    Specifications
    HS Code 136206
    Density 0.900 g/cm3
    Melt Flow Rate 3.0 g/10 min (230°C/2.16 kg)
    Tensile Strength At Yield 30 MPa
    Elongation At Break 30%
    Flexural Modulus 1400 MPa
    Notched Izod Impact Strength 4 kJ/m2
    Heat Deflection Temperature 100°C
    Vicat Softening Temperature 150°C
    Molding Shrinkage 1.5%
    Rockwell Hardness 100 R
    Processing Method Injection Molding
    Form Pellets

    As an accredited Kingfa PP-300,PP Homopolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa PP-300 PP Homopolymer is supplied in 25 kg moisture-resistant woven bags, palletized for industrial handling and storage.
    Container Loading (20′ FCL) Kingfa PP-300 PP Homopolymer is loaded into a 20-foot FCL container, palletized, evenly distributed, and secured for safe ocean transport.
    Shipping Kingfa PP-300 PP Homopolymer is supplied as solid resin pellets in 25 kg moisture-barrier bags, jumbo bags, or bulk containers. It is non-hazardous for transport and should be kept dry, ventilated, away from direct sunlight, heat, and ignition sources, following local shipping regulations.
    Storage Store Kingfa PP-300 PP Homopolymer in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers closed and protect from moisture, dust, and contamination. Use appropriate secondary containment and follow SDS and local regulations. Avoid prolonged storage near strong oxidizers. Maintain good housekeeping and label containers clearly. Store only in original or compatible containers.
    Shelf Life Typically 24 months in original unopened packaging, stored cool, dry, ventilated, away from direct sunlight and moisture.
    Application of Kingfa PP-300,PP Homopolymer

    At wall thicknesses below 0.45 mm, Kingfa PP-300 is converted for dairy cups, delicatessen containers, and single-use food trays where PP homopolymer crystallinity provides the required top-load strength without the lower modulus associated with random copolymers. The grade is processed on high-speed injection moulding machines with screw L/D ratios of 20:1 to 25:1, and the recommended melt temperature is 230 °C ± 5 °C, with mould temperature held at 25 °C ± 3 °C. These starting values require adjustment against the batch MFR determined in accordance with ISO 1133-1:2022, because a shift of 1 g/10 min above target can generate gate blush and gloss variation in the moulded sidewall. Injection speed is set to fill the cavity within 0.20 s to 0.35 s, and holding pressure is maintained between 30 MPa and 45 MPa to minimise sink marks around the rim sealing edge. The food-contact formulation is compounded at 100 parts PP-H with 1.5 wt% to 4.0 wt% titanium dioxide masterbatch, the upper limit governed by opacity targets, because exceedance reduces melt strength and leads to silver streaking along the flow front. Compliance is verified under FDA 21 CFR 177.1520(c) for olefin polymers and Regulation (EU) No 10/2011 Annex I with overall migration not exceeding 10 mg/dm² under OM2 conditions. For the Chinese market, GB 4806.7-2016 total migration and potassium permanganate consumption tests are applied to the finished container after post-moulding crystallisation equilibrium. Terminal products include 200 mL to 500 mL stackable dairy tubs with wall thickness 0.30 mm to 0.45 mm and lid-seating diameters held to a tolerance of ±0.08 mm.

    ApplicationStandard or RegulationVerification Point
    Food-contact resinFDA 21 CFR 177.1520(c)Olefin polymer extractables; end-use conditions
    Food-contact moulded articleEU Regulation (EU) No 10/2011 Annex IOverall migration ≤ 10 mg/dm²; OM2 test
    Food-contact moulded articleGB 4806.7-2016Total migration; potassium permanganate consumption
    Pharmaceutical/medical polymerUSP 661Physicochemical tests; buffering capacity
    CytotoxicityISO 10993-5:2009L929 cell viability

    What limits PP-H service life in underhood air handling components?

    Kingfa PP-300 can be specified as the base resin for injection-moulded HVAC blower housings, air cleaner support brackets, and fan shroud frames only where the continuous air temperature does not exceed 105 °C and the part is not subjected to cold-start impact below -10 °C. Because unfilled PP homopolymer has lower impact resistance than impact-modified PP copolymer at low temperatures, underhood components are compounded with talc masterbatch at 20 wt% to 30 wt% addition, and the blend is pelletised on a twin-screw extruder with L/D 40:1 before final injection moulding. The compounding temperature profile is 200 °C to 230 °C from feed throat to die plate, and the melt temperature at the die is limited to 230 °C to avoid thermal degradation of the stabiliser package. The filled compound is then injection moulded at melt temperature 220 °C to 240 °C and mould temperature 15 °C to 30 °C, with injection pressure from 80 MPa to 120 MPa and holding time 8 s to 12 s for wall sections of 2.0 mm to 3.5 mm. Long-term heat ageing is assessed according to ISO 188 at 120 °C for 500 h, with tensile strength retention required above 70%. If the OEM specification requires emissions compliance, VDA 278 is run on moulded plaques and total volatile organic compound values must remain below the platform limit. The terminal products are HVAC blower distributor housings and fan shroud supports, in which boss sections are cored to maintain wall thickness below 3.5 mm and sink marks are controlled by holding pressure rather than by increasing mould temperature.

    Process conflict arises at the junction of the boss and the main wall: high packing pressure needed for dimensional stability can create frozen-in orientation that reduces heat sag resistance. In production batches, the mould fill time is held between 1.0 s and 1.8 s for the housing, and the switch-over point is set at 95% of the stroke volume. An earlier switch-over produces short shots at the fan ring, while a later switch-over raises clamp force requirement above 2500 kN for a tool with projected area of 800 cm². Published data for this specific Kingfa PP-300 configuration is limited; the melt temperature upper limit should be confirmed from the batch certificate because homopolymer lot-to-lot variation in stabiliser content can shift yellowing onset by 10 °C.

    For diagnostic specimen handling components, Kingfa PP-300 is selected only when the moulded part is a short-term disposable and not a load-bearing blood-contact device. The grade is converted as 100 parts virgin PP-H without regrind, and pigment masterbatch is limited to 0.5 wt% because higher loading changes the extraction profile under USP 661 physicochemical testing. Moulding is performed in a cleanroom at ISO 14644-1 Class 8 or higher, with melt temperature 220 °C to 235 °C and mould temperature 10 °C to 20 °C. The low mould temperature accelerates crystallisation and shortens cycle time but increases residual stress, so the gate is placed on the non-functional underside of the pipette tip rack to prevent warpage measured after conditioning at 23 °C and 50% RH for 48 h. Cytotoxicity is assessed in accordance with ISO 10993-5:2009, and the final device is sterilised by ethylene oxide or gamma irradiation. If gamma irradiation above 25 kGy is specified, the PP-H must be evaluated for post-irradiation yellowing and embrittlement because homopolymer has less radiation tolerance than radiation-stabilised copolymer grades. Terminal products include 50 µL to 1000 µL pipette tip racks, specimen transfer cups, and diagnostic microplate frames, each with flatness tolerance ±0.15 mm over a 128 mm length.

    Living hinge endurance in integral PP-H closures

    Integral hinge geometries moulded from Kingfa PP-300 exploit the crystalline orientation induced by a high flow rate through a narrow hinge land. The hinge thickness is specified at 0.25 mm to 0.50 mm, and the gate land is located to force melt through the hinge before filling the cover. This orientation gives the PP-H hinge a flexural endurance typically exceeding 105 cycles when the hinge is flexed through 90° at room temperature, but the exact value is dependent on mould temperature and must be verified on the production tool. Process development on two-platen injection machines with shot weights of 150 g to 300 g has shown that hinge quality is more sensitive to injection speed than to melt temperature. The machine is set with an injection speed of 180 mm/s to 250 mm/s at the screw, and the nozzle temperature is held at 235 °C to 245 °C. The mould is cooled to 20 °C to 25 °C so that the hinge freezes while the cover remains warm enough for shrinkage compensation. Failure modes observed on production lines include hinge whitening caused by excessive shear heating and gate blush caused by melt temperature above 250 °C; both conditions are detected by a 10% loss in flexural modulus measured in accordance with ISO 178. The compounding ratio for a nucleated version is 100 parts PP-H with 0.10 wt% to 0.30 wt% of a sorbitol-based nucleating agent, but the nucleated formulation must be re-validated for food-contact end use under EU 10/2011 because the nucleator is an intentional added substance. Terminal products are storage box lids with hinge thickness 0.35 mm and closure caps designed for a minimum 5000 open-close cycles before failure.

    In small-appliance internal support brackets, Kingfa PP-300 is introduced where the part must withstand an abnormal-heat ball-pressure test at 125 °C without softening beyond the allowed indentation. The unfilled PP-H is processed at melt temperature 230 °C to 250 °C, and the key process control point is the cooling rate through the crystallisation window between 110 °C and 80 °C. Mould temperatures above 60 °C are avoided because slow cooling increases spherulite size and produces post-moulding dimension drift of 0.3% to 0.6% over 72 h. The compliance route for appliance components is IEC 60695-10-2 for glow-wire flammability and IEC 60335-1 for abnormal operation. PP-H without flame retardant will not pass a glow-wire ignition test at 750 °C without ignition, so the component is used only in positions where the glow-wire requirement is 650 °C or where the enclosure is not directly supporting live parts. A typical starting formulation for lower-temperature appliance parts uses 100 parts PP-H and 2 wt% colour masterbatch; talc or glass addition is service-specific and is not introduced solely to lower cost. Terminal products are coffee machine water tank brackets, microwave turntable ring supports, and electric kettle base stiffeners, each checked for dimensional stability after 24 h annealing at 80 °C.

    When PP-H is used as a compounding base for flame-retardant injection grades

    Kingfa PP-300 can serve as the PP-H carrier resin for halogen-free flame-retardant compounds used in electrical junction boxes and switch housings, where the compound is diluted with mineral flame retardant at 40 wt% to 50 wt% loading. The compounding line is a co-rotating twin-screw extruder with L/D 44:1, and the PP-H is fed at the main throat while magnesium hydroxide or ammonium polyphosphate is side-fed after the polymer has reached a melt state. Barrel temperatures are held between 170 °C and 190 °C to avoid decomposition of the halogen-free flame retardant and to maintain a melt pressure below 12 MPa at the screen changer. The compound is then injection moulded at melt temperature 190 °C to 210 °C, which is 20 °C to 30 °C lower than unfilled PP-H, because higher melt temperature can cause the flame retardant to release water vapour and produce splay marks on the housing surface. The final compound is tested according to UL 94 with a V-0 classification at 1.5 mm thickness and IEC 60695-2-10 glow-wire flammability at 960 °C for materials in contact with live parts. Comparative tracking index is determined by IEC 60112 and must be declared on the compound datasheet. Terminal products are electrical junction boxes, terminal covers, and relay housings, each moulded with wall thickness 1.2 mm to 2.0 mm and no hot-runner dead spots, because PP-H flame-retardant compounds have a narrow residence-time window before the flame-retardant package degrades. Published data for this specific Kingfa PP-300 configuration is limited; the exact let-down ratio and screen pack are line-specific and must be established by a compounding trial because the melt flow of the base resin directly controls dispersion of the mineral filler.

    Free Quote

    Competitive Kingfa PP-300,PP Homopolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    For specification engineers evaluating an unfilled polypropylene homopolymer with a nominal melt mass-flow rate class of 3.0 g/10 min, Kingfa PP-300 is supplied by Kingfa Sci & Tech Co., Ltd. as a pelletised resin, CAS 9003-07-0. The grade belongs to the PP-H family under ISO 19069-2:2016 and is not a random or impact copolymer. The suffix 300 is conventionally read as a nominal melt flow rate of 3.0 g/10 min at 230 °C/2.16 kg using ISO 1133-1:2022, though the manufacturer certificate of analysis must confirm the lot-specific value. Published independent data for this exact Kingfa SKU remain limited in the open literature; class-level performance values cited below are therefore drawn from PP-H material designations and should not replace a certified technical datasheet.

    Typical unfilled PP homopolymer of this flow class exhibits a density of 0.90–0.91 g/cm³ when measured by ISO 1183-1:2019, a tensile stress at yield near 33–36 MPa under ISO 527-2:2012 at 50 mm/min, and a flexural modulus in the range 1.35–1.65 GPa under ISO 178:2019. These values reflect the higher crystallinity of the homopolymer architecture and are higher than those of random copolymers at equivalent melt flow rate, but the trade-off is lower multiaxial impact resistance and reduced ductility below ambient temperature.

    When a Moulding Line Switches from High-Flow Copolymer to PP-300 Homopolymer

    The principal processing conflict is the combination of lower melt flow and a relatively narrow thermal-oxidative window. If the nominal MFR is confirmed at 3.0 g/10 min, the melt viscosity is materially higher than a 25–35 g/10 min random copolymer, increasing screw torque and peak injection pressure. On a reciprocating-screw injection moulding machine fitted with a general-purpose polyolefin screw with a compression ratio of 2.5:1–3.0:1 and an L/D ratio of 20:1–25:1, a barrel thermal profile from rear 180 °C to nozzle 230 °C is typical. The mould surface temperature should be held between 20 °C and 50 °C; lower temperatures increase flow hesitation and sink marks, while higher temperatures lengthen cycle time and may increase post-moulding shrinkage. Injection velocity is profiled to prevent jetting, with screw-advance speed commonly 100–200 mm/s for thin-walled parts, and hold pressure is set at 60%–80% of peak injection hydraulic pressure until gate-seal mass stabilisation is confirmed.

    Below 210 °C melt temperature, flow length is reduced and short-shot defects become more likely in long or thin flow paths. Above 255–260 °C, thermal-oxidative chain scission accelerates; barrel residence time should not exceed 5 min when set temperatures exceed 250 °C. Degradation is often detected as yellowing, reduced notched impact, and a rise in MFR caused by molecular weight loss. For warehouse-stored pellets at relative humidity above 60%, pre-drying at 80–85 °C for 2–3 h in a desiccant dryer with dew point ≤ -30 °C prevents surface moisture splay. Regrind should not exceed 20% by weight unless melt flow and colour are monitored after each recycling pass.

    On manufacturing lines, two recurring failure modes are observed when an unfilled homopolymer is substituted into tools designed for high-flow random or impact copolymers: gate blush and sink marks opposite ribs. Gate blush develops when local shear rate at the gate exceeds approximately 20,000–30,000 s⁻¹; gate diameter should be increased, or melt temperature raised within the allowable window. Sink marks occur where nominal wall thickness varies by more than 25% and packing is insufficient; rib thickness should be limited to 50%–60% of the adjacent wall, and hold time should be extended until part mass stabilisation is confirmed. Shot-weight variance of ±0.2–0.5 g on small parts may also arise from non-uniform pellet geometry and hopper bridging; pellet size classification and hopper throat vibration are common corrective actions.

    For sheet extrusion, a single-screw extruder with L/D 30:1 and a barrier screw is sufficient. Die temperatures are typically 220–240 °C, with chill-roll temperatures 40–60 °C. The lower melt flow of PP-H near 3.0 g/10 min provides higher melt strength than high-flow random copolymers, reducing draw resonance in cast sheet take-off. However, edge trim cannot be reintroduced without careful particle-size control because the grade’s melt-flow reserve is limited and excessive regrind will shift viscosity downward.

    Unfilled PP-H grades near 3.0 g/10 min are commonly specified for rigid housewares, appliance brackets, laboratory trays, non-pressure fluid-handling components, and semi-finished sheet for thermoforming. The absence of ethylene comonomer yields higher short-term heat resistance and creep resistance than PP random copolymers, but impact performance drops sharply below 0 °C. Kingfa PP-300 should not be selected for frozen-food packaging, automotive interior pillars requiring ductile failure at -20 °C, or thin-wall containers expected to survive drop tests from cold storage; PP impact copolymers or random copolymers are better suited for those conditions.

    What Comparative Data Separate PP-300 from Random and Impact Copolymer Grades?

    The following table compares class-level values for unfilled PP-H, PP-R, and PP-B materials at 23 °C after conditioning to ISO 291:2008. Values are not lot-specific for Kingfa PP-300 and should be used only as a preliminary material-selection screen.

    Property Test method PP-H class near 3.0 g/10 min PP-R random copolymer PP-B impact copolymer
    Density ISO 1183-1:2019 0.90–0.91 g/cm³ 0.89–0.91 g/cm³ 0.89–0.91 g/cm³
    Tensile stress at yield ISO 527-2:2012 33–36 MPa 25–30 MPa 22–28 MPa
    Tensile elongation at yield ISO 527-2:2012 7%–10% 10%–15% 5%–8%
    Flexural modulus ISO 178:2019 1.35–1.65 GPa 0.90–1.20 GPa 0.80–1.10 GPa
    Notched Izod at 23 °C ISO 180/A 2.0–3.0 kJ/m² 4.0–10.0 kJ/m² 10.0–40.0 kJ/m²
    Notched Izod at -20 °C ISO 180/A 0.8–1.5 kJ/m² 1.5–3.0 kJ/m² 4.0–8.0 kJ/m²
    Heat deflection temperature ISO 75-2:2013 method B 90–105 °C 75–90 °C 85–95 °C
    Shore D hardness ISO 868:2003 68–72 62–68 58–65

    The notched Izod values for PP-B impact copolymer often report partial break rather than complete break. Where a ductile failure response is required, notched impact testing at -20 °C is more discriminating than ambient-temperature data because PP-H loses significant ductility below its glass transition and ethylene-bearing copolymers retain greater chain mobility in the amorphous phase.

    Polypropylene homopolymer has a low surface energy of approximately 29–31 mN/m; bonding, printing, or coating without treatment produces inconsistent adhesion. Corona or atmospheric plasma treatment to a wetting tension of at least 38–42 mN/m measured by ISO 8296:2003 is required for inks and adhesives. Flame treatment is an alternative for injection-moulded surfaces. This applies to Kingfa PP-300 in common with other unfilled PP-H grades and is not a grade-specific limitation.

    Regulatory acceptability is formulation-dependent and cannot be established by base-polymer type alone. A PP-H base resin may fall within the scope of FDA 21 CFR 177.1520 for olefin polymers, but food-contact compliance requires end-article migration testing with the intended food simulant. Under Regulation (EU) No 10/2011, the overall migration limit is 10 mg/dm²; specific migration limits apply to each intentionally added substance and non-intentionally added substance. For China domestic food-contact applications, compliance is assessed under GB 4806.6-2016. Under REACH, a supplier must disclose SVHC presence above 0.1% w/w per article. Under RoHS Directive 2011/65/EU, homogeneous-material limits are 1000 ppm lead, 100 ppm cadmium, 1000 ppm mercury, 1000 ppm hexavalent chromium, and 1000 ppm PBB/PBDE. A batch-specific certificate is required; a generic supplier statement is not sufficient for lot release.

    Regulation / Standard Scope Verification limit or test method
    FDA 21 CFR 177.1520 Olefin polymers in food-contact articles End-test extraction with food simulant; no resin-only compliance
    EU 10/2011 Food-contact plastics Overall migration ≤ 10 mg/dm²; specific migration by EN 1186-1:2002 and EN 13130 series
    REACH SVHC disclosure and restrictions SVHC 0.1% w/w per article; Annex XVII restrictions
    RoHS 2011/65/EU Electrical and electronic equipment Pb 1000 ppm, Cd 100 ppm, Hg 1000 ppm, Cr(VI) 1000 ppm, PBB/PBDE 1000 ppm in homogeneous material
    GB 4806.6-2016 China food-contact plastic materials Overall migration and consumption tests per Chinese standard

    Nucleation packages shift crystallisation temperature and cycle time. For PP homopolymer, conventional crystallisation onset is 110–115 °C; a nucleated system can raise onset to 125–130 °C, reducing cooling time by 10%–20%. If Kingfa PP-300 is supplied non-nucleated, adding a nucleating masterbatch may improve stiffness and shorten cycle time but can increase shrinkage anisotropy. Published data for this exact grade with a specific nucleant package is limited; line trials should be performed before mould release settings or dimensional tolerances are changed.