Kingfa CK-92010,PP Reinforced,Glass Fiber

    • Product Name: Kingfa CK-92010,PP Reinforced,Glass Fiber
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 502178
    Glass Fiber Content 10%
    Density 1.03 g/cm³
    Melt Flow Rate 8 g/10 min (230°C/2.16 kg)
    Tensile Strength 45 MPa
    Elongation At Break 5%
    Flexural Modulus 2500 MPa
    Flexural Strength 70 MPa
    Notched Izod Impact Strength 50 J/m
    Heat Deflection Temperature At 0 45 Mpa 140°C
    Heat Deflection Temperature At 1 82 Mpa 120°C
    Vicat Softening Temperature 150°C
    Molding Shrinkage 0.5-0.8%
    Water Absorption 0.02%
    Flammability HB
    Processing Method Injection Molding

    As an accredited Kingfa CK-92010,PP Reinforced,Glass Fiber factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa CK-92010 PP reinforced glass fiber packed in 25 kg moisture-barrier bags, palletized and stretch-wrapped for secure transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with Kingfa CK-92010 PP reinforced glass fiber, bagged/palletized, approx. 20–22 MT net, secure and moisture-protected.
    Shipping Kingfa CK-92010 is a glass-fiber-reinforced polypropylene compound supplied as pellets. Ship in sealed, moisture-barrier bags or lined containers, labeled with product name and lot, protected from moisture, heat, and sunlight. Classify per SDS; typically non-hazardous for transport.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and ignition sources. Keep bags/containers tightly closed in original or compatible labeled containers, palletized off the floor to prevent moisture and contamination. Avoid dust generation and static buildup. Segregate from oxidizers and incompatible chemicals. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Indefinite shelf life when stored cool, dry, ventilated, away from sunlight and moisture in original sealed packaging.
    Application of Kingfa CK-92010,PP Reinforced,Glass Fiber

    In engine-compartment cooling modules, Kingfa CK-92010 is qualified for fan shroud carriers, radiator end tanks, and intercooler air ducts only after long-term heat aging demonstrates that tensile strength retention remains acceptable when air temperatures at the component surface approach 130 °C. On production-scale injection molding machines with 1200–1600 t clamp force, 60 mm screw diameter, and L/D 22:1, the compound is processed at a melt temperature of 230–245 °C and mold temperature of 40–70 °C. The formulation addition ratio is 100 wt% CK-92010 pellets with 2 wt% carbon black masterbatch for outdoor UV resistance; in-plant regrind from sprues and runners is limited to 15 wt%, but when fan blade weld-line strength is an acceptance criterion, the regrind fraction is capped at 10 wt% because repeated heat history accelerates glass-fiber attrition and reduces weld-line Charpy impact. The downstream production sequence includes sequential valve-gated hot runners with 4–8 drops, injection speeds of 40–80 mm/s, back pressure of 3–6 MPa, and post-mold fixturing at 80 °C for 20 min to hold shroud flatness before the part cools below 60 °C. Process audits use ISO 1133-1:2022 melt flow-rate checks at 230 °C/2.16 kg; lot-to-lot variations of more than ±2 g/10 min against the supplier certificate require readjustment of shot size and screw recovery speed. Fiber orientation at the fan blade root is known to produce sharp reductions in notched Charpy impact when the melt front meets after multi-gate filling; the effect is quantified in mold trials by cutting specimens across the weld line and testing per ISO 179-1/1eA. Long-term heat aging is conducted per ISO 188:2023 at 150 °C for 1000 h; tensile strength retention of at least 70% is used as the internal acceptance criterion, while multiaxial puncture is checked per ISO 6603-2 at 23 °C and -30 °C. Terminal components include radiator fan shroud modules, fan support brackets, intercooler ducts, and shroud baffles.

    What Limits Hydrolytic Aging in Washing Machine Outer Tubs Molded from Glass-Reinforced PP?

    Washing machine outer tub production subjects CK-92010 to warm alkaline detergent solutions and oxygenated water, which makes hydrolytic stability of the glass-fiber/coupling-agent interface the limiting factor rather than short-term stiffness. The industry compliance framework for the application includes IEC 60335-1:2020 for electrical safety of the appliance and ISO 175:2010 as the chemical resistance test method; immersion is performed in 0.5 wt% sodium hydroxide and 1 wt% sodium hypochlorite at 60 °C for 168 h, with mass change held below 1.5% and tensile strength retention above 80%. The formulation addition ratio is 88 wt% CK-92010, 10 wt% heat-stabilized PP copolymer for low-temperature impact improvement, and 2 wt% antioxidant/acid-scavenger masterbatch; when regrind from rejected outer tubs is reused, the ratio is capped at 12 wt% and the antioxidant package is enriched to compensate for prior heat history. The downstream production process uses two injection-molded halves produced on 1800 t clamp machines with 80 mm screw diameter at melt temperature 225–240 °C and mold temperature 60–80 °C; the halves are joined by hot-plate welding at 210 °C, and weld strength is validated by tensile testing across the weld per ISO 527-2:2012, with an acceptance threshold of at least 70% of parent material strength.

    Production experience on tub lines has shown that weld-line failures occur primarily when hydrolytic attack reduces interfacial adhesion between glass fibers and the PP matrix after 4–6 months of service, so post-weld annealing at 90 °C for 4 h is specified to relieve residual stresses and delay crack initiation. Operational boundaries include exclusion of copper-based heat stabilizers because their presence accelerates oxidative chain scission in the presence of hypochlorite-containing water; only hindered phenolic and phosphate-based stabilizer packages are approved for this application. No pre-drying is required when surface moisture is below 0.05 wt%; if cold warehouse condensation is observed or storage relative humidity has exceeded 60%, a desiccant dryer set at 80 °C for 2 h is imposed. Terminal product types are washing machine outer tubs, tub bases, and balance rings.

    Double-insulated power tool enclosures impose drop-impact and heat-deflection requirements that CK-92010 must meet before it can replace PC/ABS in housing shells without violating dimensional requirements under static load. Compliance testing follows IEC 62841-1:2014 for hand-held motor-operated electric tools, IEC 60068-2-31:2008 for rough-handling drop impacts, and ISO 75-2:2013 method A for heat deflection temperature under 1.8 MPa. The formulation addition ratio in the molding shop is 92 wt% CK-92010, 5 wt% elastomer-modified PP masterbatch to reduce cold-temperature brittleness, and 3 wt% color/UV masterbatch; regrind from gate and runner waste is limited to 10 wt% to avoid surface streaking and knit-line visual defects. The downstream production process runs two-shell housings on 350–600 t injection molding machines with 35–40 mm screw diameter at melt temperature 235–250 °C and mold temperature 40–60 °C; injection speed is set from 180 mm/s to 260 mm/s to avoid premature freeze-off at thin ribs, while pack pressure of 40–60 MPa is held for 4–8 s. Mold shrinkage is measured per ISO 294-4:2018; in flow direction shrinkage is typically 0.3–0.5% and transverse shrinkage is 0.7–1.0%, which dictates draft angles and screw boss clearances. Ultrasonic insertion at 20 kHz is used for brass thread inserts in driving-gear housings, and insert pull-out force is audited on a tensile machine at 5 mm/min crosshead speed using a fixture defined by the toolmaker. Terminal products include angle grinder housing halves, drill body shells, and reciprocating saw motor housings.

    When CK-92010 Replaces Talc-Filled PP in Automotive Door Module Carriers Under Elevated Screw Torque

    Door module carriers for four-door sedans require a combination of low creep under screw clamping and high stiffness across a 1.2 m flow path, which makes CK-92010 a candidate only if glass-fiber orientation at bosses and differential shrinkage between reinforced and unreinforced zones are controlled. The qualification program includes ISO 527-2:2012 tensile modulus, ISO 179-1/1eA Charpy notched impact at 23 °C and -20 °C, and ISO 899-1:2017 tensile creep at 80 °C under a static load corresponding to 20% of the yield stress, with creep strain acceptance below 1.0% at 1000 h. The formulation addition ratio is 93 wt% CK-92010 with 7 wt% elastomer masterbatch at the window-motor mounting boss region; the dry blend is introduced only in the hot-runner drops feeding those bosses, while the surrounding wall remains 100 wt% CK-92010. The downstream production process is a large side-gated injection molding cell with 1600–2400 t clamp force and 90 mm screw diameter; melt temperature is 230–245 °C, mold temperature is 40–70 °C, and 4–8 sequential valve gates open in cascade to reduce weld formation. Fiber orientation at the transition between boss and planar surface creates anisotropic shrinkage; if ejection occurs before the gate freeze temperature falls below 130 °C, warpage at the carrier edges and boss-base cracking during assembly at 4–6 N·m screw torque have been observed on production trials. The gate seal time and holding pressure decay are therefore audited at each shot with cavity pressure sensors located at the last-filled flow position; a cavity pressure of 300–500 bar is maintained through the packing phase. Terminal product types include door module carriers, window regulator brackets, and speaker ring reinforcements.

    Application contextStandard designationTest conditionAcceptance threshold
    Engine-compartment cooling moduleISO 188:2023150 °C, 1000 htensile strength retention ≥70%
    Washing machine outer tubISO 175:20100.5 wt% NaOH, 60 °C, 168 hmass change ≤1.5%, tensile retention ≥80%
    Power tool housingIEC 62841-1:2014drop impact per IEC 60068-2-31:2008no crack exposing live parts
    Automotive door module carrierISO 899-1:201780 °C, 20% yield stresscreep strain ≤1.0% at 1000 h
    Outdoor meter enclosureISO 4892-2:20132500 kJ/m² at 340 nmDelta E ≤3.0
    Chemical metering pumpASTM D543-205 wt% NaOH, 40 °C, 168 hmass change ≤0.8%, tensile retention ≥85%

    Outdoor Electrical Meter Box Weatherability and the Influence of Glass-Fiber Orientation on UV Retention

    Long-term weatherability in outdoor electrical meter enclosures depends on the ultraviolet stabilizer package rather than on the glass-fiber reinforcement itself, so CK-92010 is considered for base housings and non-arcing structural parts only after UV retention is demonstrated. The industry compliance framework includes IEC 62208:2011 for empty enclosures, IEC 60529:2013 for IP65 dust and water ingress protection, and IEC 60695-2-11:2014 glow-wire testing at 650 °C for 30 s; however, published data for CK-92010 under UL 746C f1 outdoor UV rating is limited, so qualification is performed by xenon-arc weathering per ISO 4892-2:2013 with total irradiance of 2500 kJ/m² at 340 nm and a Delta E acceptance limit below 3.0. The formulation addition ratio is 95 wt% CK-92010, 2 wt% UV masterbatch based on HALS plus benzotriazole UV absorber, 1 wt% erucamide slip additive, and 2 wt% antistatic masterbatch; regrind is capped at 10 wt% because repeated processing consumes the hindered amine stabilizer and accelerates chalking. The downstream production process molds enclosure bases on 1000–1400 t machines with 70 mm screw diameter at melt temperature 220–240 °C and mold temperature 30–60 °C; a two-stage hot runner with sequential valve gates is used to manage the long flow path, and post-mold dimensional checks are performed on a coordinate measuring machine with reference to ISO 2768-1:1989 general tolerances. Mold temperature is regulated within ±5 °C of the set point during the packing phase; excursions outside this band produce visible glass-fiber read-through on the enclosure side walls and can shift post-mold shrinkage by more than 0.15%. Terminal product types are outdoor meter enclosure bases, terminal covers, and mounting plates.

    Before CK-92010 is molded into chemical transfer pump volutes and impellers for dilute alkaline cleaning solutions at 40 °C, ASTM D543-20 immersion data must establish that mass uptake and dimensional swelling remain within C-slot tolerances. Compliance testing follows ASTM D543-20 Test Method for Resistance of Plastics to Chemical Reagents and ISO 175:2010; the immersion medium is 5 wt% sodium hydroxide at 40 °C for 168 h, with mass change below 0.8% and tensile strength retention above 85%. The formulation addition ratio is 99 wt% CK-92010 with 1 wt% hydrolysis-stabilizer masterbatch; no regrind is permitted in the impeller shot because melt-flow variation from repeated heat history disturbs final balance. The downstream production process uses 500–800 t injection machines with 50 mm screw diameter, melt temperature 225–235 °C, mold temperature 60–80 °C, and packing pressure 50–70 MPa held for 20–30 s to eliminate thick-wall voids. After demolding, impellers are annealed at 120 °C for 2 h in an air-circulation oven to reduce internal stress, then machined on carbide tooling because glass fibers are abrasive. Balance is verified to ISO 1940-1:2003 grade G6.3. Process audits have shown that when the screw cushion falls below 3 mm, gas entrapment increases and fiber crowding at the shroud-to-blade transition reduces Charpy impact tested per ISO 179-1/1eA; gate location at the hub center is therefore fixed to preserve fiber orientation. Terminal product types include chemical metering pump impellers, volute casings, and filter housings.

    Free Quote

    Competitive Kingfa CK-92010,PP Reinforced,Glass Fiber prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa CK-92010 is a chemically coupled 10 wt% E-glass fiber–reinforced polypropylene compound in the CK series. The grade belongs to the PP-GF family and is intended for injection-molded semi-structural parts that require higher modulus, reduced linear thermal expansion, and improved dimensional stability relative to unfilled PP while retaining lower density and lower melt viscosity than 20 wt% and 30 wt% glass-fiber grades. The product is distinguished by a nominal glass fiber content of 10 wt%, a silane coupling package, and a heat-stabilized polypropylene matrix. The pellet form is typically cylindrical granules of 3–4 mm nominal length.

    Because the current CK-92010 datasheet is not publicly distributed in full, the numerical ranges in Table 1 are compiled from publicly available Kingfa PP-GF product-family data and from representative values for a coupled 10 wt% E-glass-filled PP homopolymer. They are suitable for preliminary material selection but should be replaced by lot-specific certificates of analysis for production part qualification.

    Table 1. Typical property ranges for Kingfa CK-92010 PP-GF10
    PropertyTest methodTypical range or condition
    Glass fiber contentISO 3451-110 ± 2 wt%
    DensityISO 1183-10.96–0.98 g/cm³
    Melt flow rateISO 1133-18–15 g/10 min at 230 °C/2.16 kg
    Tensile strength at yieldISO 527-232–42 MPa
    Tensile modulusISO 527-22100–2600 MPa
    Flexural modulusISO 1781900–2400 MPa
    Elongation at breakISO 527-25–12%
    Notched Charpy impact at 23 °CISO 179-1/1eA4–7 kJ/m²
    Heat deflection temperature BISO 75-2/B, 0.45 MPa95–110 °C
    Mold shrinkage, flow directionISO 294-40.5–0.8%

    The 10 wt% fiber loading modifies the polymer morphology and processing behavior in measurable ways. Flow-direction coefficient of linear thermal expansion is typically 45–65 × 10⁻⁶ K⁻¹, while transverse-direction values fall near 70–90 × 10⁻⁶ K⁻¹; unfilled PP homopolymer commonly exhibits 100–120 × 10⁻⁶ K⁻¹. This anisotropy is the primary source of out-of-plane distortion in flat, ribbed parts. Shrinkage parallel to flow is lower than transverse shrinkage by 0.3–0.5 percentage points, which requires gate placement and packing pressure to be evaluated before tool steel is cut.

    In relation to unfilled PP, CK-92010 raises tensile modulus by 60–120%, flexural modulus by 70–130%, and heat deflection temperature by 20–35 °C, depending on matrix melt flow rate and coupling efficiency. These gains are obtained with a density penalty of 0.06–0.08 g/cm³ and a reduction in elongation at break from typical unfilled values of 30–300% to 5–12%. Weld-line tensile strength retention is a known limitation: glass fibers orient predominantly in the flow direction and do not bridge knit lines effectively, so weld-line strength is commonly 35–50% of the bulk tensile strength. Load-bearing rib structures should therefore avoid placing knit lines in high-tensile-stress zones.

    Thermal Processing Envelope and Screw Configuration Requirements

    Injection molding of CK-92010 should be treated as a moderately abrasive, mildly hygroscopic glass-filled PP process. Drying is not mandatory when packaging is intact and ambient relative humidity is below 60%, but surface moisture from open storage requires predrying in a desiccant dryer at 80 °C for 2–4 h. Melt temperature should be held between 210 °C and 240 °C; short excursions above 260 °C should be avoided because polypropylene undergoes oxidative chain scission and the silane sizing on glass fibers degrades. Mold temperature should be controlled in the range of 20–60 °C, with the upper half used where weld-line strength and transverse dimensional stability are more important than cycle time. For thin-wall sections of 1.5–3.0 mm, filling pressure typically falls between 60 MPa and 100 MPa, and hold pressure is usually 60–80% of peak filling pressure.

    General-purpose polyolefin screw geometry is preferred. A screw with L/D of 20:1–24:1 and compression ratio of 2.2:1–2.8:1 limits glass fiber attrition. High-shear mixing sections should be avoided because excessive screw speed fractures fiber bundles and reduces final fiber length. Screw speed is typically set at 40–80 rpm, and back pressure is maintained at 0.5–1.0 MPa. Production-scale compounding studies indicate that fiber length distribution shifts toward 0.15–0.35 mm when screw speed exceeds 600 rpm on a 40:1 twin-screw extruder, reducing tensile modulus by 8–12% relative to lower-shear profiles. Injection molding machines processing glass-filled PP should use nitrided or bimetallic barrels, through-hardened screw tips, and frequent check-ring clearance inspection. For production runs exceeding 100 t, non-return valve clearance should be verified every 10,000 cycles because glass fibers accelerate screw, barrel, and check-ring wear.

    Residence time at melt temperature should not exceed 8–10 min in the barrel; longer residence times produce yellowing, black specks from degraded sizing, and reductions in notched Charpy impact. Hot runner systems should use externally heated manifolds with low-shear tip geometries. Internal hot runner dead spots can accumulate degraded polymer that later releases visual contamination into molded parts. Regrind of CK-92010 should be limited to 20 wt% of total shot mass because repeated processing reduces fiber length and impact resistance. After three regrind cycles, fiber length commonly falls below 0.2 mm, and notched impact may drop by 25–35% relative to virgin material.

    What Distinguishes a 10 wt% Glass-Fiber PP from Talc-Filled and Higher-Glass Systems?

    Against a 20 wt% glass-fiber PP, CK-92010 gives approximately 10–18% lower density, 20–25% lower tensile modulus, and 15–25 °C lower heat deflection temperature. The compensating advantages are reduced mold filling pressure, less fiber-related mold abrasion, fewer surface splay defects, and lower warpage in complex geometries. Against a 30 wt% glass-fiber PP, the density difference reaches roughly 0.15 g/cm³, while tensile modulus is 45–60% lower. The 10 wt% grade is therefore not a substitute for high-load-bearing seating structures or underhood structural brackets that require continuous stress at elevated temperature.

    Compared with 20 wt% talc-filled PP, CK-92010 has similar density and heat deflection temperature but higher tensile strength and better creep resistance above 80 °C. However, talc-filled PP produces less anisotropic shrinkage and less warpage in flat thin-wall parts because talc platelets align less strongly than glass fibers. Glass fiber gives higher notched impact and better resistance to fatigue crack growth, but it also increases mold wear and visible fiber orientation at the part surface. For flat parts where low warpage dominates, talc-filled PP may be selected; for parts requiring higher tensile strength, vibration resistance, or creep resistance, glass-fiber reinforcement is preferred.

    Table 2. Comparative property matrix for mineral- and glass-reinforced PP systems
    MaterialDensity rangeTensile modulus rangeFlow-direction CLTE rangeMold shrinkage rangeHDT B range
    Unfilled PP homopolymer0.90–0.91 g/cm³1300–1800 MPa100–120 × 10⁻⁶ K⁻¹1.2–1.8%75–90 °C
    Kingfa CK-92010 PP-GF100.96–0.98 g/cm³2100–2600 MPa45–65 × 10⁻⁶ K⁻¹0.5–0.8%95–110 °C
    PP-GF201.03–1.06 g/cm³3500–4500 MPa30–45 × 10⁻⁶ K⁻¹0.3–0.5%120–140 °C
    PP-GF301.12–1.15 g/cm³5000–6500 MPa25–35 × 10⁻⁶ K⁻¹0.2–0.4%130–150 °C
    PP-T20 talc-filled1.04–1.06 g/cm³2200–2800 MPa60–80 × 10⁻⁶ K⁻¹0.7–0.9%95–110 °C

    Automotive applications for CK-92010 include cooling fan shrouds, air intake brackets, battery trays, and interior structural frames where continuous service temperatures remain below 100 °C and short-term peaks do not exceed 120 °C. Published data for this specific configuration is limited; an application-specific heat-aging study at 120 °C for 1000 h per ISO 188 is required before use in continuous underhood service. Mold flow simulation using measured fiber orientation and pvT data should be considered before tool release because glass-filled PP warpage prediction is unreliable when unfilled PP shrinkage data are used.

    Electrical and appliance housing use is limited to non-flame-retardant service. CK-92010 is normally rated UL 94 HB at 1.5 mm; any enclosure requiring V-2, V-0, or glow-wire ignition below 850 °C per IEC 60695-2-12 must use a flame-retardant variant unless the specific CK-92010 lot is explicitly certified otherwise. Comparative tracking index of glass-filled PP can fall from unfilled PP values above 600 V to 500–600 V per IEC 60112; the exact value depends on surface finish, colorant package, and glass content and must be verified on the molded part.

    The polypropylene matrix resists dilute acids, alkalis, ethylene glycol coolant, and many aqueous salt solutions. It is incompatible with strong oxidizing acids, aromatic solvents, and chlorinated hydrocarbons at elevated temperature. Contact with copper-based alloys may accelerate thermo-oxidative degradation in long-term hot-air service. For food-contact use, lot-specific verification of migration limits under EU 10/2011 or FDA 21 CFR 177.1520 is required, including the glass fiber sizing package. The base polypropylene may meet the olefin polymer specification, but the silane coupling agent and sizing components are not automatically included in food-contact approvals and must be confirmed with the manufacturer.