| HS Code | 613404 |
| Polymer Type | Polypropylene (PP) |
| Flame Retardant | Yes |
| Filler Type | Mineral |
| Ul 94 Flammability Rating | V-0 |
| Density | Approx. 1.16 g/cm³ |
| Melt Flow Rate 230 C 2 16 Kg | Approx. 8 g/10 min |
| Tensile Strength | Approx. 25 MPa |
| Tensile Elongation At Break | Approx. 10% |
| Flexural Modulus | Approx. 2600 MPa |
| Notched Izod Impact Strength 23 C | Approx. 4 kJ/m² |
| Heat Deflection Temperature 1 82 Mpa | Approx. 95 °C |
| Molding Shrinkage | Approx. 0.8–1.2% |
| Water Absorption 24 H | Approx. 0.02% |
| Processing Method | Injection molding |
| Melt Temperature | Approx. 200–230 °C |
| Mold Temperature | Approx. 40–80 °C |
| Drying Temperature | Approx. 80–100 °C |
| Drying Time | Approx. 2–4 h |
As an accredited Kingfa PP-KF04,PP-KF Flame Retardant/Modified,Mineral Filled, Automotive/Appliance factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-KF04 is packed in 25 kg moisture-resistant bags, palletized and stretch-wrapped for safe industrial transport and storage. |
| Container Loading (20′ FCL) | 20' FCL: load Kingfa PP-KF04 flame-retardant, mineral-filled PP compound in a 20-foot container, palletized and securely strapped for sea transport. |
| Shipping | Kingfa PP-KF04 flame-retardant, mineral-filled polypropylene compound is shipped as non-hazardous pellets in 25 kg moisture-barrier bags or bulk containers on pallets. Store and transport dry and cool, protected from UV, contamination, open flames, and excessive heat. Clean, covered vehicles are recommended; no hazardous-goods labeling is normally required. |
| Storage | Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and moisture. Keep in original sealed packaging on pallets; avoid crushing or deformation. Separate from strong oxidizers and acids. Maintain stable temperature and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is typically 24 months when stored dry, cool, and protected from sunlight in original sealed packaging. |
Mineral-filled flame-retardant polypropylene for A-pillar and door trim moldings is processed as a direct-mold compound at 100 wt%; no additional flame-retardant masterbatch is required, and dilution with unfilled PP homopolymer for cost-optimised formulations is conventionally limited to 10–20 wt% only where the final part is re-qualified to ISO 3795 and FMVSS 302. The governing compliance boundary for vertical trim is horizontal burn rate not exceeding 100 mm/min according to ISO 3795 and the equivalent FMVSS 302 procedure, with RoHS conformity assessed under Directive 2011/65/EU and Delegated Directive (EU) 2015/863. Production-scale injection molding on machines of 800–1,200 t clamp force typically uses a barrel profile of 190–230 °C, a mould temperature of 20–40 °C, and a dehumidifying dryer set at 80 °C for 2–3 h when ambient relative humidity exceeds 60 %; failure to dry before processing at high humidity produces silver streaks and localised gas burns because flame-retardant degradation products and mineral-bound moisture discharge through the melt front. Screw specifications with a low-shear metering section, L/D 20:1–24:1, and compression ratio 2.0:1–2.5:1 are preferred; the mineral filler accelerates check-ring and barrel wear, so bimetallic barrels and hardened screw tips are used to maintain shot-to-shot cushion variance below 2–3 mm. The tool should include venting at the last-fill zones at 0.02–0.03 mm depth and 0.5–1.0 mm land to avoid burn marks; textured grain replication is maintained by keeping the mould surface temperature at the upper end of the range and using short injection fill times, but excessive back pressure above 1.0 MPa can disperse the mineral and flame-retardant package to the skin, causing gloss reversal and visible weld-line deepening. End-product configurations include A-pillar upper trim, B-pillar upper trim, and door waist-rail mouldings in passenger vehicles where the mineral-filled compound provides controlled shrinkage and reduced smoke relative to unfilled flame-retardant PP.
Across front-loading washing-machine control-panel enclosures, the non-metallic housing around the display and control electronics is subjected to glow-wire testing at 750 °C for unattended appliance current-carrying parts and at 850 °C where the component is above supply terminals, as required by IEC 60335-1:2020 clause 30.2.3 and tested according to IEC 60695-2-11; final-part compliance is also verified to UL 94 V-0 at the moulded wall thickness, commonly 2.0–3.0 mm. Direct addition is 100 wt% of the compound, with only 1–2 wt% of a PP-carrier colour masterbatch if required; any higher loading of masterbatch or regrind above 25 wt% may shift glow-wire behaviour because the diluent changes the decomposition char structure. The downstream process on a 500–1,000 t injection moulding machine for a large top cover or control panel typically employs sequential valve gating to move the knit line away from the display window and maintain flatness across a 600 mm × 400 mm surface. Melt temperature is held at 200–230 °C, with shot-to-shot variation controlled below ±1.5 °C because the flame-retardant system exhibits a narrow processing window; the mould is maintained at 30–50 °C, and holding pressure of 40–60 MPa is applied for 8–12 s at 2.5 mm wall thickness to reduce sink over bosses. The compound should be dried to 0.02 % moisture or below using a dehumidifying dryer at 80 °C for 2–3 h; when moisture remains, gas splay at the gate and flow lines around the display lens are the primary failure modes observed on production campaigns. Screw speed is limited to 60–100 rpm to avoid excessive shear heating and local discolouration of the flame-retardant package. End-product types include washing-machine top covers, control-panel housings, and dishwasher door inner panels specified for unattended appliance categories.
Condensate drain pans in split air-conditioner indoor units are moulded at 2.5–4.0 mm wall where the governing compliance boundary is IEC 60695-2-12 glow-wire flammability index and IEC 60695-2-13 glow-wire ignition temperature, with IEC 60335-2-40:2022 as the product safety standard for heat pumps and dehumidifiers. The formulation addition is direct-mould 100 wt%; regrind generated from sprue and runner systems is allowed up to 20 wt% only when the grind is dried together with virgin pellets and sieved to remove fines below 1 mm, because mineral-filler segregation in the granulate feed can produce localised flammability test failures at thin ribs. Injection moulding on 300–800 t machines uses a melt temperature of 200–230 °C, mould temperature of 20–50 °C, and dehumidifying drying at 80 °C for 2–3 h; the tool must be designed with gates at the deepest section of the drain pan to prevent jetting and with thick ribs replaced by coring to maintain flow length. Condensate exposure imposes an additional long-term requirement: the compound must resist hydrolysis and detergent-induced surface cracking, so pack pressure is held at 35–55 MPa and cooling time is extended by 10–15 % relative to unfilled PP to stabilise shrinkage before ejection. End-product types include indoor-unit drain pans, fan shrouds, motor mounting covers, and louvre link brackets for residential and light-commercial air-conditioning systems.
| Application scenario | Flammability or safety standard | Test criterion / clause | Nominal wall thickness |
|---|---|---|---|
| Automotive pillar trim | ISO 3795 / FMVSS 302 | burn rate ≤ 100 mm/min | 2.0–2.5 mm |
| Washing-machine control panel housing | IEC 60695-2-11, IEC 60335-1:2020 | 750/850 °C glow wire | 2.0–3.0 mm |
| Condensate drain pan | IEC 60695-2-12 / IEC 60695-2-13 | GWFI / GWIT 850 °C | 2.5–4.0 mm |
| Under-bonnet acoustic cover | OEM UL 94 V-0 at 3.0 mm | vertical burn V-0 | 2.5–3.5 mm |
| Terminal block carrier | IEC 60695-2-11, UL 94 V-0 | 750 °C / 1.6 mm | 1.6–2.0 mm |
Under-bonnet acoustic cover production with mineral-filled flame-retardant PP is constrained less by tool filling and more by the thermal map of the engine bay; continuous service above 110 °C can produce creep, odour, and premature flame-retardant extraction, so the material is normally restricted to regions where thermocouple measurements remain below 105 °C. Compliance for such covers is usually an OEM specification requiring UL 94 V-0 at 3.0 mm, although adjacent interior-facing surfaces may also require ISO 3795; no general automotive regulation applies to under-bonnet parts. The polymer charge is 100 wt%, and regrind is limited to 10 wt% maximum because the thermal history of multiple passes darkens the flame-retardant mineral system and can reduce flow stability. Injection moulding on 1,200–2,000 t machines with sequential valve-gated hot runners is typical for engine covers, with melt temperature 200–230 °C, mould temperature 30–50 °C, and drying at 80 °C for 2–3 h; if the tool has deep ribs or boss arrays, gas-counterpressure or low-pressure structural foam variants are sometimes used, but published data for this specific configuration is limited and must be validated on the production tool. The main failure modes observed in pilot trials are gloss banding at the hot-runner valve gates and distortion after ejection when the part is demoulded below 60 °C surface temperature. End-product types include engine acoustic covers, cowl-side closeouts, and fuel-rail cover panels for passenger vehicles where the peak radiant soak remains within the stated service boundary.
Because terminal block carriers in washing machines and dishwashers must maintain creep resistance under contact pressure from screw terminals, the mineral-filled grade is selected over unfilled flame-retardant PP for higher stiffness and lower shrinkage at 1.6–2.0 mm wall. The applicable test boundary is IEC 60695-2-11 glow-wire testing at 750 °C for live parts, with UL 94 V-0 certified at 1.6 mm on the part drawing; the product safety standard remains IEC 60335-1:2020 clause 30.2.3. The addition ratio is direct-mould 100 wt%, with regrind restricted to 15 wt% and only from the same lot to prevent batch-to-batch shift in the flame-retardant package; higher regrind fractions have been observed to reduce glow-wire resistance at the thinnest ribs because of mineral attrition and thermal degradation. Injection moulding on 200–400 t machines with multiple-cavity tooling uses melt temperature 200–230 °C, mould temperature 20–40 °C, and drying at 80 °C for 2–3 h; cavity-filling pressure is kept below 80 MPa to avoid flash at thin shut-offs. Screw speed is maintained at 50–90 rpm, and back pressure is set at 0.3–0.8 MPa to stabilise short-shot weight without overworking the mineral filler. End-product types include terminal block carriers, relay mounts, wiring clips, and earthing-point brackets assembled into household laundry and kitchen appliances.
Refrigerator evaporator covers and interior air-duct panels present a low-temperature impact requirement at −20 °C while still requiring UL 94 V-0 at 1.5 mm; the production route uses fast-injection thin-wall tools and requires the compound to be dried to 0.02 % moisture or below to prevent blush at the gate. The material is used at 100 wt%, and closed-loop regrind addition up to 20 wt% is acceptable only where the final part is not in direct food contact and the evaporator cover thickness does not fall below 1.5 mm. Processing on 400–800 t injection moulding machines uses melt temperature 200–230 °C, mould temperature 30–50 °C, and fill speeds above 150 mm/s to prevent premature freeze-off at the end of flow; the tool requires full-round runners with generous cold-slug wells because the mineral filler raises melt viscosity and increases the tendency for jetting at restricted gates. Holding pressure is applied at 40–60 MPa for 6–10 s, and pack-pressure transfer is set by screw position rather than time to reduce cavity-to-cavity mass variation in multi-cavity tools. End-product types include refrigerator evaporator covers, interior air-duct panels, fan motor brackets, and defrost-drain troughs where low-temperature ductility and flame-retardant classification must be maintained simultaneously.
| Injection moulding parameter | Automotive pillar trim | Appliance control panel |
|---|---|---|
| Melt temperature | 200–230 °C | 200–230 °C |
| Mould temperature | 20–40 °C | 30–50 °C |
| Drying condition | 80 °C, 2–3 h, dew point −30 °C | 80 °C, 2–3 h, moisture ≤ 0.02 % |
| Holding pressure | 30–50 MPa | 40–60 MPa |
| Screw speed | 60–100 rpm | 60–100 rpm |
Competitive Kingfa PP-KF04,PP-KF Flame Retardant/Modified,Mineral Filled, Automotive/Appliance prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-KF04, a PP-KF Flame Retardant/Modified, Mineral Filled, Automotive/Appliance compound, is a member of a flame-retardant/mineral-filled polypropylene series developed for injection-moulded automotive interior and appliance housing applications. The designation identifies a modified polypropylene matrix with a mineral filler package and a flame-retardant system, supplied in pellet form for screw plasticising equipment. Materials of this class are selected when a part must satisfy a combination of UL 94 flammability performance, low post-mould shrinkage, and heat-deflection stability without moving to higher-density engineering thermoplastics. The PP-KF04 grade is positioned among Kingfa appliance and automotive grades where dimensional repeatability and flame resistance are prioritised; however, grade-specific values for melt flow rate, filler content, and mechanical strength should be taken from the manufacturer’s current material datasheet and colour-specific certificate of analysis.
Compounds in the PP-KF04 category are conventionally processed on single-screw reciprocating-screw injection-moulding machines with general-purpose polyolefin screws, although pre-drying at 80 °C to 90 °C for 2 h to 4 h may be required when packaging has been breached or ambient relative humidity exceeds 60 %. Published processing guides for mineral-filled flame-retardant PP grades in this segment recommend melt temperatures from 190 °C to 230 °C and mould temperatures from 20 °C to 50 °C; higher mould temperatures reduce visible weld lines but lengthen cycle time. The mineral filler increases melt viscosity and reduces melt elasticity, so gate sizes and runner diameters are typically increased relative to unfilled PP to prevent shear heating and flow hesitation at thin-wall sections below 1.2 mm.
Tooling for PP-KF04-class materials should incorporate positive venting along the flow path because volatile species from the flame-retardant package can deposit on vents. Vent depths of 0.01 mm to 0.02 mm are common for mineral-filled PP, but vent lands should be cleaned at intervals established during a production trial. Clamp force requirements follow the cavity pressure at the gate; for thin-wall housing components with 1.5 mm wall thickness, hydraulic clamping machines in the 80 t to 200 t range are typical for single-cavity tools, although the actual value is determined by projected area and process pressure.
Melt flow rate for mineral-filled FR-PP in this class is frequently reported between 8 g/10 min and 15 g/10 min at 230 °C under 2.16 kg load by ISO 1133-1:2022. The exact PP-KF04 value should be selected based on flow length and wall thickness, because higher-flow variants may improve fill but can reduce impact strength and flame-retardant performance.
Flame-retardant certification for these grades is commonly reported as UL 94 V-0 at wall thicknesses between 1.5 mm and 3.0 mm, with the exact minimum thickness controlled by the grade, colour concentrate, and regrind content. The PP-KF04 model should be specified with the final production pigment and additive package because titanium dioxide and certain organic pigments can alter UL 94 performance. The compound is intended for parts such as household-appliance control housings, interior automotive trim, connector shrouds, and structural brackets where a balance of flame resistance and stiffness is required.
Mineral filler in PP-KF04 reduces anisotropic post-mould shrinkage by interrupting the semi-crystalline polypropylene matrix, which lowers both the mould shrinkage and the coefficient of linear thermal expansion. Shrinkage data for mineral-filled FR-PP compounds are normally measured by ISO 294-4 or ASTM D955; publicly available values for this class commonly fall between 0.6 % and 1.0 % in the flow direction and 0.7 % to 1.1 % transverse to flow for 2 mm plaques. The mineral phase also raises flexural modulus; however, notched Izod impact strength decreases as filler loading increases, and the material becomes more sensitive to sharp internal corners and knit-line stress concentration. Therefore, design practice for PP-KF04 components should avoid abrupt changes in wall thickness and should use radiused corners not below 0.5 mm if impact loading is present.
The flame-retardant system in this compound class works primarily by solid-phase char formation and mineral-filler dilution of combustible polymer. Under test protocols such as UL 94 vertical burning, the char layer reduces dripping and flame spread. The mineral filler contributes to char rigidity but can also increase density relative to unfilled flame-retardant PP. Density is typically determined by ISO 1183-1 or ASTM D792; mineral-filled FR-PP formulations in this market segment usually range from 1.02 g/cm³ to 1.10 g/cm³, compared with 0.94 g/cm³ to 0.98 g/cm³ for unfilled FR-PP. This density increase must be included in part mass and cost estimates.
In addition to UL 94, candidate materials for appliance applications may be screened by ASTM D2863 limiting oxygen index or ISO 5660-1 cone calorimetry. Mineral-filled flame-retardant PP systems often show LOI values in the 24 % to 30 % range, depending on the flame-retardant loading, but these values should not be used as the sole acceptance criterion. The cone calorimeter peak heat release rate is more indicative of contribution to room fire growth; published data for this specific configuration is limited.
Thermal behaviour is commonly characterised by ISO 75-2 or ASTM D648 for heat deflection temperature and ISO 11357-3 for melting temperature. Mineral-filled FR-PP usually maintains an HDT in the range of 100 °C to 125 °C at 0.45 MPa, which supports appliance and automotive interior use but excludes continuous load-bearing service above 90 °C unless heat-stabilised variants are selected. Thermal oxidative stabilisation should be specified for parts exposed to under-hood or close-to-heater environments; published data for this specific configuration is limited.
Filler particle size and surface treatment influence both mechanical performance and flame-retardant efficiency. Coupling agents such as maleic anhydride-grafted polypropylene can improve mineral-matrix adhesion, raising tensile strength and flexural modulus, but they may also increase melt viscosity. The optimum addition level is set by compounding trials because the flame-retardant package can compete for the coupling-agent reaction sites.
If the replacement target is an unfilled flame-retardant PP, PP-KF04 offers lower mould shrinkage, higher flexural modulus, and better dimensional stability, but at a penalty in elongation at break and notched impact strength. Comparative tensile properties are usually measured by ISO 527-2 or ASTM D638-14. Unfilled FR-PP may exhibit tensile elongation above 15 % to 30 %, whereas mineral-filled FR-PP grades commonly fall below 10 % in the same test. The increase in stiffness is measurable as flexural modulus under ISO 178 or ASTM D790; mineral-filled grades may show values from 2.5 GPa to 4.0 GPa depending on filler content and coupling chemistry. This shift from ductile to semi-ductile behaviour must be considered for snap-fit features and self-tapping screw bosses, which can crack if designed with unfilled PP geometry.
Against halogenated flame-retardant polypropylene, the PP-KF series is usually formulated for lower smoke density and lower corrosive gas evolution during burning, although published data for this specific configuration is limited. Halogenated FR-PP systems may achieve UL 94 V-0 at lower additive loading and can retain higher melt flow, but they may generate acidic combustion by-products that complicate recycling and can corrode processing equipment. When specified as a non-halogenated grade, the formulation places greater emphasis on filler dispersion and may show higher plate-out on mould vents after prolonged runs. Production machines with closed-loop barrel cooling and vented screws are recommended to minimise thermal decomposition of the flame-retardant package during compounding and moulding.
| Property | Test method | Mineral-filled FR-PP (PP-KF04 class) | Unfilled FR-PP | Halogenated FR-PP |
|---|---|---|---|---|
| Density | ISO 1183-1 | 1.02–1.10 g/cm³ | 0.94–0.98 g/cm³ | Often 1.00–1.06 g/cm³ depending on filler |
| Tensile elongation at break | ISO 527-2 | Typically 3–10 % | Typically 15–30 % | Typically 5–20 % |
| Flexural modulus | ISO 178 | 2.5–4.0 GPa | 1.3–2.0 GPa | 1.8–3.0 GPa |
| Mould shrinkage | ISO 294-4 | 0.6–1.0 % flow; 0.7–1.1 % transverse | 1.2–2.0 % flow | 0.8–1.4 % flow |
| Flammability rating | UL 94 | V-0 at 1.5–3.0 mm | V-0 at 1.5–3.0 mm | V-0 at 1.5–3.0 mm |
Regulatory documentation for Kingfa PP-KF04 should be requested from the manufacturer for the specific production plant and colour code. Typical compliance claims for appliance and automotive PP compounds are evaluated under RoHS Directive 2011/65/EU, REACH Regulation (EC) No 1907/2006 SVHC screening, and, where applicable, IEC 61249-2-21 or customer-specific prohibited-substance lists. For automotive interior applications, odour, fogging, and total volatile organic compound limits are often tested by methods such as VDA 270, VDA 278, and ISO 12219-3; grade performance depends on the stabiliser package, mineral filler surface treatment, and regrind policy. Published data for this specific configuration is limited, so compliance judgments should be based on a Kingfa certificate of approval for the production compound, not on series-level literature values.
If halogen-free performance is required, the purchaser should verify halogen content against IEC 61249-2-21 or the end-use specification rather than inferring from the PP-KF04 tradename alone.
| Requirement | Reference standard/code | Documentation to verify |
|---|---|---|
| Flammability class | UL 94 vertical burning | Supplier UL yellow card or laboratory test report at final part thickness and colour |
| Halogen content | IEC 61249-2-21 | Certificate showing chloride, bromide, and total halogen maxima |
| Restricted substances | RoHS 2011/65/EU | Supplier declaration for lead, mercury, cadmium, hexavalent chromium, PBB, PBDE |
| SVHC screening | REACH 1907/2006 | Statement covering applicable candidate-list substances |
| Automotive interior emissions | VDA 278 / ISO 12219-3 | VOC and fogging values for the production colour and regrind level |
On production-scale compounding lines, the main processing bottleneck for mineral-filled FR-PP compounds of this type is not melt temperature but filler dispersion and screw torque. Co-rotating twin-screw extruders with L/D 32:1 to L/D 44:1 are typical, with side-feed addition of mineral filler after the polymer melting zone to limit barrel wear. In injection moulding, the use of hardened screw and barrel assemblies is specified where filler loadings exceed 20 wt% to reduce abrasive wear. Observed batch-to-batch variance in flame-retardant performance is commonly traced to particle-size distribution of the mineral filler, moisture absorption by the flame-retardant package, or inconsistent regrind addition above 15 %. Therefore, closed-loop weight feeders and in-line melt-pressure monitoring are used to maintain lot-to-lot consistency.
Plate-out deposits on mould vents can appear after 8 h to 12 h of continuous cycling when mould temperature exceeds 50 °C, depending on additive chemistry. Maintenance intervals should be validated on the production tool because the mineral filler and flame-retardant package interact with mould surface deposits. Published data for this specific configuration is limited, and process parameters should be established from a moulding trial using the production colour and regrind level.