| HS Code | 399373 |
| Density | 0.90 g/cm³ |
| Melt Flow Rate | 21 g/10 min (230°C/2.16 kg) |
| Tensile Strength At Yield | 22 MPa |
| Tensile Elongation At Break | 200% |
| Flexural Modulus | 1000 MPa |
| Notched Izod Impact Strength | 5 kJ/m² (23°C) |
| Heat Deflection Temperature | 90°C (0.45 MPa) |
| Vicat Softening Temperature | 150°C |
| Molding Shrinkage | 1.5% |
| Water Absorption | 0.01% |
| Shore D Hardness | 60 |
| Coefficient Of Linear Thermal Expansion | 1.5E-4 1/°C |
| Ul 94 Flame Rating | HB |
As an accredited Kingfa PP-DN21,PP Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-DN21 PP Copolymer is supplied in 25 kg moisture-proof bags, palletized and stretch-wrapped for safe industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL dry container loaded with palletized 25 kg bags of Kingfa PP-DN21 PP Copolymer, protected from moisture, within net weight limits. |
| Shipping | Kingfa PP-DN21 PP Copolymer is shipped as non-hazardous thermoplastic resin pellets, typically in 25 kg moisture-barrier bags or 500–1000 kg jumbo bags on pallets. Transport in clean, dry trucks or containers at ambient temperature; keep dry, avoid direct sunlight, sharp impacts, and contamination. No special dangerous-goods labeling required. |
| Storage | Store Kingfa PP-DN21 (PP copolymer) in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, ignition sources, and strong oxidizing agents. Keep original containers closed to prevent moisture, dust, and contamination. Avoid prolonged outdoor exposure and excessive stacking. Use grounding/anti-static precautions where dust or fines may accumulate. Follow the supplier SDS and local regulations. |
| Shelf Life | Kingfa PP-DN21 PP Copolymer shelf life: typically 24 months when stored cool, dry, and in sealed original packaging. |
Injection molding of instrument panel substrates and door carrier modules using PP-DN21 as the continuous matrix resin is dominated by the need to balance low-temperature ductility after paint-line oven exposure with the dimensional stability required for two-shot overmolding of soft skins. A production-validated starting formulation for door substrate compounds uses PP-DN21 at 68–78 wt%, talc masterbatch at 15–22 wt%, POE impact modifier at 5–10 wt%, and a phenolic-phosphite antioxidant package at 0.15–0.30 phr. Compounding is carried out on a co-rotating twin-screw extruder with L/D 40:1, barrel profile 180–230 °C, screw speed 350–500 rpm, and side-feeding of talc after the melt seal to reduce screw wear and preserve impingement mixing. Injection molding of door carriers and instrument panel substrates is performed on hydraulic or servo-hydraulic machines with clamp force from 12,000 kN to 25,000 kN; melt temperature is held at 220–250 °C, mold surface temperature at 30–60 °C, and holding pressure at 40–70 bar hydraulic equivalent to minimize sink over ribs and bosses. Compliance for automotive interior use is anchored to ISO 3795:1989 or FMVSS 302 for horizontal burning rate, with a target below 100 mm/min for 3.0 mm plaques; tensile properties are tested per ISO 527-2:2012, flexural modulus per ISO 178:2019, Charpy notched impact at -30 °C per ISO 179-1:2010, and heat deflection temperature per ISO 75-2:2013 at 0.45 MPa. VOC and fogging behavior is evaluated per VDA 278:2011 with typical acceptance ceilings of 100 µg/g VOC and 250 µg/g FOG in most Tier 1 specifications; published grade-specific data for PP-DN21 in every OEM color-matching system is limited. Terminal finished product types include instrument panel substrates, door carrier plates, glove box bins, trunk side trims, and HVAC distribution housings. Processing limitations include pre-drying at 80 °C for 2–4 h when pellets have been stored above 60% RH or after cold-weather ocean freight, because surface condensation produces splay and dimensional variation exceeding 0.4% in long flow paths; hopper dryer dew point below -30 °C is recommended for multi-gate tools where knit-line integrity is critical.
Tub geometries below 3.2 mm wall thickness expose the copolymer to high shear and long flow length during single-point tunnel gating, making weld-line ductility the principal control variable. A typical formulation for washing machine outer tubs uses PP-DN21 at 70–82 wt%, talc masterbatch at 10–18 wt%, POE impact modifier at 8–15 wt%, nucleating agent at 0.05–0.15 wt%, and antioxidant package at 0.2–0.4 phr. Compounding uses a twin-screw extruder with L/D 44:1, vacuum devolatilization at -0.08 MPa gauge, and melt temperature below 240 °C to avoid over-dispersing the rubber phase. Injection molding is performed on accumulator-assisted machines with clamp force from 8,000 kN to 15,000 kN, barrel profile 210–250 °C, injection speed 60–120 mm/s, and mold temperature 40–70 °C via conformal cooling circuits to control warpage of the tub rim. Holding pressure is profiled from 70 bar to 35 bar over 8–12 s; early switch-over from speed to pressure control reduces gate blush and avoids flow hesitation at bottom rib intersections. Compliance for the finished appliance is evaluated under IEC 60335-1 with glow-wire testing per IEC 60695-2-11:2014; material flammability is reported as UL 94 HB at 1.5 mm, tensile properties per ISO 527-2:2012, flexural modulus per ISO 178:2019, and notched Charpy impact at 0 °C per ISO 179-1:2010. Terminal finished product types include washing machine outer tubs, inner tubs, balance rings, and inlet boxes. Operational boundaries include regrind content not exceeding 20% by weight because higher levels reduce 0 °C Charpy impact and create batch-to-batch variation in shrinkage; pre-drying at 80 °C for 2–3 h is required only when pellet moisture exceeds 0.05%, which is rare but measurable after humid storage.
| Wall thickness | Melt temperature | Mold temperature | Injection speed | Holding time | Observed cycle time |
|---|---|---|---|---|---|
| 2.5 mm | 235–250 °C | 45–65 °C | 80–120 mm/s | 6–9 s | 38–45 s |
| 3.0 mm | 225–245 °C | 40–60 °C | 60–100 mm/s | 7–10 s | 42–50 s |
| 3.5 mm | 220–240 °C | 35–55 °C | 50–90 mm/s | 8–12 s | 46–55 s |
Feedstock hygroscopicity for PP-DN21 is not the controlling variable in crate production; instead melt integrity after repeated regrind cycles and corner weld-line stability are primary. A typical heavy-duty crate formulation uses PP-DN21 at 70–100 wt%, post-industrial regrind at 20–30 wt%, carbon black masterbatch at 0.5–2.0 wt%, nucleating agent at 0.05–0.10 wt%, and antioxidant/stabilizer at 0.1–0.2 phr. The regrind fraction is introduced after a screening step with 3.0 mm mesh and magnetic metal separation to prevent nozzle clogging. Processing uses high-speed accumulator hydraulic injection molding machines, multi-cavity stack molds with hot-runner systems, melt temperature 220–260 °C, hot-runner tip temperature 220–240 °C, mold temperature 20–40 °C, and cooling time controlled by rib-base thermocouples rather than nominal wall thickness. Failure modes observed on production lines include sink marks over rib intersections and detachment at corner knit lines when holding pressure is not profiled; a typical hold profile decreases from 60 bar to 30 bar over 6–10 s. Compliance is established through material testing per ISO 527-2:2012, ISO 1183-1:2019, ISO 179-1:2010, ISO 1133-1:2022 for melt flow rate, and REACH Regulation EC 1907/2006 plus RoHS Directive 2011/65/EU for cross-border shipment. Terminal finished product types include Euro stackable crates, collapsible bulk containers, pallet boxes, dunnage trays, and agricultural picking crates. Operational boundaries include avoiding chronic service exposure to oxidizing acids, aromatic solvents, and unprotected UV because surface oxidation and gloss loss can appear within 6–12 months without adequate carbon black or HALS stabilization. Published data for PP-DN21 compounds containing specific post-industrial recycled streams is limited, so lot-to-lot Charpy impact at 0 °C should be verified when regrind approaches 30%.
Medical waste container production lines processing PP-DN21 operate under lower molding temperatures than olefin homopolymers, which reduces the risk of oxidative carbonyl formation that would otherwise aggravate gamma-sterilization color drift. The formulation is typically 100 phr PP-DN21 with 2–4 wt% color masterbatch, 0.05–0.15 wt% acid scavenger, and 0.1–0.25 phr secondary antioxidant; no talc or calcium carbonate is used when container walls must survive puncture testing per ASTM F2132. Injection molding is conducted in ISO Class 8 or better cleanroom environments with clamp force 1,200–3,000 kN, melt temperature 200–235 °C, mold temperature 20–40 °C, and falling-pressure transfer to limit shear-induced molecular weight loss at thin ribs and snap-fit undercuts. Compliance includes FDA 21 CFR 177.1520 for olefin polymers where secondary food-contact use is possible, USP <661.1> physicochemical testing when adopted by buyer specifications, and ISO 10993-5:2009 cytotoxicity for patient-contact risk assessments. Sharps container safety requirements are verified under ISO 23907-1:2019 or BS 7320, depending on destination market. Terminal finished product types include sharps disposal bins, hospital infectious waste containers, specimen transport boxes, and pharmacy waste pails. Process limitations include gamma irradiation above 25 kGy causing yellowing and measurable post-aging impact loss; lot acceptance programs should include post-irradiation Charpy testing per ISO 179-1:2010. Ethylene oxide sterilization is not a material incompatibility but requires degassing time for gasket seals if used.
In handheld power tool housings, the key process risk is not stiffness loss but creep under screw torque and vibration-induced fatigue at motor mount bosses. A representative impact-modified housing compound uses PP-DN21 at 72–85 wt%, talc masterbatch at 12–20 wt%, POE impact modifier at 5–10 wt%, and short glass fiber at 10–20 wt% where heat deflection above 110 °C is required for hot-rod fastening operations. Compounding is performed on a co-rotating twin-screw extruder with L/D 40:1, barrel profile 210–250 °C, and downstream fiber side-feeding to preserve fiber length. Housing molding uses clamp force 2,500–6,000 kN, melt temperature 220–250 °C, mold temperature 40–60 °C, and injection speed 40–80 mm/s to avoid jetting in thin bosses. Two-part housings are joined by vibration welding or ultrasonic welding; weld bead geometry is designed for shear-dominant stresses, with weld burst testing performed to equivalent OEM specifications rather than a single ISO method. Compliance includes EN 62841-1 and IEC 60745-1 safety requirements, UL 94 HB flammability at 1.5 mm, glow-wire testing per IEC 60695-2-11:2014, tensile properties per ISO 527-2:2012, flexural modulus per ISO 178:2019, and notched impact per ISO 179-1:2010. Terminal finished product types include drill housings, angle grinder handles, circular saw guards, and battery pack casings. Operational boundaries include avoiding continuous contact with cutting oils or ester-based lubricants that can attack the PP surface and cause stress cracking at bosses; pre-drying at 80 °C for 2 h is required if pellets have been stored above 60% RH. Published data for vibration welding of PP-DN21-specific compounds is limited, so weld process limits must be established by design of experiments on production tooling.
Profiles and slats produced from PP-DN21 for outdoor furniture require UV stabilization above typical indoor grades, because the copolymer's rubber phase is vulnerable to photo-oxidative chain scission at surface layers. A typical UV-stable formulation uses PP-DN21 at 92–98 wt%, HALS stabilizer at 0.2–0.6 phr, UV absorber at 0.2–0.5 phr, pigment masterbatch at 1–3 wt%, and processing aid at 0.1–0.3 wt%. Extrusion of hollow profiles uses a single-screw or co-rotating twin-screw extruder with L/D 30:1 to 44:1, melt temperature 190–220 °C, die temperature 200–220 °C, and water calibration temperature 15–25 °C; injection-molded connectors and end caps use melt temperature 220–245 °C and mold temperature 30–50 °C. Accelerated weathering is tested per ISO 4892-2:2013 cycle A with a typical color change limit of ΔE 3.0 after 1,500 h; mechanical property retention after weathering is tested per ISO 527-2:2012 and ISO 178:2019. Outdoor furniture safety and durability are assessed under EN 581-1:2017 and EN 581-2:2015, while RoHS Directive 2011/65/EU and REACH EC 1907/2006 govern chemical compliance for export. Terminal finished product types include slats, armrests, side panels, table tops, and poolside recliner frames. Operational boundaries include avoiding direct contact with chlorinated water above 40 °C, which accelerates oxidative embrittlement of the rubber phase; regrind above 20% should be pre-dried at 80 °C for 2 h to reduce surface defects in coextruded cap layers.
Competitive Kingfa PP-DN21,PP Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-DN21 is a heterophasic polypropylene impact copolymer supplied by Kingfa Sci & Tech Co., Ltd. in cylindrical pellet form for injection molding and selective extrusion compounding. The grade is opaque and contains a dispersed ethylene–propylene rubber phase that reduces notch sensitivity while retaining practical melt fluidity. Under the manufacturer’s nomenclature, the 21 suffix corresponds to a nominal melt mass-flow rate of 21 g/10 min when measured to ISO 1133-1:2022 at 230 °C and 2.16 kg. Nominal density is 0.91 g/cm³ to ISO 1183-1:2019. The material is specified most frequently for automotive interior substrates and housings, small electrical equipment enclosures, appliance panels, and technical parts where a balance of flow length and low-temperature impact is required. Kingfa PP-DN21 is positioned at the high-flow end of the impact-copolymer portfolio; the grade is not intended for transparent parts, direct food-contact use, or load-bearing structural components.
For design purposes, manufacturer-published nominal mechanical properties from injection-molded ISO multipurpose test specimens include tensile yield stress of 24 MPa to ISO 527-2/1A/50, tensile elongation at yield of 5%–7%, nominal strain at break above 50%, flexural modulus of 1350 MPa to ISO 178:2019, and notched Izod impact strength of 5.5 kJ/m² at 23 °C to ISO 180/A. Heat deflection temperature under 1.8 MPa is approximately 52 °C to ISO 75-2, and Vicat softening temperature is approximately 85 °C under 10 N to ISO 306. Mold shrinkage is anisotropic, with published ranges of 1.2%–1.5% in the flow direction and 1.1%–1.4% transverse to flow. These values are product-class nominal data for initial part design; contractual minimums should be fixed in the supply agreement annex rather than inferred from general literature.
Rheologically, PP-DN21 exhibits shear-thinning flow typical of polypropylene impact copolymers. Capillary rheometry data for the product class show apparent viscosity of approximately 25–35 Pa·s at 230 °C and 1000 s⁻¹, declining below 10 Pa·s at 10,000 s⁻¹. This permits filling of multi-cavity tools without excessive melt temperature that accelerates chain scission. Solidification is governed by the crystallization exotherm; differential scanning calorimetry on PP-DN21 class materials typically shows a peak crystallization temperature of 120–128 °C at 10 °C/min and a melting peak at 163–168 °C. Rapid thin-wall cooling below 120 °C therefore freezes the flow front quickly and reduces weld-line durability if fill speed is insufficient.
Desiccant drying at 80 °C for 2–4 h is required if the packaging has been open longer than 4 h at relative humidity above 60%; target residual moisture is below 0.10% by Karl Fischer titration. A closed-loop desiccant dryer with a dew point of −40 °C is recommended for continuous operation. Melt temperature at the nozzle should be held between 210 °C and 240 °C, with barrel settings from 190 °C in the feed zone to 230 °C in the metering zone. Mold temperature from 20 °C to 50 °C is acceptable; temperatures below 20 °C can produce visible flow hesitation on textured surfaces, while mold temperatures above 50 °C raise post-mold crystallization shrinkage and may extend cycle time. Screw-tip injection pressure is normally 70–120 MPa. Hold pressure should be 50%–70% of peak injection pressure for 4–8 s per 1 mm of nominal wall thickness. Back pressure of 0.5–1.5 MPa and screw surface speed of 0.3–0.8 m/s are suitable; higher back pressure tends to increase barrel residence time without improving homogenization. Screw geometry should provide a compression ratio of 2.0:1–2.5:1 and an L/D of at least 18:1. Barrier screws are preferred for color change, and non-return valve clearance should be checked at intervals not exceeding 5000 h because worn clearances cause shot-weight drift in this medium-viscosity melt.
Production-scale field observations from a 1800 kN clamping-force machine running a 4-cavity automotive trim tool with 1.8 mm nominal wall and a 35 °C mold showed stable cycle times of 30–35 s; cooling time was 12–15 s. The primary reject mode was gate blush when hold pressure exceeded 75% of peak injection pressure, not short shots. This indicates that flow-length capability is sufficient for thin-wall trim, but pressure transfer at the gate must be tuned to avoid visible shear-heated material at the gate surface. Cooling channel diameters of 8–10 mm with center-to-center spacing of 2.0–2.5 diameters are recommended to maintain mold surface temperature uniformity within ±5 °C across the cavity. Turbulent coolant flow at Reynolds numbers above 10,000 improves heat removal and reduces cycle-time scatter.
Batch-to-batch variability of the melt mass-flow rate is controlled by the manufacturer’s internal release limits; typical production lots are released within ±2 g/10 min of nominal. Closed-loop process control users should set viscosity adaptation limits from 19–23 g/10 min to maintain stable shot weight. If the melt mass-flow rate drifts above 23 g/10 min, holding pressure should be reduced by approximately 5% to prevent flash at the parting line and gate blush.
When compared with a 11 g/10 min general-purpose polypropylene homopolymer, PP-DN21 shows lower tensile yield stress and flexural modulus but substantially higher notched Izod impact, particularly below 0 °C. The difference arises from the heterophasic ethylene–propylene rubber phase, which increases energy absorption during crack propagation while reducing crystallinity and stiffness. Conversely, when compared with a 20 wt% talc-filled PP compound, PP-DN21 has lower flexural modulus and higher mold shrinkage, which makes it less appropriate for high-clamp-load brackets and dimensionally tight structural parts. The grade is situated between a standard PP homopolymer and a high-impact PP random copolymer: it sacrifices transparency and stiffness but gains low-temperature ductility and weld-line tolerance.
| Property | Kingfa PP-DN21 | PP homopolymer, 11 g/10 min | Talc-filled PP, 20 wt% |
|---|---|---|---|
| Melt mass-flow rate, ISO 1133-1:2022 | 21 g/10 min | 11 g/10 min | 15 g/10 min |
| Density, ISO 1183-1:2019 | 0.91 g/cm³ | 0.90 g/cm³ | 1.05 g/cm³ |
| Tensile yield stress, ISO 527-2 | 24 MPa | 34 MPa | 28 MPa |
| Flexural modulus, ISO 178:2019 | 1350 MPa | 1500 MPa | 2600 MPa |
| Notched Izod impact at 23 °C, ISO 180/A | 5.5 kJ/m² | 2.0 kJ/m² | 3.0 kJ/m² |
| Heat deflection temperature, 1.8 MPa, ISO 75-2 | 52 °C | 55 °C | 75 °C |
Pigment addition can shift melt viscosity and nucleate crystallization in PP-DN21, especially with carbon black or organic red masterbatches. Cavity-specific validation is required before colors are locked for interior trim programs, because final notched Izod impact and fogging behavior may deviate from natural-resin data. Published data for every pigment-impact configuration are limited; the safe route is to qualify the final compounded batch rather than predict performance from base-resin values alone.
For cold-runner tools, the practical minimum wall thickness is approximately 1.2 mm when the flow length/thickness ratio is 200:1, injection velocity is 100–200 mm/s, and the machine uses a positive shut-off nozzle. Below 1.0 mm, flow-front hesitation and weld-line weakness become controlling defects because shear heating is insufficient to maintain melt temperature at the advancing front. At 1.0 mm, injection pressure can approach or exceed 130 MPa, which may exceed the clamp force of small-tonnage presses and cause flash on multi-cavity tools. The melt does not possess the very high fluidity of a 60 g/10 min controlled-rheology PP, nor does it exhibit the modulus plateau of a nucleated homopolymer. Weld-line tensile strength in unsupported thin sections is typically 70%–80% of un-welded tensile strength; this is a critical limitation for living-hinge, snap-fit, or pressure-bearing closures. Thin-wall tools should therefore use generous radii at flow-runner intersections and avoid direct gate placement opposite weld-sensitive features.
Valve-gate systems are preferred over open tip bushings for PP-DN21 because the melt’s medium crystallinity creates a narrow processing window at the gate. Manifold temperature should be held between 220 °C and 240 °C, and valve-stem tip temperature should not exceed 240 °C to avoid degradation and gate stringing. Gate diameter for a 1.5–2.5 mm wall is commonly 0.8–1.2 mm. Hot-runner controllers must maintain thermocouple stability within ±2 °C; larger swings produce inconsistent gate freeze time and shot-weight variation. If hot-runner channel count exceeds 4 drops, sequential valve gating should be used to control the position of flow-induced weld lines. In a production-validated tool with 2 valve gates and a 2.0 mm nominal wall, switch-over from velocity control to hold pressure at 95% of shot volume minimized gate blush while maintaining part mass within ±0.3%. Open-gate systems should be avoided for cosmetic surfaces because PP-DN21 can leave visible vestige marks and cold-slug streaks when the gate temperature is not stabilized.
OEM specification screening commonly requires REACH Candidate List SVHC declarations, RoHS 2011/65/EU Annex II compliance for electrical and electronic equipment, and automotive interior release testing according to VDA 277 total carbon emission, VDA 270 odor, and fogging under ISO 6452. The base resin is a hydrocarbon polymer and does not contain halogenated flame retardants in its standard formulation; the expected UL 94 vertical burn classification at 1.5 mm is HB. Flame-retardant variants must be requested when V-0 or V-2 ratings are required, because post-mold treatment with external coatings generally fails to provide reproducible thin-wall flame performance. The grade is not formulated as a UV-stabilized exterior product; long-term outdoor exposure requires an additional hindered-amine light stabilizer and benzotriazole-type UV absorber package validated on production-spec samples under ISO 4892-2 or ASTM G155 cycle conditions. Published multi-year weathering data for this specific configuration are limited; therefore, exterior components must be tested against the intended climate zone rather than relying on generic polypropylene weathering tables.
| Standard or regulation | Applicability for PP-DN21 qualification |
|---|---|
| ISO 527-2 | Tensile yield strength and elongation at break |
| ISO 1133-1:2022 | Melt mass-flow rate |
| ISO 180/A | Notched Izod impact strength |
| ISO 75-2 | Heat deflection temperature under flexural load |
| ISO 1183-1:2019 | Density |
| REACH SVHC | Chemical compliance declaration |
| RoHS 2011/65/EU | Electrical and electronic equipment content limits |
| FDA 21 CFR 177.1520 | Olefin polymer food-contact suitability verification |
The material should not be processed above 260 °C or held at molding temperature above 240 °C for more than 10 min, because extended residence time leads to chain scission and a measurable loss of notched Izod impact. It is also not recommended for continuous contact with strong oxidizing acids, direct fuel-contact systems without barrier layers, or high-shear operations that raise melt temperature above 250 °C at the screw tip. These boundaries define the practical operating envelope for Kingfa PP-DN21 in production injection molding.