| HS Code | 547998 |
| Manufacturer | Kingfa Sci. & Tech. Co., Ltd. |
| Grade | PP-92989 |
| Polymer Type | Polypropylene Homopolymer |
| Reinforcement | Glass fiber reinforced |
| Physical Form | Pellets |
| Processing Method | Injection molding |
| Density | 1.12 g/cm³ (typical) |
| Melt Flow Rate | 8.0 g/10 min (typical) |
| Tensile Strength | 80 MPa (typical) |
| Elongation At Break | 3.0% (typical) |
| Flexural Modulus | 5500 MPa (typical) |
| Notched Izod Impact Strength | 80 J/m (typical) |
| Heat Deflection Temperature At 1 82 Mpa | 150°C (typical) |
| Vicat Softening Temperature | 155°C (typical) |
| Mold Shrinkage | 0.4% (typical) |
| Flammability Rating | HB (typical) |
As an accredited Kingfa PP-92989,PP Homopolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-92989 PP Homopolymer is packaged in 25 kg moisture-resistant bags, palletized and labeled for secure industrial storage and transport. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Kingfa PP-92989 PP Homopolymer in 25 kg bags, palletized and securely stowed for export. |
| Shipping | Kingfa PP-92989, PP Homopolymer is not regulated as dangerous goods for transport. It is a non-hazardous solid polymer; ship in suitable closed containers, protected from moisture, heat, and sunlight. No UN number, hazard class, packing group, or marine pollutant designation applies. Follow applicable national and international transport regulations. |
| Storage | Store Kingfa PP-92989, PP Homopolymer in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and ignition sources. Keep original containers or packaging closed, labeled, and protected from physical damage. Prevent moisture, dust, and static buildup; use grounding/bonding where applicable. Avoid contact with incompatible chemicals and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is typically 24 months from date of manufacture when stored dry, cool, and in original sealed packaging. |
Kingfa PP-92989 PP homopolymer is introduced at the extruder feed throat as controlled-rheology virgin pellets; in raffia tape extrusion for flexible intermediate bulk containers (FIBCs) and woven sacks, pellets are metered into a single-screw extruder with a 30:1 L/D barrier screw, melted at 230–260°C, and extruded through a slit die into a water-quench bath held at 25–35°C. The cast film is then passed through a hot-air oven or over heated godets for solid-state orientation at a draw ratio between 1:6 and 1:8. This orientation raises tape tenacity from an isotropic cast-film value commonly below 30 MPa to oriented values above 120 MPa, although the exact response depends on lot-to-lot isotacticity, draw-roll speed differential, and die-lip set. Tape tensile properties are reported after conditioning at 23±2°C and 50±5% relative humidity using ASTM D638 or ISO 527-3; circular-loom weaving runs on six- or eight-shuttle looms. Production-scale failure modes include web sag in the hot-air oven when the draw ratio deviates by more than ±0.3, fibrillation at the pinning station when quench-water temperature exceeds 40°C, and loom-side tape breakage when oriented-tape elongation at break falls below 15%. FIBC fabric must comply with ISO 21898; if used outdoors, the woven structure requires a UV-stabilization package, with accelerated weathering assessed by ISO 4892-2. Physical-property data for Kingfa PP-92989 at every draw ratio is limited in public sources, so a draw-ratio curve should be generated on the target line before specification lock, and melt mass-flow rate must be confirmed by ISO 1133-1:2022. Pre-drying is not routinely required for virgin pellets, but when surface moisture exceeds 0.1% by mass due to silo condensation or regrind inclusion, drying at 80°C for 2–4 hours in a dehumidifying hopper dryer is the minimum corrective step.
Continuous filament spunbond lines demand a stable melt mass-flow rate because the metering pumps deliver a fixed volumetric throughput to spinnerets with 4,000–8,000 holes per metre of spinneret width; MFR drift alters shear viscosity and hole throughput, producing denier variation across the web. For PP homopolymer grades in spunbond, the MFR specified by the manufacturer must be checked against ISO 1133-1:2022 at 230°C/2.16 kg, and deviations exceeding ±1 g/10 min from the target are sufficient to shift filament diameter by more than 4% at constant pump speed. Extruders are typically 90–150 mm single-screw machines with 30:1 L/D and water-cooled feed throats; melt temperature at the die is held at 230–250°C, while quench air at 10–25°C and 0.3–0.8 m/s stabilizes the filaments before drawdown. Filament drawing through high-speed aspirators at 2,500–4,500 m/min induces tensile strength in the nonwoven; web strength is then assessed according to ISO 9073-3. A process conflict arises when the base resin contains peroxide-controlled rheology modifiers: excessive melt temperature above 260°C can accelerate residual peroxide decomposition and reduce viscosity after the breaker plate, causing inconsistent web basis weight. Kingfa PP-92989 PP homopolymer may be used in spunbond if its rheology curve and ash content are confirmed against the grade technical datasheet; no published spunbond performance data for this exact grade was identified at the time of writing, so a pilot trial at 1–2 m web width is the minimum verification step before production. For hygiene applications, the nonwoven must comply with ISO 10993-5 cytotoxicity testing when used as a medical fabric component, and with FDA 21 CFR 177.1520 for olefin polymers in food-contact layers.
In thin-wall cap and closure injection moulding, Kingfa PP-92989 PP homopolymer is processed at melt temperatures of 230–250°C and mould temperatures of 20–40°C. The process window is constrained by the crystallisation rate of isotactic PP homopolymer: cooling below 70°C in the cavity rapidly freezes orientation at the frozen layer, while elevated mould temperatures above 60°C increase cycle time without adequate stiffness improvement. The grade should be evaluated on a machine with a screw diameter matched to shot volume and a hydraulic accumulator if short injection times below 0.2 s are required. Fill is normally achieved with a flow-length-to-wall-thickness ratio of 150:1 to 250:1 in high-flow PP homopolymers; moulding trials must confirm the actual flow length in a standard cavity because gate geometry and melt-pressure loss determine the result. When two melt fronts meet opposite a valve gate, a weak weld line forms; with unfilled PP homopolymer, weld-line strength retention is strongly mould-temperature dependent and must be measured on the actual cavity rather than estimated from datasheet values. Dimensional control requires shrinkage measurement after 24 hours at 23±2°C using ISO 294-4; tool allowance must account for anisotropic shrinkage between the parallel and normal directions. This grade does not contain impact modifiers, so low-temperature drop performance below -10°C must be verified before use in closures that require sub-zero crack resistance. For food-contact caps, migration requirements under EU 10/2011 and FDA 21 CFR 177.1520 must be confirmed on the finished article, not solely on the base resin.
| Evaluation item | Test method | Process relevance |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | Confirms control of thin-wall fill at fixed injection pressure |
| Tensile stress at yield | ISO 527-2 | Correlates with cap retention force after deformation |
| Flexural modulus | ISO 178 | Quantifies sidewall stiffness at 0.3–0.5 mm thickness |
| Notched Izod impact | ISO 180/A | Captures low-temperature brittle risk in closure tamper-evident bands |
| Moulding shrinkage parallel/normal | ISO 294-4 | Determines tool allowance after 24 h at 23±2°C |
Bulked continuous filament (BCF) extrusion of Kingfa PP-92989 PP homopolymer is carried out on a single-screw extruder with a multifilament die pack; the molten strands are quenched, drawn at ratios of 3:1 to 4:1, and textured in a hot-air jet before winding. The process is highly sensitive to filament denier uniformity; a melt-temperature fluctuation of ±2°C at the die plate can shift individual filament titres because the shear viscosity of linear PP homopolymer decreases nonlinearly with temperature. Yarn tenacity and elongation are assessed by ISO 3341; carpet construction performance is evaluated according to the applicable tufted-carpet thickness and pile-density standards. For automotive flooring, ISO 3795 or FMVSS 302 flammability limits are often applied; PP homopolymer burns and would require an external flame-retardant masterbatch to satisfy these tests. Dyeability is a process boundary: PP homopolymer is not dyeable with disperse or acid dyes, so colour must be introduced by melt pigmentation, and colour consistency across batches depends on the dosing accuracy of the gravimetric side-feeder system, typically ±0.2% of melt throughput. Published data for Kingfa PP-92989 in BCF extrusion is limited; a single-spinnerette pilot run should be performed before multi-position investment.
Sheet extrusion of Kingfa PP-92989 PP homopolymer is run on a single-screw extruder with a sheeting die and a vertical or horizontal three-roll stack; sheet thickness between 1.5 mm and 4.0 mm is typical for cut-sheet or roll-fed thermoforming. The homopolymer has a narrow thermoforming window compared with random copolymers because the crystalline melting peak measured by ISO 11357-3 is sharp. Sheet surface temperature for plug-assisted forming is normally held at 150–160°C; below 150°C, wall stress increases and plug marks become visible, while above 160°C, sag causes premature sheet contact and uneven wall thickness. Plug assist is mandatory for deep draw ratios above 1:1; plug material, plug temperature, and plug speed must be tuned to avoid sheet chill mark defects. Thermoformed food trays, cups, and lids must comply with EU 10/2011 and FDA 21 CFR 177.1520 on the finished article; organoleptic migration testing is required if the package is used with fatty foods above 40°C. Because PP homopolymer has lower melt strength than high-melt-strength grades, edge-web sag in a roll-fed oven between heating zones is a documented failure mode; reorientation of the sag band and independent zone temperature control are the usual corrective actions. Specific sag-depth data for Kingfa PP-92989 sheet is not publicly available, so an oven mapping trial with infrared pyrometers and a digital sheet-sag gauge is the only reliable method for establishing a production window.
In high-tension strapping extrusion, Kingfa PP-92989 PP homopolymer is melted in a single-screw extruder at 220–250°C, extruded through a flat-film or slot die, quenched in a water bath, and oriented at draw ratios from 1:8 to 1:10. The oriented strapping must retain tensile strength under elongation without longitudinal splitting; fibrillation occurs when the draw temperature is too low, when the quench-water temperature is outside 20–30°C, or when the die-lip shear history creates an oriented skin layer before the main draw stage. Strapping tensile properties are measured after conditioning at 23±2°C using ASTM D638 or ISO 527-3; pallet-load retention testing is performed according to the applicable distribution-packaging protocol. A frequent production-line bottleneck is width change during orientation: the drawn strap narrows by 30–40% and then must be annealed in a hot-air or hot-roll unit to reduce shrinkage. If the annealing temperature is more than 10°C below the crystallisation onset, residual shrinkage above 5% in a 60°C air environment can loosen palletised loads during transport. Kingfa PP-92989 PP homopolymer is suitable only where a single-layer strap is regulated by a non-food industrial packaging standard; if the strap is to be printed with high-speed inkjet systems, surface polarity must be improved by inline corona treatment above 38 mN/m and verified with dyne solutions at production speed.
Competitive Kingfa PP-92989,PP Homopolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-92989 is classified as a polypropylene homopolymer injection-molding grade supplied in stabilized pellet form. The homopolymer designation indicates that the polymer backbone consists essentially of propylene repeat units without intentional ethylene or 1-butene comonomer insertion, which differentiates the material from polypropylene random copolymers and impact copolymers. The product code places the grade in a high-flow segment intended for thin-wall injection molding; however, published product-specific data for this configuration is limited, and the manufacturer’s certificate of analysis and technical datasheet should be treated as the controlling documents for design inputs. Class-typical values for unfilled high-flow PP homopolymer include a melt mass-flow rate range of 30–100 g/10 min at 230°C under 2.16 kg load when tested to ISO 1133-1:2022 or ASTM D1238-23, and a density of 0.90–0.91 g/cm³ when measured to ISO 1183-1:2019. These class-typical ranges are not a substitute for grade-specific data but establish the material’s position relative to other polyolefin grades.
Polypropylene homopolymer grades such as Kingfa PP-92989 are differentiated from random copolymers by the structural regularity of the polymer chain. Random copolymers introduce ethylene co-units along the propylene chain, which reduces crystallinity, decreases flexural modulus, and improves optical clarity and seal initiation behavior. For a homopolymer, tensile yield stress class-typically falls in the 30–40 MPa range under ISO 527-2:2012, while a random copolymer typically falls near 22–30 MPa. Flexural modulus measured to ISO 178:2019 is generally 1500–1900 MPa for unfilled homopolymer classes, compared with 900–1400 MPa for random copolymer. These differences are relevant in rigid packaging and appliance housings where top-load strength and wall stiffness dominate.
Compared with impact copolymers, which contain a discrete ethylene-propylene rubber phase, PP-92989 as a homopolymer has lower notched Izod impact strength. Class-typical values at 23°C are 2–5 kJ/m² for homopolymer under ISO 180:2023, while impact copolymers may range from 10 kJ/m² to values exceeding 50 kJ/m². The homopolymer’s advantage is its higher stiffness and heat resistance. Heat deflection temperature under 0.45 MPa load is class-typically 100–115°C for the homopolymer category under ISO 75-2:2013, whereas random copolymers often fall between 85°C and 100°C. These thermal and rheological distinctions are the primary selection factors when replacing PP-92989 with an ethylene-modified alternative.
Processing of a high-flow polypropylene homopolymer on production-scale injection molding equipment requires attention to screw geometry, melt temperature, and mold-filling speed. General-purpose screws with a length-to-diameter ratio of 20:1 to 24:1 and a compression ratio of 2.0:1 to 3.5:1 are commonly used for unfilled PP; no unusual screw design is required unless high-speed thin-wall filling demands a larger check-ring flow path. Melt temperature is normally maintained between 220°C and 260°C, with thin-wall applications often favoring the upper half of the range to reduce viscosity and prevent premature freeze-off. Mold temperature is typically set between 20°C and 50°C; higher mold temperatures can improve surface gloss and reduce weld-line depth but increase cycle time.
High-flow PP grades can exhibit nozzle drool when the decompression stroke is insufficient or the shut-off nozzle seat is worn. On a production line, the defect appears as solidified material at the sprue bushing during mold-open time. Positive shut-off nozzles or hot-runner valve gates are recommended for thin-wall tools operating with short cycle times. Pre-drying is not required for dry pellets, but surface moisture from storage at relative humidity above 60% can produce splay. In that case, pre-drying at 80°C for approximately 2 h in a desiccant hopper dryer is typically sufficient. The low equilibrium moisture content of polypropylene means that drying time is driven by surface water removal rather than bulk diffusion. Melt temperature exceeding 280°C without sufficient stabilizer can initiate oxidative degradation, producing yellowing, viscosity shift, and acrid odor.
Dimensional stability of unfilled PP homopolymer is governed by crystallization shrinkage and orientation. Class-typical molding shrinkage measured to ISO 294-4:2018 is 1.2–2.0% in the flow direction and 1.4–2.2% in the transverse direction for unfilled homopolymer, although gate geometry, packing pressure profile, and wall thickness can shift results outside these ranges. Control of packing time and pressure is the primary process variable for reducing sink marks and warpage in PP-92989 moldings. Back pressure is generally maintained between 5 bar and 15 bar to avoid excessive shear heating while still providing adequate homogenization; when the screw includes a designed mixing section, lower back pressure may be acceptable. On high-cavitation hot-runner tools, pressure drop across the manifold and valve gate can exceed 30–50 MPa if the hot-runner system is undersized, negating the flow advantage of a high-MFR grade and causing cavity-to-cavity filling imbalance.
Regulatory status for food-contact applications is not automatic for any polypropylene grade. Polypropylene homopolymers can be formulated to meet FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011 when the stabilizer package and processing aids comply with the appropriate positive lists. A converter must verify overall migration and specific migration limits under the intended food simulants and time-temperature conditions. REACH SVHC screening and RoHS Directive 2011/65/EU are separate product-level obligations and must be confirmed against the compounder’s regulatory statement for the specific production lot. Color concentrates used with PP-92989 should employ a polypropylene carrier rather than a polyethylene carrier; an incompatible carrier can reduce stiffness, alter shrinkage, and produce visible delamination streaks in thin-wall parts at addition levels above 2–4 wt%.
High-flow PP homopolymer is selected when a thin-wall part requires sufficient bending resistance without increasing wall thickness. The flexural modulus of the unfilled homopolymer class is high enough to reduce sidewall deflection in containers and caps, but the trade-off is reduced impact resistance. For a rectangular thin-wall container with nominal wall thickness below 1.0 mm, short-shot prevention is often controlled by melt temperature, injection velocity, and gate size rather than by melt-flow rate alone. The sprue, runner, and gate dimensions must be sized for the viscosity of the actual PP-92989 lot. A melt flow rate at the upper end of the class range can reduce injection pressure requirement, but it may also increase the tendency for flash at parting lines if the clamp force margin is low.
When stiffness must exceed the unfilled homopolymer range, converters may evaluate talc-filled PP compounds. Typical talc-filled PP with 10–20 wt% talc can raise flexural modulus to 2000–3500 MPa, but density rises toward 0.97–1.05 g/cm³ and melt flow rate generally decreases. In contrast, PP-92989 remains an unfilled grade and therefore avoids the abrasive wear on screws, check rings, and hot-runner tips that mineral-filled systems introduce. This distinction is important when a high-cavitation, thin-wall tool must run continuously without component replacement.
Transparent packaging is a further boundary condition. Unfilled polypropylene homopolymer has relatively high haze because light scattering occurs at the boundaries of large spherulites. If the application requires contact clarity, ethylene-containing random copolymers or clarified random copolymers are preferred. PP-92989 should be considered for opaque or tinted rigid packaging where haze is not a specification and where the higher modulus of homopolymer permits down-gauging.
High melt flow rate is inversely related to molecular weight. A high-flow homopolymer such as PP-92989 will generally exhibit lower notched impact resistance than a low-flow PP homopolymer with lower melt mass-flow rate because shorter chains provide fewer load-bearing tie molecules across spherulite boundaries. Under ISO 180:2023, low-flow homopolymer grades may exceed 5 kJ/m² at 23°C, whereas high-flow homopolymer grades are more likely to fall below 4 kJ/m². This distinction is significant when a molder replaces a lower-flow homopolymer with PP-92989 to improve fill; the impact performance must be reassessed against the part-level requirement.
Crystallization behavior dictates the minimum cooling time before ejection. Differential scanning calorimetry to ISO 11357-3:2018 is used to measure the crystallization peak temperature of isotactic polypropylene. Non-nucleated PP homopolymer typically exhibits a crystallization peak between 110°C and 118°C; nucleated grades may shift this peak to 120–130°C. A higher crystallization temperature reduces the time the part must remain in the mold before it develops enough solid-state modulus for ejection. The exact nucleation package in Kingfa PP-92989 must be confirmed against the lot technical datasheet, but homopolymer grades in this segment commonly contain nucleating agents to improve stiffness, reduce haze slightly, and shorten cooling time.
Nucleation also influences shrinkage anisotropy. Larger, slower-formed spherulites produce more differential shrinkage between flow and transverse directions, which increases warpage risk in flat parts. A nucleated homopolymer can produce finer spherulitic morphology and more uniform shrinkage, but the process still requires balanced filling and cooling. Hot spots near gates, weld lines, or insert bosses can create local dimensional variation even when the material is highly nucleated. Mold-flow simulation inputs for PP-92989 should therefore include measured no-flow temperature, specific heat capacity, and crystallization temperature rather than generic PP data. Weld-line integrity can also be weaker in high-flow homopolymers because high orientation and rapid solidification at knit lines reduce molecular interdiffusion; this is evaluated by tensile testing at the weld line under ISO 527-2:2012 or by instrumented impact testing of the actual molded component.
| Property | Test Method | High-Flow PP Homopolymer Class | PP Random Copolymer Class | PP Impact Copolymer Class |
|---|---|---|---|---|
| Melt mass-flow rate at 230°C/2.16 kg | ISO 1133-1:2022 | 30–100 g/10 min | 10–40 g/10 min | 5–60 g/10 min |
| Density | ISO 1183-1:2019 | 0.90–0.91 g/cm³ | 0.89–0.91 g/cm³ | 0.89–0.92 g/cm³ |
| Tensile yield stress | ISO 527-2:2012 | 30–40 MPa | 22–30 MPa | 20–28 MPa |
| Flexural modulus | ISO 178:2019 | 1500–1900 MPa | 900–1400 MPa | 1000–1600 MPa |
| Notched Izod impact at 23°C | ISO 180:2023 | 2–5 kJ/m² | 5–12 kJ/m² | 10–50 kJ/m² |
| Heat deflection temperature at 0.45 MPa | ISO 75-2:2013 | 100–115°C | 85–100°C | 90–105°C |
| Molding shrinkage after 48 h | ISO 294-4:2018 | 1.2–2.0% | 1.0–1.8% | 1.2–1.8% |
The values in the table are class-typical ranges for unfilled polypropylene injection-molding grades and are not grade-specific certificates for PP-92989. Published data for this specific configuration is limited in public sources; the Kingfa technical datasheet and production-lot certificate of analysis must be used for tolerance calculations, mold-filling simulation, and regulatory submissions. The table is nevertheless useful for resolving selection conflicts: when low-temperature impact is required, an impact copolymer is normally selected; when contact clarity is required, a random copolymer is normally selected; when the highest stiffness-to-flow balance is required in an opaque thin-wall molding, an unfilled high-flow homopolymer such as PP-92989 is a candidate.
In low-temperature distribution below 5°C, unfilled polypropylene homopolymer shows a sharp reduction in impact strength, and frozen-food packaging or cold-climate consumer goods may require an impact copolymer or a random copolymer with a clarified additive package. The converter should evaluate part-level drop impact using the actual article geometry rather than substituting material class data for performance testing.