| HS Code | 637573 |
| Density | 1.05 g/cm³ |
| Melt Flow Rate | 8.0 g/10 min (230°C/2.16 kg) |
| Tensile Strength | 25 MPa |
| Elongation At Break | 20% |
| Flexural Modulus | 1200 MPa |
| Notched Izod Impact Strength | 5 kJ/m² |
| Heat Deflection Temperature | 90°C |
| Flammability Rating | UL94 V-0 |
| Glow Wire Flammability Index | 750°C |
| Glow Wire Ignition Temperature | 750°C |
| Molding Shrinkage | 1.0–1.5% |
As an accredited Kingfa PP-R001,PP Flame Retardant V-0 (General),Appliance/E&E factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-R001 flame-retardant V-0 resin, appliance/E&E grade, supplied in 25 kg moisture-proof bags, 40 bags per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized Kingfa PP-R001 flame-retardant V-0 polypropylene for appliance/E&E applications; cargo secured for sea transport. |
| Shipping | Kingfa PP-R001 (PP flame-retardant V-0, general appliance/E&E) is typically shipped as non-hazardous polypropylene pellets in sealed moisture-barrier bags or containers. Keep dry, cool, and protected from sunlight and physical damage. No UN number or transport hazard class applies; follow the SDS, local regulations, and carrier requirements. |
| Storage | Store Kingfa PP-R001 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep bags/containers closed and palletized to prevent moisture, dust, and damage. Avoid prolonged high temperatures and UV exposure. Stack securely, protect from tearing, rotate stock first-in-first-out, and follow local fire/environmental regulations. Do not store near food or drink. |
| Shelf Life | Shelf life is typically 24 months when stored dry, cool, well-ventilated, and away from direct sunlight and moisture. |
Kingfa PP-R001 is specified as a flame-retardant polypropylene injection moulding compound for appliance and E&E components where a UL 94 V-0 classification at 1.6 mm is the baseline flammability requirement. In appliance internal structural parts such as washing machine motor control housings and door interlock brackets, the primary end-product requirement is normally derived from IEC 60335-1 clause 30.2, which invokes glow-wire testing under IEC 60695-2-11; depending on the current carried by live parts and whether the appliance is classified as attended or unattended, the glow-wire temperature applied is commonly 750 °C or 850 °C for a specified time, with no ignition or with flame extinction within 2 s after removal of the wire. The grade must therefore be processed to maintain the flame-retardant package without thermal decomposition. The melt temperature window for flame-retardant PP compounds of this class is narrow, with the upper barrel and nozzle temperature commonly limited to 230 °C, while the lower melt temperature must remain above 190 °C to avoid poor homogenization and visible flow lines. Any excursion above 230 °C can initiate acid generation from the halogenated flame-retardant system, producing brown streaks, black specks, screw/barrel corrosion, and a loss of UL 94 V-0 performance in thin sections. The practical melt-temperature control band between the lower homogenization limit and the upper decomposition limit can be as narrow as ±5 °C around the selected setpoint when shear heating is included.
Pre-drying is normally not required for unfilled PP; however, where storage relative humidity exceeds 60% or where the material is exposed to moisture, drying at 80 °C for 2–4 h in a dehumidifying dryer is recommended to prevent surface silver streaking. The injection moulding machine should use a general-purpose polypropylene screw with a length-to-diameter ratio of 20:1 to 24:1 and a compression ratio of 2.0:1 to 2.5:1; high-compression or high-shear screws are not recommended because shear heating can raise local melt temperature above the decomposition threshold. Rheological data for this class indicates a melt flow rate under ISO 1133-1 at 230 °C/2.16 kg commonly in the range of 5–20 g/10 min; lower-viscosity grades are used for long flow lengths, but the flame-retardant package and UL certification may be thickness-dependent. The total barrel residence time should be held below 5 min, and the shot size should be not less than 30–70% of the injection unit capacity for full plasticating stability. Regrind of sprues and runners may be added up to 20% by weight, provided that the regrind is dry, free of contamination, and limited to material that has not been degraded by previous heat history; exceeding 20% regrind can reduce flame-retardant uniformity and lower the comparative tracking index under IEC 60112. In production-scale moulding of washing machine motor control housings, the common failure modes are cavity-to-cavity fill imbalance in multi-cavity tools, gate blush caused by excessive injection velocity, and burn marks at vent locations due to trapped air and volatile degradation products. Gate land length should be kept as short as the part design allows, and mould vents should be cleaned on a regular preventive maintenance schedule because the decomposition by-products of halogenated flame-retardant packages can deposit on vent surfaces and reduce vent effectiveness.
Lot acceptance should include plaque moulding and UL 94 vertical burn testing on five specimens from each lot, combined with a flexural modulus check under ISO 178 on the same plaques; batch-to-batch variation in flame-retardant dispersion can be detected more readily by gate-zone colour change and local char formation than by melt flow rate alone. For appliance parts requiring a UL 94 V-0 classification at 1.6 mm, the reported rating is thickness-dependent under the UL standard; transition of a tool to a lower nominal wall thickness below 1.6 mm voids the assumption of V-0 performance, and a new first-article evaluation is required. The terminal products in this application include motor control housings, door interlock brackets, and wire-harness retainers for washing machines and tumble dryers.
Electrical junction boxes and low-voltage distribution enclosures represent a separate application track for Kingfa PP-R001 because the component standards differ from appliance end-product standards. Under IEC 60670-1 and relevant part 22 requirements for boxes and enclosures for electrical accessories, materials used for live-part retention and insulation must demonstrate adequate resistance to abnormal heat and fire; the test method is normally IEC 60695-2-11 with a glow-wire temperature of 850 °C for parts retaining live parts, or 750 °C for other enclosures, depending on the installation environment and national wiring rules. The material is also commonly assessed under IEC 60695-2-12 for glow-wire flammability index and IEC 60695-2-13 for glow-wire ignition temperature when the part is above 0.5 A current-carrying components. Moulded wall thickness in this application is typically 2.0–3.0 mm, which assists the formation of an intumescent char layer and supports the UL 94 V-0 rating at 1.6 mm; however, thick sections increase cycle time and sink-mark tendency, so the holding-pressure profile must be adjusted to maintain packing at the gate without inducing overpacking near the sprue. A practical let-down ratio for colour masterbatch is 2–3% by weight using a polypropylene carrier only; PE-carrier masterbatches are to be avoided because they can alter flame-retardant distribution and reduce glow-wire performance. Regrind ratios in electrical box moulding are usually limited to 15% by weight because these parts must pass both flammability and dimensional stability tests; higher regrind content increases lot-to-lot variability in wall thickness and the risk of failing IEC 60670-1 ball-pressure requirements at 125 °C for insulating parts.
In conjunction with the above requirements, the following test matrix is applicable to electrical accessory housings using this grade.
| Standard/Test | Test condition | Acceptance threshold for E&E accessory housings |
|---|---|---|
| UL 94 vertical burn | Thickness 1.6 mm, 50 W flame | Individual afterflame ≤ 10 s; total afterflame ≤ 50 s; afterflame + afterglow ≤ 30 s; no cotton ignition |
| IEC 60695-2-11 glow wire | 750–850 °C, 30 s application | No ignition, or flame extinction within 2 s of glow-wire removal |
| IEC 60112 CTI | 50 drops ammonium chloride solution | Tracking failure shall not occur at the voltage specified by the end-product standard |
| IEC 60695-2-12 GWFI | Glow wire 850 °C on 60 mm × 60 mm specimen | No ignition or self-extinction within 30 s |
Terminal products include flush-mount wall boxes, ceiling rose bases, and low-voltage terminal junction boxes used in residential and commercial fixed wiring.
Replacing a brominated FR-ABS housing material with Kingfa PP-R001 in small kitchen appliances such as electric kettle bases and rice cooker steam housings alters the dimensional management, not only the flame-retardant compliance route. Polypropylene has a lower density than ABS, typically in the order of 0.90–0.95 g/cm³ for unfilled PP and 1.04–1.10 g/cm³ for filled FR-PP, under ISO 1183; FR-ABS is commonly around 1.19 g/cm³. The mass reduction is therefore measurable, but the flexural modulus of unfilled or lightly filled PP is lower than that of FR-ABS, at least 20–30% lower depending on filler content under ISO 178. For parts originally tooled for FR-ABS, this stiffness deficit requires an increase in nominal wall thickness, often in the range of 1.2–1.4 × the original thickness, or the addition of ribbing with a rib-to-wall thickness ratio no greater than 0.6 to avoid sink marks. The mould shrinkage is also different; PP typically exhibits a mould shrinkage of 1.0–2.0% under ISO 294-4, whereas ABS is usually 0.4–0.7%. Existing tools must be evaluated for gate size, corner radii, and ejection draft because PP shrinks more and may grip cores or show more sink at bosses. The processing window is lower than FR-ABS: melt temperature 190–230 °C for the FR-PP grade versus 220–250 °C for FR-ABS, and mould temperature can be lower, typically 20–60 °C for PP rather than 50–80 °C for ABS. This lower melt temperature reduces energy input per shot, but also increases the risk of poor flow in thin sections, so gate diameters should be at least 0.8 mm and flow length should be checked against spiral-flow data at the selected wall thickness.
In end-product testing under IEC 60335-1 clause 30.2, small kitchen appliances are usually attended appliances; the glow-wire test temperature for accessible enclosure surfaces may be 750 °C, while parts supporting live connections may require 850 °C. The grade must not be used where continuous service temperatures exceed the material's UL relative thermal index; for flame-retardant polypropylene compounds, RTI values are commonly in the region of 65–105 °C depending on thickness and property, but the certified UL Yellow Card for Kingfa PP-R001 is the controlling document, and published data for this specific configuration is limited if the card does not list a required property. Compliance with RoHS and REACH must be verified at the lot level because flame-retardant additive systems can vary between supply batches. The terminal products in this application include electric kettle lower bases, rice cooker outer covers, and small food processor internal motor housings. For each of these parts, the ventilation openings should be designed so that the part is not subjected to direct contact with exposed heating elements; PP cannot substitute for high-temperature polyamide or PBT in direct metal-contact applications above its continuous service temperature.
Power distribution strips and socket-outlet housings require a different balance of impact toughness, tracking resistance, and fire performance. Kingfa PP-R001 is used in multi-outlet power strips and plug bodies where the component standard is IEC 60884-1 or the relevant national derivative for plugs and socket-outlets, combined with UL 1363 for relocatable power taps in North America. The material must pass glow-wire testing at 750–850 °C under IEC 60695-2-11, and the comparative tracking index under IEC 60112 should be checked because the presence of antimony oxide and brominated flame-retardant additives can lower CTI relative to unfilled PP. Processing these parts involves high-cavitation tools, often 8–32 cavities, with hot-runner systems. Cavity-to-cavity fill imbalance should be maintained within ±5% of shot weight to avoid selective over-degradation in restricted drops; hot-runner manifold and nozzle temperatures are typically limited to 210–230 °C because the residence time of molten material in the hot runner can exceed the barrel residence time. Injection velocity is set moderate to avoid shear heating at the gate and to prevent jetting in the tall thin walls of socket housing; venting at the last cavity is critical because decomposition gases from the flame-retardant system accumulate at the end-of-fill. Regrind ratio is kept at 20% maximum and should be produced from designated controlled waste streams to avoid contamination with non-FR PP or other polymers, which would compromise the UL 94 V-0 rating and the electrical safety certification.
For these higher-volume applications, moulders should monitor nozzle drool and hot-runner pressure drop, because small increases in melt viscosity after lot changes can shift the cavity filling pattern and produce charred gate vestiges. Part weight is a more sensitive process monitor than dimensional inspection alone; a shift of more than 1.5% in part weight under stable packing pressure can indicate gate freeze variation, non-return valve leakage, or poor mixing. Terminal products include relocatable power strips, plug shells, socket-outlet base plates, and multi-socket adaptors.
Continuous production of thin-walled E&E enclosures from Kingfa PP-R001 imposes specific equipment requirements. The screw should be a general-purpose polyolefin screw with an L/D ratio of 20:1 to 24:1 and a compression ratio between 2.0:1 and 2.5:1; high-compression screws with ratios above 3.0:1 generate excessive shear work that can push the melt temperature locally above 230 °C. The screw and barrel should be made from nitrided steel or bimetallic materials resistant to corrosion, because the halogenated flame-retardant package can release acidic degradation products if the material is overheated or held at melt temperature too long. Hard chrome plating alone is not sufficient for long production runs; a nitrided barrel with a clearance of 0.03–0.05 mm between screw flight and barrel wall is a practical starting specification, but the screw supplier should be consulted. Check for wear on the non-return valve because flame-retardant PP compounds can be abrasive at higher filler loadings; shot weight inconsistency and part density variation are early indicators of non-return valve leakage. The barrel temperature profile is usually set as a reverse or flat profile to limit heat input, for example feed zone 180 °C, compression zone 200 °C, metering zone 210–220 °C, and nozzle 210–220 °C. This profile keeps the melt temperature below the decomposition threshold while maintaining sufficient fluidity for injection moulding of parts with nominal wall thickness from 1.6 mm to 3.0 mm.
The terminal application in this process window is high-volume E&E housing production, such as adaptor shells, terminal box covers, and control panel housings. For these products, the nozzle should be fitted with a temperature-controlled heater band and a shut-off nozzle when hot-runner systems are used, because the low melt viscosity at the upper processing temperatures can cause drool at the nozzle. Mould cooling should be sufficient to hold the cavity surface temperature below 60 °C; higher mould temperatures extend cycle time and increase post-mould shrinkage, while lower mould temperatures can produce high internal stress. Cycle times for 2.0 mm wall thickness are generally in the range of 25–45 s depending on part geometry and cooling circuit design, but published data for this specific grade regarding cycle-time optimization is limited and should be validated on the target tool with a production-scale trial. Clamp force must be calculated from the projected area and the expected cavity pressure; for PP compounds, cavity pressures commonly range from 30–60 MPa, so a part with 200 cm² projected area may require clamp force in the region of 60–120 tonnes depending on gate design and fill speed.
Tumble dryer internal air-duct brackets and blower housing covers are a specific appliance application where the flame-retardant rating must survive hot, humid, and lint-contaminated service conditions. Kingfa PP-R001 processed at a wall thickness of 1.6 mm is relevant where the end-product standard for tumble dryers requires a UL 94 V-0 classification under IEC 60695-11-10 or UL 94 vertical burn testing, and where the part is not located in direct contact with the heating element. The material must be dried before moulding if the relative humidity during storage exceeds 60%; a dehumidifying dryer set to 80 °C with 2–4 h residence is the standard preparation. The processing parameters are selected to avoid local overheating in the hot-runner drops and to maintain a uniform melt cushion, normally 2–5 mm, at the screw tip. For these structural parts, rib-to-wall thickness ratio should be held at 0.5:1 to 0.6:1, and bosses should be cored to 60% of the nominal wall thickness to minimize sink marks while retaining screw-boss strength. Regrind addition is limited to 20% by weight; regrind must be separated from other PP compounds because mixing with non-flame-retardant PP will destroy the V-0 classification.
A further constraint in this application is the accumulation of lint and household dust on internal surfaces. Because the part is not a sealed enclosure, surface contamination can act as a secondary fuel source in the event of an electrical fault; therefore the design should avoid deep ribs, blind pockets, and horizontal ledges facing upward, where lint can accumulate and compromise the end-product glow-wire result under IEC 60695-2-11. Weld-line locations should be moved away from screw bosses and snap-fit retention points; at 1.6 mm wall thickness, the material's impact resistance at the weld line under ISO 179-1 is lower than in the bulk section, and a poorly placed weld line can produce brittle snap-fit failure during assembly or servicing. Terminal parts include dryer duct brackets, blower housing covers, and moisture-sensor mounting frames, all of which are subject to long-term exposure to warm air and lint but not to direct flame or heating-element contact.
Competitive Kingfa PP-R001,PP Flame Retardant V-0 (General),Appliance/E&E prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-R001 is a flame-retardant polypropylene compound designated as V-0 general purpose for appliance and electrical/electronic enclosures, switchgear covers, relay boxes, terminal shrouds, and non-structural power-supply housings. The designation does not identify the flame-retardant chemistry; regional variants may use halogenated or halogen-free additive systems, and the converter should confirm the exact package against the safety data sheet when halogen-content or corrosive smoke restrictions apply. Representative property ranges for PP-R001 are generated on injection-moulded specimens conditioned at 23 °C and 50 % relative humidity for 48 h in accordance with ISO 291. Single-point datasheet values are lot-specific and should not be interpreted as design allowables.
Compared with unfilled polypropylene homopolymer, PP-R001 contains a higher loading of char-forming or gas-phase flame-retardant additives. This increases melt viscosity and solid density while reducing tensile elongation, weld-line strength, and flow length. The grade is therefore specified only where flammability certification is mandatory. In appliance applications governed by IEC 60335-1, glow-wire ignition and flame-spread requirements frequently exclude unfilled PP; PP-R001 can satisfy the required bench-scale vertical burn and glow-wire screening tests when moulded at the thickness range stated in the manufacturer’s technical datasheet.
Under UL 94 vertical burning, a V-0 classification requires afterflame time no greater than 10 s per specimen, total afterflame time no greater than 50 s for five specimens, and no flaming or glowing particles that ignite the cotton indicator. The material is reported as V-0 at 1.5 mm and 2.0 mm nominal thickness. For appliance housings, glow-wire testing is often more restrictive than UL 94; IEC 60695-2-12 GWFI is commonly reported at 850 °C at 1.5 mm, but IEC 60695-2-12/13 GWIT values must be verified on the final moulded part because wall thinning, rib junctions, and printed-circuit-board spacing alter heat transfer and flame propagation. The comparative tracking index under IEC 60112 is frequently above 600 V on clean, dry plaques, but this value cannot be extrapolated to dust-contaminated, humid, or aged service without end-product evaluation.
At combustion temperatures, intumescent systems form a multicellular carbonaceous char that insulates the underlying polymer and reduces fuel release; brominated systems operate through gas-phase radical quenching in combination with antimony synergists. The char-forming route is sensitive to moulded-in stress and high filler loading, while the brominated route can produce higher smoke density and corrosive gas generation. The exact mechanism for PP-R001 should be confirmed from the supplier datasheet because halogen-free and halogenated variants do not have identical re-qualification behaviour under custom colour concentrates or regrind addition.
| Property | Test standard | Representative datasheet range or condition |
|---|---|---|
| Density | ISO 1183-1:2019 | 0.95–1.00 g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022, 230 °C/2.16 kg | 15–25 g/10 min |
| Tensile stress at yield | ISO 527-2:2012, type 1A, 50 mm/min | 20–28 MPa |
| Tensile strain at break | ISO 527-2:2012, type 1A | 15–30 % |
| Flexural modulus | ISO 178:2019 | 1500–2200 MPa |
| Charpy notched impact strength, 23 °C | ISO 179-1:2010/1eA | 3.0–6.0 kJ/m² |
| Heat deflection temperature, 1.80 MPa | ISO 75-2:2013/A | 95–120 °C |
| Vertical burning classification | UL 94 | V-0 at 1.5 mm, 2.0 mm |
Published data for this specific configuration is limited for long-term creep, fatigue, and dielectric strength. Load-bearing parts or parts subjected to thermal cycling require generation of design allowables under ISO 899-1:2017 and ISO 6602-2:2012, especially where bosses, snap-fits, or press-fit inserts are present.
Production-scale injection moulding of PP-R001 is performed on hydraulic or servo-driven machines with clamp force from 80 tonnes to 500 tonnes. Barrel zone settings are maintained from 190 °C at the feed throat to 230 °C at the nozzle; melt temperature measured by an immersion probe should remain between 210 °C and 230 °C. Mould temperature is controlled at 20 °C to 60 °C. Higher mould temperature improves weld-line strength and surface gloss but increases cycle time and worsens sink-marks in thick sections. Drying is not required when pellets are stored in sealed containers below 60 % relative humidity; when storage exceeds 60 % relative humidity, pre-drying at 80 °C for 2 h to 4 h in a desiccant or hot-air dryer is recommended to prevent surface splay and hydrolytic damage to the flame-retardant additive system.
Screw selection should favour a general-purpose polyolefin metering profile with a compression ratio of 2.5:1 to 3.0:1 and an L/D ratio of 20:1 to 25:1. High-shear barrier screws can generate local melt temperatures above 240 °C, causing flame-retardant decomposition, black specks, and mould deposit. Holding pressure is typically 40 % to 60 % of injection pressure, and back pressure is limited to 0.3 MPa to 0.7 MPa to prevent additive over-dispersion and streaking. Screw speed for a 40 mm screw is normally 30 rpm to 80 rpm. Vent depth greater than 0.02 mm to 0.03 mm can produce flash and serve as a deposition edge for flame-retardant volatiles. Total residence time in the barrel should not exceed 5 min at melt temperatures above 220 °C; prolonged residence shifts melt flow rate and may reduce the V-0 rating.
Unmodified PP homopolymer typically cannot achieve V-0 under UL 94 and fails glow-wire ignition requirements for unattended appliance housings carrying current above 0.2 A. PP-R001 raises the limiting oxygen index and promotes char formation, but the additive package reduces tensile strain at break to 15 %–30 %, making snap-fit geometry sensitive to corner radii and gate-induced orientation. Glass-fibre-reinforced flame-retardant PP containing 20 wt% to 30 wt% glass exhibits a flexural modulus of 3500 MPa to 5500 MPa, more than double the 1500 MPa to 2200 MPa range of PP-R001, but it also produces higher notch sensitivity and stronger anisotropic shrinkage. PP-R001 is therefore used in thin-wall enclosures where warpage control and moderate impact toughness are more important than structural stiffness; glass-filled grades are preferred for brackets and frames exposed to elevated temperature or sustained mechanical load.
Compared with halogenated bromine-antimony PP systems, a halogen-free PP-R001 variant may show reduced smoke density and lower corrosive gas emission in fire conditions, but it usually requires higher flame-retardant loading. That raises density and reduces flow length in thin-wall moulds; it also increases sensitivity to mould deposit at sustained melt temperatures above 240 °C. Comparative smoke-density assessment must be performed on the final assembly using ISO 5659-2 if low-smoke performance is a specification requirement. Published data for this specific configuration is limited; therefore, substitution from one flame-retardant chemistry to another should trigger re-qualification at the minimum and maximum wall thickness of the part.
Wall thickness below 1.2 mm can erode the UL 94 V-0 margin because thinner sections dissipate heat rapidly and may reach afterflame-time limits during vertical burn testing. Rib-to-wall ratio should not exceed 0.6:1 to limit sink marks and internal voids, and flow length should be calculated from spiral-flow data generated with the intended gate configuration. Typical post-mould shrinkage is 1.0 % to 1.5 % in the flow direction and 0.8 % to 1.2 % transverse after 24 h at 23 °C; these values are directional and should be validated with cavity-pressure transducers rather than inferred from unfilled PP homopolymer.
Electrical clearance and creepage distances specified in IEC 60335-1 and IEC 60664-1 are not reduced solely by a high CTI value above 600 V. Pollution degree classification, board spacing, and through-hole apertures control the final creepage design. Continuous contact with strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents can extract flame-retardant additives at the surface and reduce V-0 performance. Unstabilised polypropylene flame-retardant systems are not inherently UV-stable; black pigmentation or an additional UV stabiliser package should be specified where outdoor exposure or strong artificial lighting is anticipated.
Compliance documentation for PP-R001 typically includes a supplier declaration for RoHS Directive 2011/65/EU Annex II and REACH Regulation EC 1907/2006 Article 33. The compound alone does not confer IEC 60335-1 conformity; the final part must be tested for glow-wire flammability, ball-pressure temperature, and tracking resistance at the actual wall thickness and colour. Lot traceability is maintained through compounding batch records. Converters should record batch number, drying conditions, melt temperature, and residence time for each production run because flame-retardant thermal history affects regrind quality. Regrind addition is generally limited to 10 wt% to 20 wt% with no more than two heat histories; higher regrind ratios may shift MFR and reduce the V-0 classification. Published data for this specific configuration is limited for long-term exposure to hot, humid, current-carrying environments; end-product thermal cycling to IEC 60068-2-14 or IEC 60335-1 Clause 11 should be evaluated by the original equipment manufacturer.