| HS Code | 384193 |
| Density | 0.99 g/cm3 |
| Glass Fiber Content | 10% |
| Melt Flow Rate | 10 g/10 min |
| Tensile Strength | 45 MPa |
| Tensile Elongation At Break | 5% |
| Flexural Modulus | 2500 MPa |
| Notched Izod Impact Strength | 5 kJ/m2 |
| Heat Deflection Temperature | 120 °C at 0.45 MPa |
| Melting Temperature | 165 °C |
| Vicat Softening Temperature | 150 °C |
| Water Absorption | 0.02% |
| Mold Shrinkage | 0.6% |
| Flammability | HB |
As an accredited Kingfa GFPP-10,PP-GF10,Glass Fiber Reinforced factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg moisture-proof, polyethylene-lined paper bags, palletized and shrink-wrapped for safe transport. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25 kg bags of Kingfa GFPP-10 PP-GF10 glass fiber reinforced compound, properly secured for export shipment. |
| Shipping | Kingfa GFPP-10 (PP-GF10) glass fiber reinforced polypropylene compound ships as non-hazardous solid pellets in moisture-barrier bags or octabins. Store dry, away from direct sunlight and heat. Handle per SDS; no UN hazard class, special transport labeling, or segregation normally required. Use sealed, labeled containers and avoid moisture ingress during loading. |
| Storage | Store Kingfa GFPP-10 (PP-GF10, glass fiber reinforced polypropylene) in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep in original, closed containers to prevent moisture and dust contamination. Avoid contact with incompatible chemicals and strong oxidizing agents. Maintain good housekeeping to control dust and static; use appropriate PPE and follow local regulations. |
| Shelf Life | Kingfa GFPP-10 typically has a 24-month shelf life when stored unopened in a cool, dry, well-ventilated area away from direct sunlight. |
Kingfa GFPP-10, also designated PP-GF10, is a 10% glass fiber reinforced polypropylene injection molding grade in which chopped E-glass strands are dispersed in a polypropylene matrix. The reinforcement level is nominal and should be confirmed by ISO 3451-1 Method A ash determination, with an expected ash content of 10% ± 2% after accounting for pigment and stabilizer residue. Before molding, the pellets must be dried to a residual moisture content below 0.05% by weight as measured by ISO 15512 Method A. A dehumidifying hopper dryer set at 80°C for 2 h is acceptable when the material has been stored in sealed original packaging below 60% relative humidity. If the package has remained open for more than 4 h or the plant relative humidity exceeds 60%, the drying time should be extended to 3 h. Drying above 90°C should be avoided because the antioxidant package can be partially consumed and surface oxidation may occur. Processing should begin with a nozzle melt temperature between 230°C and 250°C, a mold surface temperature between 30°C and 60°C depending on skin-layer and gloss requirements, and hydraulic back pressure between 50 bar and 100 bar to maintain fiber dispersion. These values are starting ranges, not lot-specific processing guarantees; the certificate of analysis for each Kingfa GFPP-10 lot should be checked for melt flow rate measured under ISO 1133-1:2022 at 230°C/2.16 kg.
| Processing parameter | Starting setpoint range | Instrument or test basis |
|---|---|---|
| Hopper throat temperature | 30°C to 50°C | Contact thermocouple |
| Barrel zones, rear to front | 220°C to 250°C | Machine controller thermocouple |
| Nozzle melt temperature | 230°C to 250°C | Insertion pyrometer |
| Mold surface temperature | 30°C to 60°C | ISO 294-4:2018 surface probe |
| Hydraulic back pressure | 50 bar to 100 bar | Hydraulic pressure gauge |
| Injection speed | 60 cm³/s to 120 cm³/s | Screw displacement transducer |
| Holding pressure | 35 MPa to 55 MPa | Hydraulic or cavity transducer |
| Shot cushion | 3 mm to 6 mm | Screw position indicator |
| Screw specification | L/D 20:1 to 24:1, 2.5:1 compression ratio | General-purpose PP screw |
In automotive cabin HVAC blower impellers, the component is exposed to centrifugal stress, thermal soak near 80°C, and rotational speeds that can reach 3,500 rpm in compact blower units. Kingfa GFPP-10 is used where unfilled polypropylene would exhibit excess creep deflection and where 20% glass fiber would raise density and produce noisier gate vestiges. The 10% glass fiber content increases flexural modulus measured by ISO 178 sufficiently to hold blade tip gap below 1.5 mm across the operating temperature window, but only when the gate location produces a predominantly radial flow pattern. A single center gate or a valve-gated hot runner at the hub is preferred; edge-gated layouts generate multiple weld lines at the blade root, where short glass fibers align parallel to the melt front and sacrifice reinforced tensile strength. Published studies on short-glass polypropylene systems indicate that weld-line tensile strength can be 20% to 40% lower than bulk material, depending on melt front angle and fiber content. The cavity filling phase should use an injection speed of 80 cm³/s to 100 cm³/s to avoid shear heating above 250°C, while holding pressure is maintained at 40 MPa to 50 MPa for 4 s to 8 s. Mold temperature is held at 50°C to 60°C to form a resin-rich skin that reduces exposed fiber at the blade surface. For impellers with a shot weight of 150 g to 400 g, clamp force of 1200 kN to 1800 kN is normally sufficient; the exact requirement must be calculated from projected area and a cavity pressure estimate of 30 MPa to 40 MPa. Dimensional testing per ISO 294-4:2018 should confirm longitudinal shrinkage of approximately 0.4% to 0.8% and transverse shrinkage below 1.0%, because fiber orientation produces anisotropic contraction. The terminal component is a cabin blower impeller or HVAC fan shroud in which residual imbalance is specified by the OEM but frequently controlled to grade G 6.3 per ISO 21940-11.
Washing machine drain pump housings and filter caps molded from Kingfa GFPP-10 operate in intermittent contact with dilute alkaline detergent solutions at 40°C to 60°C, with short-term exposure to sodium perborate and protease-containing detergents. The part is not a pressure vessel; the main requirements are chemical resistance, thread dimensional stability, and low water uptake. At 10% glass fiber by weight, the compound provides sufficient hoop stiffness for a wall section of 1.5 mm to 2.5 mm, but exposed glass fiber ends can produce capillary wicking if the resin-rich outer skin is disrupted by low mold temperature or high fiber breakage at the gate. A mold surface temperature of 60°C is therefore preferred to promote skin-layer formation at the thread roots, while the injection speed should be set to fill the cavity in 0.8 s to 1.5 s to avoid premature freeze-off in thin thread flanks. Hydraulic holding pressure is typically 35 MPa to 50 MPa; the gate land should be inspected after every 5,000 cycles because glass fiber abrasion can reduce land depth and produce jetting marks. Water uptake after 24 h immersion at 23°C should be below 0.5% by ISO 62; parts that exceed this threshold often show surface delamination or exposed fiber bundles from excessive screw wear. Threaded inserts are post-molded, not insert-molded, because differential shrinkage around metal inserts generates hoop stresses that can exceed the weld-line strength of short-glass polypropylene. The terminal parts are drain pump housings and filter caps for domestic washing machines; their appliance safety context is IEC 60335-1, and the mechanical data baseline includes ISO 527-2 for tensile properties and ISO 178 for flexural modulus.
Low-voltage junction boxes and consumer electrical enclosures molded from Kingfa GFPP-10 rely on glass fiber reinforcement to reduce post-mold shrinkage and lid distortion that occur with unfilled polypropylene during warehouse storage at elevated ambient temperature. At 10% glass fiber by weight, the material carries a UL 94 HB classification at 1.5 mm; a V-2 or V-0 classification requires a flame-retardant package that must be validated with the specific masterbatch and not assumed from the base resin data sheet. The processing window for a junction box with 1.5 mm to 2.0 mm wall thickness uses a valve-gated hot runner to eliminate cold-runner stringing and to control gate freeze time. Barrel temperatures are set from 220°C at the throat to 245°C at the nozzle; mold temperature should be held at 40°C to 50°C to balance cycle time and dimensional repeatability. A flow-length to wall-thickness ratio of 100:1 is generally achievable, but beyond this value the melt pressure requirement increases rapidly and glass fiber orientation near the flow front produces unacceptable warpage. After molding, the cover and base should be assembled dry and subjected to a 24 h dimensional check at 23°C ± 2°C and 50% ± 10% relative humidity per ISO 291. Heat ageing at 85°C for 1000 h according to ISO 188 should be used to identify lot-to-lot variation in stabilizer efficiency; published data for this specific grade under all pigment variants is limited, so aged tensile strength retention must be measured on production lots rather than inferred from general PP-GF10 literature. The terminal product is a junction box or consumer electrical enclosure where dimensions are specified by IEC 60670-1 and the material must withstand screw-torque assembly without boss cracking. Electrical products must also be evaluated against RoHS 2011/65/EU and REACH SVHC disclosure requirements for the specific color and additive package.
| Downstream segment | Material property or test | Standard designation | Acceptance basis |
|---|---|---|---|
| Automotive HVAC impeller | Dynamic balance grade | ISO 21940-11 | G 6.3 unless OEM specifies otherwise |
| Washing machine pump housing | Water uptake | ISO 62 | Below 0.5% after 24 h |
| Junction box | Heat ageing tensile retention | ISO 188 at 85°C for 1000 h | Report measured value per production lot |
| Office chair armrest frame | Cyclic durability protocol | ANSI/BIFMA X5.1-2017 | Pass/fail per referenced test method |
| Outdoor power equipment housing | Xenon arc weathering | ISO 4892-2 | ΔE below 3.0 after 500 h for black |
| Under-hood bracket | Creep deflection | ISO 899-2:2003 at 80°C | Fixture-specific measurement required |
In contract furniture, Kingfa GFPP-10 is processed into armrest frames, lumbar support shells, and chair back components where 10% glass fiber provides a measurable increase in rigidity over talc-filled polypropylene without the higher density and brittleness of 20% glass fiber compounds. The mechanical loading in these components is often one-sided bending and cyclic fatigue rather than constant creep; therefore the relevant laboratory test is ISO 178 flexural modulus combined with a cyclic load protocol under ANSI/BIFMA X5.1-2017 for contract seating. The material should be dried at 90°C for 2 h if the plant environment is above 55% relative humidity, because surface splay on large curved shells cannot be removed by rework. During injection, mold temperature is maintained at 30°C to 40°C to achieve a matte surface finish, but the low surface temperature increases frozen-in stress near mounting bosses. To prevent boss cracking during threaded fastener installation, the boss should be designed with a diameter ratio of 2.0 to 2.5 times the screw outer diameter and a receive length that allows screw torque of 1.5 N·m to 2.0 N·m without stripping. The glass fiber content is verified by ISO 3451-1 ash; lot-to-lot variation above 2% absolute fiber content can shift shrinkage enough to affect snap-fit gaps on chair backs. The terminal products are office chair armrest frames and lumbar supports; these parts must pass the cyclic durability protocols in ANSI/BIFMA X5.1-2017, and any color masterbatch used at the press must be checked for melt flow and UV stability before production, because dark colored parts exposed near windows may fade unevenly in field service.
Outdoor power equipment covers, string trimmer engine housings, and blower volutes made from Kingfa GFPP-10 require a balance of stiffness, low density, and surface durability under UV radiation. The component wall thickness is normally 2.0 mm to 3.0 mm, allowing the 10% glass fiber content to raise flexural modulus without causing severe warpage at the housing perimeter. Weathering resistance should be evaluated using ISO 4892-2 Xenon arc exposure; for black housings, a ΔE shift below 3.0 after 500 h is a common starting criterion, but product-specific performance must be confirmed because pigments and UV stabilizers interact with glass fiber sizing. The notched impact strength measured by ISO 180/A is typically lower than that of unfilled polypropylene, so the design should avoid sharp corners and abrupt wall-section transitions that concentrate stress at the fiber-matrix interface. Molding is performed with a melt temperature of 235°C to 245°C, a mold temperature of 40°C, and a slow to medium injection speed to minimize fiber orientation anisotropy across the volute tongue. Post-molding dimensional stability is checked after 48 h at 23°C ± 2°C; parts measured before full crystallization may show shrinkage drift of up to 0.2% and should not be used for quality release. The terminal product is a lawn tool housing or blower volute in which the material must survive stone impact and vibration without cracking, and the glass fiber reinforcement must not protrude through the outer surface because exposed fibers accelerate moisture intake and UV discoloration.
Because under-hood brackets and sensor mounts absorb continuous underbonnet heat, the selection of Kingfa GFPP-10 is restricted to locations where the metal part temperature does not exceed 95°C in continuous operation and 110°C for intermittent spikes. The 10% glass fiber reinforcement raises the heat deflection temperature under ISO 75-2:2013 Method B by roughly 10°C to 20°C compared with unfilled polypropylene, but this remains below the performance of PA66-GF or PBT-GF in the same bracket geometry. The relevant material test is creep modulus under ISO 899-2:2003 at 80°C; published data for this specific Kingfa grade under a tensile creep load is limited, so long-term deflection must be validated on a fixture that reproduces the exact mounting bolt torque and air gap. In processing, the bracket should be center-gated or fed through a tab gate at the thickest section to avoid fiber orientation perpendicular to the principal bending direction. The melt temperature is held at 240°C, the mold temperature at 50°C, and the packing pressure is increased in two steps from 30 MPa to 45 MPa to reduce sink marks around the mounting bosses. After ejection, parts should be placed on a cooling fixture for 20 min to control flatness; free cooling on a mesh belt can produce warpage of 0.5 mm to 1.0 mm across a 200 mm span. The terminal products are engine-bay brackets and sensor mounting plates in which dimensional stability during thermal cycling to 110°C must be verified by measurement after 10 cycles of 30 min heat soak and 30 min ambient cooling per ISO 188 or the OEM-specific thermal cycle protocol.
Competitive Kingfa GFPP-10,PP-GF10,Glass Fiber Reinforced prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa GFPP-10, designated PP-GF10, is a short glass fiber reinforced polypropylene compound containing 10% by weight chopped E-glass fiber. The compound is produced by melt compounding a polypropylene homopolymer or copolymer matrix with glass fiber and a coupling agent, typically maleic anhydride grafted polypropylene. The product belongs to the lower glass loading segment of the Kingfa GFPP series and is specified where stiffness, heat deflection temperature, and dimensional stability must exceed unfilled polypropylene without the density increase and weld-line strength reduction associated with 20% or 30% glass fiber reinforced grades. In injection molding operations, GFPP-10 is used for structural brackets, fan shrouds, appliance housings, electrical enclosure frames, and automotive interior carrier components.
Because the material is a semicrystalline thermoplastic with discontinuous fibers, mechanical properties are direction-dependent. Flow-induced fiber orientation during mold filling produces higher tensile modulus along the flow direction and lower properties transverse to flow. This anisotropy is less pronounced at 10% glass loading than at 20% or 30%, which is one of the principal differences from higher glass fiber grades. The lower fiber content also reduces melt viscosity and improves surface appearance, although it sacrifices some flexural modulus and heat deflection temperature.
The property envelope for a 10% glass fiber reinforced polypropylene compound class is summarized in the following comparative table. Values represent typical published ranges under the cited test standards and should not be interpreted as guaranteed lot-specific values for Kingfa GFPP-10 without a certificate of analysis.
| Property | Test method | Unfilled PP | GFPP-10 / PP-GF10 typical range | GFPP-20 typical range |
|---|---|---|---|---|
| Density | ISO 1183-1 | 0.90–0.92 g/cm³ | 0.96–1.00 g/cm³ | 1.03–1.06 g/cm³ |
| Tensile strength at yield | ISO 527-2 | 25–35 MPa | 40–55 MPa | 55–70 MPa |
| Tensile modulus | ISO 527-2 | 1.2–1.7 GPa | 2.5–4.0 GPa | 3.5–5.5 GPa |
| Flexural modulus | ISO 178 | 1.0–1.6 GPa | 2.2–3.2 GPa | 3.0–4.5 GPa |
| Charpy notched impact, 23 °C | ISO 179-1/1eA | 2–5 kJ/m² | 5–8 kJ/m² | 6–10 kJ/m² |
| Heat deflection temperature A, 1.8 MPa | ISO 75-2 | 50–65 °C | 105–135 °C | 120–150 °C |
| Melt flow rate, 230 °C, 2.16 kg | ISO 1133-1 | 10–30 g/10 min | 5–15 g/10 min | 4–12 g/10 min |
| Molding shrinkage | ISO 294-4 | 1.2–2.0 % | 0.6–1.0 % | 0.3–0.7 % |
Compared with unfilled polypropylene, GFPP-10 raises tensile modulus by a factor of roughly 2, flexural modulus by roughly 2–3, and heat deflection temperature by approximately 50–80 °C. Compared with GFPP-20, GFPP-10 typically exhibits lower density by 0.04–0.08 g/cm³, lower tensile strength by 10–15 MPa, and slightly higher molding shrinkage. The 10% glass content also produces less notch sensitivity than 20% glass content when evaluated with Charpy impact at 23 °C, although values remain below unfilled impact-copolymer polypropylene. These differences are relevant when selecting between GFPP-10 and GFPP-20 for thin-wall parts that require a balance of stiffness and impact performance.
On production-scale injection molding lines, GFPP-10 feedstock is normally processed with a melt temperature of 190–230 °C measured at the nozzle, a mold surface temperature of 30–60 °C, and a holding pressure of 30–70 MPa. Injection velocity is selected to fill the cavity in 0.5–2.0 s for parts of 2–3 mm nominal wall thickness; slower velocities risk premature freeze-off of the fiber-filled melt, while excessively fast filling increases shear heating and fiber breakage. Screw back pressure in the range of 2–6 MPa is applied to maintain homogeneous fiber distribution. Pre-drying is not always mandatory for sealed packaging, but pellets exposed to relative humidity above 60 % should be dried at 80 °C for 2–4 hours in a desiccant dryer to prevent surface splay. In twin-screw compounding, screw L/D ratios of 40:1 or greater are common, and fiber length retention after compounding is typically in the 0.2–0.5 mm number average range. The resulting fiber length distribution influences mechanical properties more than the nominal glass weight fraction alone.
Melt flow rate for GFPP-10 is typically reported in the range of 5–15 g/10 min under ISO 1133-1 at 230 °C with a 2.16 kg load. This is lower than unfilled polypropylene of equivalent base resin, due to the restriction of chain mobility by glass fibers. The melt viscosity of glass-filled polypropylene is shear-thinning; higher injection speeds therefore improve flow length more than proportional increases in melt temperature. The maximum recommended processing temperature is 240 °C; exposure above this limit can initiate thermal oxidative degradation of the polypropylene matrix and coupling agent, leading to discoloration and loss of fiber–matrix adhesion. Barrel residence time should be kept below 10 minutes at temperatures above 220 °C to avoid molecular weight reduction.
In washing machine outer tubs, fan shrouds, and electrical enclosure frames, GFPP-10 is selected when the component undergoes cyclic mechanical loading at temperatures up to approximately 90–100 °C. The material is not recommended for continuous load-bearing applications above 100 °C unless creep data under ISO 899-1 confirm adequate deformation control. For automotive interior carrier structures, GFPP-10 can replace talc-filled polypropylene in parts where lower density and higher tensile strength are required, but the surface finish of glass-filled grades is generally inferior to talc-filled grades. When a Class A visible surface is required, GFPP-10 must be painted, grain-textured, or covered with a decorative layer. Published data for OEM approval status of this specific configuration are limited; technical approval must be validated against the relevant OEM material specification.
Molding shrinkage of GFPP-10 is lower and more directionally anisotropic than unfilled polypropylene. Under ISO 294-4, linear shrinkage parallel to flow is typically 0.3–0.6 %, whereas transverse shrinkage is typically 0.7–1.0 %. Higher glass contents reduce overall shrinkage further, but increase the difference between flow and transverse directions, which can increase warpage in flat, unreinforced geometries. GFPP-10 therefore offers a middle point: lower overall shrinkage than unfilled PP and less anisotropy than GFPP-20 or GFPP-30. Tooling design should anticipate this by specifying gate placement that aligns the primary flow direction with the part’s longest dimension or with the axis of expected thermal contraction. For precision parts, prototype tools should be built with steel-safe dimensions and adjusted after mold shrinkage studies.
GFPP-10 is not inherently flame retardant. If a UL 94 V-0 or V-1 classification is required, the molder must select a specifically flame-retardant compounded grade; standard GFPP-10 without FR additives is generally rated HB under UL 94. The coupling system used for glass fiber adhesion is sensitive to acidic or basic additive packages. Combining GFPP-10 with amine-based heat stabilizers or certain primary antioxidants can reduce fiber–matrix adhesion and lower tensile strength after heat aging. The material should not be exposed to strong oxidizing acids, concentrated peroxides, or boiling chlorinated solvents. Regulatory declarations must be obtained for each production lot; glass fiber reinforced polypropylene compounds are typically evaluated under REACH SVHC screening, RoHS Directive 2011/65/EU Annex II, and, for Chinese domestic applications, GB/T 15588-2013. Food-contact suitability is not automatic and requires explicit testing under FDA 21 CFR 177.1520 or EU Regulation 10/2011.