Kingfa GFPP-20,PP-GF20,Glass Fiber Reinforced

    • Product Name: Kingfa GFPP-20,PP-GF20,Glass Fiber Reinforced
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 493344
    Polymer Type Polypropylene
    Glass Fiber Content 20% by weight
    Density 1.04 g/cm³
    Melt Flow Rate 10 g/10 min
    Tensile Strength 60 MPa
    Elongation At Break 3%
    Flexural Modulus 3000 MPa
    Flexural Strength 85 MPa
    Notched Izod Impact Strength 50 J/m
    Heat Deflection Temperature 1 8 Mpa 150 °C
    Molding Shrinkage 0.4–0.8%
    Water Absorption 0.02%
    Flammability HB
    Thermal Expansion Coefficient 3.0×10⁻⁵ /°C

    As an accredited Kingfa GFPP-20,PP-GF20,Glass Fiber Reinforced factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa GFPP-20 glass fiber reinforced polypropylene is packaged in 25 kg sealed moisture-barrier bags, palletized for industrial shipping.
    Container Loading (20′ FCL) Kingfa GFPP-20 glass fiber reinforced PP pellets in 20′ FCL, 25 kg palletized bags, securely stowed with moisture protection and weight limits observed.
    Shipping Kingfa GFPP-20 (PP-GF20, glass fiber reinforced polypropylene) is normally shipped as a non-hazardous solid in sealed moisture-barrier bags, packed in cartons/boxes on pallets. Keep dry, cool, ventilated, and protected from sunlight; handle with standard industrial precautions.
    Storage Store Kingfa GFPP-20 (PP-GF20, glass fiber reinforced polypropylene) in a cool, dry, well-ventilated area away from direct sunlight, heat sources, ignition, moisture, and strong oxidizers. Keep in original sealed packaging, protect from physical damage and dust, and use first-in-first-out stock rotation. Avoid prolonged high humidity or temperature exposure to preserve material properties.
    Shelf Life No specific shelf life is stated; material is stable under normal storage conditions in a cool, dry, sealed container.
    Application of Kingfa GFPP-20,PP-GF20,Glass Fiber Reinforced

    Kingfa GFPP-20, a 20 wt% chemically coupled short glass fibre reinforced polypropylene compound, is evaluated for injection-moulded automotive cooling fan shrouds in a thermal environment defined by continuous radiator outlet air at 90–105°C and intermittent under-bonnet soak peaks up to 120°C. The material is not a direct dimensional substitute for unreinforced polypropylene because the ISO 294-4 longitudinal mould shrinkage falls to 0.4–0.8% while transverse shrinkage remains 0.8–1.2%; this anisotropy produces out-of-round fan ring conditions if a tool originally machined for neat PP is used without gate and wall-stock revision. The ISO 178 flexural modulus of the glass-filled grade lies in the range 3800–4600 MPa at 23°C, which controls fan ring distortion when the rotating assembly carries a static out-of-balance load of 50 g·mm. Drying is executed in a dry-air desiccant dryer at 80°C for 2–4 h with an inlet air dew point below -30°C when regrind content exceeds 15%; moisture levels above 0.08% by weight cause gate-area splay and measurably weaken fibre-matrix adhesion at the outer ring weld line.

    The processing window on a 500–800 t hydraulic clamp injection moulding machine is established around a barrel profile of 210/220/230/240/240°C from feed throat to nozzle, with screw peripheral speed held at 0.3–0.5 m/s and back pressure at 0.5–1.0 MPa. The screw is specified with an L/D of 20:1 to 22:1 and a compression ratio of 2.5:1; a barrier screw with a shallow metering depth is preferred because glass fibre breaks during plastication and reduces mean fibre length from a pellet value of 300–500 µm to 180–250 µm in the moulded part. The gate is placed on the central hub boss rather than on the outer ring because radial flow from a hub gate orients glass fibres tangentially at the ring, increases hoop-direction stiffness, and reduces the tensile strength loss associated with the ring weld front. Weld-line tensile strength retention under ISO 527-2/1A must be validated on the production tool; published retention factors for 20 wt% short-glass polypropylene range from 0.55 to 0.75 depending on melt contact temperature at the weld front and pack time. Mould temperature is not raised above 60°C because higher temperatures increase additive migration to the surface and produce white blush at the fan ring; mould temperatures below 30°C create an excessively thick quenched skin layer that reduces notched impact response at ring ribs under ISO 179-1/1eA.

    The finished shroud is tested under SAE J1639 for under-bonnet plastic components, and the mineral/glass formulation is checked for coolant resistance by immersion according to ISO 175 with a 50/50 ethylene glycol-water mixture at 90°C for 7 days. The flammability classification is UL 94 HB at 3.0 mm thickness; a thicker wall does not automatically improve the rating because glass fibre tends to increase afterglow if ignition occurs. The terminal moulded product is a cooling module fan shroud with a nominal wall of 2.5–3.0 mm, a hot runner valve gate at the hub, and an outer ring flatness tolerance of 1.0 mm across a 400 mm diameter. The operational boundary is set by long-term heat aging: continuous service above 120°C requires a heat-stabilised package validated under ISO 188 because neat GFPP-20 will embrittle as antioxidant additives are consumed.

    RequirementStandard or clauseGFPP-20 target or boundary
    DensityISO 1183-11.04–1.06 g/cm³
    Tensile stress at breakISO 527-2/1A80–100 MPa
    Flexural modulusISO 1783800–4600 MPa
    Charpy notched impact at 23°CISO 179-1/1eA8–12 kJ/m²
    Heat deflection temperature at 1.8 MPaISO 75-2/Af150–155°C
    FlammabilityUL 94HB at 3.0 mm
    Longitudinal mould shrinkageISO 294-40.4–0.8%
    Transverse mould shrinkageISO 294-40.8–1.2%

    What Limits Weld-Line Strength in 20 wt% Glass-Filled Polypropylene Battery Tray Sub-Frames?

    Under-bonnet and packaged battery tray sub-frames moulded from GFPP-20 are subjected to multi-axis vibration, clamp force from the tray lid, and intermittent exposure to dilute sulphuric acid mist from vented lead-acid cells. The first design constraint is not bulk tensile strength, which is 80–100 MPa under ISO 527-2/1A, but weld-line strength at the fusion of two or more flow fronts behind mounting bosses, because glass fibres do not cross the weld interface in substantial volume. The weld-line tensile strength retention for short glass fibre polypropylene is governed by melt temperature, pack pressure, and the position of the weld relative to the gate; when the melt front temperature at the junction falls below 210°C, the skin layers do not inter-diffuse sufficiently and the weld line behaves as a low-strength notch. Production tool trials are conducted with a cavity pressure sensor located 10 mm from the weld line to ensure a pack pressure of 40–60 MPa is applied for 2–4 s after filling. The tensile creep modulus at 80°C and 1000 h under ISO 899-1 is more relevant than short-term modulus for a tray support that must retain torque on embedded brass inserts; publicly reported short-glass PP data indicate that creep modulus at 20 MPa initial stress may fall to 2200–2600 MPa, while exact values for Kingfa GFPP-20 must be taken from the supplier validation report because filler orientation and coupling chemistry shift the creep response.

    Insert moulding of M6 and M8 brass threaded bushes is allowed only when the insert is preheated to 90–110°C to prevent a frozen skin around the metal and to reduce hoop stress cracking under assembly torque. The barrel profile for this component is 215/225/235/245/245°C, and the mould temperature is held at 40–55°C to reduce post-mould crystallisation shrinkage after insert placement. The boss design uses an outer diameter-to-insert diameter ratio of at least 2.0 and a minimum boss wall of 3.0 mm around the bush; lower ratios create excessive tangential stress after cooling and lead to insert pull-out at torque levels below 8 N·m. The tray is dried at 80°C for 2–4 h before moulding when the storage relative humidity has exceeded 60%, because moisture on the glass fibre surface can generate splay and lower weld-line strength. The continuous service temperature for demoulded GFPP-20 battery trays is limited to 100°C; excursions above 120°C cause oxidative embrittlement unless a heat-stabilised package specified under ISO 188 is used.

    The compliance chain for this component includes ISO 16750-3 vibration profiles, ISO 179-1/1eA notched impact testing at -30°C, and UL 94 HB classification at 3.0 mm. The terminal product is a two-piece tray sub-frame with a mass of 1.1–1.4 kg, integrally moulded lid latch bosses, and a base plate rib pitch of 35–40 mm. The main failure mode observed on production-scale tools is not bulk fracture but crack initiation at the weld line under the central tie-down bracket; this is corrected by moving the weld line away from the tensile stress concentration and by increasing the hot runner nozzle temperature to 245°C to maintain the melt front above 220°C at the fusion zone.

    Power tool housing components made from 20 wt% glass fibre reinforced polypropylene require a deliberate rib-to-wall thickness ratio below 0.6 because the glass fibre alignment at the intersection of a 2.5 mm nominal wall and a 1.5 mm rib creates a local tensile zone that reduces impact energy absorption. Drop testing according to IEC 60068-2-31 with a 1.0 m drop on a 10 kg tool typically exposes failure not at the outer shell but at the screw boss base where a short glass fibre skin layer meets an unfavourable weld line. The grade is dried at 80°C for 2–3 h, then injected at 230–250°C and mould temperature 30–50°C; injection speed is set high enough to keep the flow front velocity above 200 mm/s at the gate but low enough to prevent jetting, because jetting produces chaotic fibre orientation and visible flow lines on textured surfaces. The tool is gated at the handle base rather than through the motor housing side wall to avoid a long flow path across the vent slots, which would lower mean fibre length and reduce the ISO 527-2/1A tensile strength at the far side of the housing.

    The formulation for this application typically includes 0.2–0.5 wt% of a hindered amine light stabiliser package when the tool is specified for outdoor cordless tool storage, and a 2 wt% colour masterbatch is used for brand-specific grey or orange colouring. The addition of colour masterbatch changes the viscosity and crystallisation rate; the melt temperature should be raised by 5°C when a high-carbon black masterbatch is compounded to avoid surface streaking. The finished housing is painted only after flame treatment or plasma surface activation because the glass fibres at the surface reduce wetting and create visible fibre read-through under a solid topcoat. The wear at the gate land is controlled by using hardened tool steel at 52 HRC or by applying a nitride coating at the gate and runner areas; glass fibre filled PP is more abrasive than unfilled PP and will open the gate diameter after 100,000–300,000 shots if the gate is not hardened.

    The compliance evaluation for the power tool housing uses IEC 60745-1 for mechanical strength and insulation, UL 94 HB for flammability at 3.0 mm, and RoHS 2011/65/EU for restricted substances. The GFPP-20 compound without flame retardant does not meet a V-0 requirement; if a V-0 classification is required, a separate flame-retardant grade must be selected and the processing window must be lowered because intumescent packages decompose above 230°C. The terminal product is a left-right split shell with an assembly flatness tolerance of 0.5 mm across a 200 mm matting face, and the moulded part accepts ultrasonic welding at the periphery only when the weld bead is placed away from glass-rich end-of-flow regions.

    When GFPP-20 Replaces 30 wt% Glass-Reinforced PA6 in Circulator Pump Housings

    Substitution of 30 wt% glass-reinforced polyamide 6 with GFPP-20 in circulator pump housings is driven by hydrolytic stability and lower water uptake, but the replacement is not stress-equivalent. Polyamide 6 absorbs up to 2.5–3.0% water at equilibrium at 50% RH, which reduces its ISO 527-2/1A tensile modulus by 20–30% and creates dimensional growth; GFPP-20 has a water absorption below 0.05% under ISO 62 at 24 h, so the housing remains stable in contact with water-glycol mixtures. The trade-off is that the flexural strength of GFPP-20 is typically 40–50% lower than that of conditioned PA6-GF30; therefore the pump housing wall thickness is increased from 3.0 mm to 4.0 mm and rib density is raised to compensate for lower load capacity. The processing window changes from a PA6 melt temperature of 280–300°C to a PP melt temperature of 230–250°C; the tool temperature is reduced from 80–90°C to 30–50°C, which alters crystallisation shrinkage and requires new tooling or insert adjustments.

    The mechanical sealing surface of the pump housing must be moulded or machined with a flatness tolerance below 0.15 mm across a 120 mm flange. GFPP-20 parts exhibit anisotropic shrinkage, with ISO 294-4 longitudinal shrinkage 0.4–0.8% and transverse shrinkage 0.8–1.2%; a tool designed without CAE compensation for glass orientation typically produces flange flatness above 0.3 mm and leakage at the lip seal. Inserted brass bearing sockets are preheated to 100°C and moulded with a 1.5 mm surrounding wall to reduce differential thermal stress during the -30°C cold start phase. The melt is processed through a screw with L/D 20:1 and a check ring clearance below 0.1 mm because glass fibre agglomerates at the non-return valve when shear heating is excessive. Back pressure is set at 0.3–0.6 MPa; higher back pressure increases fibre attrition and lowers the Charpy notched impact strength under ISO 179-1/1eA from 8–12 kJ/m² to below 6 kJ/m² at 23°C.

    The pump housing is not suitable for continuous service above 95°C with pressurised water because the polypropylene matrix softens and the creep rate accelerates; the grade should be specified only for cold-water circulation, solar thermal drainback circuits, or dishwasher internal circulation where the fluid temperature remains below 85°C. Chemical resistance is tested under ISO 175 with a 50/50 water-glycol mixture at 90°C for 7 days; the tensile strength retention should be above 85% against the unconditioned reference. The terminal product is a wet-rotor circulator pump housing with an integrally moulded volute and a split-line seal groove produced without flash exceeding 0.05 mm. The main field failure mode for improperly processed GFPP-20 in this application is fatigue crack initiation at the intersection of the volute tongue and the discharge flange, caused by glass fibre orientation transverse to the hydraulic load path.

    Electrical Enclosure Warpage Control Under IEC 60695-2-13 Glow-Wire Exposure

    Electrical distribution enclosures moulded from GFPP-20 require low voltage tracking resistance and mechanical protection under IEC 62208. The comparative tracking index of Polypropylene is generally above 600 V, but glass fibre can shift the result under IEC 60112 depending on coupling agent and surface finish; the enclosure supplier therefore requests batch-specific CTI data and tests the moulded surface rather than the pellet. The material is not inherently ignition-resistant: a UL 94 HB classification applies at 3.0 mm, and the glow wire ignition temperature under IEC 60695-2-13 is evaluated at 750°C for unattended appliances. GFPP-20 without flame retardant will not pass at 1.5 mm because polypropylene ignites and continues to burn; when a V-2 or V-0 rating is required, the grade must be modified with a flame-retardant system that can reduce tensile strength by 10–20% and requires a lower barrel profile to avoid package decomposition.

    For a 300 mm × 200 mm enclosure box with a nominal wall of 3.0 mm, the warpage mechanism is driven by differential shrinkage between the flow and cross-flow directions. The tool is gated centrally into the base wall or through a side film gate; fibre orientation creates a diagonal warpage pattern that is controlled by keeping the mould temperature at 45–55°C and applying a pack pressure of 60–80 MPa for 5–8 s after filling. Cooling time is set by the wall thickness and is typically 25–35 s with water at 15–20°C; the moulded flatness is held within 0.8 mm only when the tool temperature is uniform and the gate is placed to align glass fibres with the longest unsupported wall. Uneven cooling or a single edge gate produces a twist that exceeds 1.5 mm flatness and prevents the cover from sealing against the box gasket. The terminal product is a low-voltage distribution box with an IP55 sealing interface, an integrally moulded DIN rail support, and a wall thickness that supports knock-out openings without fracturing during installation.

    The enclosure is dried at 80°C for 2–4 h and processed with a melt temperature of 230–245°C; a nitrogen blanket on the hopper is not required but prevents moisture re-uptake when ambient relative humidity exceeds 70%. The regrind ratio is held below 25% because repeated processing reduces the mean glass fibre length and lowers the flexural modulus under ISO 178 from 3800–4600 MPa to below 3200 MPa after three grinding cycles. The main processing defect observed on production lines is a flow line at the knockout diaphragm, which is corrected by increasing the local wall thickness to 1.5 mm and by placing a small overflow tab to displace the cold slug. The compliance matrix for this application includes IEC 62208 for empty enclosure testing, IEC 60112 for CTI, IEC 60695-2-13 for glow wire, and RoHS 2011/65/EU for restricted substances.

    Reusable Logistics Pallet Loading Is Limited by Frozen Fibre Orientation at the Sprue Post

    In pallet and dunnage applications, GFPP-20 is used as a structural skin over a foamed or recycled PP core or as a solid injection-moulded runner. The grade’s flexural modulus under ISO 178 at 23°C is 3800–4600 MPa, but creep under a 1000 kg uniformly distributed load over 120 h at 40°C reduces the effective stiffness; racking performance according to ISO 8611-1 is therefore evaluated with the glass-filled PP top deck reinforced by ribs at 50 mm pitch. The sprue cone and the gate land are identified as the primary failure sites because the frozen orientation around the sprue post produces a notch-sensitive zone; a hot runner valve gate or a tab gate with a width of 8–10 mm and a depth of 2.0–2.5 mm reduces this effect. Drying is required at 80°C for 2 h when regrind is used above 20%, and the melt temperature is held at 230–245°C; lower melt temperatures increase fibre attrition and drop the Charpy notched impact strength under ISO 179-1/1eA from 8–12 kJ/m² to below 6 kJ/m² at 23°C.

    The application boundary for GFPP-20 in logistics pallets is set by low-temperature drop impact at -20°C. At this temperature, the notched Charpy impact strength under ISO 179-1/1eA declines to 5–7 kJ/m², and the pallet leg may crack when subjected to a corner drop of 0.8 m. This is the reason GFPP-20 pallets are generally limited to 3–5 trips in closed-loop distribution rather than long-term shared-pool use; PP-GF20 parts can be reground and blended with virgin material at 20–30% without complete loss of stiffness, but the glass fibre length distribution shifts downward after 3 regrind cycles and the notched impact strength falls below the ISO 8611-1 threshold for cold storage handling. The terminal product is a stackable nestable pallet with a mass of 7–9 kg, an integrally moulded anti-slip texture on the top deck, and a bottom runner design that avoids unvented blind pockets because entrapped gas causes short shots at the end of the runner.The main process conflict on a 1000–1300 t injection moulding machine is the long flow length from the central sprue to the outer leg, which produces a glass fibre length gradient and anisotropic shrinkage. The outer legs are therefore gated through sub-runners or the pallet is redesigned with a central film gate into the top deck to align glass fibres along the deck surface. Outdoor storage of GFPP-20 pallets requires a hindered amine light stabiliser package; if the pallet is not UV-stabilised, surface chalking and impact strength loss occur under accelerated weathering according to ISO 4892-2, and the outdoor service life may be below 6 months in high-sunlight regions. The compliance framework for this application includes ISO 8611-1 for pallet performance, ISO 179-1/1eA for impact, and ISO 4892-2 for UV validation when the pallet is stored in uncovered yards.

    Free Quote

    Competitive Kingfa GFPP-20,PP-GF20,Glass Fiber Reinforced prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa GFPP-20 is designated under ISO 1043-1 as a PP-GF20 compound: a polypropylene matrix carrying 20% by mass short-glass-fibre reinforcement, with a coupling-agent package, heat stabilisation, and processing lubricant. The product is supplied as cylindrical pellets for injection moulding and, in selected flow paths, for compression or extrusion of thick-section semi-structural parts. Batch release data are normally recorded against ISO 1183-1:2019, ISO 3451-1:2019, ISO 1133-1:2022, ISO 527-2:2012, ISO 178:2019, and ISO 179-1/1eA:2010. Ash content is nominal 20% by weight, with production lots typically controlled in an 18–22% band depending on pigment and coupling-agent batch. The Kingfa certificate of analysis is the controlling document for each lot.

    When GFPP-20 Replaces Talc-Filled PP in Under-Hood Housings

    In under-hood housings, a 20 wt% talc-filled PP compound typically exhibits a flexural modulus near 2500 MPa under ISO 178:2019 and a heat deflection temperature below 100°C under ISO 75-2:2013 method A at 1.8 MPa. GFPP-20 substitutes short glass fibre for lamellar talc, lifting flexural modulus into a 3200–4500 MPa window and HDT-A into a 145–158°C envelope for well-coupled short-glass systems. The change is not a direct drop-in: glass reinforcement increases anisotropic mould shrinkage. PP-GF20 parts commonly show flow-direction shrinkage of 0.2–0.5% and cross-flow shrinkage of 0.6–1.0% when measured from plaques produced by ISO 294-4:2018, whereas talc-filled PP develops a more balanced shrinkage field.

    Injection-moulding trials on semi-structural brackets with a 1200 kN clamp force machine and a 40 mm plasticising screw show that gate location and weld-line placement dominate warpage more than a 5°C mould-temperature shift within the 30–60°C range. For talc-filled PP replacements, feed-gate repositioning, rib thinning, or flow-leader adjustment is typically required before flatness is stabilised, because glass-fibre orientation during cavity filling creates local modulus gradients that are not present in mineral-filled parts.

    Pre-drying at 80°C for 2 h in a dehumidifying hopper dryer is recommended when ambient relative humidity exceeds 60%; although unfilled PP is often processed without drying, glass-fibre sizing hydrolysis can generate surface defects and unstable melt pressure in a 40:1 L/D twin-screw extruder. Barrel-temperature profiles for GFPP-20 are typically set from 210°C near the feed throat to 240°C at the nozzle, with a maximum melt temperature of 250°C. Residence time above 230°C should not exceed 10 min in a shutdown sequence. Screw designs with low-shear mixing elements and side-fed glass roving downstream of the polymer melting zone reduce fibre attrition; a compression ratio of 2.0:1–2.5:1 and a 40:1 L/D extruder with vacuum venting at −0.08 MPa are used on production-scale compounding lines.

    Injection moulding should use a low-to-moderate back pressure of 0.5–1.0 MPa and an injection velocity profile that avoids jetting through gates; excessive shear at melt temperatures below 220°C can break glass fibres below 0.2 mm critical length, lowering notched Charpy impact toward the lower bound of a 6–12 kJ/m² envelope under ISO 179-1/1eA:2010. For direct gating into thick sections, a shot-volume to barrel-capacity ratio of 50–70% is recommended to limit residence-time distribution. Surface fibre read-through is a known limitation for visible applications. A mould surface texture of 25–40 µm depth and a mould temperature at the upper end of the 40–60°C range reduce visual fibre prominence; tensile strength at weld lines is not improved by surface texturing.

    For flat panel applications such as washing-machine control-panel substrates, the mould cavity should be designed with flow-length-to-wall-thickness ratios below 200:1 and with ribs not exceeding 60% of the adjoining wall thickness to avoid sink marks and glass orientation defects. Annealing at 100°C for 30 min in a forced-air oven is used on some production lines to stabilise dimensions before assembly; published data for this specific configuration is limited, but dimensional-stability trials on similar PP-GF20 systems report post-anneal shrinkage reduction of 0.05–0.15 percentage points. Fixture cooling after ejection should be applied when flatness tolerances are tighter than 0.3 mm over 300 mm, because differential crystallisation between thick bosses and thin walls is amplified by the high thermal conductivity of glass fibre.

    What Limits Melt Homogeneity and Glass Dispersion in GFPP-20 Processing?

    Three parameters control melt homogeneity: fibre length retention, matrix wetting, and melt-flow stability. In a 40 mm twin-screw extruder at 250–350 rpm, glass-fibre length after compounding typically falls from 3–4 mm feed length to a number-average length of 0.3–0.6 mm; higher specific energy inputs above 0.25 kWh/kg can reduce mean fibre length and shift tensile strength from the upper bound of a 75–95 MPa range toward the lower bound under ISO 527-2:2012. Matrix wetting is assessed by fractured-surface microscopy on injection-moulded tensile bars produced according to ISO 294-1:2017; poor coupling appears as bare fibre pull-out and lowers notched impact. Melt-flow stability is measured by ISO 1133-1:2022 at 230°C and 2.16 kg; a PP-GF20 compound with an MFR of 5–15 g/10 min is typical, but the Kingfa GFPP-20 lot certificate should be consulted because MFR shifts of 2–4 g/10 min can occur between production campaigns.

    Use of regrind above 20 wt% is not recommended in high-impact applications because repeated thermal history reduces the polypropylene molecular weight and lowers notched Charpy impact at 23°C. Combination with unsaturated peroxide masterbatches for controlled rheology can reduce molecular weight further; formulators should avoid adding copper-containing pigments unless a proven long-term heat-ageing package is present, because copper ions can catalyse thermo-oxidative degradation of PP at continuous-use temperatures above 100°C.

    Moulded Part Behaviour Depends on Weld-Line Placement and Glass Orientation

    On production-scale injection moulding machines from 800 to 1600 kN clamp force, GFPP-20 moulds with melt temperatures of 220–240°C and mould temperatures of 40–60°C. For automotive fan shrouds, the part mass and rib design must account for glass-fibre orientation: flow-direction flexural modulus is typically 15–25% higher than cross-flow flexural modulus in the same moulded plaque. Weld lines in PP-GF20 reduce tensile strength by 30–50% relative to unwelded sections under ISO 527-2:2012; placing the weld line in low-stress regions or using sequential valve gating avoids premature failure. Batch-to-batch variation in pellet moisture above 0.08% by Karl Fischer titration produces splay and silver streaking; therefore incoming inspection should include moisture measurement before silo transfer.

    Property Profile Under ISO 527-2, ISO 178, and ISO 75-2 Thermal Loading

    The property profile is generated from injection-moulded specimens prepared according to ISO 294-1:2017 and conditioned at 23°C and 50% relative humidity for at least 16 h. Table 1 lists representative PP-GF20 class values; Kingfa GFPP-20 lot-specific certificate data supersede these generic windows.

    Property Test method Typical PP-GF20 class value Remarks
    Density ISO 1183-1:2019 1.02–1.06 g/cm³ Pigment and coupling affect lot value
    Ash content ISO 3451-1:2019 18–22 wt% 625°C muffle furnace
    Tensile strength at yield ISO 527-2:2012 75–95 MPa 5A specimen, 5 mm/min
    Flexural modulus ISO 178:2019 3200–4500 MPa 2 mm/min, 80×10×4 mm bar
    Notched Charpy impact, 23°C ISO 179-1/1eA:2010 6–12 kJ/m² Edgewise notch
    HDT-A, 1.8 MPa ISO 75-2:2013 method A 145–158°C Flatwise, 120°C/h heating rate
    Melt flow rate ISO 1133-1:2022 5–15 g/10 min 230°C, 2.16 kg load
    Moulding shrinkage ISO 294-4:2018 flow 0.2–0.5% / cross-flow 0.6–1.0% 40°C mould

    The property set positions GFPP-20 between PP-GF10 and PP-GF30. A 10 wt% glass-fibre compound typically raises flexural modulus to 2200–2800 MPa, while a 30 wt% glass-fibre compound pushes flexural modulus to 5000–6000 MPa but reduces melt flow and increases screw/barrel wear in compounding. GFPP-20 is selected when a stiffness target of 3500–4000 MPa must be met without the density, compound viscosity, and moulded-surface roughness penalties of a 30% glass-filled system. Compared with a 20 wt% talc-filled PP of equivalent filler mass fraction, glass fibre raises heat deflection temperature by approximately 40–60°C and tensile strength by a factor of roughly 2–3, but it also increases machine wear and anisotropic warpage.

    Compared with a 20 wt% glass-fibre polyamide 6 compound, GFPP-20 offers lower density near 1.04 g/cm³ and lower equilibrium moisture regain, but it cannot match PA6-GF20 tensile strength, which is commonly 150–180 MPa under dry-as-moulded conditions, or HDT-A above 200°C. Selection of GFPP-20 over PA6-GF20 is therefore driven by mass, cost, moisture-stability, and lower drying-energy requirements, not by absolute load-bearing capacity. In chemically aggressive under-hood environments, polypropylene’s resistance to coolants and battery acid is generally superior to PA6, but continuous oil exposure above 120°C can reduce stabiliser efficacy.

    In non-food-contact industrial applications, Kingfa GFPP-20 is normally supplied under a lot-specific SDS; RoHS compliance is evaluated against Directive 2011/65/EU Annex II and REACH obligations against Regulation (EC) No 1907/2006. For automotive cabin components, emission and odour test requirements such as VDA 277 or PV 3341 are application-specific and must be requested; published data for this specific configuration is limited for interior VOC performance. The grade is not recommended for continuous exposure to hot aqueous environments above 80°C unless a hydrolysis-resistant sizing is specified, because glass-fibre sizing degradation can reduce interfacial adhesion over 1000 h at 85°C and 85% relative humidity. For long-term outdoor use, carbon black or a UV-stabilised variant is required; natural grades should not be used without weather-stabilisation verification according to ISO 4892-2.