Kingfa KF-T30S,Homopolymer PP (Fiber Grade)

    • Product Name: Kingfa KF-T30S,Homopolymer PP (Fiber Grade)
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 653216
    Product Name Kingfa KF-T30S
    Polymer Type Homopolymer Polypropylene
    Grade Fiber Grade
    Density 0.91 g/cm³
    Melt Flow Rate 3.0 g/10 min (230°C/2.16 kg)
    Tensile Strength At Yield 32 MPa
    Tensile Elongation At Break 30%
    Flexural Modulus 1400 MPa
    Notched Izod Impact Strength 3.0 kJ/m² (23°C)
    Heat Deflection Temperature 100°C (0.45 MPa)
    Vicat Softening Temperature 150°C
    Melting Temperature 165°C
    Mold Shrinkage 1.5-2.0%
    Processing Temperature 200-240°C

    As an accredited Kingfa KF-T30S,Homopolymer PP (Fiber Grade) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa KF-T30S Homopolymer PP Fiber Grade is supplied in 25 kg moisture-proof woven bags, 40 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with Kingfa KF-T30S homopolymer PP fiber grade in 25 kg bags, palletized, shrink-wrapped, dry container.
    Shipping Kingfa KF-T30S Homopolymer PP (Fiber Grade) ships as a non-hazardous, non-regulated polymer in moisture-proof 25 kg woven bags on pallets. Store and transport in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and contamination. Keep bags sealed and undamaged.
    Storage Store Kingfa KF-T30S in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizing agents. Keep bags sealed, palletized, and off the floor to prevent moisture pickup and contamination. Avoid prolonged high temperatures and physical damage. Use first-in, first-out stock rotation; maintain good housekeeping and prevent dust accumulation. Do not store near foodstuffs or incompatible materials.
    Shelf Life Typical shelf life is 12 months from production date when stored dry, cool, ventilated, and protected from sunlight in unopened packaging.
    Application of Kingfa KF-T30S,Homopolymer PP (Fiber Grade)

    Why Does Melt Residence Time Shift Spunbond Filament Denier Uniformity?

    In spunbond nonwoven manufacture, Kingfa KF-T30S homopolymer polypropylene fibre grade is extruded on high-output lines equipped with single-screw extruders having L/D 30:1 to 36:1 and positive-displacement melt pumps mounted between screw tip and spinneret. The resin carries a nominal melt mass-flow rate of 3.0 g/10 min measured at 230 °C with a 2.16 kg piston load under ISO 1133-1:2022. Barrel zones are profiled from 180 °C at the feed throat to 230 °C in the metering section, while the die body is held at 250 °C to 260 °C. Residence time above 250 °C is maintained below 12 minutes; longer hold-up initiates thermo-oxidative chain scission that raises the carbonyl index and deposits oligomer on the spinneret face. Quench air at 15 °C to 22 °C with velocity 0.4 m/s to 0.8 m/s is drawn through the filament bundle. Air velocity below 0.4 m/s widens denier distribution, while air velocity above 0.8 m/s increases mid-air filament breakage. Calender bonding is run between patterned and smooth rolls at 145 °C to 160 °C with nip pressure 50 N/mm to 80 N/mm. For hygiene coverstock, fabric mass per unit area is 15 g/m² to 70 g/m²; for surgical gown outer layers, 25 g/m² to 50 g/m² is common. The finished fabric is tested under ISO 9073-1:1989 for mass, ISO 9073-2:1995 for thickness, and ISO 9073-3:1989 for tensile strength and elongation. Medical-grade spunbond is assessed under ISO 10993-5:2009 for cytotoxicity and EN 13795-1:2019 for surgical drapes and gowns. The unmodified resin complies with REACH Annex XVII restrictions and contains no restricted phthalates or heavy metals above RoHS limits. When ambient storage relative humidity exceeds 60%, surface moisture is removed by pre-drying at 80 °C for 2 h to 4 h before extrusion.

    Test standardParameterBoundary or accepted range
    ISO 1133-1:2022Melt mass-flow rate3.0 g/10 min at 230 °C/2.16 kg
    ISO 9073-1:1989Nonwoven mass per unit area15 g/m² to 70 g/m²
    ISO 9073-3:1989Nonwoven tensile strength and elongationMD/CD ratio 1.2:1 to 2.0:1
    ISO 10993-5:2009CytotoxicityNo lysis above Grade 1
    EN 13795-1:2019Surgical gown/drape performanceClass I/II according to barrier level

    On a heavy-duty rope yarn line, KF-T30S is processed at a melt temperature of 245 °C to 265 °C through a 75 mm single-screw extruder and a 120-hole spinneret. The quench air temperature is maintained at 18 °C to 25 °C with air speed below 0.5 m/s to avoid surface skin formation before drawing. Filament draw ratio is set at 1:7 to 1:9 over heated godets at 120 °C to 140 °C, producing a final linear density of 110 dtex to 220 dtex per filament bundle. The resulting high-tenacity multifilament yarn is twisted at 80 twists/m to 120 twists/m and then braided or laid into three-strand or eight-strand ropes. Breaking force is measured under ISO 2307:2019, and the polypropylene rope product is specified under ISO 1346:2012 for split film, monofilament, and multifilament constructions. A minimum tenacity of 0.60 N/tex after conditioning at 23 °C and 50% RH is required for marine mooring and general industrial cordage. KF-T30S homopolymer PP is also used in baler twine and agricultural rope because the resin's low gel count reduces filter pack pressure rise and spinneret hole blockage. For outdoor service, a UV stabilizer masterbatch is introduced at 2 wt% to 5 wt%; without this addition, tensile strength retention drops below 50% after 12 months of direct weathering in subtropical latitudes. Alkaline wash tanks and saturated seawater immersion do not hydrolyze the polymer, but continuous load above 20% of break strength at temperatures above 60 °C produces creep rupture in polypropylene fibre. Published data for long-term cyclic loading of this specific grade in braided rope is limited.

    Staple Fibre Crimp Retention in Dynamic Puncture Geotextile Lines

    Needlefelt geotextile production from KF-T30S starts with melt spinning of staple tow followed by drawing, crimping, and cutting to 40 mm to 90 mm fibre length. Fibre linear density is controlled at 3.3 dtex to 6.7 dtex. The crimp frequency after steam annealing is 10 to 14 crimps per 25 mm, and crimp retention after carding must stay above 60% to maintain web bulk. Carding machines with worker-stripper roll settings of 0.25 mm to 0.40 mm convert the staple into a batt of 100 g/m² to 800 g/m². Needlepunch lines operate with barbed needles at 100 to 200 punches/cm² and penetration depth 10 mm to 14 mm, depending on target geotextile mass per unit area. Dynamic puncture resistance is measured under ISO 13433:2006, tensile properties under ISO 10319:2015, and static puncture under ISO 12236:2006. Reported CBR puncture resistance values for 400 g/m² to 500 g/m² needlepunched PP are typically 1.5 kN to 4.0 kN; higher pile density improves this only until fibre breakage limits further densification. For permanent drainage layers below pH 9, the polymer is chemically inert and resists soil-borne acids and alkali. A limitation is that continuous exposure to strong oxidizing agents, such as 5% sodium hypochlorite, embrittles the fibre. Needlefelt geotextiles made from KF-T30S are supplied as separation and filtration layers in road and railway subgrades under national highway authority specifications; lot-to-lot MFR variation should be held within ±0.3 g/10 min to avoid batch-to-batch tensile strength changes.

    Woven sack tape extrusion consumes the grade through a water-quench process that is common to FIBC and cement bag lines. Melt is pumped from a 90 mm extruder at 210 °C to 250 °C through a flat die into a water bath held at 30 °C to 40 °C. The quenched film is slit into tapes and drawn in a hot air oven at 120 °C to 150 °C using a draw ratio of 1:6 to 1:8. The drawn tape exhibits a linear density of 80 tex to 120 tex and a tenacity of 0.55 N/tex to 0.70 N/tex. Circular loom weaving is performed at 400 rpm to 600 rpm with polypropylene tapes as warp and weft, producing fabric of 60 g/m² to 200 g/m². For food contact bags, KF-T30S meets FDA 21 CFR 177.1520 olefin polymers conditions of use C to G, provided that the converting line does not add unapproved slip agents or printing solvents. Fabric tensile strength is measured by ISO 13934-1:2013, and FIBC containment performance is verified under ISO 21898:2004. Processing conflict arises when draw ratio exceeds 1:8: tape fibrillation increases, lowering loom efficiency and reducing seam strength. Surface moisture on recycled trim above 0.1% by weight also causes tape splitting at high draw ratios, so regrind is pre-dried before blending with virgin KF-T30S at levels above 30 wt%.

    When Polypropylene Fibre Replaces Steel at Dosages Below 0.3% by Volume

    Fibrillated staple fibre produced from KF-T30S is added to ready-mix concrete at 0.1 vol% to 0.3 vol%, equivalent to 0.9 kg/m³ to 2.7 kg/m³, for plastic shrinkage crack control. The fibre length is 19 mm to 38 mm and the aspect ratio is controlled below 50 to prevent balling in high-range water-reducing admixtures. Mixing is conducted in a pan mixer at 20 rpm to 30 rpm for 2 minutes to 4 minutes after coarse aggregate addition; fibre clumps at the mixer wall indicate that discharged air temperature is below 5 °C or that aggregate moisture exceeds 7%. The product is classified under ASTM C1116/C1116M-10a Type III fibre and EN 14889-2:2006 Class I microfibre for concrete. Plastic shrinkage cracking resistance is evaluated under ASTM C1579-21, while compressive strength is tested under ISO 1920-4:2020. Slump is reduced by 10 mm to 30 mm at a dosage of 1.8 kg/m³, but compressive strength is not increased. The fibre is not a structural substitute for steel reinforcement; modulus of PP fibre is 1.5 GPa to 3.5 GPa versus 200 GPa for steel, and post-crack residual flexural strength is below the EN 14889-2 Class III threshold. Use in tunnels and pavements is limited to secondary crack control, fire spalling protection, and abrasion resistance improvement; published data for KF-T30S specifically in hydrocarbon fire scenarios is limited.

    In tubular netting and agricultural support textiles, low-flow homopolymer polypropylene is extruded through annular spinnerets at 230 °C to 250 °C and drawn at 1:5 to 1:7 to produce continuous filaments of 100 dtex to 300 dtex. The filament bundles are knitted or woven into netting with mesh openings of 5 mm to 25 mm for crop support, bird exclusion, and packaging of fresh produce. The resin's melt mass-flow rate of 3.0 g/10 min under ISO 1133-1:2022 reduces necking during the air gap; however, the absence of a comonomer means thermal sealing windows are narrower than those of random copolymer PP. Film lamination onto the netting is performed at 150 °C to 170 °C. Final netting tensile strength is measured by ISO 13934-1:2013 for woven fabric and ISO 1806:2002 for knotted netting. UV-stabilized versions are required for multi-season outdoor use; unstabilized KF-T30S is not specified where ISO 4892-3:2016 test duration exceeds 2,500 h because tensile strength retention falls below 50% of initial value.

    Free Quote

    Competitive Kingfa KF-T30S,Homopolymer PP (Fiber Grade) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa KF-T30S is classified as a homopolymer polypropylene resin developed for fiber-grade conversion. The grade is specifically positioned for high-shear fiber extrusion, including spunbond nonwoven production, staple fiber, and continuous filament operations. Incoming resin is supplied as pelletized material with a melt mass-flow rate of 30 g/10 min at 230 °C under 2.16 kg load when tested to ISO 1133-1:2022. The primary differentiation from general-purpose homopolymers is a controlled molecular weight distribution and low oligomer content, both of which influence spinline stability and spinneret cleanliness during extended production campaigns.

    Typical property envelope for Kingfa KF-T30S
    PropertyTypical valueTest method
    Melt mass-flow rate, 230 °C/2.16 kg30 g/10 minISO 1133-1:2022
    Density0.905 g/cm³ISO 1183-1:2019
    Tensile stress at yield33 MPaISO 527-2:2012
    Tensile elongation at yield8 %ISO 527-2:2012
    Flexural modulus1450 MPaISO 178:2019
    Notched Izod impact, 23 °C2.5 kJ/m²ISO 180/A
    Vicat softening temperature, A50154 °CISO 306:2022
    Heat deflection temperature, 0.45 MPa92 °CISO 75-2
    Xylene soluble fraction3.0 wt%ISO 16152:2005

    Because KF-T30S is a fiber grade, the melt flow rate is deliberately higher than raffia or injection-molding homopolymers with MFR values of 2–4 g/10 min. The higher flow reduces melt pressure in multi-hole spinnerets and permits higher hole density. However, the same flow level places the resin outside the typical meltblown window of 800–1500 g/10 min. It does not generate the low-viscosity melt structure required for submicron fiber formation without additional peroxide vis-breaking.

    Compared with random copolymer polypropylene of similar MFR, KF-T30S does not contain ethylene comonomer. This absence increases crystallinity and thermal resistance but removes the low-temperature seal initiation typical of random copolymers. Heat-seal response for homopolymer fibers generally develops above 150 °C, whereas random copolymers seal between 110 °C and 125 °C depending on comonomer content. Against impact-modified heterophasic grades, KF-T30S exhibits lower notched Izod impact strength at 23 °C; the typical value of 2.5 kJ/m² is below the 8–15 kJ/m² range observed for medium-impact copolymers. The resin is therefore not specified for low-temperature ductile applications.

    Rheological comparisons with similar 30 g/10 min homopolymers indicate an apparent capillary shear viscosity on the order of 45 Pa·s at 230 °C and 1000 s⁻¹. Published data for this exact configuration should be verified on the converter’s capillary rheometer before spin pack design changes are implemented. The shear-thinning response is typical of linear polypropylene, with a power-law index in the approximate range of 0.3–0.4 over shear rates from 10² to 10⁴ s⁻¹.

    What Limits Stable Operation in Spunbond Nonwoven Lines?

    On production-scale spunbond lines using single-screw extruders with screw diameters from 90 mm to 150 mm and L/D ratios of 30:1 to 34:1, KF-T30S typically operates within a melt temperature window of 220 °C to 260 °C. Barrel set points are commonly programmed from 190 °C near the feed throat to 245 °C in the metering zone, with the melt pump and spin beam held at 230–250 °C. A barrier-flighted screw with a mixing tip is preferred for this resin; compression ratios of 3.0:1 to 3.5:1 provide sufficient melting while avoiding excessive shear heating. The extruder is typically coupled to a melt pump with inlet pressure maintained between 60 bar and 120 bar and outlet pressure between 100 bar and 180 bar. Melt temperature above 270 °C for more than 30 min causes thermo-oxidative chain scission, increasing MFR and reducing melt strength. Temperatures below 215 °C produce unmolten crystalline domains and draw resonance.

    Quench air control is the most critical spinline variable. The recommended quench air temperature is 12–18 °C, with air velocity from 0.4 m/s to 1.0 m/s. Higher velocities over-quench the filament skin and increase brittleness, while lower velocities leave the core under-solidified. Draw ratios between 30:1 and 80:1 are typical for KF-T30S in spunbond operations. For a 12 g/m² web, line speeds of 200–350 m/min are commonly achievable before spinline resonance becomes limiting. The upper speed is determined by molecular orientation and web uniformity rather than extruder output. Spinneret hole diameters of 0.3–0.6 mm with capillary L/D of 2:1 to 4:1 are used.

    Resulting spunbond web tensile properties depend on bond pattern and basis weight. At 20 g/m², machine-direction tensile strength values in the range of 25–45 N/5 cm are typical for calendered materials when tested to ISO 9073-3. The high crystallinity of homopolymer polypropylene contributes web stiffness, while the narrow molecular weight distribution reduces gel-like high-molecular-weight fractions that can block spinneret holes during 24 h production campaigns.

    When KF-T30S Replaces a 25 MFR Homopolymer in Continuous Filament Spinning

    Substitution of a 25 g/10 min homopolymer with KF-T30S can lower melt pressure at the spin pack by 10–20%, depending on throughput and spinneret hole density. Barrel set points should be reduced by 5–10 °C to prevent low-viscosity melt from sagging at the spinneret. Screw speed is trimmed to keep melt pump inlet pressure in the 60–120 bar range; high inlet pressure reduces melting efficiency and may increase pellet slippage in the feed section. The screen pack configuration of 60/120/250 mesh or equivalent is retained, but pack life may extend due to the lower content of high-molecular-weight gels. For continuous filament and partially oriented yarn, the lower melt stiffness of the 30 MFR grade may require a draw ratio reduction of 5–10% relative to a 25 MFR grade at constant line speed to avoid breaks.

    Fiber property measurements on drawn specimens generally follow ISO 5079 and ISO 2062. For a draw ratio of 4:1, achievable tenacity is typically in the range of 3.5–4.5 cN/dtex with elongation at break between 25% and 40%. Published data for this specific configuration is limited because final fiber properties are strongly dependent on draw ratio, quench air, and spin finish. No single tenacity value can be assigned independently of line configuration.

    Thermo-oxidative Stabilization and Additive Interference

    The base stabilization system in KF-T30S typically combines a hindered phenolic primary antioxidant and a phosphite secondary antioxidant, with a calcium stearate acid scavenger maintained below 0.05 wt%. This package protects the polymer during melt processing but does not eliminate the need for inert gas blanketing in long residence-time melt lines. Nitrogen-containing additives in masterbatches should be avoided where gas-fading resistance is required, because amine-based chemistries can interact with phenolic antioxidants and cause post-processing color shift. Surface moisture from silo storage in relative humidity above 60% should be removed by pre-drying at 80 °C for 2 h. Although polypropylene does not undergo hydrolysis, condensed water can induce feed fluctuation and spinneret steam erosion.

    Long-term thermal aging of fibers made from KF-T30S depends on antioxidant retention and environmental exposure. In oven aging at 120 °C, unstabilized or under-stabilized polypropylene degrades rapidly, but the stabilized grade is intended to retain useful mechanical properties for a period determined by fiber denier, draw ratio, and package ventilation. Converter-conducted testing to ISO 188 or ISO 4577 is required for specific end-use lifetime claims.

    For food-contact and article compliance, the applicable framework is FDA 21 CFR 177.1520 for olefin polymers. Finished articles intended for food contact in the European Union are evaluated under EU Regulation (EU) No 10/2011, with an overall migration limit of 10 mg/dm² assigned according to food simulant and contact conditions. REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU apply at article level; typical additive systems do not contain SVHCs above 0.1 wt% and are below RoHS thresholds for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE.

    Regulatory and compliance references
    Standard or regulationScope
    FDA 21 CFR 177.1520Olefin polymers for food-contact articles
    EU Regulation (EU) No 10/2011Plastic materials and articles intended to contact food
    REACH Regulation (EC) No 1907/2006Registration, evaluation, authorisation, and restriction of chemicals
    RoHS Directive 2011/65/EURestriction of hazardous substances in electrical and electronic equipment
    ISO 9001:2015Quality management system for manufacturing consistency

    Incoming lot testing for fiber operations should record melt flow rate, ash content, and pellet color because batch-to-batch variation in catalyst residues and stabilizer levels can shift spinline behavior. A received MFR below 27 g/10 min may require an increase of 5 °C in spin beam temperature or a proportional reduction in draw ratio to maintain line speed. An MFR above 33 g/10 min may produce dripping at the spinneret and is managed by lowering melt temperature and increasing quench air velocity. These thresholds are operational control limits rather than specification limits and should be validated against the converter’s spin pack geometry.