Kingfa MF-6202,Mineral Filled PP (UV, High Rigidity),Mineral/Mica Filled

    • Product Name: Kingfa MF-6202,Mineral Filled PP (UV, High Rigidity),Mineral/Mica Filled
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 954557
    Material Mineral/Mica filled polypropylene
    Filler Type Mineral/Mica
    Uv Stabilization Yes
    Rigidity High
    Density 1.03-1.05 g/cm³
    Melt Flow Rate 230 C 2 16 Kg 8-12 g/10 min
    Tensile Strength 30-35 MPa
    Tensile Elongation At Break 10-20%
    Flexural Modulus 2500-3000 MPa
    Flexural Strength 40-45 MPa
    Notched Izod Impact Strength 23 C 4-6 kJ/m²
    Heat Deflection Temperature 0 45 Mpa 100-110°C
    Vicat Softening Temperature 145-155°C
    Molding Shrinkage 1.0-1.5%
    Water Absorption ≤0.02%

    As an accredited Kingfa MF-6202,Mineral Filled PP (UV, High Rigidity),Mineral/Mica Filled factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa MF-6202 is supplied in 25 kg moisture-barrier polyethylene bags, palletized and stretch-wrapped; store dry, away from direct sunlight and UV exposure.
    Container Loading (20′ FCL) 20′ FCL: load Kingfa MF-6202 mineral/mica-filled PP (UV, high rigidity) in dry, palletized 25 kg bags; secure stowage.
    Shipping Kingfa MF-6202 is shipped as non-hazardous, mineral-filled PP pellets in sealed moisture-barrier bags or octabins on pallets. Keep dry, ventilated, and away from direct sunlight, heat, and contamination. Handle with care; avoid bag damage. Store below 40°C and use within the recommended shelf life.
    Storage Store Kingfa MF-6202 (Mineral/Mica Filled PP) in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and ignition sources. Keep in original sealed packaging on pallets to prevent moisture, dust, and contamination. Avoid prolonged UV/high-temperature exposure and excessive stacking. Protect from mechanical damage, maintain stable ambient conditions, follow local regulations, and use oldest stock first.
    Shelf Life Shelf life is typically 24 months in original sealed packaging, stored dry at ≤30°C, protected from sunlight, moisture, and contamination.
    Application of Kingfa MF-6202,Mineral Filled PP (UV, High Rigidity),Mineral/Mica Filled

    Why Does Mica Orientation Control Differential Shrinkage in Thin-wall IP Carriers?

    Injection-molded mineral/mica-filled PP instrument panel carriers exhibit flow-direction shrinkage values between 0.5% and 0.8% measured under ISO 294-4:2018 when melt temperature is held between 210°C and 230°C and mold temperature remains between 30°C and 50°C; cross-flow shrinkage is frequently 0.3% to 0.5% lower because mica platelets orient parallel to flow and constrain transverse contraction. This anisotropy is the dominant cause of post-demolding warpage in carrier substrates that transition from 2.5 mm to 3.0 mm rib bosses to 0.8 mm leg walls. Compliance for occupant-facing automotive applications is defined by ISO 3795:1989 with a maximum burning rate of 100 mm/min, supplemented by VDA 278:2011 for VOC and FOG emission limits and the REACH SVHC substance screening applicable to European supply chains. The formulation addition strategy treats MF-6202 as a ready-to-mold compound introduced at 100% compound; regrind recovered from cold runners and gate vestiges is introduced at no more than 20 wt% of total shot weight, while further external mica or mineral masterbatch addition is avoided because the additional filler raises melt viscosity and reduces notched impact below door-carrier requirements.

    Downstream processing in this segment uses a single-screw reciprocating injection unit with screw L/D 20:1 to 22:1 and compression ratio 2.0:1 to 2.5:1, feeding a two-plate mold with sequential valve gating to delay knit-line formation until after the melt has filled the lower carrier surface. Clamp force is sized between 3.5 kN/cm² and 4.5 kN/cm² of projected area; hold pressure is maintained at 60% to 80% of peak injection pressure until gate freeze is confirmed by cavity pressure sensors. If mold temperature falls below 20°C, the skin layer freezes before mica orientation relaxes, producing visible flow lines near vents and thickness transitions. Pre-drying at 80°C for 2 h to 3 h is required only when pellet moisture exceeds 0.05% after storage above 60% RH, because trapped water vapor produces splay on textured surfaces. Terminal product types in this segment include instrument panel lower retainers, door panel carriers, center console substrates, and steering column covers; the compound is not appropriate for ungrained Class A painted surfaces unless an adhesion promoter validated under ISO 2409:2020 cross-cut testing is applied, and published data for MF-6202-specific paint adhesion is limited.

    Condensate pH in outdoor air-conditioning drain pans fluctuates between 4.5 and 7.5 due to dissolved carbon dioxide, sulfur dioxide, and periodic coil-cleaner residues; mineral/mica-filled PP is selected for this wetted envelope because the mica platelets reduce moisture transmission and dimensional creep relative to unfilled copolymer PP. The compliance set for outdoor HVAC components includes UL 746C outdoor suitability with UV and water exposure indices, IEC 60335-2-40:2022 for heat pumps and dehumidifiers, ISO 5149 for refrigerating systems, and RoHS 2011/65/EU hazardous substance restrictions. For addition strategy, MF-6202 is processed as supplied at 100% compound without further UV stabilizer loading; adding separate high-concentration UV masterbatch above 1 wt% can cause surface bloom on textured gray panels. Color masterbatch is metered at 2 wt% to 4 wt% only when a non-compounded house color is required, and post-industrial regrind is limited to 25 wt% of shot weight. Downstream production for outdoor condenser louver and drain-pan platforms is typically performed on large vertical-clamp injection machines of 800 t to 1600 t clamp force, with hot-runner systems using 3 to 5 valve-gated drops to avoid cold-slug marks on visible surfaces. Barrel temperature is segmented from 190°C at the feed throat to 210°C to 230°C at the nozzle, while mold temperature is maintained at 20°C to 40°C to balance nucleation against warpage. Terminal product types include condensing unit base pans, fan grilles, front panels, side louver covers, and outdoor cabinet frames.

    Electrical Enclosure Base Plates: Creep, UV Exposure and Flame Class

    Electrical enclosure base plates made from mineral/mica-filled PP operate under continuous static load from busbars and terminal blocks at internal temperatures up to 60°C; the relevant design property is creep modulus under ISO 899-2:2003 rather than short-term flexural modulus. Published creep curves for MF-6202 specifically are limited, so batch verification should request supplier-generated data at 1000 h and compare the retained modulus against an allowable deflection limit specified in IEC 62208:2023. The compliance framework for fixed wiring enclosures includes IEC 60670-1 for junction boxes, IEC 62208:2023 for empty enclosures, UL 746C for polymeric electrical materials, and glow-wire testing under IEC 60695-2-11:2021 at the end-product threshold temperature. MF-6202 should not be used for live parts requiring UL 94 V-0 unless a validated non-halogenated flame retardant system is incorporated and the resulting compound is re-qualified for mechanical and electrical properties.

    The formulation addition strategy restricts regrind to 15 wt% of total shot weight because creep consistency in enclosure bases is sensitive to lot-to-lot variation in regrind mineral content. MF-6202 is introduced at 100% compound for first-pass production; no further mineral or mica masterbatch should be added, and color concentrate is limited to 2 wt% for dark gray or black enclosure colors to avoid shifting shrinkage outside the mold dimension tolerance band. Downstream production uses medium-tonnage injection machines of 500 t to 900 t clamp force, with melt temperature controlled between 210°C and 230°C, mold temperature at 25°C to 45°C, and a holding-pressure profile that applies 70% of peak injection pressure for 8 s to 12 s to minimize sink marks around screw bosses. Terminal product types include distribution box bases, fixed wiring enclosure shells, meter box bases, and junction box covers.

    Weld-line failures in mineral-filled PP power tool clamshells usually initiate at gate junctions where two melt streams converge; mica platelets align perpendicular to the weld line, reducing local tensile strength by 20% to 40% compared with bulk flow direction under ISO 527-2:2012. The applicable compliance set for power tools and garden tools includes IEC 62841-1:2014, EN 62841-1:2015, RoHS 2011/65/EU, and PAH limits defined by AfPS GS 2019:01 for consumer-grade surfaces. MF-6202 is used as supplied at 100% compound for first-shot production; internal regrind from sprues and runners is kept at or below 20 wt% because higher regrind levels widen notched Izod impact distribution under ISO 180:2000 method A. Injection molding is performed with melt temperature 215°C ± 10°C, mold temperature 30°C to 40°C, and filling speeds above 200 mm/s at the cavity edge to force the melt fronts into a cohesive weld; barrel residence time is limited to 5 min to avoid surface degradation. Terminal product types in this segment include angle grinder clamshells, lawn trimmer motor housings, leaf blower intake covers, and cordless drill battery housings.

    When Thermal Expansion Mismatch Drives Bracket Distortion in Washing Machines

    In washing machine structural modules, mineral-filled PP brackets are bolted to stainless-steel drum shells and zinc-coated steel frames; the linear coefficient of thermal expansion is 50 × 10⁻⁶ K⁻¹ to 70 × 10⁻⁶ K⁻¹ under ISO 11359-2:1999 for mineral-filled PP, while carbon steel is approximately 11 × 10⁻⁶ K⁻¹. At 85°C wash-cycle temperature, a 300 mm bracket span develops a differential expansion of approximately 1.1 mm to 1.6 mm, producing rotational distortion at the fastening bosses. The compliance framework is IEC 60335-1:2020 Clause 30.2 for resistance to heat and fire, plus the specific requirements of IEC 60335-2-7:2019 for washing machines; material certification is supported by RoHS 2011/65/EU and REACH SVHC documentation.

    The addition strategy uses MF-6202 at 100% compound with internal regrind limited to 20 wt% of shot weight; color masterbatch is held at 1 wt% to 2 wt% because higher pigmentation can reduce low-temperature impact retention required for transport in cold climates. Injection molding of bracket components is carried out at melt temperature 210°C to 230°C, mold temperature 30°C to 50°C, and clamp force from 4.0 kN/cm² to 5.0 kN/cm² of projected area; low-shear screw geometry with L/D 20:1 to 22:1 is specified to prevent mica platelet breakage. Terminal product types include drum support brackets, motor mounting flanges, base frame adapters, and door hinge carriers.

    Accelerated weathering under xenon-arc exposure per ISO 4892-2:2013 method A cycle 1 evaluates UV-stabilized mineral-filled PP outdoor furniture shells by tracking Delta E and impact retention after 2000 h; compounds without high-molecular-mass hindered amine stabilizers lose more than 50% of initial Charpy impact under ISO 179-1:2020. The compliance set for outdoor furniture includes EN 581-1:2017, ISO 4892-2:2013, and ISO 4892-3:2016 for UV/condensation exposure, plus REACH Annex XVII restrictions on PAHs. MF-6202 is processed as supplied at 100% compound for outdoor-grade parts; post-industrial regrind is limited to 20 wt% because UV-exposed scrap from previously failed parts carries depleted stabilizer and shifts failure time under xenon-arc testing. Color masterbatch is metered at 2 wt% to 3 wt% for earth-tone brown or anthracite furniture lines; the use of additional UV masterbatch is unnecessary and can create mold plate-out. Downstream production of park bench slats and planter walls uses large injection presses of 1200 t to 1800 t clamp force with accumulator-assisted injection for shot weights from 4 kg to 8 kg, melt temperature 210°C to 230°C, mold temperature 25°C to 40°C, and gas-assisted molding where hollow slats require stiffness without an increase in wall thickness. Terminal product types in this segment include park bench slats, seat shells, table tops, planter wall panels, and litter bin side panels.

    Free Quote

    Competitive Kingfa MF-6202,Mineral Filled PP (UV, High Rigidity),Mineral/Mica Filled prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The grade designation MF-6202 identifies a mineral-filled polypropylene compound in which mica platelet reinforcement is dispersed within a UV-stabilized polypropylene matrix. The product is classified among high-rigidity thermoplastic olefin compounds intended for injection-molded components requiring dimensional stability under thermal load, resistance to ultraviolet degradation in exterior service, and elevated flexural modulus relative to unfilled polypropylene. Published literature for mica-filled polypropylene systems indicates that mica loadings between 20 wt% and 40 wt% elevate flexural modulus into the range of 2,500 MPa to 6,500 MPa when measured in accordance with ISO 178:2019 or ASTM D790-17, while tensile strength typically ranges from 25 MPa to 40 MPa under ISO 527-2:2012. Density for such compounds falls between 1.05 g/cm³ and 1.25 g/cm³ when determined per ISO 1183-1:2019. Grade-specific datasheet values for MF-6202 should be confirmed against the manufacturer's current technical documentation, as compounding variables—including mica particle size distribution, coupling agent selection, and matrix copolymer ratio—produce measurable shifts within these ranges. Heat deflection temperature under a 0.45 MPa load, measured per ISO 75-2:2013, typically exceeds 100 °C for mica-reinforced polypropylene, whereas notched Izod impact resistance measured per ISO 180:2019 generally declines as mica content increases beyond 30 wt%, reflecting the characteristic stiffness–toughness trade-off inherent to platelet reinforcement systems.

    Rheological Response and Morphological Stability in Mineral-Filled PP

    In mineral-filled polypropylene compounds, melt viscosity deviates from that of unfilled resin through a combination of hydrodynamic reinforcement and platelet orientation effects. Melt flow rate, determined per ISO 1133-1:2022 at 230 °C under 2.16 kg load, is typically lower than that of the base resin due to increased solids content; compounds in this class commonly exhibit MFR values between 5 g/10 min and 20 g/10 min, though the grade-specific specification for MF-6202 must be verified against the manufacturer's datasheet. The shear-thinning behavior of mica-filled PP is more pronounced than that of spherical or low-aspect-ratio fillers because platelet alignment under shear reduces flow resistance in the direction of orientation. Capillary rheometry data reported in polymer processing literature show that mica-filled polypropylene exhibits a Carreau model relaxation time that increases with mica loading, indicating that the low-shear-rate plateau viscosity rises disproportionately as platelet aspect ratio increases. On production-scale injection molding machines with screw diameters of 25 mm to 60 mm and L/D ratios of 18:1 to 22:1, back pressure settings between 0.3 MPa and 0.7 MPa are typically required to maintain homogeneous melt temperature and filler distribution. Screw recovery times are extended by 10% to 20% relative to unfilled PP due to elevated melt viscosity. Compounding of MF-6202 is performed on twin-screw extruders with L/D ratios of 36:1 to 44:1, where distributive mixing elements are employed to minimize particle attrition and preserve platelet aspect ratio; excessive specific energy input during compounding degrades mechanical reinforcement by reducing effective aspect ratio. Published research on mica-filled PP indicates that plate-like fillers are more susceptible to aspect-ratio degradation in high-shear zones than blocky mineral fillers such as calcium carbonate.

    When storage conditions exceed 60% relative humidity or packaging integrity has been compromised, pre-drying of MF-6202 becomes mandatory. Moisture absorption in mineral-filled polypropylene compounds is primarily attributable to the filler phase; mica is hygroscopic to a limited degree, and compounds exposed to humid environments can develop surface splay and internal voiding during injection molding. A desiccant dryer operating at 80 °C to 90 °C for 2 to 4 hours is sufficient to reduce residual moisture below the 0.02 wt% threshold that prevents hydrolysis-related surface defects. Dry hopper residence time should not exceed 6 hours to avoid oxidative degradation of the UV stabilizer package. The material is supplied in pellet form with average pellet size between 2.5 mm and 4.0 mm, suitable for gravimetric feed systems and volumetric dosing units commonly encountered in non-return valve injection molding operations.

    How Does Mica Reinforcement Alter Warpage, Shrinkage, and Anisotropy Relative to Talc?

    Both mica and talc are platy magnesium silicate minerals, yet their reinforcement behavior in polypropylene differs substantially due to particle geometry, surface chemistry, and thermal stability. Mica platelets exhibit higher aspect ratios than talc—typically in the range of 20:1 to 100:1, compared with 6:1 to 20:1 for talc—and this difference translates into distinct shrinkage and warpage patterns in molded components. Mold shrinkage of mica-filled PP measured per ISO 294-4:2018 is lower than that of unfilled PP and more isotropic than that of glass-fiber-reinforced PP, with typical values ranging from 0.4% to 0.8% in the flow direction and 0.6% to 1.0% in the transverse direction for mica loadings of 30 wt% to 40 wt%. Talc-filled compounds at equivalent loading exhibit higher shrinkage anisotropy and greater propensity for differential shrinkage-induced warpage in thin-wall sections. The increased isotropy of mica-filled systems derives from the random planar orientation of platelets in the melt front during mold filling, as opposed to the flow-induced alignment that fiber reinforcement undergoes. Differential scanning calorimetry per ISO 11357-1:2016 shows that mica does not significantly alter the melting temperature of the polypropylene matrix, which remains between 160 °C and 170 °C for homopolymer and 142 °C to 155 °C for block copolymer matrices. Impact performance, as measured by notched Izod per ISO 180:2019, is generally lower for mica-filled compounds than for talc-filled counterparts at identical filler loading, because the larger mica platelets act as stress concentrators with longer crack propagation paths. The trade-off is compensated by improved flexural modulus retention at elevated temperatures: dynamic mechanical analysis shows that mica-filled PP retains a greater proportion of its room-temperature storage modulus at 80 °C than talc-filled PP of equivalent loading.

    PropertyTest StandardUnfilled PP (homopolymer)Talc-Filled PP (30 wt%)Mica-Filled PP (30 wt%)
    Flexural modulus (MPa)ISO 178:20191,200–1,6002,800–3,8003,500–5,500
    Tensile yield strength (MPa)ISO 527-2:201230–3525–3025–32
    Notched Izod impact (kJ/m²)ISO 180:20194–84–72–5
    Heat deflection temperature, 0.45 MPa (°C)ISO 75-2:201395–110115–125115–135
    Density (g/cm³)ISO 1183-1:20190.90–0.911.10–1.151.08–1.18
    Mold shrinkage, flow direction (%)ISO 294-4:20181.2–1.80.8–1.20.4–0.8

    Among the primary differentiators of MF-6202 is the ultraviolet stabilization package, engineered through incorporation of hindered amine light stabilizers (HALS) and UV absorbers within the polypropylene matrix. Accelerated weathering performance is evaluated under ASTM G154-16 Cycle 1 using UVA-340 fluorescent lamps with a 0.89 W/m² irradiance at 340 nm, where mineral-filled PP compounds of this class demonstrate color retention with ΔE below 3.0 after 1,000 hours and gloss retention exceeding 70% when assessed per ISO 2813:2014 at 60° geometry. Xenon arc exposure per ISO 4892-2:2013 Method A with daylight filters and a 0.51 W/m² irradiance at 340 nm provides complementary assessment of photodegradation resistance. The presence of mica platelets affects weathering behavior by increasing the path length for moisture diffusion and by creating interfacial zones where photo-oxidation initiates; this necessitates a higher stabilizer loading than unfilled polypropylene to achieve equivalent outdoor service life. Typical application contexts for UV-stabilized mineral-filled PP include exterior automotive cowl vents, mirror housings, lower bumper grilles, and outdoor enclosure components for HVAC and agricultural equipment, where sustained exposure to direct sunlight without significant mechanical property loss is specified by end-use standards such as SAE J2527 for automotive exterior materials.

    When High-Speed Injection Molding Demands Controlled Shear History

    In high-speed injection molding operations, the processing of MF-6202 requires explicit attention to shear history because platelet aspect ratio—the primary determinant of mechanical reinforcement efficiency—is irreversibly degraded by excessive shear energy input. Melt temperature should be maintained between 220 °C and 250 °C at the nozzle, measured via infrared pyrometry or needle thermocouple. Mold temperature is conventionally set between 20 °C and 60 °C; higher mold temperatures within this range improve surface replication and reduce weld-line visibility but extend cycle time. Injection pressure requirements for mica-filled PP exceed those of unfilled PP by 15% to 30% due to elevated melt viscosity; typical peak injection pressures range from 80 MPa to 120 MPa for thin-wall components with section thickness below 2.5 mm. Hold pressure is typically established at 50% to 70% of peak injection pressure, with hold time determined by gate freeze-off criteria, generally 1.5 to 3.0 seconds per millimeter of part thickness. Screw speed during recovery should be limited to 40 rpm to 80 rpm for screw diameters of 35 mm to 50 mm to minimize shear-induced filler attrition. Shot size should be selected such that the melt cushion remains between 3 mm and 6 mm to ensure consistent hold pressure transmission. Non-return valve wear is accelerated by the abrasive nature of mica; bimetallic barrels and hardened screw surfaces with nitriding treatment to 62 HRC or higher are recommended for production volumes exceeding 500,000 cycles annually. The use of hot runner systems with valve gates is preferred over cold runner edge gates when part geometry permits, because the reduced pressure drop through the gate zone limits shear-induced degradation of the platelet reinforcement phase.

    Processing ParameterRecommended RangeMeasurement Location
    Melt temperature220 °C – 250 °CNozzle, needle thermocouple
    Mold temperature20 °C – 60 °CCavity surface
    Peak injection pressure80 MPa – 120 MPaHydraulic line or nozzle transducer
    Hold pressure50% – 70% of peakHydraulic circuit
    Screw recovery speed40 rpm – 80 rpmMachine controller
    Back pressure0.3 MPa – 0.7 MPaHydraulic circuit
    Melt cushion3 mm – 6 mmScrew position transducer

    Across global regulatory frameworks, MF-6202 falls under the scope of the European REACH Regulation (EC 1907/2006) and EU RoHS Directive 2011/65/EU Annex II, where lead, cadmium, mercury, and hexavalent chromium concentrations are restricted to below 0.1 wt% per homogeneous material, with the total restricted substance burden confirmed by X-ray fluorescence screening per IEC 62321-5:2013. The product is not specified for direct food-contact applications under FDA 21 CFR or EU Regulation (EC) 1935/2004 unless explicitly designated by the manufacturer for such use with migration testing per the applicable simulant protocols. Automotive interior emissions testing per VDA 278:2011 for volatile organic compounds and condensable substances may be specified by OEM material standards; published data for this specific configuration of MF-6202 is limited, and verification against the current OEM approval certificate is required before serial production.

    The operational envelope of MF-6202 is bounded by a maximum recommended regrind incorporation level of 20 wt%, beyond which progressive reduction in notched Izod impact resistance and elongation at break is observed due to cumulative thermal and shear history effects on both the matrix and the mineral reinforcement. The compound should not be processed at melt temperatures exceeding 260 °C for prolonged residence times, as thermal degradation of the UV stabilizer package and chain scission of the polypropylene matrix produce surface silver streaking, odor formation, and measurable loss of tensile strength. Extended hot air aging at temperatures above 100 °C is not recommended for continuous service exceeding 1,000 hours unless validated by Arrhenius extrapolation from data collected per ISO 188:2011. Chemical incompatibilities include prolonged contact with strong oxidizing acids and chlorinated solvents, which extract low-molecular-weight fractions from the compound and initiate surface microcracking. Published data for the long-term creep behavior of this specific grade under load at 80 °C in humid environments is limited; design calculations for load-bearing applications should incorporate safety factors derived from creep modulus measurements per ISO 899-1:2017 on the actual production compound. Storage should be maintained at temperatures below 35 °C in closed packaging, with inventory rotation governed by the 12-month shelf life assigned to the UV stabilizer formulation.