fiber increases viscosity; increasing melt temperature above 230 °C is not the first corrective action because it can degrade the halogen-free FR package. Instead, increase injection speed, enlarge gate dimensions, or move the gate to a thicker section. Silver streaking at the gate indicates moisture or gas from FR decomposition; check dryer dew point and residence time. Splay may also appear when regrind content exceeds 20%; higher regrind levels can reduce UL 94 performance because the intumescent char precursor may be partially degraded.
Avoid mixing with amine-based additives or color concentrates that contain amines, because amine groups can interfere with the acid source in the intumescent FR system and reduce char formation. Avoid silane coupling agents not specified for the grade; inappropriate coupling can alter interfacial adhesion and lower impact resistance. Store in sealed, moisture-tight packaging at 5 °C to 35 °C; avoid direct sunlight and relative humidity above 60%.
Shear viscosity should be characterized by capillary rheometry per ISO 11443:2021 at shear rates spanning 10^1 s^-1 to 10^5 s^-1 and at three melt temperatures. For glass-reinforced PP, the shear-thinning exponent commonly lies between 0.25 and 0.40; flow simulation using only melt mass-flow rate can underestimate fill pressure in thin sections. Mold-filling simulation should use cross-WLF viscosity coefficients derived from actual PP-NPG25 lots, not from generic PP-GF25 databases.
On production-scale injection molding machines, batch-to-batch variance in the halogen-free FR package can present as intermittent UL 94 failures even when MFR and ash are within specification. Therefore processors should retain molded flammability bars from each lot and perform internal screening before releasing production lots. The root cause of intermittent flammability failure in glass-reinforced intumescent PP is often traceable to poor dispersion of the phosphorus–nitrogen synergist, excessive residence time in the barrel, or regrind accumulation above the permitted level.
Application areas that are compatible with the product’s expected stiffness and halogen-free flame retardancy include electrical switchgear enclosures, terminal blocks, busbar insulating supports, capacitor housings, and structural brackets inside appliances. In each case, end-product standards such as IEC 61439-1 for low-voltage switchgear and controlgear assemblies or appliance-specific glow-wire requirements may govern material acceptance. Published data for PP-NPG25 performance in these exact applications is limited, so pre-production validation is mandatory.
Against a PA66 FR-GF25, PP-NPG25 generally offers lower density and lower moisture absorption, but higher creep under sustained load and lower heat deflection temperature; comparative material selection should be based on ISO 75-1/-2 HDT and long-term creep data rather than short-term tensile values. Mechanical property data for this class are usually generated on injection molded test specimens conditioned at 23 °C and 50% RH for at least 40 h per ISO 291 before testing. The elastic modulus of a 25 wt% short-glass-fiber PP compound can exhibit orientation-dependent scatter of ±5% or more across molded specimens; therefore accept/reject decisions for PP-NPG25 should use the manufacturer’s specified test method and specimen geometry rather than repurposing values from generic material databases.
Thermal aging resistance of halogen-free FR PP-GF25 may be evaluated by ISO 4577 or UL 746B relative thermal index, depending on end-use voltage and insulation requirements. Long-term heat aging can reduce char-forming capacity because the intumescent precursor slowly undergoes thermal oxidation; therefore continuous use temperatures should be derived from lot-specific data, not from the melting temperature of the base PP. For electrical insulation parts, comparative tracking index measured per IEC 60112 can be sensitive to surface contamination from release agents and external lubricants; processors should validate CTI on production parts after mechanical cleaning if required.
During injection molding, mold temperature should be set to 20 °C to 60 °C for semicrystalline polypropylene, with higher settings near 60 °C improving surface appearance but extending cycle time. Holding pressure and packing time should be derived from gate freeze study using cavity pressure transducers; premature gate seal can increase sink marks near bosses and ribs, while excessive pack pressure can increase molded-in stress and warp. Because glass fiber reduces shrinkage, sink-mark risk is lower than unfilled FR PP but not eliminated in thick sections adjacent to thin walls.
As busbar insulating supports in low-voltage switchgear, the compound is expected to combine stiffness, dimensional stability under mechanical fastening, and flame retardancy. The end-use standard IEC 61439-1 prescribes temperature-rise and short-circuit withstand requirements; material selection must include creep behavior under clamping force and possible glass fiber stress relaxation. Published data for PP-NPG25 specific creep behavior is limited, so component-level testing is required.