    Specifications
    HS Code 692199
    Polymer Type Polypropylene Homopolymer
    Purity 99%
    Density 0.905 g/cm³
    Melt Flow Rate 230 C 2 16 Kg 12 g/10 min
    Tensile Strength At Yield 32 MPa
    Elongation At Break 50%
    Flexural Modulus 1400 MPa
    Notched Izod Impact Strength 23 C 3 kJ/m²
    Heat Deflection Temperature 0 45 Mpa 90°C
    Vicat Softening Temperature 150°C
    Rockwell Hardness R90
    Molding Shrinkage 1.2-1.8%
    Processing Method Injection Molding

    As an accredited Kingfa PP-92345,PP Homopolymer (99%) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa PP-92345 PP Homopolymer (99%) is supplied in 25 kg moisture-resistant bags, palletized and stretch-wrapped for secure industrial transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of Kingfa PP-92345 PP Homopolymer (99%), palletized and secured for shipment.
    Shipping Shipping description: Kingfa PP-92345, PP Homopolymer (99%), solid polypropylene pellets, non-hazardous. Not regulated as dangerous goods for transport; no UN number, hazard class, or packing group required. Ship in clean, dry, closed packaging, protected from moisture, heat, and contamination.
    Storage Store Kingfa PP-92345 in a cool, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers closed to prevent moisture and contamination. Avoid dust generation and accumulation; use grounding/bonding where applicable. Protect from UV and weather. Do not store near food, feed, or incompatible materials. Follow local regulations and the SDS.
    Shelf Life Shelf Life: Not established; stable when stored cool, dry, well-ventilated, and away from sunlight and ignition sources.
    Application of Kingfa PP-92345,PP Homopolymer (99%)

    What Restricts Melt Temperature Window in High-Speed BOPP Line?

    For biaxially oriented polypropylene film production, Kingfa PP-92345 homopolymer pellets are extruded through a slot die at melt temperatures between 230°C and 260°C. Excursions above 270°C initiate visible gel formation from thermo-oxidative degradation even when residual catalyst content is low. The cast film is pinned to a chill roll held at 20–30°C, where the high crystallization rate of a 99% homopolymer creates a low-order crystalline skin that later governs tear resistance and haze. Machine-direction orientation is performed at 120–130°C with MD draw ratios between 4.5:1 and 5.5:1. Below 4.0:1, draw resonance appears as periodic thickness bands across the web; above 5.8:1, edge fibrillation becomes a statistically frequent defect on production-scale Stahlkontor or Brückner lines. Transverse orientation follows in a tenter oven with TD draw ratios of 8:1 to 10:1 at 150–165°C. Haze values measured according to ASTM D1003-21 remain below 1.5% for 20 µm film only when chill-roll water temperature fluctuation is held within ±1°C; otherwise surface micro-roughness from spherulitic growth raises light scattering. The grade’s narrow melting range requires the tenter preheat zone to stay at least 5°C below the onset of melting to avoid premature sagging. Published data for this specific configuration is limited; film producers should validate line speed against the supplier’s extrusion batch data.

    Kingfa PP-92345 is processed as a high-isotacticity polypropylene homopolymer on production-scale injection molding lines where dimensional stability at elevated under-hood temperatures is specified. Barrel temperature profiling is controlled from 210°C to 240°C across feed, compression, and metering zones, with nozzle temperature held at 230°C ± 5°C to maintain homogeneous melt delivery. On machines with clamp force ratings from 1,200 kN to 2,500 kN, a screw back pressure of 6–10 bar and a screw speed of 40–80 rpm are typical starting parameters; however, lot-to-lot variation in isotacticity requires adjustment of plasticizing stroke to avoid unmelted granules in the check ring. Mold temperature is controlled at 20–45°C with P20 or H13 steel inserts, because higher cavity temperatures increase cooling time and can shift shrinkage outside the nominal 1.2–1.8% range measured according to ASTM D955-08. A gate diameter of at least 0.5 mm per 1.0 mm wall thickness is advised to prevent early freeze-off, while a holding pressure of 70–85% of peak injection pressure reduces sink marks in bosses and ribs. The homopolymer’s high crystalline fraction contributes to tensile modulus values above 1,500 MPa when tested per ISO 527-2:2012; however, the same high crystallinity lowers notched Izod impact resistance below 2.5 kJ/m² under ASTM D256-23 at 23°C and makes the material unsuitable for snap-fit designs that see impact loading below 0°C. For under-hood brackets, exposure to continuous service temperatures above 100°C requires validation against ISO 75-2:2013 HDT/A and ISO 306:2022 Vicat softening temperature because oxidative stabilizers in the masterbatch may be consumed by hot spots in a poorly designed hot runner manifold.

    Thermoforming Sag Resistance and Melt Strength Limits in PP Homopolymer

    Sheet extruded from PP-92345 at 220–245°C and calendered through a three-roll stack at 70–90°C reaches a fully crystalline state suitable for cut-sheet thermoforming. The homopolymer structure exhibits lower melt strength than block copolymers, and sag becomes the governing process defect when oven air temperature exceeds 165°C. The practical forming window for a 2 mm sheet is often no wider than ±4°C; at the low end, spring-back causes incomplete reproduction of mold corners, while at the high end, sheet thinning exceeds 25% in plug-assisted areas. A plug temperature of 90–110°C, made from syntactic foam or PPSU, is used to pre-stretch the sheet before final vacuum. Draw ratios should remain below 0.6:1 depth-to-width for female tools and below 1.2:1 for male tools; deeper geometries require transition to a heterophasic PP copolymer because the homopolymer will fail at corners with whitening. Mold temperature is controlled at 50–70°C to prevent marking and to maintain part gloss, while cycle time depends on sheet thickness and is limited by thermal conductivity rather than by crystallization. Dimensional stability after forming is assessed by ASTM D7027-20 scratch resistance and ISO 291 conditioning; final parts should be allowed to relax for 24 h before dimensional audit.

    On spunbond lines with melt-blown or calender bonding, PP-92345 homopolymer is processed at spinneret melt temperatures of 210–235°C. At the lower end, the higher melt viscosity limits throughput, while above 240°C the risk of filament breakage increases because the 99% homopolymer has a narrow molecular weight distribution and no copolymer fraction to stabilize attenuating filaments. Quench air at 12–18°C with relative humidity 65–75% is delivered at 0.3–0.6 m/s across the filament bundle; insufficient quench produces roping defects in the web, and excessive quench reduces filament orientation before the draw jet. A draw-jet air pressure of 0.6–1.2 bar is typical for fabric weights from 12 g/m² to 50 g/m². The draw ratio must be tuned by measuring filament diameter under an optical microscope because offline tensile tests cannot separate orientation-induced strength from bonding-induced strength. Thermal bonding is performed with an engraved and a smooth calender roll at 145–160°C and nip pressure of 40–80 N/mm; bond area is typically 12–18% of the web. Fabric tensile strength is evaluated according to ISO 9073-3:2022 strip method, and air permeability by ASTM D737-18. The homopolymer’s high crystallinity produces stiffer hand than copolymer webs, which limits use in hygiene applications requiring cotton-like drape. For medical packaging, the fabric must meet ISO 11607-1:2019 microbial barrier requirements after ethylene oxide or gamma sterilization; oxidative stabilizers in the grade should be confirmed to survive the selected dose.

    When PP-92345 Replaces Impact Copolymer in Living Hinge and Closure Applications

    In injection molded caps, closures, and living-hinge packaging components, a 99% homopolymer such as PP-92345 can replace a propylene-ethylene copolymer only when the application does not require sub-zero impact resistance. The hinge region requires through-thickness orientation; this is achieved with a gate located so that melt flow crosses the hinge transversely, an injection speed in the upper range of 150–300 mm/s, and a melt temperature of 240–260°C. Hinge thickness is maintained between 0.25 mm and 0.40 mm; below 0.20 mm the homopolymer exhibits brittle fracture after fewer than 100 flexural cycles, while above 0.50 mm enough orientation is lost that whitening occurs immediately. Mold surface temperature in the hinge zone is not allowed to exceed 30°C because slower cooling relaxes orientation and increases flexural fatigue failure. Parts are tested by repeated opening to a 180° angle at 1 Hz until failure; homopolymer grades may pass 10⁵ cycles at 23°C but can fail below 10³ cycles at -10°C. Dimensional stability of closure threads is validated against ASTM D2063-10 and ISO 16725:2004 torque retention. The grade’s higher flexural modulus, measured by ISO 178:2019, allows a thinner hinge but increases the demand on the torque-limiting capping head.

    Raffia Tape Orientation and Draw Ratio Thresholds

    Flat film for woven sack tape is cast from PP-92345 at 220–240°C through a slot die with a die gap of 0.6–1.0 mm, then quenched in a water bath at 30–40°C. Slit tapes are oriented in a hot-air oven at 120–150°C; the target draw ratio is 6:1 to 7:1. At 5:1 the tape retains excessive elongation under load, causing creep in filled sacks, while above 8:1 the homopolymer splits or fibrillates along micro-scratches created by the slitting blades. Tensile strength of oriented tape rises to 35–45 cN/tex and elongation at break falls to 10–20% when tested by ASTM D638-14; these values are strongly dependent on water-bath temperature homogeneity because uneven quench creates variable spherulite sizes that later produce warp in woven fabric. A denier of 600–1000 is common for sack lamination; the tape should be conditioned at 23°C and 50% RH prior to tensile testing. Weave-line tension must remain below 5% of tape breaking strength to avoid premature failure at selvedge. The 99% homopolymer provides high stiffness and low fibrillation during weaving, but the narrow molecular weight distribution reduces the maximum stable draw ratio compared with reactor-grade PP with broader polydispersity.

    Thin-wall containers with flow length-to-wall thickness ratios above 150:1 are molded from PP-92345 only when the melt temperature is pushed to 250–270°C and injection speed is set to fill the cavity in less than 0.5 s; lower speeds allow the high-crystallinity homopolymer to solidify before filling thin ribs or snap-fit undercuts. The mold is cooled at 10–15°C with high-turbulence water circuits, and ejection is initiated when the part surface reaches 70–80°C, because hot ejection causes corner distortion and post-mold shrinkage. Wall thickness is typically 0.35–0.80 mm; dimensions are validated after 48 h conditioning under ISO 291:2008 standard atmosphere to account for post-crystallization shrinkage of 0.2–0.4%. Hot runner systems with valve gates are preferred over cold runners to minimize residual stress in the gate area; a valve-gate delay of 0.1–0.2 s after packing reduces stringing. For food-contact containers, the finished article must comply with EU 10/2011 overall migration limits and FDA 21 CFR 177.1520 olefin polymer specifications; the converter is responsible for verifying that the final additive package does not exceed specific migration limits. This processing window is narrower than for random copolymers, and published data for this specific configuration is limited; pilot-tool trials are used to establish the acceptable cavity-to-cavity imbalance.

    Free Quote

    Competitive Kingfa PP-92345,PP Homopolymer (99%) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa PP-92345 is a 99% polypropylene homopolymer injection-moulding grade supplied in pellet form. The designation denotes the polymer phase before incorporation of the stabilizer and processing-aid system; the remaining 1% consists of non-polymeric additives. Applications are concentrated in thin-wall packaging, caps, closures, and appliance housings where flexural modulus above 1400 MPa per ISO 178 and a melt-volume-flow rate suitable for wall thickness below 1.0 mm per ISO 1133-1:2022 are required. Because supplier lot certificates govern exact melt-volume-flow rate and additive content, the class-typical values below are for a high-flow unfilled PP homopolymer; published data for this specific configuration is limited and should be verified against the manufacturer’s current certificate of analysis.

    What Distinguishes a 99% Homopolymer Architecture from Random Copolymer and Talc-Filled Systems?

    The homopolymer structure consists almost entirely of propylene repeat units, yielding an isotactic α-phase crystalline morphology with a melting peak measured by differential scanning calorimetry in the range 160–166 °C per ISO 11357-3. This distinguishes the grade from polypropylene random copolymers containing 1.5–4 wt% ethylene comonomer, which disrupt crystallinity, reduce flexural modulus, improve optical clarity, and raise cold-temperature impact. In PP-92345, the absence of a rubbery ethylene-propylene dispersed phase also separates it from impact copolymer grades; the result is higher tensile yield stress and lower Charpy notched impact values. Against talc-filled homopolymer, the unfilled PP-92345 offers lower density and better surface gloss but lower flexural modulus and higher mould shrinkage.

    Rheologically, the material is a high-flow linear isotactic PP. For MFR above 25 g/10 min at 230 °C and 2.16 kg per ISO 1133-1:2022, apparent viscosity at 100 s⁻¹ and 230 °C typically falls below 100 Pa·s, reducing injection pressure in thin-wall tools. Compared with a broad-molecular-weight PP homopolymer of MFR below 5 g/10 min, spiral flow length at identical injection pressure can be 20–35% higher, but melt strength and parison sag resistance are lower. PP-92345 is therefore unsuitable for extrusion blow moulding and is specified primarily for injection-moulded parts requiring high flow length-to-wall-thickness ratios.

    For high-cavitation thin-wall packaging tools with wall thickness below 1.0 mm, the material is processed on all-electric injection moulding machines with screw diameter 25–40 mm, L/D 20:1–24:1, and compression ratio 2.5:1–3:1. Clamp force requirement is typically 0.5–0.8 tonnes/cm² of projected cavity area for flow length-to-wall thickness ratios exceeding 150:1. Moulds are operated with cold sprue or hot-runner valve-gated systems; valve-gated hot runners reduce gate freeze-off and allow sequential packing of thin-wall containers, lids, and caps. Integral hinge endurance is not governed by a single ISO/ASTM method; validation is tool-specific and depends on nucleating state, mould temperature, and gate design rather than ethylene comonomer plasticization.

    When Mould Temperature and Packing Pressure Shift Shrinkage Anisotropy

    Unfilled PP homopolymer exhibits post-moulding shrinkage of 1.2–2.0% in the flow direction and 1.0–1.6% transverse, measured after 48 h at 23 °C per ISO 294-4. The exact anisotropy is driven by shear-induced orientation and the crystallization half-time in the mould. If mould temperature is held below 15 °C, the skin layer freezes before complete crystallization, reducing stiffness and increasing warpage risk; above 40 °C, cycle time increases but secondary crystallization and shrinkage uniformity improve. Class-typical cavity pressure holding is 35–60 MPa, with supplier recommendations governing the specific PP-92345 lot.

    Thermal degradation in the melt phase follows chain-scission kinetics. Residence time at melt temperatures above 250 °C should not exceed 5 min; at 280 °C, the induction period drops below 15 min. Feed throat temperature must remain below 40 °C to prevent pellet bridging. Pre-drying is not required for sealed packaging at ambient relative humidity below 60%; when exposure to RH above 60% has exceeded 4 h, a 80 °C desiccant or hot-air drying step for 2 h is applied. On 25 mm screw machines, high-flow PP may exhibit screw recovery times below 2 s for a 40 g shot, but back pressure above 15 bar can raise melt temperature by 10–20 °C through frictional heat, causing nozzle drool and gate stringing. Melt cushion of 3–6 mm is typically maintained to stabilize packing.

    Typical production-line failure modes include gate blush at injection speeds above 300 mm/s, sink marks where cavity pressure drops below 35 MPa during packing, and weld-line brittle failure. Notched impact strength at a weld line can be 30–50% lower than bulk values; weld-line performance should be evaluated per ISO 179-1/1eA on machined specimens taken perpendicular to the weld. The material is not recommended for continuous service above 90 °C without additional heat stabilization and is not suitable for cold impact below -10 °C where impact copolymer or random copolymer grades are required.

    Regulatory data for the compound are supplied as an additive declaration rather than a polymer certification. The base PP homopolymer can meet food-contact provisions of FDA 21 CFR 177.1520 when all additives comply with the same regulation. EU food-contact compliance is evaluated under EU 10/2011 with overall migration limit of 10 mg/dm²; specific migration limits apply by substance. The governing compliance matrix is shown in Table 2.

    Comparative Engineering Properties Across Unfilled Homopolymer, Random Copolymer, and Talc-Filled Polypropylene

    The property ranges in Table 1 are class-typical for high-flow unfilled PP homopolymer and comparative systems. PP-92345 lot-specific data should be taken from the manufacturer’s test report.

    Table 1: Representative property ranges for unfilled PP homopolymer, random copolymer, and talc-filled systems
    Property Test standard High-flow PP homopolymer class Random copolymer typical Talc-filled homopolymer
    Melt flow rate ISO 1133-1:2022 25–40 g/10 min at 230 °C, 2.16 kg 8–25 g/10 min 5–30 g/10 min
    Density ISO 1183-1 0.900–0.910 g/cm³ 0.890–0.905 g/cm³ 1.05–1.25 g/cm³
    Tensile yield stress ISO 527-2 32–36 MPa 25–32 MPa 27–35 MPa
    Flexural modulus ISO 178 1400–1600 MPa 900–1300 MPa 2200–3500 MPa
    Charpy notched impact, 23 °C ISO 179-1/1eA 2.0–4.0 kJ/m² 5.0–12.0 kJ/m² 3.0–6.0 kJ/m²
    Heat deflection temperature, 0.45 MPa ISO 75-2/B 90–105 °C 70–90 °C 100–135 °C
    Melting peak ISO 11357-3 160–166 °C 130–148 °C 162–166 °C
    Mould shrinkage, 24 h ISO 294-4 1.2–2.0% flow, 1.0–1.6% transverse 0.8–1.5% 0.5–0.9%

    Compared with PP random copolymer, PP-92345 class material raises tensile yield stress by approximately 10–20% and flexural modulus by 20–40%, but reduces notched impact at 0 °C by more than 50%. Compared with talc-filled homopolymer, density is lower by 15–25%, but shrinkage is approximately 2–4× higher and dimensional stability is poorer. These differences govern substitution decisions in caps, closures, and thin-wall packaging.

    Table 2: Compliance assessment matrix for PP homopolymer food-contact and chemical regulation
    Regulatory domain Standard or clause Assessment basis
    U.S. food contact FDA 21 CFR 177.1520 Olefin polymer; additive compliance and end-use conditions govern
    EU food contact EU 10/2011 Overall migration 10 mg/dm²; specific migration limits by substance
    REACH EC 1907/2006 SVHC declaration through supplier certificate
    RoHS 2011/65/EU Pb, Hg, Cr(VI), PBB, PBDE ≤ 0.1%; Cd ≤ 0.01%
    China food contact GB 4806.7-2016 Total migration, potassium permanganate consumption, heavy metal limits

    Where sealed original bags are stored below 30 °C and away from direct ultraviolet sources, oxidative stability is maintained within the supplier shelf-life, typically 24 months from production date. Moisture regain of sealed PP homopolymer is below 0.05% under dry conditions; regrind incorporation up to 30% is acceptable in non-impact applications, but repeated heat history shifts MFR upward and reduces notched impact. Outdoor use without ultraviolet stabilization leads to surface cracking under ISO 4892-2 xenon arc exposure; a hindered amine light stabilizer and carbon black package is required for extended service. The material is incompatible with strong oxidizers and should not be combined with copper-based stabilizer systems where long-term heat ageing above 120 °C is specified. Replacement of an impact copolymer with PP-92345 in a cap or closure is justified only when top-load strength and dimensional stability at elevated warehouse temperatures are the controlling requirements. If drop impact at -20 °C is mandatory, a copolymer grade or nucleated impact-modified system should be selected instead.