| HS Code | 415178 |
| Gradename | Kingfa MF-NC501 |
| Materialtype | Mineral/Mica Filled Polypropylene |
| Fillertype | Mineral/Mica |
| Fillercontent | 20% typical |
| Density | 1.05 g/cm³ typical |
| Meltflowrate | 12 g/10 min at 230°C/2.16 kg typical |
| Tensilestrength | 27 MPa typical |
| Tensileelongationatbreak | 15% typical |
| Flexuralmodulus | 2800 MPa typical |
| Notchedizodimpactstrength | 5 kJ/m² at 23°C typical |
| Heatdeflectiontemperature | 115°C at 0.45 MPa typical |
| Vicatsofteningtemperature | 140°C typical |
| Moldingshrinkage | 0.8–1.2% typical |
| Flammability | HB typical |
| Processingmethod | Injection molding |
As an accredited Kingfa MF-NC501,Mineral/Mica Filled PP factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa MF-NC501 Mineral/Mica Filled PP is supplied in 25 kg moisture-resistant paper bags, palletized for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL: Kingfa MF-NC501 mineral/mica-filled PP in 25 kg bags, palletized and shrink-wrapped, approximately 18–20 MT net, loaded in standard dry container. |
| Shipping | Shipping description: Kingfa MF-NC501, Mineral/Mica Filled PP, is a non-hazardous polypropylene compound in pellet form. It is typically packed in 25 kg bags or jumbo bags. Transport as non-DG cargo; keep dry and away from direct sunlight, heat, and contamination. No special handling required. |
| Storage | Store Kingfa MF-NC501 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, sparks, and open flames. Keep containers or bags sealed and palletized to prevent moisture pickup, contamination, and dust generation. Avoid prolonged UV exposure and store away from incompatible chemicals. Maintain clean, labeled storage and follow local regulations and SDS guidance. |
| Shelf Life | Typically two years when stored unopened in a cool, dry, well-ventilated area, protected from direct sunlight and moisture. |
Processing of MF-NC501 for automotive HVAC blower housings and fan shrouds is dominated by mica platelet orientation during the high-shear injection phase. On hydraulic injection moulding machines with a 45 mm screw diameter and a 20:1 L/D ratio, melt temperature measured by air-shot pyrometer is maintained at 225–240°C; the nozzle zone is set 5–10°C below the metering zone to prevent drool and stringing. Mould surface temperature is kept at 30–50°C because fast skin solidification locks mica platelets parallel to the cavity wall in the scroll and reduces Z-direction shrinkage non-uniformity. Injection velocity is staged from 60 mm/s to 120 mm/s across the flow length. Transfer from velocity to pressure control occurs at 95–98% filled volume. Packing pressure is 50–65% of peak injection pressure and is held for 8–15 s depending on gate seal. Back pressure is set at 0.5–1.0 MPa, screw recovery speed at 60–100 rpm, and melt cushion at 3–6 mm. Failure modes documented on production lines include gate blush when sprue or hot-tip diameters fall below 1.5 mm because mica platelets accumulate in the gate land, and surface splay when pellet moisture exceeds 0.05 wt% because filler-bound water is released during plasticisation. Pre-drying at 80°C for 2–4 h is required when storage relative humidity exceeds 60% or when regrind content exceeds 20 wt%. Dimensional audit follows ISO 291 conditioning for 48 h at 23°C and 50% RH; warpage across a 400 mm fan shroud flange is typically held below 1.2 mm. Interior HVAC parts are additionally screened by VDA 270 for odour and DIN 75201-B for gravimetric fogging. The grade is not recommended for continuous air temperatures above 120°C unless additional long-term heat stabilisation is specified, because oxidative embrittlement of the polypropylene matrix becomes the dominant failure mode.
| Sector | Controlling standard or method | Critical end-product threshold | Key processing setpoint |
|---|---|---|---|
| Automotive HVAC blower housing | DIN 75201-B / VDA 270 | Fogging below 2 mg; odour ≤ 3.0 | Melt 225–240°C; mould 30–50°C |
| Appliance control panel housing | IEC 60335-1 / IEC 60695-2-11 | Glow-wire 650°C, no flame longer than 2 s | Melt 230–245°C; gate 1.2–1.8 mm |
| Washing machine pump housing | IEC 60335-2-7 / ISO 175 | Dimensional change ≤ 0.5% after 7 d detergent soak | Melt 225–235°C; wall ≥ 2.0 mm |
| Low-voltage distribution box | IEC 62208 / IEC 60695-10-2 | Ball pressure 125°C; glow-wire 650°C | Melt 220–240°C; draft 1.5–2.0° |
For air-conditioner front display housings and washing machine control panel frames, wall thickness below 1.2 mm creates a narrow processing window because mica platelets increase shear viscosity at low shear rates and reduce melt extensibility at the flow front. Trials on 1.2 mm-thick panels show that raising melt temperature from 230°C to 245°C improves short-shot margin but also increases exudation of low-molecular-weight additives; the resulting surface haze is detected as a drop in 20° gloss under ISO 2813. Gate location is placed at the thicker rib intersection rather than at a direct edge to suppress jetting and mica flow-direction streaks. The control housing is validated for dimensional stability in the 35–50°C operating range; creep of the snap-fit rib under a 3 MPa flexural load at 50°C is evaluated for 1,000 h by ISO 899-2. End-product standards include IEC 60335-1 for appliance safety and IEC 60695-2-11 glow-wire at 650°C where the part is adjacent to live parts. Mineral-filled PP compounds without flame retardant are classified as HB under UL 94, and MF-NC501 falls into this category unless the supplier’s certification states otherwise; therefore the part is limited to enclosures where no V-2 or higher rating is required. Comparative tracking index under IEC 60112 commonly exceeds 600 V for mineral-filled PP, but lot-specific certification is required before substitution. Hot-runner needle valve gates below 1.0 mm produce high shear heating and black specks; acceptable gate diameter is 1.2–1.8 mm with a valve-pin opening profile of 10–15 ms to maintain clean gate vestige and avoid stringing.
In washing machine drain pump base plates and detergent drawer frames, MF-NC501 is processed for resistance to warm water, cationic and anionic surfactant solutions, and dilute sodium hypochlorite at 60–90°C. Mica-filled PP does not undergo hydrolytic chain scission in the manner of aliphatic polyamide; however, prolonged contact with oxidising bleach can consume the hindered phenol stabiliser package and reduce long-term thermal oxidative resistance. Tool design therefore uses wall sections not below 2.0 mm and internal radii above 1.5 mm to reduce stress concentrations where chemical attack initiates. Gate position is offset from the sealing groove because mica orientation around the gate creates local shrinkage distortion that forms a leak path under 0.3 MPa water pressure testing. Melt temperature is 225–235°C, mould surface temperature 35–45°C, packing pressure 45–60 MPa held for 8–12 s, and cooling time 18–25 s for a 2.5 mm wall. Chemical exposure is assessed by ISO 175 for 7 days in 5% aqueous detergent at 80°C; dimensional change is controlled below 0.5% and post-mould annealing at 90°C for 2 h is applied if necessary. IEC 60335-2-7 requires creepage and clearance distances to remain stable after chemical exposure; because MF-NC501 is a mineral/mica filled compound, it provides stable insulation geometry but is not certified for live-part separation above 250 V unless the manufacturer’s test report explicitly supports the design.
Cordless power tool battery pack upper covers and bench charger shells are moulded from MF-NC501 in applications where mechanical attack is limited to 1 m drop height onto concrete at 23°C. The grade is not a direct replacement for impact-modified polyamide or PC/ABS in motor housings or gear cases because mica-filled PP exhibits lower notched impact strength under ISO 179-1/1eA; average values for this compound class are commonly below 10 kJ/m² at 23°C, and the ductile-to-brittle transition of polypropylene must be considered below 0°C. Tooling for charger shells uses two-plate cold runner moulds with edge gates or submarine gates; gate inserts and shut-off faces are hardened to 52–56 HRC because the mica filler is abrasive. Melt temperature is 220–235°C, mould temperature 25–45°C, injection velocity 80–120 mm/s, and hold pressure 40–55 MPa. Clamp force is selected on projected area at 35–50 MPa cavity pressure to avoid flash at the parting line. After 48 h conditioning, flatness on a 300 mm linear span is audited to ≤0.8 mm. Under IEC 60335-2-29 for battery charger safety, glow-wire testing per IEC 60695-2-11 at 650°C may be adequate for supervised appliances, but unattended charger circuits above 0.2 A often require 750°C glow wire or a V-2/V-0 final rating. MF-NC501 as supplied is HB under UL 94; if an end product requires V-2 or higher, a different flame-retardant grade is necessary.
When processing MF-NC501 into horizontal louvres and connecting rods for split air-conditioner indoor units, sequential valve gating is used to eliminate weld lines at hinge bosses. The tool often has three hot tips with gate delays of 1.5–2.0 s to maintain a continuous melt front; melt temperature is 220–235°C, hot runner manifold temperature 230°C, and mould surface temperature 35–50°C. Increasing mould temperature to 60°C improves gloss uniformity but slows skin freeze and can cause mica platelets to reorient perpendicular to the wall under high shear, increasing local shrinkage in the louvre rib. The louvre is tested under IEC 60068-2-30 damp heat cycling for 48 h; because polypropylene absorbs negligible moisture, dimensional change after 24 h water immersion at 23°C is typically below 0.05%. Low-velocity edge impact is applied with a 500 g steel ball dropped from 0.5 m; cracking at the hinge root is the dominant failure mode, so hinge thickness is set at 1.8 mm minimum and the melt cushion is held at 5 mm to prevent cold slugs. The replacement of GPPS or ABS requires adjusting packing pressure rather than melt temperature; MF-NC501 has a broader processing window but lower surface hardness, so scratch behaviour is verified by ISO 19252 with a 10 N load. Compliance includes RoHS 2011/65/EU and REACH; no brominated flame retardant or phthalate plasticizer is present in the nominal formulation.
For indoor low-voltage distribution boxes and terminal support brackets, MF-NC501 is constrained by its non-flame-retardant character. The as-supplied grade is HB under UL 94; the application is only viable where IEC 62208 permits a non-current-carrying enclosure or where the final product safety category accepts HB. The mineral/mica filler improves creep resistance at the 50–60°C internal air temperature of a sealed enclosure. Short-term tensile modulus under ISO 527-2 is not sufficient for busbar support sag assessment; ISO 899-2 creep at 40°C and 4 MPa for 1,000 h is the relevant qualification. For mineral-filled PP in this class, creep modulus often falls to 50–70% of the instantaneous ISO 178 flexural modulus; published data for this specific configuration is limited, so lot-specific specimens must be tested before tool release. Wall thickness is 2.5–3.0 mm, draft angle 1.5–2.0° per side, and ejection force is estimated with a steel-to-PP coefficient of friction of 0.35 to avoid ejection white marks. The enclosure must pass IEC 60695-2-11 glow-wire at 650°C; if flame persists longer than 2 s, the design is rejected. Ball pressure testing under IEC 60695-10-2 at 125°C verifies local terminal hot-spot stability. For outdoor distribution boxes, UV and heat stability are assessed by ISO 4892-2 for 500 h; colour shift must remain below 3.0 ΔE in many utility specifications. The coefficient of linear thermal expansion is reduced by mica orientation to approximately 50–70 × 10⁻⁶ K⁻¹ in the flow direction; anisotropic shrinkage across the weld line must be controlled by relocating the gate rather than by increasing packing pressure alone.
For outdoor garden tool motor covers and fan cowls where the part is shielded from direct ground impact, MF-NC501 is processed at 220–235°C melt temperature and 25–40°C mould temperature, with UV weathering validation under ISO 4892-2 for 300 h and a ΔE limit of 3.0.
Competitive Kingfa MF-NC501,Mineral/Mica Filled PP prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa MF-NC501 is a mineral/mica filled polypropylene compound in which mica is incorporated at a loading sufficient to modify dimensional stability, flexural modulus, and heat deflection behavior. The grade is supplied in pellet form for injection molding and extrusion; exact melt mass-flow rate, filler content, tensile stress at yield, flexural modulus, and mold shrinkage are controlled by the current Kingfa technical datasheet and should not be transferred from similar grades without lot-specific verification. The product is typically selected when unfilled polypropylene shows excessive shrinkage, creep, or thermal expansion, but short-glass-filled polypropylene introduces unacceptable warpage, surface roughness, or tool wear. Mica platelets provide reinforcement through their high aspect ratio, which distinguishes MF-NC501 from calcium-carbonate-filled PP and imposes different processing limitations compared with talc-filled PP.
Mica-filled polypropylene compounds such as MF-NC501 carry a narrower practical melt-temperature window than calcium-carbonate-filled PP because the polypropylene matrix degrades at high temperatures while the filler platelets undergo mechanical attrition under excessive shear. Melt temperatures above 250 °C accelerate chain scission and carbonyl formation; melt temperatures below 200 °C may produce inhomogeneous melt fronts and poor wet-out of the mineral surface. Unlike glass-fiber reinforcement, mica reinforcement depends strongly on platelet aspect ratio, so high-shear screw elements can reduce modulus by breaking platelets during compounding or molding. Production-scale compounding typically uses co-rotating twin-screw extruders with L/D ratios of 40:1 to 48:1, with downstream side-feeding of mica after the polymer is molten. Vacuum devolatilization removes low-molecular-weight fractions and moisture. Injection molding machines for MF-NC501 class materials often use a compression ratio of 2.0:1 to 2.8:1, a shut-off nozzle, and hardened non-return valves. Mold temperatures of 20 °C to 60 °C are generally used; higher mold temperatures improve surface quality at the expense of cycle time. Clamp force requirements generally fall between 3 kN/cm² and 5 kN/cm² of projected part area, although deep ribs or thin-wall sections may require higher values. Cushion stability should be monitored because non-return valve wear from mica abrasion can appear as a cushion variation exceeding 2 mm. Melt residence time should be kept below supplier-specified limits, and any temperature overshoot above 250 °C during recovery should be treated as a quality deviation.
In production-scale molding shops, selection of MF-NC501 over a talc-filled PP grade is often driven by higher flexural modulus at equal density, but that selection introduces a trade-off in impact and surface appearance. Talc has a Mohs hardness of approximately 1, whereas mica can range from 2.5 to 4 depending on mineral source. This increases abrasion on screw elements, non-return valves, and mold parting lines. Field experience with mica-filled PP indicates that nitrided or bimetallic screws and hardened mold inserts are required to avoid excessive wear after 50 000 to 100 000 cycles. Existing equipment used for short-glass-filled PP is often acceptable, but direct conversion from talc-filled PP without metallurgy upgrades can produce visible surface streaking and dimensional drift. Batch-to-batch variation in mica particle size distribution can shift flexural modulus by 10 % to 15 % if incoming lot inspection does not include laser diffraction particle-size screening. This is an operational boundary, not a cosmetic issue: changes in platelet aspect ratio alter flow-direction shrinkage and warpage even when melt flow rate remains within specification.
The following table provides class-level values from published polymer-science and compounder literature. The ranges are not product-specific to MF-NC501; they illustrate the direction and magnitude of property shifts associated with platelet mineral fillers. Exact values for MF-NC501 must come from the current manufacturer datasheet.
| Property | Test standard | Unfilled PP homopolymer | Mica-filled PP class | Talc-filled PP class |
|---|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.90–0.91 g/cm³ | 1.05–1.15 g/cm³ | 1.05–1.15 g/cm³ |
| Flexural modulus | ISO 178:2019 | 1 200–1 600 MPa | 2 500–4 000 MPa | 2 200–3 500 MPa |
| Heat deflection temperature, 0.45 MPa | ISO 75-2:2013 | 90–105 °C | 120–140 °C | 115–135 °C |
| Notched Charpy impact | ISO 179-1:2010 | 3.0–6.0 kJ/m² | 2.0–4.0 kJ/m² | 2.5–5.0 kJ/m² |
| CLTE | ISO 11359-2:1999 | 100–150 × 10⁻⁶ K⁻¹ | 40–70 × 10⁻⁶ K⁻¹ | 50–80 × 10⁻⁶ K⁻¹ |
| Mold shrinkage | ISO 294-4:2018 | 1.2–1.8 % | 0.6–1.0 % | 0.7–1.1 % |
Because mica-filled PP is specified primarily for dimensional stability and low warpage, acceptance criteria for MF-NC501 components typically reference flexural modulus, heat deflection temperature, and shrinkage rather than tensile strength alone. The table shows why mica-filled PP is chosen over unfilled PP: flexural modulus increases from 1 200–1 600 MPa to 2 500–4 000 MPa under ISO 178:2019, and coefficient of linear thermal expansion drops from 100–150 × 10⁻⁶ K⁻¹ to 40–70 × 10⁻⁶ K⁻¹. Compared with talc-filled PP at equal filler content, the higher aspect ratio of mica can produce higher flexural modulus but lower notched impact and greater flow-to-transverse shrinkage differential. Calcium-carbonate-filled PP generally provides lower flexural modulus and higher elongation at break but less anisotropy; it is used for cost reduction and ductility rather than structural stiffness. For MF-NC501, the table should be treated as a screening guide, and lot-specific data should be requested for production release.
When weld lines, flow hesitations, or rib-to-wall ratios are pushed beyond standard design limits, mica-filled PP compounds display failure modes that are not always predicted by neat-PP flow simulation. Flow-induced platelet orientation creates a layered morphology with low orientation at the frozen layer and high orientation in the shear zone. At a weld line, platelet-rich fronts meet but do not interpenetrate; tensile strength measured perpendicular to the weld line according to ASTM D638-14 can fall below 60 % of the bulk value, with published studies reporting reductions of 20 % to 50 % depending on filler content and gate location. This is a critical threshold for structural brackets and load-bearing housings. Short-glass-filled PP typically retains higher weld-line strength because fibers can bridge the weld interface, but mica platelets align parallel to the flow front and act as mechanical discontinuities. Design mitigation includes relocating gates to move weld lines out of highly stressed zones, increasing wall thickness at knit lines, using sequential valve gates, and raising melt temperature within the supplier-approved window. Mold-flow simulation for mica-filled PP requires anisotropic material data; isotropic shrinkage and elastic-modulus assumptions underestimate warpage in flat panels and cause dimensional nonconformance after ejection.
Automotive interior applications for mineral-filled PP include instrument-panel substrates, door-panel carriers, center-console substrates, and HVAC housings. Qualification of MF-NC501 for these uses normally follows the OEM material specification rather than a generic datasheet comparison. Production-scale injection-molding trials are used to assess dimensional stability after thermal aging at 100 °C to 120 °C for durations such as 500 h or 1 000 h, depending on the component class. Mechanical acceptance often includes notched impact at -30 °C or -40 °C according to ISO 179-1:2010, because mica-filled PP can embrittle at low temperature despite improved heat deflection. Occupant safety and interior air quality require fogging, odor, and emission testing; methods such as DIN 75201 for fogging and VDA 278 for VOC/SVOC are common, but OEM-specific limits vary. Scratch and mar resistance are evaluated by OEM procedures or standardized methods such as VDA 230-213. Creep and fatigue data may be required for structural substrates; if specified, creep modulus at 1 000 h under 10 MPa load is a typical screening point, but exact values for MF-NC501 must be generated on molded specimens. Published data for MF-NC501 in specific OEM approval matrices is limited; qualification data are generally held in OEM material approval reports or supplier PPAP packages.
For appliance housings, washing-machine tub surrounds, dishwasher bases, and small electrical enclosures, mineral/mica filled PP is used where repeated exposure to warm humid air and detergent solutions requires dimensional stability without metallic corrosion. The lower coefficient of linear thermal expansion relative to unfilled PP reduces interface gaps and fastener loosening in multi-material assemblies. Electrical properties for MF-NC501 are not governed solely by the filler; comparative tracking index and surface resistivity depend on additive packages, color concentrates, and surface finish. Manufacturers evaluating the grade for electrical applications should test finished plaques according to IEC 60112:2020 for tracking index and IEC 62631-3-2:2016 for surface resistivity, rather than relying on class-level values. Because mica is an inorganic dielectric, its use does not inherently improve flame retardancy; ignition resistance must be evaluated under the relevant end-product standard such as IEC 60695-11-10 or UL 94. If food-contact use is proposed, a migration study under 21 CFR 177.1520 or EU 10/2011 is required for the filled compound, because the mineral filler and any coupling agents may require additional compliance testing. Moisture uptake is generally low, but condensation on cold pellets should be managed by closed storage or drying. Published data for MF-NC501 in specific appliance compliance regimes is limited; suppliers provide lot-specific certificates for REACH and RoHS when requested.
Tooling for MF-NC501 must account for anisotropic shrinkage and platelet orientation, whereas talc-filled or calcium-carbonate-filled PP often behaves more nearly isotropically. In a flat rectangular plaque gated at one edge, mica platelets align along the flow direction, producing lower shrinkage in the flow direction and higher shrinkage in the transverse direction. This can generate post-ejection curvature if cooling is asymmetric. Mold designers addressing this issue typically use corner gates or multiple gates to create a more balanced orientation, and they add stiffening ribs rather than relying solely on material modulus. Published mold-shrinkage data for the mica-filled PP class in ISO 294-4:2018 show flow-direction shrinkage of 0.6 % to 0.9 % and transverse shrinkage of 0.8 % to 1.1 %. Talc-filled PP under the same test method generally has a narrower differential between flow and transverse directions. Non-standard gate locations or excessively high packing pressure can amplify orientation-induced warpage rather than correct it. Tool wear is also a design variable: mold parting-line abrasion from mica can reduce seal integrity over time, so hardened inserts and regular dimensional checks are part of production control for MF-NC501.
Drying of MF-NC501 is not always required for mineral-filled PP, but storage in unheated warehouses or outdoor silos can introduce surface moisture from condensation. If hopper relative humidity exceeds 60 %, moisture adsorption at the pellet surface can exceed 0.05 wt%, producing splay or gas splay on molded surfaces. A desiccant dryer set at 80 °C for 2 h to 4 h is typical for mica-filled PP, but the manufacturer’s recommendation for MF-NC501 should be followed because coupling agents can hydrolyze if exposed to prolonged high-temperature drying. Drying time beyond 6 h at 90 °C can oxidize the PP surface and shift color; hopper residence time should be minimized. Moisture determination by ISO 15512:2019 should be used when incoming material shows surface defects or when processing in humid climates. Operators should not assume that mineral filler eliminates the need for material handling controls; condensation on cold pellets can introduce batch-to-batch surface variability even when the polymer melt is dry.