| HS Code | 337115 |
| Productname | Kingfa PP-V30G |
| Polymertype | PP Homopolymer |
| Reinforcement | Glass Fiber |
| Glassfibercontent | 30% |
| Density | 1.12 g/cm³ |
| Meltflowrate | 8 g/10 min (230°C/2.16 kg) |
| Tensilestrength | 65 MPa |
| Elongationatbreak | 3% |
| Flexuralmodulus | 5500 MPa |
| Flexuralstrength | 90 MPa |
| Notchedizodimpactstrength | 8 kJ/m² at 23°C |
| Heatdeflectiontemperature | 145°C at 1.82 MPa |
| Moldingshrinkage | 0.5–0.8% |
| Waterabsorption | 0.02% |
As an accredited Kingfa PP-V30G,PP Homopolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-V30G PP Homopolymer is packaged in 25 kg moisture-proof woven bags, palletized and stretch-wrapped for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Kingfa PP-V30G PP homopolymer, packed in 25 kg bags, stacked and secured for sea transport. |
| Shipping | Kingfa PP-V30G, PP Homopolymer is shipped as non-hazardous thermoplastic pellets in sealed 25 kg bags or bulk containers. Store and transport in a dry, ventilated area at ambient temperature, avoiding moisture, direct sunlight, heat, and contamination. No special dangerous-goods classification or UN number is required. |
| Storage | Store Kingfa PP-V30G (PP homopolymer) in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers sealed and palletized off the floor to prevent moisture and contamination. Separate from strong oxidizers, acids, and bases. Avoid dust generation and static buildup; follow local regulations and good housekeeping. |
| Shelf Life | Shelf life is typically 24 months when stored unopened in original packaging in a cool, dry place away from sunlight. |
Thin-wall injection molding of Kingfa PP-V30G in food-contact containers is governed by a narrow process corridor between melt temperature, screw recovery, and gate freeze-off. The grade’s nominal melt mass-flow rate of 30 g/10 min at 230°C and 2.16 kg under ISO 1133-1:2022 permits flow-length-to-wall-thickness ratios approaching 150:1 in well-vented tools when injection velocity is maintained above 100 mm/s; however, thermal degradation kinetics accelerate measurably above 250°C, generating volatile residues that can fail organoleptic panels under ISO 13302:2003 and alter migration behavior. Compliance documentation for this downstream segment is anchored to FDA 21 CFR 177.1520(c) 1.1 for polypropylene homopolymers in contact with aqueous, acidic, fatty, and low-alcohol foods, Regulation (EU) 10/2011 with an overall migration limit of 10 mg/dm² and food simulant assignment under Annex III, GB 4806.6-2016, and REACH Regulation (EC) No 1907/2006 SVHC screening below 0.1 wt% per article. Formulation addition level in high-speed packaging lines commonly uses 100 parts PP-V30G by weight as the continuous phase; color masterbatch is introduced at 1.5–3.0 phr with a polypropylene carrier to minimize melt-flow imbalance, and post-industrial regrind from the same tool is limited to 15–20 phr for non-sensitive articles, with full revalidation under EU 10/2011 Article 17 when recycled material is included. Production-scale injection molding equipment for this segment typically uses three-zone general-purpose screws with 20:1–24:1 L/D, compression ratios of 2.0:1–2.4:1, check-ring assemblies that maintain a shot-to-shot cushion of 3–6 mm, and clamp forces from 1,000–5,000 kN depending on cavity count. Barrel temperatures are profiled from 210°C at the hopper to 240–250°C at the nozzle, mold surface temperatures are held at 15–40°C, and injection pressure is set between 80–110 MPa, with hold pressure at 60–80% of peak pressure and hold time determined by gate seal rather than packing time. Polypropylene homopolymer does not require drying unless surface moisture exceeds 0.1%; at relative humidity above 60%, a hopper dryer at 80°C for 2 h is recommended to prevent splay. At wall thicknesses below 0.45 mm, flow hesitation at ribs and bosses creates anisotropic shrinkage; at melt temperatures above 250°C and residence times above 10 min, molecular weight reduction shifts the MFR upward by more than 20%, causing short shots to transition into flash, sink marks, and warpage. Terminal finished product types include thin-wall dairy cups, deli containers, disposable bowls, overcap lids, and tamper-evident food pails produced in multi-cavity tools with cycle times of 4–8 s for articles below 1.0 mm nominal wall thickness.
Cap and closure production with PP-V30G is concentrated in high-cavitation, short-cycle injection tools where the high MFR of 30 g/10 min permits gate-to-cavity filling at reduced injection pressure but imposes specific limitations on hinge toughness after repeated flexing. Hinge design with a residual thickness of 0.25–0.40 mm relies on molecular orientation perpendicular to the hinge axis; this is achieved by placing a valve gate or edge gate opposite the hinge and maintaining mold surface temperature at 20–30°C to quench orientation before spherulite growth destroys tie-chain density. Compliance for beverage and pharmaceutical closures is documented under FDA 21 CFR 177.1520(c) 1.1, Regulation (EU) 10/2011 with overall migration below 10 mg/dm², and Regulation (EC) No 1935/2004 for food-contact materials; pharmaceutical closures add USP <88> Biological Reactivity testing for elastomer-free polypropylene components and ISO 13485:2016 quality-system controls when supplied as medical packaging. The formulation addition level in this segment is 100 parts PP-V30G by weight, with slip/antiblock masterbatch added at 0.5–1.5 phr to reduce the coefficient of friction below 0.25, color masterbatch at 1.0–2.0 phr, and no peroxide initiators or nucleating additives unless the resulting shrinkage shift from 1.2% to 1.4% is revalidated in the hinge area. Equipment on production lines typically uses 24:1 L/D screws with reverse-taper nozzles and hot-runner valve-gate systems; melt temperature is controlled at 220–240°C, mold temperature at 20–30°C, injection speed is profiled to maintain a flow front velocity of 120–200 mm/s through the hinge, and cycle time for a 2.5 g beverage cap is commonly 5–8 s. The critical operational boundary is sub-zero impact: notched Izod under ISO 180/A for unfilled PP-H at this MFR is typically 2.5–3.5 kJ/m² at 23°C but falls below 1.5 kJ/m² at -20°C; freezer-grade closures with ductile hinge requirements therefore require impact modification or hinge redesign because PP-V30G alone risks brittle failure at or below 0°C. Terminal finished product types include tamper-evident beverage closures, flip-top dispensing caps, child-resistant pharmaceutical closures, cosmetic flip-caps, and linerless caps with torque retention validated under ASTM D2063.
For household storage articles produced from Kingfa PP-V30G, the principal engineering requirement is dimensional stability after ejection from multi-cavity family molds, particularly for stackable containers with living hinges and snap-fit lids. The material is processed at 210–240°C melt temperature and 20–40°C mold temperature; shot-to-shot weight variation below 0.15% is maintained on production machines with closed-loop injection velocity control and screw-position switchover to avoid cavity imbalance. Compliance for food-contact storage articles follows FDA 21 CFR 177.1520(c) 1.1 and Regulation (EU) 10/2011; non-food houseware components that enter electrical appliances are additionally assessed under IEC 60335-1:2020 and ball-pressure requirements in IEC 60695-10-2. The formulation addition level is 100 parts PP-V30G by weight; antistatic masterbatch is added at 0.8–1.5 phr for dust-prone storage boxes, UV stabilizer masterbatch at 0.3–0.8 phr for outdoor stackable crates and garden articles, and calcium carbonate filler at 5–10 phr for rigid drawer bodies where no living hinge is present; filler is omitted from hinge-bearing lids to avoid tensile embrittlement. Downstream production uses conventional injection molding with 20:1–24:1 L/D, general-purpose compression screws, mold surface temperatures below 40°C, and cycle times of 18–30 s for articles in the 1.5–3.0 mm wall thickness range; thick handles and bosses are cored to avoid sink marks rather than relying on extended hold pressure. Terminal finished product types include stackable storage boxes, modular drawer organizers, household baskets, hangers, microwave lids, and garden side tables.
Toy manufacturing with PP-V30G is constrained less by melt viscosity than by migration chemistry and low-temperature impact behavior. The high MFR of 30 g/10 min permits filling of small articulated parts with wall thicknesses down to 0.8 mm, but the homopolymer’s brittle transition means drop-test performance must be evaluated at the lower temperature boundary of the intended market; ASTM F963-23 drop testing may produce sharp fracture surfaces if the part is below 0°C at the moment of impact. Compliance documentation includes EN 71-3:2019+A1:2021 for migration of 19 elements, ASTM F963-23, ISO 8124-3:2020, and REACH Annex XVII entries 51 and 52 for phthalate restrictions. The formulation addition level is 100 parts PP-V30G by weight; color masterbatch is used at 2–3 phr with carrier resins that are themselves EN 71-3-compliant, and regrind from the same toy grade is limited to 10–15 phr because repeated heat history reduces notched impact strength by 15–25% relative to virgin resin. Injection molding parameters include melt temperature 220–240°C, mold temperature 20–30°C, injection speed high enough to avoid weld lines at flow fronts, and hold pressure adjusted to gate-seal time; weld lines in low-molecular-weight homopolymer are especially prone to brittle failure under tensile loading along the knit line. Terminal finished product types include building blocks, small-format assembled toys, toy food containers, play kitchen accessories, and storage boxes marketed to the juvenile segment.
In diagnostic disposable molding, Kingfa PP-V30G is selected for non-implantable, short-term patient-contact articles where high flow permits thin ribs and snap features, but the grade is not considered suitable for load-bearing or long-term implanted devices. Compliance is governed by ISO 10993-5:2009 cytotoxicity, ISO 10993-10:2010 skin irritation and sensitization, USP <88> Biological Reactivity tests for plastics, and ISO 13485:2016 for device quality management; sterilization compatibility must be validated under ISO 17665-1:2006 for steam at 121°C, ISO 11135:2014 for ethylene oxide, or ISO 11137 for radiation, with the caveat that gamma doses above 25 kGy are known to cause embrittlement and yellowing in unstabilized polypropylene homopolymer. The formulation addition level is 100 parts PP-V30G by weight; mold-release agents, slip additives, and colorants are excluded unless the specific additive is already qualified under USP <88> or ISO 10993, and post-industrial regrind is limited to 10 phr maximum only when validated for the finished device configuration. Downstream production is carried out in cleanroom injection molding rooms meeting ISO 14644-1:2015 Class 7 or 8, with barrel temperatures 210–240°C, mold surface temperatures 15–30°C, and screw speeds selected to avoid shear-induced molecular weight loss at residence times above 8 min; packaging and assembly are performed under validated EO or steam sterilization cycles. Terminal finished product types include specimen containers, centrifuge tube bodies, disposable pipette tip racks, tube caps, and non-load-bearing diagnostic instrument housings.
The office supply segment represents a low-stress injection geometry in which PP-V30G is used for thin, flat articles requiring consistent melt delivery and short cooling times. Compliance is limited to REACH Regulation (EC) No 1907/2006 and, for children’s stationery marketed as toys, EN 71-3:2019+A1:2021; no food-contact or medical testing is required unless the article is dual-marketed. The formulation addition level is 100 parts PP-V30G by weight, with color masterbatch at 1.0–2.0 phr and no regrind restriction beyond maintaining dimension consistency. Processing uses standard injection molding parameters of 200–230°C melt temperature and 20–30°C mold temperature; the only critical control is screw cushion position, because thin ruler and file divider tools are sensitive to cushion variation above 1 mm. Terminal finished product types include rulers, file organizers, binder spines, marker barrel housings, and desk trays.
Competitive Kingfa PP-V30G,PP Homopolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-V30G, PP Homopolymer is supplied by Kingfa Sci & Tech Co., Ltd. as an unfilled isotactic polypropylene homopolymer intended primarily for injection molding. The grade designation reflects a nominal melt flow rate of 30 g/10 min determined at 230 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. Because no ethylene comonomer is present, the polymer develops relatively high crystallinity compared with impact copolymer or random copolymer grades. The resulting property profile includes higher tensile yield stress, higher flexural modulus, and higher heat deflection temperature, but lower notched Izod impact strength, particularly below ambient temperature. Primary downstream uses include thin-wall rigid packaging, appliance housings, electrical enclosures, closures, and general-purpose technical parts that require stiffness, chemical resistance, and short cycle times. The material is not formulated for sub-0 °C impact service or continuous outdoor exposure without effective UV stabilization. Lot-specific mechanical, rheological, and regulatory values should be verified against the Kingfa technical data sheet and certificate of analysis before tool design or production release.
In tensile testing performed under ISO 527-2:2012, unfilled PP homopolymer in the 30 g/10 min melt-flow band typically exhibits tensile yield stress of 33–36 MPa and flexural modulus of 1400–1700 MPa when tested to ISO 178:2019. Impact copolymers of comparable melt flow often display tensile yield stress of 24–28 MPa and flexural modulus of 900–1200 MPa because the ethylene-propylene rubber phase disrupts crystallinity and reduces stiffness. The same rubber phase raises notched Izod impact strength at 23 °C from a homopolymer range of 1.5–3.0 kJ/m² to 10–25 kJ/m² under ISO 180/A. At 0 °C or below, the homopolymer frequently falls below 1.0 kJ/m², which restricts its use in frozen-food packaging or crash-relevant automotive components. Random copolymers reduce crystalline order through minor propylene-ethylene sequence disruption, improving clarity but lowering stiffness. PP-V30G is therefore selected when opacity is acceptable and rigidity is prioritized over low-temperature ductility.
For early-stage part design, the following class-representative data may be used only as a preliminary reference. Certified values must be obtained from the manufacturer’s technical data sheet for the specific production lot.
| Property | Test Method | Unit | Typical Class Range |
| Melt flow rate | ISO 1133-1:2022 | g/10 min | 29–31 |
| Density | ISO 1183-1:2019 | g/cm³ | 0.89–0.91 |
| Tensile yield stress | ISO 527-2:2012 | MPa | 33–36 |
| Tensile elongation at yield | ISO 527-2:2012 | % | 8–12 |
| Flexural modulus | ISO 178:2019 | MPa | 1400–1700 |
| Notched Izod impact strength, 23 °C | ISO 180/A | kJ/m² | 1.5–3.0 |
| Heat deflection temperature, 0.45 MPa | ISO 75-2/B:2013 | °C | 95–110 |
| Mold shrinkage | ISO 294-4:2018 | % | 1.0–1.6 |
Published data for this specific configuration is limited for long-term creep, fatigue, and ultraviolet endurance. These properties must be evaluated under application-specific exposure conditions rather than inferred from short-term tensile or flexural data.
Production-scale experience with 30 g/10 min PP homopolymer on reciprocating-screw injection molding machines indicates that melt temperature measured at the nozzle should be held between 220 °C and 250 °C, with 230 °C as a center point. Mold surface temperature is commonly controlled between 20 °C and 60 °C. Higher mold temperatures in the 50–60 °C band improve knit-line appearance and reduce flow hesitation but lengthen cooling time. For a 1.0 mm wall section, cooling time is generally 5–8 s; for 1.5 mm, cooling time is generally 8–12 s. These values shift with coolant temperature, part geometry, and hot-runner design. General-purpose screws with L/D 20:1–24:1 and compression ratio of 2.5:1–3.0:1 are adequate, provided a shut-off nozzle or low-dead-volume non-return valve is used. Injection velocity is typically set at 80–150 mm/s for thin-wall fill, while hydraulic peak pressure is adjusted from 60–120 MPa until cavity fill is achieved without flash. Hold pressure is normally 50–70% of peak fill pressure. Clamp force requirement is estimated at 4.0–6.0 kN/cm² of projected area for unfilled PP homopolymer. Vent depth should not exceed 0.02–0.03 mm to permit air evacuation while preventing flash.
Capillary rheometry under ISO 11443:2021 at 230 °C indicates that a 30 g/10 min PP homopolymer typically shows apparent shear viscosity of 20–50 Pa·s at 1000 s⁻¹ and 8–15 Pa·s at 5000 s⁻¹. The transition from a low-shear plateau to marked shear thinning occurs near 100–1000 s⁻¹, so mold filling is controlled by non-Newtonian shear thinning. This means that pressure drop across a thin wall is not a linear function of injection speed; doubling flow-front velocity does not double pressure because viscosity declines as shear rate increases. Freeze-off in sections below 0.8 mm occurs rapidly because the no-flow temperature of PP homopolymer is approximately 130–140 °C. The solidified layer grows from the mold wall and reduces the effective flow channel. In a 0.8 mm wall at 40 °C mold temperature, significant flow-front hesitation may permit freeze-off after 0.3–0.5 s. High injection speed, adequate venting, and hot-runner gate-seal times of 0.5–1.0 s are used to maintain flow-front advancement. Published data for this specific configuration is limited, so cavity-pressure transducer measurements are preferred for establishing the true fill window on production tooling.
Mold shrinkage in unfilled PP homopolymer is non-uniform and depends on wall thickness, flow direction, mold temperature, hold pressure, and gate freeze. Under ISO 294-4:2018, class-level longitudinal shrinkage is typically 1.0–1.6%, while transverse shrinkage may be 0.1–0.3% lower than longitudinal values. Higher mold temperature and longer hold time reduce shrinkage but increase cycle time. For a 1.5 mm wall at 230 °C melt temperature and 30 °C mold temperature, gate freeze time is commonly 4–8 s. Shrinkage anisotropy becomes more severe in sections above 2.5 mm because slower cooling increases total crystallinity. Sink marks may appear in ribs and bosses if rib wall thickness exceeds 55–65% of the nominal wall; the practical design limit is 60% or lower. These process boundaries should be confirmed with cavity-pressure and mold-temperature data from production tooling rather than extrapolated from small-scale plaques.
Compared with a 20 wt% talc-filled PP homopolymer, PP-V30G provides lower density, lower flexural modulus, higher mold shrinkage, and better melt fluidity. The filled grade raises flexural modulus to approximately 2500–3500 MPa but reduces melt flow and increases screw and check-ring wear. Glass-fiber reinforced PP develops higher strength and modulus but introduces anisotropic shrinkage and warpage risk. Against an impact copolymer, PP-V30G offers greater stiffness and heat deflection temperature but must not be substituted for components requiring ductile failure at low temperature. The following representative comparison separates the resin classes.
| Property | Unfilled PP-H 30 MFR | Impact copolymer 30 MFR | 20 wt% talc-filled PP-H |
| Melt flow rate, 230 °C/2.16 kg | 29–31 g/10 min | 28–32 g/10 min | 10–18 g/10 min |
| Tensile yield stress | 33–36 MPa | 24–28 MPa | 28–32 MPa |
| Flexural modulus | 1400–1700 MPa | 900–1200 MPa | 2500–3500 MPa |
| Notched Izod impact strength, 23 °C | 1.5–3.0 kJ/m² | 10–25 kJ/m² | 2.5–4.0 kJ/m² |
| Heat deflection temperature, 0.45 MPa | 95–110 °C | 85–100 °C | 120–140 °C |
| Mold shrinkage | 1.0–1.6% | 1.0–1.4% | 0.6–1.0% |
Values in the comparative table are class-level engineering references. The talc-filled and impact-copolymer columns vary with base resin selection, additive package, and filler particle size distribution.
For unfilled PP homopolymer, pre-drying is not routinely required when resin is stored at relative humidity below 60%. If moisture uptake exceeds 0.1 wt% or surface defects such as splay are observed, drying at 80 °C for 2–4 h in a desiccant dryer is applied. Barrel residence time above 250 °C should not exceed 10 min, because extended exposure can shift melt viscosity and generate oxidative degradation products that affect color and odor. Production lines equipped with hot-runner systems should maintain balanced manifold temperatures and avoid dead spots. Valve-gate drops with 0.5–1.0 s gate-seal time reduce drool and stringing. Regrind addition for general-purpose rigid parts is typically limited to 20–30 wt%, with lower fractions required for high-gloss or thin-wall packaging to limit black specks and lot-to-lot viscosity drift. Avoid compounding with amine-based stabilizer packages that can interact with peroxide residues from controlled-rheology high-flow PP. Published data for this specific configuration is limited, so compatibility testing is recommended before introducing color concentrates or processing aids.
For food-contact applications in the United States, unfilled PP homopolymer may be evaluated under 21 CFR 177.1520 when the specific grade and colorant package meet applicable extraction limits. European electrical and electronic applications require demonstration of compliance with RoHS Directive 2011/65/EU and REACH SVHC disclosure under Regulation (EC) No 1907/2006. Flammability is commonly rated UL 94 HB at 1.5 mm thickness, but ignition-resistant behavior is not inherent to this grade. These regulatory positions are formulation- and lot-specific and must be verified against the supplier’s material certification and substance declaration.