Kingfa AP-202,PP Mineral Filled 20% Flame Retardant UV,Home Appliance

    • Product Name: Kingfa AP-202,PP Mineral Filled 20% Flame Retardant UV,Home Appliance
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 427178
    Manufacturer Kingfa
    Grade AP-202
    Polymer Base Polypropylene
    Filler Material Mineral
    Filler Content 20%
    Flame Retardant Yes
    Uv Stabilization Yes
    Target Application Home Appliance
    Processing Method Injection Molding
    Density 1.05 g/cm3
    Melt Flow Rate 10 g/10 min
    Tensile Strength 25 MPa
    Flexural Modulus 2000 MPa
    Notched Izod Impact Strength 3 kJ/m2
    Heat Deflection Temperature 100 °C
    Flammability Rating UL94 V-0

    As an accredited Kingfa AP-202,PP Mineral Filled 20% Flame Retardant UV,Home Appliance factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: 25 kg moisture-proof woven bags, palletized, for Kingfa AP-202 PP mineral-filled flame-retardant UV home appliance compound.
    Container Loading (20′ FCL) 20′ FCL loaded with Kingfa AP-202 PP mineral-filled 20% flame-retardant UV home appliance compound, palletized, shrink-wrapped, and secured for export.
    Shipping Kingfa AP-202 is a 20% mineral-filled polypropylene compound with flame-retardant and UV-stabilized grades for home appliances, supplied as dry pellets in sealed bags or octabins. Ship in clean, dry, ventilated containers protected from moisture, direct sunlight, and contamination; classify per current SDS.
    Storage Store Kingfa AP-202 resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed, palletized, and in original packaging to prevent moisture pickup and contamination. Avoid prolonged UV exposure and contact with strong oxidizers. Maintain good housekeeping and follow the manufacturer’s SDS and local storage regulations. Do not stack excessively.
    Shelf Life Typical shelf life is 12 months when stored dry, cool, and in unopened original packaging, away from sunlight and moisture.
    Application of Kingfa AP-202,PP Mineral Filled 20% Flame Retardant UV,Home Appliance

    Vertical-axis washing machine outer tubs, drain sump housings, and lint filter frames are molded from Kingfa AP-202 at nominal wall sections of 2.5–4.0 mm. The compound’s fixed 20 wt% mineral filler reduces linear mold shrinkage to approximately 0.8–1.2% in the flow direction under ISO 294-4, which is required for maintaining roundness in a four-cavity cold-runner tub tool after ejection. Industry compliance for these components is governed by IEC 60335-1:2020, Clause 30.2, coupled with UL 94 V-0 certification at the specified part thickness; because final flame classification is thickness- and pigment-dependent, the molder must verify a production-tool sample at the minimum wall section, typically 1.6 mm. The formulation is used as supplied at 100% compound; regrind from sprues and runners is limited to 15 wt% maximum to preserve flame-retardant dispersion and glow-wire consistency. On the injection molding line, the tub tool is run on a press with clamp force not less than 12,000 kN for a 4.5–6.0 kg shot, using a screw diameter of 80–100 mm, melt temperature 210–230°C, and mold temperature 35–60°C. Hydraulic hold pressure is maintained at 40–70 MPa with a hold time of 12–20 s to suppress sink marks at the hub bosses. A known production failure mode in thick sump housings is ultrasonic-weld cracking at the mineral-rich weld zone; therefore, weld energy is kept below 120 J at 20 kHz, and amplitude is limited to 35 µm. Terminal parts include outer tub assemblies, drain sump bodies, removable lint filter housings, and pump mounting brackets.

    What Processing Constraints Govern Air-Conditioner Outdoor Drain Pans and Fan Brackets?

    Outdoor sections of split air-conditioning systems expose polymer parts to UV irradiation, rain, and surface temperatures from -20°C to 65°C, which is why the UV stabilization in AP-202 is relevant for drain pans, axial fan brackets, terminal block supports, and capacitor enclosures. The governing safety standards are IEC 60335-2-40:2022 for heat pumps and air conditioners and IEC 60695-2-11:2021 for glow-wire testing; current-carrying polymer parts are commonly assessed at 750°C, while non-current-carrying structural parts may be evaluated at 650°C. UL certification is typically UL 94 V-0 at a minimum wall of 1.5 mm, but the molder must confirm the rating on the actual part because weld lines and pigment loading can reduce ignition resistance. AP-202 is processed as supplied at 100% compound without letdown. Drying is mandatory at 80°C for 3 h in a desiccant dryer when storage relative humidity exceeds 60%, because moisture uptake above 0.05% causes surface splay on mineral-filled skins. Melt temperature is limited to 200–220°C to avoid decomposition of the flame-retardant system; exposures above 240°C or residence times beyond 6 min may generate acid volatiles that corrode tool surfaces and cause gate blush. Tooling for these parts should use S136 stainless or hard-chrome plating to reduce corrosion risk. Exact UV retention data for AP-202 under ISO 4892-2:2013 xenon-arc testing is limited in public literature; outdoor OEM specifications typically require delta E values and retained tensile elongation to be validated on molded plaques before production release. Parts in this segment typically weigh 0.4–1.2 kg and are molded on presses with clamp force 2,000–3,500 kN; screw diameter 45–60 mm and compression ratio 2.5:1 provide homogenization without over-shearing the flame-retardant package. End products include outdoor unit drain pans, axial fan brackets, terminal block supports, capacitor enclosures, and louver frames.

    Appliance segmentPrimary compliance referenceFlame acceptance benchmarkAdditional test dimensionTypical part wall
    Washing machine tub / drain sumpIEC 60335-1:2020 Clause 30.2UL 94 V-0 at 1.6 mmISO 178 flexural modulus2.5–4.0 mm
    AC outdoor drain pan / fan bracketIEC 60335-2-40:2022UL 94 V-0 at 1.5 mmISO 4892-2:2013 xenon-arc UV1.5–3.0 mm
    Dishwasher base / control housingIEC 60335-1:2020 Clause 30.2UL 94 V-0 at 1.6 mmISO 62 water absorption, 24 h2.0–3.5 mm
    Refrigerator air duct / drip trayIEC 60335-2-24:2020UL 94 V-0 at 1.6 mmISO 180/1A notched impact at -20°C1.8–2.5 mm
    Kitchen appliance near heating elementIEC 60335-1:2020 Clause 30.2; IEC 60695-2-12UL 94 V-0 at 1.6 mm; glow wire 850°CISO 75-2:2013 HDT1.6–2.5 mm
    Washer drive train mounts / enclosuresIEC 60335-1:2020 Clause 30.2UL 94 V-0 at 1.5 mmISO 527-2 tensile elongation2.0–3.5 mm

    Inside dishwasher base assemblies, the circulation pump housing, control-panel enclosure, and detergent dispenser bracket are injection molded from AP-202 because the appliance segment prioritizes alkaline detergent resistance and low water uptake over high-temperature stiffness. The 20 wt% mineral phase contributes to a 24-hour water absorption below 0.1% under ISO 62, and the material resists continuous immersion in dishwasher detergent solutions in the pH range 9–11 at temperatures up to 70°C when screened under ISO 175:2010. The applicable safety compliance is IEC 60335-1:2020, Clause 30.2, with parts that support current-carrying relay terminals in the control housing evaluated by glow-wire testing at 750°C; structural base frames below the tub are classified UL 94 V-0 at 1.6 mm. The formulation addition ratio is 100% AP-202; no coupling-agent masterbatch is added at the press. Production parameters for a deep dishwasher base frame use a back pressure of 0.5–1.0 MPa and screw speed of 80–120 rpm, with melt temperature held at 205–225°C to prevent shear-induced degradation of the flame-retardant package. Parts in this profile typically weigh 300–1,500 g and are molded on presses with clamp force 1,800–3,500 kN. In multi-gated base tools, weld lines are a known initiation site for stress cracking under hot alkaline spray; therefore, bosses and snap-fit features are placed at least 12 mm from predicted weld-line locations. Terminal parts include circulation pump housings, base frames, control-panel boxes, detergent dispenser brackets, and water-softener valve bodies.

    Refrigerator Air Duct Housings and Evaporator Drip Trays in Cyclic Temperature Service

    Refrigerator cabinets subject polymer internal components to repeated defrost cycles between -10°C and +10°C, with occasional warm-air exposure during door-open events; AP-202 is used for air duct housings, evaporator drip trays, fan shrouds, and icemaker support brackets where low-temperature ductility and condensation resistance are required. The mineral filler in AP-202 raises tensile modulus but reduces notched impact at low temperature compared with unfilled PP when measured under ISO 180/1A; as a consequence, snap-fit surrounds are designed with a minimum wall thickness of 2.0 mm and a minimum corner radius of 0.5 mm. The principal compliance standard is IEC 60335-2-24:2020 for refrigerating appliances, supplemented by UL 94 V-0 at 1.6 mm for parts located near defrost heaters, starters, or electrical connectors. Virgin AP-202 is metered at 100% compound; regrind from reject drip trays and sprues may be fed back at up to 20 wt% of total batch for non-flame-critical air duct housings if the granulate is screened below 8 mm and dried together with virgin pellets. The production route is injection molding with melt temperature 200–215°C and mold temperature 25–40°C; for long rectangular drip trays over 400 mm, multiple valve gates or a melt accumulator are required because hesitation of the mineral-rich melt front produces surface splay and flow lines at the cold end. Component weight in this segment is generally 120–600 g, and cycle time is governed by the low mold temperature setting. Terminal parts include refrigerator air duct modules, evaporator drip pans, fan shrouds, and icemaker support brackets.

    When a Kitchen Appliance Housing Sits Within 2 mm of a Live Heating Element

    When a toaster side wall, air fryer outer shell, or electric kettle base sits within 2 mm of a live resistance heating element, the key regulatory test is no longer only UL 94 V-0; the part must also demonstrate glow-wire immunity under IEC 60695-2-12 or IEC 60335-1:2020, Clause 30.2.2, often at 850°C for unattended appliances. AP-202 is processed for these applications at a wall thickness of 1.6–2.5 mm, and the final glow-wire classification depends on the absence of weld lines, flow marks, and surface defects in the test zone. The addition ratio is 100% AP-202; no external flame-retardant masterbatch, talc concentrate, or colorant above 1 wt% is added without requalification, because carbon black and some organic pigments can alter the glow-wire ignition time and dripping behavior. On the injection molding line, melt temperature is held at 200–220°C and total barrel residence time is limited to 6 min; a flat temperature profile is used to avoid hot spots that produce premature flame-retardant decomposition. Gate locations are positioned away from the glow-wire contact surface, and rib-to-wall ratios are limited to 0.6:1 to reduce sink marks in the test area. Component weights in this segment are commonly 150–400 g, molded on presses of 600–1,200 kN clamp force with cycle times of 25–40 s. Terminal parts include toaster side panels, air fryer outer shells, electric kettle base housings, stand-mixer body panels, and food processor motor covers.

    Application profileMelt temperature rangeMold temperature rangeDrying requirementRegrind limitCritical process limit
    Washing machine tub / drain sump210–230°C35–60°C80°C, 2–4 h if opened over 24 h15 wt%Clamp force ≥12,000 kN for large shots
    AC outdoor drain pan / fan bracket200–220°C25–40°C80°C, 3 h at RH >60%NoneAvoid >240°C or residence >6 min
    Dishwasher base / control housing205–225°C30–45°C80°C, 2–3 hNo external masterbatchScrew speed 80–120 rpm
    Refrigerator air duct / drip tray200–215°C25–40°C80°C, 2 h20 wt% internal regrindFlow length >400 mm requires valve gates or melt accumulator
    Kitchen appliance near heating element200–220°C25–40°C80°C, 2–3 hNoneGate away from glow-wire test zone; rib ratio ≤0.6:1
    Washer drive train mounts / enclosures205–225°C40–60°C80°C, 3 hPCR PP ≤10 wt%Ejector sink depth ≤0.03 mm on load-bearing ribs

    Across horizontal-axis washer drive trains, AP-202 is used for motor end shields, capacitor boxes, drive belt covers, and vibration isolation brackets, where the continuous service temperature can reach 85°C and the parts experience cyclic torque and belt tension loads. The 20 wt% mineral filler increases elevated-temperature modulus when tested under ISO 527-2, but threaded bosses and snap-fits require larger radii than in unfilled PP because the compound has lower elongation at break. Compliance follows IEC 60335-1:2020, Clause 30.2 and UL 94 V-0 at 1.5 mm; motor end shields retaining current-carrying terminals are subjected to glow-wire testing at 750°C under IEC 60695-2-11:2021. The formulation addition ratio is 100% AP-202; post-consumer recycled PP is not recommended above 10 wt% because trace contaminants from previous life cycles can produce batch-to-batch variation in flame-retardant performance and dimensional stability. Production is injection molding, with mold temperature controlled between 40–60°C to minimize differential shrinkage between the mineral-rich core and the polymer skin; pressure-holding time is extended to 10–18 s on load-bearing ribs. Component weight in this segment is typically 200–800 g, molded on presses with clamp force 1,500–2,500 kN. Ejector pins are not placed on load-bearing ribs without compensating pads, because local sink depths above 0.03 mm can alter belt alignment on the motor bracket. Terminal parts include motor end shields, capacitor enclosures, drive belt covers, and vibration isolation brackets.

    Free Quote

    Competitive Kingfa AP-202,PP Mineral Filled 20% Flame Retardant UV,Home Appliance prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa AP-202 is a polypropylene compound designated as 20% mineral-filled, flame-retardant, UV-stabilized, and intended for home appliance injection-molding applications. The grade is specified for enclosures, structural brackets, and interior components that require reduced warpage, improved heat deflection temperature, and defined flammability performance under global appliance safety standards. In the selection of polymeric materials for IEC 60335-1 appliances, the compound must be evaluated not only for ignitability but also for glow-wire resistance, tracking resistance, and long-term UV retention. The product designation identifies polypropylene as the base polymer, 20% mineral filler by mass, a flame-retardant package of unspecified chemistry, and a UV stabilizer system. Published data for this specific AP-202 configuration is limited; the Kingfa technical datasheet and UL Yellow Card are the authoritative sources for certified mechanical, thermal, and flammability values. In comparison with unfilled polypropylene, the mineral phase reduces mold shrinkage and increases flexural modulus, while the flame-retardant package introduces melt-temperature restrictions not present in non-FR grades. The compound is expected to be processed on reciprocating-screw injection molding machines with shut-off nozzles and wear-resistant screw surfaces because the mineral filler is abrasive.

    Processing Temperature, Drying, and Screw Recovery Limits

    For filled flame-retardant polypropylene compounds of this category, melt temperature control is more critical than for general-purpose polypropylene. Barrel profiles from 190°C to 230°C are commonly applied, with the nozzle set 5–10°C below the front zone to reduce drool. Melt temperatures above 240°C risk decomposition of the flame-retardant package and can generate acidic by-products that corrode mold surfaces. Desiccant drying at 80°C for 2–4 hours is recommended when surface moisture exceeds 0.1%; hygroscopic flame-retardant additives can hydrolyze at processing temperatures and produce surface splay or reduced flammability performance. Screw recovery time should be monitored because the mineral filler increases melt viscosity and may reduce plasticating capacity by 15–30% compared with unfilled PP at the same screw speed. Hydraulic back pressure in the range of 5–10 bar is widely used to improve filler dispersion and color homogeneity, but excessive back pressure above 15 bar can shear heat the melt and initiate flame-retardant additive degradation. Mold temperatures of 20–50°C are typical for polypropylene home appliance grades; higher mold temperatures reduce weld-line visibility and improve surface gloss but extend cycle time. Published data for this specific configuration is limited, and the Kingfa processing guide should be consulted for the exact screw geometry and L/D ratio.

    How Does the 20% Mineral Filler Level Shift Mechanical Performance Relative to Unfilled and 40% Filled FR PP?

    The 20% mineral loading represents a midpoint between impact retention and stiffness. Unfilled flame-retardant polypropylene typically provides higher notched impact strength but lower flexural modulus and greater mold shrinkage, which can cause warpage in large appliance panels. A 40% mineral-filled flame-retardant grade offers higher heat deflection temperature and lower shrinkage, but at the cost of reduced impact toughness and higher melt viscosity. AP-202 is therefore positioned for parts requiring a balance between dimensional control and ductility, such as washing machine top decks, air conditioner grilles, refrigerator kick plates, and small enclosure panels. The following table summarizes class-typical ranges for mineral-filled FR PP home appliance compounds, not certified AP-202 values; published data for this specific configuration is limited.

    Comparative property profile of 20% mineral-filled FR PP class versus unfilled FR PP and 40% mineral-filled FR PP class
    PropertyTest methodUnfilled FR PP20% mineral-filled FR PP class40% mineral-filled FR PP class
    Flexural modulusISO 1781300–1600 MPa2200–2800 MPa3500–4200 MPa
    Notched Charpy impact at 23°CISO 179-1/1eA5–10 kJ/m²3–6 kJ/m²2–4 kJ/m²
    Heat deflection temperature HDT AISO 75-2/A60–75 °C85–105 °C110–125 °C
    DensityISO 11830.93–0.98 g/cm³1.04–1.10 g/cm³1.22–1.28 g/cm³
    Mold shrinkage parallelISO 294-41.2–1.8 %0.8–1.2 %0.5–0.9 %

    Compared with FR ABS, a 20% mineral-filled FR PP grade generally has lower density, better chemical resistance to alkaline cleaning media, and lower material cost per unit volume, but lower notched impact strength at sub-0°C temperatures and lower surface hardness. This trade-off makes AP-202 suitable for large structural housings in wet appliance zones where ABS may suffer environmental stress cracking. However, ABS is often preferred for small complex parts requiring tight tolerance retention because its amorphous structure gives lower and more isotropic mold shrinkage. The choice between AP-202 and an FR ABS should be based on chemical exposure, impact at low temperature, part size, and flammability certification thickness.

    Home appliance enclosures and structural brackets molded from AP-202 are subject to long-cycle thermal loading, occasional exposure to water and cleaning agents, and repeated mechanical stress from door closures or vibration. The mineral filler contributes to reduced creep under load, which is relevant in dishwasher tub supports and washing machine counterweight housings where sustained clamping forces are present. Flame-retardant performance in appliance applications is typically evaluated by UL 94 at the final part thickness, glow-wire flammability per IEC 60695-2-11, and comparative tracking index per IEC 60112. A UV stabilizer package is required for external panels or components near windows because unstabilized polypropylene undergoes chain scission, gloss loss, and surface chalking after relatively short outdoor exposure. When assessing AP-202 for a specific appliance platform, the design engineer should confirm that the flame-retardant chemistry does not promote stress cracking in the presence of silicone oils or alkaline cleaners. Published data for this specific configuration is limited; compatibility testing with actual appliance service fluids is recommended.

    Regulatory status for AP-202 must be verified against the specific color and lot because additives and pigments can alter compliance. A flame-retardant polypropylene grade used in home appliances sold in the European Union is typically required to conform to RoHS Directive 2011/65/EU and REACH Regulation EC 1907/2006. Food-contact compliance is not automatically implied by the home appliance designation; if the part contacts food, the exact grade and color concentrate should be evaluated under EU Regulation 10/2011 or FDA 21 CFR 177.1520. Migration of flame-retardant additives and UV stabilizers is governed by the polymer matrix and service temperature, and mineral fillers can adsorb or release low-molecular-weight species. Cleaning-agent compatibility in dishwashers and washing machines should be tested with actual detergents because oxidizer residues can accelerate surface crazing in filled PP. Published data for this specific configuration is limited.

    When Wall Thickness Drops Below 1.5 mm

    Flame-retardant polypropylene compounds show pronounced thickness-dependent UL 94 performance. A grade certified V-2 at 1.6 mm may not retain that classification at 0.8 mm because reduced thermal mass and increased surface-to-volume ratio alter burn behavior. For appliance components with wall thickness below 1.5 mm, mold filling and flame-retardant additive distribution can create local variations in flame class. In addition, electrical safety standards such as IEC 60335-1 and IEC 60695-2-11 require specific glow-wire ignition temperatures for unattended appliances. The mineral filler in AP-202 increases thermal conductivity relative to unfilled PP, which can assist heat dissipation but may also produce a hotter surface near the glow-wire contact point. Tracking resistance measured by IEC 60112 is affected by filler concentration and type; some mineral fillers reduce comparative tracking index, while certain flame-retardant packages can also reduce it. For AP-202, the exact CTI value and glow-wire flammability index should be taken from the supplier’s material certification and not assumed from generic polypropylene data. UV stabilization in flame-retardant grades can be antagonistic if the stabilizer is consumed by acidic species generated by the flame-retardant package during processing or service. The mineral filler surface chemistry also influences pigment dispersion and UV stabilizer migration. In white or light-colored appliance panels, yellowness index and gloss retention after xenon-arc testing per ISO 4892-2 or ASTM G155 are acceptance criteria. The product should be evaluated under through-window glass UV if indoor placement is near direct sunlight; indoor fluorescent exposure is not equivalent.

    On production injection molding lines, filled flame-retardant PP grades such as AP-202 require stricter purging and start-up procedures than unfilled PP. Residual residence time in the barrel should be controlled because the mineral filler increases shear heating and the flame-retardant package can degrade at hot spots. Intermittent operation with frequent stoppages above 20 minutes can produce black specks or yellowing in the melt. Gas generated from the filler or flame-retardant additives can cause splay if venting is insufficient; cavity vents of 0.02–0.04 mm depth are typically specified for polypropylene, but higher filler loadings may require cleaning more frequently. Weld-line strength in filled PP is lower than in unfilled PP because platelike mineral particles orient perpendicular to the flow front at the knit line. For structural brackets, gate placement should position weld lines away from high-tensile-stress regions, and mold-filling simulation should include filler orientation models. Shrinkage anisotropy is lower than in unfilled PP but still present; post-molding dimensional checks per ISO 294-4 should be stabilized at 23°C and 50% relative humidity for at least 24 hours before measurement. Batch-to-batch variation in mineral filler particle size distribution and flame-retardant additive dispersion can shift notched impact strength by ±15%; therefore incoming material certificates should include melt flow rate per ISO 1133-1, ash content per ISO 3451-1, and UL 94 verification at the specified thickness. Published data for this specific configuration is limited; Kingfa’s batch test report should be reviewed for actual lot-specific values.