| HS Code | 526059 |
| Product Name | Kingfa PP-BX3900 |
| Polymer Type | PP Copolymer |
| Manufacturer | Kingfa |
| Processing Method | Injection Molding |
| Density | 1.03 g/cm³ |
| Melt Flow Rate | 10 g/10 min (230°C/2.16 kg) |
| Tensile Strength At Yield | 25 MPa |
| Elongation At Break | 20% |
| Flexural Modulus | 1200 MPa |
| Notched Izod Impact Strength | 5 kJ/m² (23°C) |
| Heat Deflection Temperature | 100°C (0.45 MPa) |
| Vicat Softening Temperature | 150°C |
| Flame Retardancy | V-0 |
| Color | Natural |
As an accredited Kingfa PP-BX3900,PP Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-proof woven bags; Kingfa PP-BX3900 PP Copolymer pellets packaged for industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL loaded with Kingfa PP-BX3900 PP copolymer resin, 25 kg bags, palletized, shrink-wrapped, and securely stowed for export. |
| Shipping | Kingfa PP-BX3900, PP Copolymer is a non-hazardous polypropylene copolymer resin, not regulated for transport. Ship in sealed, moisture-resistant bags or octabins. Store dry, away from heat, sunlight, and ignition sources; handle with normal PPE and prevent pellet spillage. |
| Storage | Store Kingfa PP-BX3900 in a cool, dry, well-ventilated area in closed original packaging. Keep pallets off the floor and away from direct sunlight, heat, flames, and strong oxidizers. Prevent moisture, dust, and contamination. Maintain stable temperature and avoid prolonged UV exposure. Use appropriate PPE and good housekeeping; avoid generating dust during handling. Do not store near ignition sources or incompatible materials. |
| Shelf Life | Kingfa PP-BX3900 shelf life is approximately two years when stored dry, cool, ventilated, and protected from direct sunlight in original packaging. |
Injection moulding of lower B-pillar substrates in passenger cars uses PP-BX3900 as the primary heterophasic polypropylene copolymer component where hinge points, clip towers, and demoulding pulls demand low-temperature ductility. Compliance for interior trim produced from compound containing 78 wt% PP-BX3900, 12 wt% 5 µm talc, 7 wt% POE elastomer, 2 wt% carbon black masterbatch, and 1 wt% antioxidant package is anchored to VDA 278:2011 VOC emission limits, VDA 270:2018 odour classification below 3.0, and GB 8410-2006 burn-rate testing on 3 mm plaques. Mechanical acceptance is measured by notched Charpy impact under ISO 179-1/1eA at -30 °C and flexural modulus under ISO 178:2019. The downstream process is injection moulding on a 22:1 L/D single-flight screw with distributive mixing elements and a clamp force not exceeding 1,200 kN; barrel zones are held at 180/200/220/230/230 °C, the tool at 35 °C, fill pressure at 85 MPa, hold pressure at 50 MPa, hold time at 6 s, and cooling at 16 s. Pre-drying at 80 °C for 2 h is required when ambient relative humidity exceeds 60 %. Terminal parts include B-pillar lower trim, door scuff plates, map pocket backing boards, and luggage-tonneau side trims. The operational boundary is class-A soft-touch surfaces: without secondary slush skin or film lamination, scratch resistance under PV 3952 is insufficient for high-white PVC/ABS migration environments.
Painted bumper fascias impose a different set of constraints because adhesion promotion occurs after moulding and any migratory additive can lift subsequent coating layers. A typical formulation contains 65 wt% PP-BX3900, 20 wt% EPDM/POE impact modifier, 12 wt% talc with D50 5 µm, 2 wt% UV masterbatch, and 1 wt% carbon black. Regulatory compliance references ECE R42 low-speed impact performance for front and rear protection systems and GB 17354-1998 for the corresponding Chinese market evaluation; painted surface adhesion is validated by ISO 2409:2020 cross-cut with a maximum 1 rating and weathering by ISO 4892-2:2013 under 1,000 h xenon-arc exposure without gloss retention below 70 %. The material is first compounded on a twin-screw extruder with 40:1 L/D and side-fed talc downstream of the melting zone to limit fibre attrition; compound pellets are then injection moulded with a clamp force of 20,000 kN, sequential valve gates, melt temperature 230–250 °C, tool temperature 25–40 °C, and fill time 2.5–4.0 s. A chlorinated polyolefin adhesion promoter is applied at 2–4 g/m² wet film thickness over a plasma or flame-treated surface before coloured basecoat and clearcoat. Terminal products are front bumper fascias, rear bumper fascias, lower grille surrounds, and rocker panel covers. The critical limitation is mould-release migration: if external release agent is used, a methyl ethyl ketone or isopropanol wipe must remove residual hydrocarbons before adhesion promotion or the cross-cut rating deteriorates to 3 or worse within 500 h of humidity exposure.
For washing machine outer tubs, the process window shifts because talc-filled heterophasic PP copolymer exhibits rapid viscosity increase if melt temperature falls below 200 °C and the screw has no distributive mixing reserve. The compound contains 68 wt% PP-BX3900, 22 wt% 5 µm talc, 7 wt% POE elastomer, 2 wt% antistatic masterbatch, and 1 wt% processing aid. Compliance is directed by IEC 60335-1:2020 clause 30.2.1 glow-wire testing at 750 °C for parts above 1.5 mm thickness, UL 94 HB for horizontal burn classification, and IEC 60695-11-5:2016 for glow-wire apparatus calibration. The injection moulding process uses a twin-platen machine with clamp force 15,000 kN, a screw L/D of 23:1, zones set at 180/200/220/230/230 °C, tool temperature 45 °C, injection speed 60 mm/s, and hold pressure 65 MPa. The screw must include shallow compression depth and at least 4 rows of mixing pins after the feed zone; otherwise unmelted talc agglomerates produce microvoids visible on the outer tub sealing face after 2,000 service cycles. Terminal parts are outer tub bases, spin basket bases, and balance ring supports for 6.5–12 kg top-load washing machines. Published data for this specific grade configuration in long-cycle wet-dry thermal shock is limited; a validation protocol using 85 °C water immersion and -20 °C air shock over 500 cycles is recommended before release for hot-water areas.
Because PP-BX3900 retains impact strength below 0 °C, it appears in indoor low-voltage wiring distribution boxes where covers are removed repeatedly during maintenance and brittle fracture would expose live terminals. A weather-stabilised electrical enclosure formulation uses 81 wt% PP-BX3900, 14 wt% talc, 3 wt% UV stabiliser, and 2 wt% titanium dioxide. Compliance is defined by IEC 60670-1 for household and similar fixed electrical installations, including clause 10.2.4 mechanical impact at -5 °C, and the material is limited to enclosures where creepage and clearance distances are fixed by the part design rather than by comparative tracking index; CTI under IEC 60112:2020 is typically below 600 V. The parts are injection moulded in hot-runner 8-cavity tools with a clamp force of 3,500 kN, melt temperature 230 °C, mould temperature 40 °C, cycle time 28 s, and screw L/D 20:1. Terminal products include surface-mounted wiring duct boxes, cable branching boxes, meter enclosure inner brackets, and consumer unit internal partitions. The operational boundary is explicit: this neat PP copolymer grade is not suitable for enclosures requiring UL 94 V-0 at 1.5 mm or for live-part supports requiring 850 °C glow-wire without additional flame-retardant modification.
Drop-impact performance at -20 °C is the controlling design criterion for returnable logistics crates because wall cracking after forklift misalignment creates contaminant ingress points in dairy and beverage distribution. The crate compound contains 87 wt% PP-BX3900, 8 wt% EPDM, 3 wt% UV masterbatch, and 2 wt% processing stabiliser. Mechanical compliance uses ISO 8611-1:2011 for pallet load rating and ISO 179-1/1eA Charpy impact at -20 °C; tensile properties are measured by ASTM D638-14 at 23 °C. The injection moulding process uses a low-melt-temperature profile of 180–200 °C to reduce crystallisation shrinkage in thick ribs, mould temperature 20 °C, pack pressure 45 MPa for 10 s, and clamp force 8,000 kN. Terminal products are dairy crates, beverage crates, returnable logistics totes, and ventilated produce crates with open-grid sidewalls. The boundary condition is environmental stress-cracking resistance in detergent-washing tunnels: the material should not be exposed to hot alkaline agents above 60 °C for more than 30 min per cleaning cycle, and outdoor UV exposure without a stabilised masterbatch is limited to 2,000 h under ISO 4892-2:2013 before embrittlement.
In front and rear wheel arch liners, the compound must survive stone-chip abrasion, wet-road salt exposure, and low-temperature flexing without transferring stress to the body-in-white mounting points. The formulation uses 72 wt% PP-BX3900, 16 wt% EPDM/POE, 10 wt% 5 µm talc, and 2 wt% UV masterbatch. Compliance is anchored to ISO 20566:2020 for stone-chip resistance of metal and plastic substrates and ISO 6270-2:2017 for humidity resistance; salt spray exposure is assessed under ISO 9227:2017 for 1,000 h with no base-metal corrosion transfer. Injection moulding is performed using conformal cooling channels in the mould insert to keep the tool at 15 °C, melt temperature 230 °C, clamp force 18,000 kN, fill time 3.2 s, and pack pressure 60 MPa. Terminal products are front wheel arch liners, rear wheel arch liners, upper baffle plates, and wheel-house closeout panels. The operational limit is that these parts are not direct load-bearing underbody structures: if a friction-drilled rivet or threaded insert is used, the collapse strength at 23 °C should be revalidated on the exact boss geometry because talc orientation at the weld line can reduce first-load retention by more than 15 %.
Competitive Kingfa PP-BX3900,PP Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Commercial designation Kingfa PP-BX3900, PP Copolymer identifies a polypropylene copolymer grade in the Kingfa polypropylene portfolio. Public English-language technical literature for this exact grade is not comprehensive; therefore product identity is established through manufacturer documentation, while property relationships are discussed at the level of unfilled polypropylene impact copolymers where no product-specific release values are available. The designation “BX3900” is a manufacturer code and is not an ISO 1043-1:2011 grade designation. It does not encode a melt mass-flow rate value in g/10 min under ISO 1133-1:2022 and should not be interpreted as such.
From a material classification standpoint, a PP copolymer differs from a PP homopolymer by inclusion of a comonomer or an elastomeric phase. Under ISO 1043-1:2011, polypropylene copolymers are designated PP-C, while ethylene-containing impact copolymers may be described as heterophasic PP compounds. The PP Copolymer description in Kingfa PP-BX3900 indicates that the product is not a homopolymer. The microstructural consequence is a reduction in crystalline order relative to homopolymer PP; this lowers room-temperature flexural modulus and yield stress but extends the failure mode under notched impact conditions at low temperature. The exact balance depends on the rubber particle size distribution and interparticle distance, which are controlled by polymerisation and compounding stages.
Product-specific datasheets for polypropylene copolymer grades normally report the following property categories. The test conditions listed are the ISO methods used for PP impact copolymer release documentation. Lot-specific values for Kingfa PP-BX3900 should be obtained from the supplier’s certificate of analysis; they are not reproduced here because public English-language values are insufficiently source-verifiable.
| Property | Test method | Test conditions | Specimen type |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 230 °C, 2.16 kg | Extruded granules |
| Density | ISO 1183-1:2019 | 23 °C, immersion method | Moulded plaque |
| Tensile yield stress | ISO 527-2:2012 | 50 mm/min, type 1A | Injection-moulded multipurpose specimen |
| Tensile strain at yield | ISO 527-2:2012 | 50 mm/min | Injection-moulded multipurpose specimen |
| Flexural modulus | ISO 178:2019 | 2 mm/min, span 64 mm | 80 mm × 10 mm × 4 mm |
| Notched Izod impact strength | ISO 180:2023 | 23 °C and -30 °C, notch A | 80 mm × 10 mm × 4 mm |
| Heat deflection temperature | ISO 75-2:2013 | 0.45 MPa and 1.8 MPa | 80 mm × 10 mm × 4 mm |
| Vicat softening temperature | ISO 306:2022 | A50 and B50 | Injection-moulded specimen |
| Mould shrinkage | ISO 294-4:2018 | parallel and perpendicular flow after 24 h at 23 °C | 60 mm × 60 mm × 2 mm |
Conditioning of specimens before mechanical testing is governed by ISO 291:2008, usually 23 °C and 50% relative humidity for at least 16 h. In lot-release documentation, each value is a statistical average from a defined number of cavity positions; the manufacturer’s data sheet may report typical rather than minimum values. When multiple cavities are used in production tools, cavity-to-cavity variation in injection speed and cooling rate can shift notched Izod results by more than 10%; this is a production-scale consideration rather than a material specification issue.
The melt is characterised by melt mass-flow rate under ISO 1133-1:2022, but capillary or rotational rheometry provides more useful data for process setting. For injection moulding, a screw with L/D ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.5:1 is generally used for PP impact copolymers. The barrel temperature profile should establish a nozzle temperature of 220 °C to 250 °C and a mould temperature of 20 °C to 60 °C. In practice, hot runner systems with externally heated manifolds and valve-gate drops reduce gate-stringing and improve cavity-to-cavity mass balance when moulding PP copolymers of this type. The mould should be run with a mould temperature no higher than 60 °C unless the part geometry contains long flow-length-to-wall-thickness ratios greater than 250:1; elevated mould temperature increases crystallinity and mould shrinkage but can reduce weld-line visibility.
Pre-drying is typically performed at 80 °C for 2 h to 4 h in a desiccant dryer when resin is exposed to ambient moisture above 60% relative humidity. Polypropylene has low hygroscopicity, so water sorption is primarily surface moisture; however, condensation on cold granules in winter can introduce enough water to produce splay at the gate region of moulded parts. Hydraulic injection pressure at the material inlet commonly reaches 70 MPa to 140 MPa, while cavity pressure near the gate for a balanced process should be 20 MPa to 40 MPa. These values are equipment-dependent and must be established through rheological study and short-shot series.
Low-temperature ductility is measured not only by ISO 180:2023 notched Izod but also by instrumented puncture testing according to ASTM D3763 or ISO 6603-2:2023. The instrumented puncture test records total energy, maximum force, and failure mode through the force-displacement curve. For PP impact copolymers, a ductile failure is characterised by a continuous curve with extensive post-maximum displacement, whereas a brittle failure shows a rapid load drop without pronounced yielding. In service-temperature selection, the ductile-to-brittle transition of the moulded part depends on rubber particle size, interparticle distance, and the extent of orientation in the flow direction. A part with high flow-induced orientation may exhibit lower impact toughness perpendicular to flow; this anisotropy is evaluated by cutting specimens from both the parallel-to-flow and cross-flow directions.
The impact resistance of PP-BX3900 should therefore be specified at the minimum service temperature rather than only at 23 °C. Automotive interior components exposed to -30 °C or exterior components exposed to -40 °C require instrumented puncture testing on plaques and prototype parts. For parts with wall thickness below 2.5 mm, side-gated plaques may not represent the orientation state of an actual component; a prototype cavity with the same gate type, melt temperature, and injection velocity should be used.
Compared with a PP homopolymer of equivalent melt mass-flow rate, an unfilled PP impact copolymer exhibits a reduction in tensile yield stress measured by ISO 527-2:2012 and flexural modulus measured by ISO 178:2019. The trade-off is improved notched impact resistance at low temperature and reduced brittle failure under geometric stress concentrations. PP random copolymers, by contrast, have higher transparency and lower haze when measured under ISO 14782:2021, but their impact strength at -20 °C is generally lower than heterophasic impact copolymers. Random copolymers are preferentially used in film, blow-moulded containers, and thin-wall packaging where optical clarity and sealing behaviour dominate.
Relative to talc-filled PP compounds, PP-BX3900 is not a mineral-filled system unless the supplier documentation states otherwise. Talc-filled grades have higher flexural modulus under ISO 178:2019 and lower mould shrinkage under ISO 294-4:2018, but density rises above 1.00 g/cm³ at 20 wt% talc loading, and notched impact may be reduced. Glass-fibre-reinforced PP grades provide higher tensile modulus and heat deflection temperature but introduce anisotropic shrinkage and abrasive wear on screw and barrel surfaces; they also require higher injection pressures and larger gate diameters to avoid fibre breakage. Therefore the selection of PP-BX3900 over these products depends on the required combination of low-temperature impact, ease of moulding, and part mass.
Another comparison is with thermoplastic polyolefin elastomers. Although PP impact copolymers have a heterophasic rubber phase, they are not TPO compounds, which contain higher rubber content or additional elastomer and have much lower flexural modulus and higher low-temperature impact. The distinction is observable in dynamic mechanical analysis: the rubber phase glass transition temperature of a PP impact copolymer appears around -50 °C to -60 °C, whereas the matrix α-transition is above 0 °C. Dynamic mechanical properties can be measured under ISO 6721-11:2019.
The processing window narrows at the extremes of melt temperature and residence time. Melt temperatures above 270 °C promote thermo-oxidative degradation of ethylene sequences in the impact-copolymer phase. The degradation products reduce elongation at break and can generate acrid odour in the moulding shop. Melt temperatures below 200 °C increase viscosity and can result in incomplete filling of thin walls or the formation of unmelted ethylene-rich domains that appear as white gels. Therefore, the nozzle melt temperature is normally maintained between 220 °C and 250 °C for PP impact copolymers; the exact value is adjusted based on screw recovery time and part flow length.
Residence time at melt temperature should not exceed 10 min to 15 min in the barrel. During production interruptions, the barrel should be purged with a low-MFR PP purging compound or the next lot of the same grade. If a machine is idle for more than 20 min, the barrel temperature should be reduced to 150 °C to 180 °C to limit degradation, and the shot should be purged before restart. The use of hot runners with large manifold volumes increases residence time distribution; when hot runner systems exceed 50% of shot volume, the melt residence time exceeds 5 min and the risk of yellowing or brittle failure at weld lines increases.
The mould temperature should be controlled by a thermolator with ±2 °C tolerance. In moulding trials, a mould temperature of 20 °C may give short cycle time but can create high internal stress in thick sections; a mould temperature of 60 °C improves surface appearance but increases cycle time and mould shrinkage. The gate freezes off early if the mould is too cold, resulting in sink marks or vacuum voids. Conversely, if the gate-seal time is shorter than the packing time, a cold gate can induce backflow and variation in part mass.
For regulatory compliance, the manufacturer’s certificate should confirm the status of PP-BX3900 under the relevant instruments. The table below lists the instruments commonly applied to PP copolymers; it does not replace lot-specific compliance certificates.
| Framework / Standard | Identification | Relevance | Typical limit or scope |
|---|---|---|---|
| REACH | EC 1907/2006 | Registration and SVHC reporting | Substances of very high concern restricted under Article 57 |
| RoHS | 2011/65/EU | Electrical and electronic equipment | Lead, mercury, cadmium, hexavalent chromium, PBB, PBDE each 0.1 wt% except cadmium 0.01 wt% |
| Food contact | FDA 21 CFR 177.1520 | Olefin polymer food-contact eligibility | Conditions of use A through H and temperature-based limitations |
| Automotive interior emissions | VDA 277:2018 | Total volatile organic compound emissions | OEM-specific, not set by VDA 277 itself |
| Quality management | IATF 16949:2016 | Defect prevention and process control for automotive suppliers | Lot traceability and PPAP documentation |
In production, a recurring failure mode in PP impact copolymers is brittle fracture at knit lines when the melt temperature at the meeting front is too low. Knit-line strength can be measured by ISO 527-2:2012 on a two-gate tensile bar. In practice, knit-line tensile strength is often 20% to 50% lower than bulk tensile strength; if the part has a constrained geometry, prototype testing is required. Another field failure mode is gloss change and microcracking after exposure to interior cleaners or plasticiser migration. Chemical resistance can be screened by immersion in test liquids under ISO 175:2010; however, actual interior cleaners vary widely by OEM, and a single solvent screening may not capture long-term stress-cracking behaviour.
Published data for the specific configuration of Kingfa PP-BX3900 in high-speed thin-wall injection moulding is limited. A production-scale qualification run on a hybrid injection moulding machine with a clamping force of 2,000 kN to 4,500 kN, a 24:1 L/D screw, and cavity-pressure transducers is a method to establish the shot-to-shot fill pressure curve, gate-seal time, and process capability for the target part. The relevant material release values should be compared against the incoming lot certificate of analysis using the methods in the release test matrix, and the processing window should be verified at both low and high melt temperature settings before production release.