| HS Code | 734733 |
| Density | 0.90 g/cm³ |
| Melt Flow Rate 230 C 2 16 Kg | 35 g/10 min |
| Tensile Strength At Yield | 24 MPa |
| Elongation At Break | 10% |
| Flexural Modulus | 1100 MPa |
| Notched Izod Impact Strength 23 C | 5 kJ/m² |
| Heat Deflection Temperature 0 45 Mpa | 100 °C |
| Vicat Softening Temperature | 150 °C |
| Rockwell Hardness | R80 |
| Molding Shrinkage | 1.5% |
| Flammability Rating | HB |
| Processing Temperature | 200-230 °C |
| Mold Temperature | 40-60 °C |
As an accredited Kingfa PP-BX3500,PP Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-BX3500 PP Copolymer is supplied in 25 kg moisture-resistant woven bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | Kingfa PP-BX3500 PP Copolymer loaded in a 20-foot FCL, palletized in 25 kg bags, shrink-wrapped and secured for shipment. |
| Shipping | Kingfa PP-BX3500 PP Copolymer is generally shipped as non-hazardous thermoplastic pellets in moisture-proof 25 kg bags or jumbo bags on pallets. Keep dry, away from direct sunlight and heat. Follow the SDS and applicable local transport regulations. |
| Storage | Kingfa PP-BX3500, PP Copolymer should be stored in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizing agents. Use proper grounding to control static, maintain clean storage, follow the manufacturer’s SDS and local regulations, and store away from food and drink. |
| Shelf Life | Typically 24 months when stored unopened in original packaging in a cool, dry, ventilated area away from sunlight and heat. |
Low-fogging door-panel lower substrates are injection-moulded from PP-BX3500 as an unfilled impact copolymer where the ethylene-propylene rubber phase retains ductility at cabin extremes. The moulding window on a large-format direct-clamp press of 1,200 t to 1,800 t clamp force uses barrel temperatures from 210 °C at the feed throat to 235 °C at the nozzle, hot-runner manifold set points between 220 °C and 235 °C, and steel-tool surface temperatures between 30 °C and 50 °C. Injection velocities of 80 mm/s to 140 mm/s are maintained through valve-gated direct drops to prevent hesitation in ribbed map-pocket bosses. Filling pressure normally remains below 110 MPa, with switch-over at 95–98 % volumetric fill and packing at 35–50 MPa for 4–8 s. When the part is subjected to DIN 75201-B fogging, the condensate limit is commonly set below 1.2 mg/10 g, which excludes excessive talc masterbatch and requires a stabiliser package of 0.20–0.35 wt% phenolic antioxidant and 0.10–0.20 wt% acid scavenger. Low-temperature impact qualification follows ISO 180/1A notched Izod at −30 °C, with many interior lower-trim specifications requiring a minimum of 3.5 kJ/m²; if the measured value drops below this threshold, the gate vestige and rib-to-wall ratio are reduced before filler is added. Dimensional stability is checked after 24 h at 80 °C using ISO 2818 specimen preparation and ISO 62 water absorption at 23 °C, with warpage acceptance typically held within 0.8 mm across a 600 mm span. Mould release is controlled with 0.2–0.4 wt% ethylene bis-stearamide; above 0.6 wt%, risk of surface bloom increases.
Impact retention in a front-load washer outer tub fails predominantly at weld lines formed around the bearing hub and balancing-ring anchor ribs, where plate-like talc orientations act as planes of low crack resistance. When PP-BX3500 is extended with 20–30 wt% talc masterbatch to raise ISO 178 flexural modulus from approximately 1,200 MPa to 2,200–2,600 MPa, the notched Izod retention at a weld line can drop to 40–55 % of the bulk value measured at 23 °C; at −20 °C, scatter widens and minimum values may approach 3.0 kJ/m² under ISO 180/1A. The processing conflict is thermal: a higher melt temperature of 240 °C improves weld-line healing by delaying crystallisation, but excessive residence time in the barrel above 245 °C accelerates peroxide decomposition in the coupling package and causes yellowing. A mould temperature of 60 °C, rather than the lower 30 °C used for fast cycling, shifts skin-core morphology and improves weld-line Izod by 10–20 %, although cycle time increases by 10–15 s. Injection velocity across the weld line should exceed 120 mm/s; short-shot trials with sequentially opened valves are used to confirm that the flow fronts merge while still above the crystallisation onset measured by DSC at 10 °C/min cooling. Packing pressure is limited to 30–40 MPa because higher pressure compresses the talc-rich weld plane and intensifies notch sensitivity. The assembled tub must pass ISO 6603-2 puncture at 23 °C and no-load deformation after 1,000 h hot-water exposure at 60 °C; published data for the specific BX3500 tub configuration is limited, so each tool requires an initial short-shot mapping study.
Lead-acid battery containers with side-wall thickness between 1.8 mm and 2.5 mm impose a narrow balance between flow length, pin-hole resistance, and acid-induced stress-cracking. In multi-cavity hot-runner production, PP-BX3500 is processed at melt temperatures of 210–230 °C, and the MFR determined under ISO 1133-1:2022 at 230 °C with 2.16 kg load is typically expected to remain in the 8–20 g/10 min range for this application. If the MFR is above 20 g/10 min, the amorphous tie chains are shorter and the container may develop micro-cracks after prolonged contact with sulfuric acid at 60 °C; if the MFR is below 8 g/10 min, short shots and warping appear in thin-wall tools with 6–12 cavities. Injection pressure at the material inlet is set from 90 MPa to 120 MPa, with holding pressure between 50 MPa and 70 MPa and cooling times of 25–45 s depending on wall thickness. Mould temperature is kept below 30 °C to control cycle time, but an excessively cold mould below 15 °C produces flow marks around rib intersections and lowers weld strength. Weld lines at handle windows and terminal-post webs are checked with an air-leak test at 0.03 MPa and a drop test after conditioning at −10 °C. Compliance is assessed under RoHS 2011/65/EU Annex II, REACH SVHC, and UL 94 HB according to IEC 60695-11-10 at 3.0 mm; the unmodified grade is not suitable for a V-2 or V-0 enclosure claim without flame-retardant recompounding.
In warehouse stacking trials, crates moulded from PP-BX3500 are loaded to 800–1,200 kg per pallet position and held for 6–12 months at ambient temperatures that reach 40 °C in unventilated upper racks. Under these conditions, creep modulus rather than short-term stiffness controls the allowable rib design, and the relevant measurement is ISO 899-1:2017 tensile creep or ASTM D2990 compressive creep on specimens cut from the side wall and corner ribs. The unfilled impact copolymer has sufficient room-temperature notched Izod, but its long-term load resistance at 40 °C is lower than a homopolymer of equivalent short-term modulus; therefore, compounders add 10–20 wt% calcium carbonate masterbatch or 8–15 wt% talc to raise creep resistance at a cost in cold impact. Wall thickness is held at 3.5–5.0 mm, rib pitch at 25–35 mm, and rib-to-wall ratio at 0.5:1 to avoid sink marks across the top surface of the pallet deck. On a 1,500–2,200 t toggle machine, barrel temperatures are profiled from 200 °C to 225 °C, mould temperature is set between 20 °C and 40 °C, and total cycle time is 45–70 s. Gate-freeze time is confirmed by part-weight stabilisation rather than look-up tables because recycled content ratios above 30 wt% can shift the crystallisation plateau and increase the required packing time by 3–7 s. β-nucleation at 0.05–0.10 wt% can reduce warpage in the deck and raise impact strength, but sustained load testing at 40 °C is required before acceptance because β-phase crystals may soften earlier than α-phase if the part is not annealed. Dimensional control after 48 h at 40 °C is referenced to the crate footprint; stack interlock features and pallet-jack openings are measured with a coordinate caliper against a tolerance of ±1.5 mm.
Outdoor power-tool housings moulded from PP-BX3500 require ultraviolet stabilisation and rib-corner impact performance under intermittent loads. The compound is prepared with 1.0–2.0 wt% carbon black masterbatch or 0.5–1.0 wt% HALS-based UV stabiliser for non-black colours, and the mixture is injection-moulded at melt temperatures from 200 °C to 230 °C with a mould surface temperature of 20–50 °C. Gate land length is set to 0.8–1.2 mm and runner diameter to 6–8 mm in cold-runner tools; hot-runner drops above 2.5 mm diameter may create visible gate blush on textured surfaces. UV resistance is evaluated according to ISO 4892-2 cycle 1 for 1,000 h, and colour shift below 3.0 Δb* is commonly required for commercial power-tool housings; surface micro-cracking after 500 h is a rejection criterion. Rib corners and motor-mount bosses are sized with a nominal wall-to-rib ratio of 0.6:1 to prevent sink while retaining drop resistance. Charpy notched impact per ISO 179-1/1eA at −10 °C is used because many outdoor tools are assembled in cold warehouses; a value below 4.0 kJ/m² in a ribbed moulded specimen requires increasing the ethylene-propylene rubber content or reducing filler, not merely increasing part wall thickness. Internal lubricants such as ethylene bis-stearamide at 0.3–0.5 wt% assist ejection from deep battery cavities, but concentrations above 0.6 wt% can cause surface streaking after 200–300 cycles due to mould deposit. The material is not inherently flame-retardant; if the tool housing must meet a V-2 rating, the specific UL 94 designation must be confirmed on a moulded plaque because unreinforced PP-BX3500 typically remains in the HB class at 3.0 mm.
Underbody wheel-arch liners are injection-moulded as semi-structural shells with nominal wall thickness between 2.0 mm and 2.8 mm; PP-BX3500 is selected for the balance of cold-crack resistance and stiffness after the addition of 5–15 wt% talc masterbatch or 10–20 wt% calcium carbonate. The tool is a large two-cavity or four-cavity mould with sequential valve gating to move the weld line away from the high stone-impact zone near the tyre profile. Melt temperature is held between 220 °C and 240 °C, mould temperature between 25 °C and 50 °C, and filling is completed with injection speeds above 100 mm/s to avoid hesitation in the draw depth that can exceed 120 mm. The cold-impact requirement is typically notched Izod ISO 180/1A at −20 °C or multiaxial ISO 6603-2 puncture at −20 °C; stone-impact is evaluated by a gravelometer procedure such as DIN EN ISO 20567-1, where chipping depth and delamination are recorded after 10 kg of chilled cast shot. Resistance to de-icing salt is assessed by immersion in 10 wt% NaCl solution at 60 °C for 72 h, followed by a visual check for surface whitening; the acid scavenger in the stabiliser package must be maintained at 0.10–0.20 wt% because chloride exposure accelerates oxidation at the talc-polymer interface. Clamp force on the press is generally 1,000–1,500 t, and cycle time is 50–70 s; packing pressure is limited to 25–35 MPa on deep-draw sections to reduce stress at the gate. If the liner carries an OEM approval, fogging and odour limits are typically less strict than cabin interior parts, but REACH Annex XVII restrictions on PAH and heavy metals still apply to the finished article.
For micromobility battery cradles and charger base housings, the use of unmodified PP-BX3500 is restricted by the flame-retardant class achievable on thin-walled parts. In its untreated state the grade is suitable only for enclosures where IEC 60695-11-10 UL 94 HB at 3.0 mm is acceptable, because thin sections below 1.5 mm can exhibit extended afterflame or burning drips. When a V-2 or V-0 claim is required, downstream compounders blend the copolymer with an intumescent ammonium polyphosphate-based package at 25–35 wt%, which increases melt viscosity and reduces notched impact by 30–50 % relative to the unfilled base; the exact retention depends on the flame-retardant particle size and coupling chemistry. The processing window then narrows to 190–215 °C at the nozzle because excessive residence time above 220 °C can trigger early foaming from the intumescent system and deposit a rough white residue on the vent and gate areas. Mould temperature is set at 50–70 °C to improve skin formation, and the required packing pressure is typically 40–60 MPa. Impact-critical snap-fit bosses and cradle latch arms are gated at the thick section and use 0.8:1 wall-to-rib ratios to prevent localised brittleness in the flame-retarded matrix. Compliance for lithium-ion auxiliary circuits is assessed against the enclosure flammability clause of the applicable end-product standard, but published data for this specific BX3500 flame-retarded configuration is limited; each formulation must be re-qualified on moulded plaques rather than relying only on resin supplier datasheets. Pre-drying at 80 °C for 2–3 h is required only when moisture-exposed regrind exceeds 0.10 wt% water content, because polypropylene is not hydrolytically sensitive but wet filler packages reduce part gloss and increase splay.
Competitive Kingfa PP-BX3500,PP Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-BX3500, PP Copolymer is a propylene-based copolymer supplied by Kingfa Sci & Tech Co., Ltd. The product designation separates the material from homopolymer polypropylene grades and from compounded polyolefin elastomers, but the sequence distribution of the copolymer fraction is not specified by the short trade name. Grade-specific values for melt flow rate, tensile yield stress, flexural modulus, notched impact strength, heat deflection temperature, and density must therefore be obtained from the supplier’s lot-specific certificate of analysis and technical datasheet. Published data for this specific configuration is limited; the process and property notes below therefore address the general class of propylene-ethylene copolymer resins and production-scale moulding practice. Any class-level value in this document is not a substitute for PP-BX3500 release testing.
At the molecular level, propylene copolymer grades contain an ethylene comonomer fraction that disrupts the crystallinity of isotactic polypropylene. In homopolymer, regular chain packing yields higher tensile yield stress and flexural modulus; these are typically measured by ISO 527-1:2019 and ISO 178:2019. In copolymers, the comonomer reduces crystalline order, which lowers short-term stiffness but can raise notched impact strength and low-temperature ductility. The impact response is commonly assessed by ISO 179-1/1eA Charpy or ISO 180 Izod methods; a ductile-to-brittle transition temperature is often reported below 0°C for impact-modified architectures. For the BX3500 designation, the exact comonomer content and rubber particle size distribution must be confirmed from the manufacturer, because the designation alone does not identify whether the product is a random copolymer or an impact copolymer.
The following table summarises class-level property bands for propylene-ethylene copolymers from publicly available PP literature; the values are not grade-specific to PP-BX3500.
| Property | Test standard | PP copolymer class band |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | 2–50 g/10 min |
| Density | ISO 1183-1:2019 | 0.89–0.91 g/cm³ |
| Tensile yield stress | ISO 527-1:2019 | 20–30 MPa |
| Flexural modulus | ISO 178:2019 | 800–1,500 MPa |
| Notched Charpy impact at 23°C | ISO 179-1/1eA | 5–60 kJ/m² |
| Heat deflection temperature at 0.45 MPa | ISO 75-2:2013 | 50–100°C |
| Vicat softening temperature A50 | ISO 306:2022 | 120–155°C |
Beyond short-term mechanical properties, the copolymer fraction also changes shrinkage and warpage. Moulding shrinkage is normally determined on ISO 294-3:2020 plaques; class-level total shrinkage for PP copolymers is often in the 1.0%–2.0% band, with less uniform shrinkage in filled or highly nucleated variants. Because the BX3500 grade-specific filler content is not public, tooling designers should obtain the supplier’s measured parallel and perpendicular shrinkage values before cutting steel. Weld-line strength in impact copolymers is influenced by the rubber phase and the melt front temperature; weld-line impact retention is assessed by comparing notched Charpy values of a weld line against the base resin, but no universal acceptance limit applies.
Because the melt viscosity of PP-BX3500 is not assumed from the copolymer designation, processing parameters should be derived from the melt flow rate measured under ISO 1133-1:2022 at 230°C and 2.16 kg. If the lot exhibits a medium flow rate in the 5–25 g/10 min band, barrel set-points in injection moulding are commonly initiated between 200°C and 250°C, with mould temperatures from 20°C to 60°C. The copolymer fraction tends to produce a more pseudoplastic melt than a homopolymer of equal melt flow rate, as shown by capillary rheometry according to ISO 11443:2021; this can increase apparent flow length in thin-wall tooling. However, spiral-flow data or cavity-pressure studies on the specific hot-runner configuration are required to confirm filling behaviour. Polypropylene copolymers in this class do not require predrying under normal dry storage. If condensed moisture is suspected after transfer from cold storage at RH > 60%, a hopper dryer set at 80°C for 2 h is a typical handling precaution; drying above 100°C for extended periods is avoided because it can accelerate additive migration or oxidative changes.
On production-scale compounding lines, PP copolymers are typically melt-blended with color concentrates and processing stabilizers in co-rotating twin-screw extruders with 36:1 to 48:1 L/D and modular screw segments. The specific energy input is controlled by screw speed and throughput; for PP copolymers, melt temperatures above 260°C are normally avoided to prevent chain scission and discoloration. Batch-to-batch variance in melt flow rate and pellet temperature entering the feed throat can shift the plastication profile along the barrel, so screw torque, die pressure, and melt temperature at the die are monitored as indicators of lot-to-lot uniformity. When recycled PP copolymer regrind is introduced, the addition level is typically limited to maintain impact performance; any proposed regrind ratio for PP-BX3500 should be validated by notched impact testing according to ISO 180 on moulded plaques from the actual production run.
Incoming inspection of PP copolymer lots usually records the supplier’s melt flow rate and retains moulded plaques for density and impact checks according to ISO 1183-1:2019 and ISO 179-1/1eA. A shift in melt flow rate of more than ±10% from the approved baseline may require barrel temperature compensation or hold-pressure adjustment. Because the BX3500 supplier-specific tolerance is not publicly available, the lot qualification protocol should be copied from the supplier’s certificate of analysis and from the moulder’s production history.
Mass production of PP copolymer components on injection moulding machines requires the clamp force to be matched to the projected area of the cavity and the peak cavity pressure during packing. A conservative starting point for polypropylene copolymers is 0.35–0.70 kN/cm² of projected mould area, with the lower half used for larger flow-length ratios and the upper half reserved for thin-wall parts with high packing pressures. Screw back pressure normally does not need to exceed 5–15 bar, as excessive shear can generate frictional heat and alter the melt residence time. Injection speed is set by cavity geometry; for PP copolymers, medium-to-high injection speeds are often required to reduce premature freeze-off in walls below 1.5 mm. Holding pressure and time are then adjusted after injection using cavity-pressure sensors and gate-seal studies. Processors evaluating PP-BX3500 should replace the generic values above with the recommendations in the Kingfa moulding guide, because the optimal set-points depend on the lot melt flow rate and the hot-runner manifold temperature uniformity.
When a manufacturer substitutes PP-BX3500 for a random copolymer or an elastomer-modified polypropylene, the comparative performance cannot be inferred from the designation alone. Random copolymers typically have higher optical clarity and lower haze values than impact copolymers, but their low-temperature impact strength is generally lower unless additional nucleation or impact modification is used. Impact copolymers provide a dispersed rubber phase that improves energy absorption but reduces gloss and flexural modulus; these trade-offs are measured by ISO 1183-1:2019 density, ISO 178:2019 flexural modulus, ISO 179-1/1eA Charpy impact, and ISO 2813 gloss, respectively. The BX3500 designation should be cross-referenced with the supplier’s injection-moulded plaque data to determine whether it is formulated for high-impact, high-gloss, or reduced-warp applications. In the absence of such data, a head-to-head moulding trial on the target tool is the only reliable method for comparing cycle time, shrinkage, and part weight stability.
Electrical enclosures with wall stock below 1.5 mm impose a combination of flow-length, flame-retardant, and impact-resistance requirements. If PP-BX3500 is proposed for such parts, the finished component must be qualified under the relevant end-product standards, including but not limited to IEC 60695-2-11 or IEC 60695-2-12 for glow-wire flammability, and IEC 60112 for comparative tracking index, where applicable. The copolymer feedstock alone does not confer flame-retardant classification; any ignition-resistance formulation is achieved through additives that must be disclosed on the supplier’s safety data sheet. Production-scale trials should record melt temperature, hot-runner tip temperature, injection velocity, hold pressure, and gate-seal time. Shrinkage after 24 h at 23°C and 50% RH is typically measured in accordance with ISO 294-4:2018; PP copolymers generally exhibit anisotropic shrinkage of approximately 0.8%–1.5%, depending on part thickness, weld-line position, and mould temperature. Published data for this specific configuration is limited, so the supplier’s gate location and shrinkage recommendations should control.
Thermal ageing is a separate qualification axis. For PP copolymers, oxidative stability is commonly characterized by oxidation induction time under ISO 11357-6:2018 or by long-term heat ageing in forced-air ovens according to ISO 4577. Any claim that PP-BX3500 is suitable for sustained hot-air exposure above 90°C should be supported by supplier data, because stabilizer content and molecular architecture determine the failure envelope. Published data for this specific configuration is limited, and the absence of a supplier-applied heat stabilization package cannot be excluded from the trade designation.
Regulatory compliance for Kingfa PP-BX3500, PP Copolymer should be verified through the supplier’s certificate of compliance and not assumed from the polymer class. Polypropylene homopolymers and copolymers are frequently evaluated for food-contact suitability under FDA 21 CFR 177.1520 and for European food-contact frameworks under Regulation (EU) No 10/2011; however, PP-BX3500 is not automatically compliant with those requirements unless the supplier provides written confirmation covering the specific packaging or repeated-use condition. The grade may also be subject to RoHS Directive 2011/65/EU and REACH Regulation (EC) No 1907/2006; compliance with RoHS requires supplier documentation showing restricted substance concentrations below 0.1 wt% for lead, mercury, hexavalent chromium, polybrominated biphenyls, and certain polybrominated diphenyl ethers, and below 0.01 wt% for cadmium in homogeneous materials. For automotive applications, the material may be supplied with International Material Data System or supplier material data sheets but not necessarily with full OEM approval; end-user validation remains required.
| Parameter | Standard or regulation | Typical acceptance criterion |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | Supplier’s specified tolerance |
| Density | ISO 1183-1:2019 | 0.89–0.91 g/cm³ |
| Tensile yield stress | ISO 527-1:2019 | Supplier’s specified minimum |
| Notched Charpy impact | ISO 179-1/1eA | Supplier’s specified minimum |
| RoHS restricted substances | RoHS Directive 2011/65/EU | Lead < 0.1 wt%; cadmium < 0.01 wt% |
| REACH SVHC notification | REACH Regulation (EC) No 1907/2006 | Article 33 if > 0.1% w/w |