| HS Code | 532088 |
| Density | 1.05 g/cm³ |
| Melt Flow Rate | 15 g/10 min |
| Tensile Strength At Yield | 22 MPa |
| Elongation At Break | 30% |
| Flexural Modulus | 2200 MPa |
| Notched Izod Impact Strength | 30 kJ/m² |
| Heat Deflection Temperature | 110 °C |
| Vicat Softening Temperature | 150 °C |
| Molding Shrinkage | 1.0% |
| Rockwell Hardness | R 95 |
| Flammability Rating | HB |
| Processing Temperature | 220–240 °C |
As an accredited Kingfa API-2012,PP Resin,Automotive, Interior/Dashboard factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-barrier bags, 40 bags per pallet (1,000 kg), for Kingfa API-2012 PP resin automotive interior/dashboard. |
| Container Loading (20′ FCL) | 20′ FCL loaded with Kingfa API-2012 PP Resin, automotive interior/dashboard grade, in 25 kg bags on pallets, secured for export. |
| Shipping | Kingfa API-2012 PP Resin is supplied as solid polypropylene pellets for automotive interior/dashboard parts. Ship in sealed, moisture-proof bags or lined cartons at ambient temperature, protected from direct sunlight, moisture, and contamination. It is not classified as dangerous goods; standard industrial handling and no special shipping labels are required. |
| Storage | Store Kingfa API-2012 PP Resin in original sealed bags/containers in a cool, dry, well-ventilated area, protected from direct sunlight, heat, sparks, and flames. Keep away from strong oxidizers. Prevent moisture pickup and contamination, stack securely, use FIFO, and follow the SDS and local regulations. |
| Shelf Life | Shelf life is typically 24 months when stored dry, in original unopened packaging, away from direct sunlight and heat. |
In instrument panel substrate production, Kingfa API-2012 is introduced as a controlled-rheology polypropylene impact copolymer. The lot melt flow rate is verified to ISO 1133-1:2022 Method A at 230 °C/2.16 kg; thin-wall dashboard moulding requires a value in the 10–15 g/10 min band, though published datasheet limits for this specific Kingfa designation are narrow and must be confirmed by lot report. The dry blend is prepared with 20–25 wt% high-aspect-ratio talc masterbatch and 3–8 wt% ethylene-octene impact modifier. Drying at 80 °C for 2–4 h is imposed when ambient relative humidity exceeds 60 %; retained moisture above 0.05 % produces steam streaks behind the defroster ribs. Injection moulding is performed on a reciprocating screw unit with L/D 24:1 to 25:1, clamp force between 12,000 kN and 25,000 kN, and shot capacity not less than 60 % of barrel volume. Melt temperature is held at 210–240 °C; excursions above 250 °C cause volatile cracking from the talc carrier and surface splay, while sustained operation below 205 °C freezes the flow front prematurely at the glove box hinge bosses. Mould temperature is 30–50 °C, with the higher end used on grained surfaces to maintain replication. Packing switch-over is set at 97–98 % of fill, and hold pressure is profiled in two stages from 45 MPa to 25 MPa to prevent sink around the airbag channel. The finished component is a full instrument panel substrate carrying insert-moulded defroster grille anchors, cowl attachment bosses, and an invisible passenger airbag channel. Flammability is screened to ISO 3795 at a burn rate below 100 mm/min; fogging is assessed by VDA 275, and heat ageing is performed to ISO 188 at 140 °C for 500 h with no visible surface degradation. Amine-containing mould release agents are excluded; zinc stearate or semipermanent fluoropolymer releases are preferred because residual amine species interact with catalyst residues.
Glove box outer door and knee bolster parts derived from Kingfa API-2012 use a lower filler content than the instrument panel substrate because the latch boss and hinge sockets are loaded in snap-fit assembly rather than structural bending. The compound is typically prepared with 12–18 wt% talc masterbatch and 2–4 wt% custom colour masterbatch; additional impact modifier is omitted unless the component must pass instrumented knee impact at -30 °C. The melt temperature is set at 205–225 °C, and the mould temperature is held at 25–40 °C. Two tunnel gates feed the hinge boss, creating a weld line at the latch tower; the boss wall thickness is increased by 0.5 mm relative to the rib root to shift the weld line away from the stress concentration. Back pressure is kept below 0.8 MPa to prevent colour masterbatch streaking, and screw retraction is limited to 50 mm for melt cushion consistency. Instrumented puncture resistance is tested to ASTM D3763 at 2.2 m/s; the required energy absorption is set by ECE R21 or FMVSS 201U, depending on sale region. Scratch and mar resistance is monitored by GMW14650 or VW PV3952, with delta L values below 1.5 after 10 N load. The delivered terminal part is the glove box outer door with integrally moulded hinge pin sockets and the knee bolster trim panel with crush ribs that collapse without brittle fracture.
Map pocket and lower door trim configurations replace glass-fibre reinforcement with 10–15 wt% talc to preserve cold hinge flexibility and avoid visible fibre read-through on grained surfaces. Kingfa API-2012 is metered with 2–3 wt% black masterbatch and a weather-resistant stabilizer package; compounded density is controlled to 0.99–1.04 g/cm³ by ISO 1183-1:2019. Injection speed is profiled as slow-fast-slow to prevent jetting at the map pocket base; the fast segment does not exceed 85 mm/s screw advance on machines with 50 mm screw diameter. Chemical-etched grain depth is specified at 25–30 µm, and demould temperature is 45 °C to avoid gloss shift on the grained surface. Ultraviolet exposure is screened on plaques according to ISO 105-B06 cycle 4 for 1,000 h; severe OEM programmes may require 2,700 kJ/m² total irradiance with delta E below 3.0 before acceptance. The terminal products are the lower door trim panel, integrated map pocket, and speaker grille bridge; the speaker bridge rib spacing is 6 mm to reduce buzz-frequency transmission without creating sink marks.
For B-pillar upper trim in Kingfa API-2012, the moulded part is specified at 1.5–2.0 mm nominal wall to permit side curtain airbag deployment without fragment ejection. The compound contains 5–8 wt% talc and no recycle fraction; low-temperature ductility is checked by ISO 179-1:2010 Charpy impact at -30 °C with a minimum energy threshold set by the airbag integrator. Sequential valve gating is used to move the weld line away from the curtain airbag tear path; valve gate timing is offset by 0.3 s between the upper and lower gate. Melt temperature is 215–235 °C, and mould temperature is 25–35 °C. The injection profile uses 0.8 mm decompression after screw recovery to prevent drool at the hot tip. Interior head impact obligations are met under FMVSS 201U or ECE R21 as applicable, with the part inspected for sharp edges below R 2.5 mm in the head-impact zone. The terminal part is the B-pillar upper cover with integrated curtain airbag break-through ribs and energy-absorbing stand-off bosses.
HVAC ductwork and defroster nozzle mouldings from Kingfa API-2012 require the lowest volatile contribution in the interior thermoplastic set because recirculated cabin air passes directly over the polymer surface. The compound is built at 8–12 wt% talc with a high-molecular-weight phenolic antioxidant and a phosphite secondary stabilizer; no post-consumer recyclate and no amine-based light stabilizer are used. Melt temperature is capped at 220 °C, and residence time is held below 5 min at temperature to avoid chain scission and aldehyde formation. Wall sections are 1.2–1.8 mm, with rib-to-wall ratio kept under 0.6:1 to prevent sink on the visible edge. The tool runs with vacuum venting at the end of fill; vent depth is 0.015 mm. Fogging condensate is measured by VDA 275 on 100 mm diameter test discs, odor by VDA 270, and VOC emission by VDA 278. Release agents are restricted to those with no fatty amine chemistry. The terminal products are the heater outlet, defroster nozzle, and air mixing chamber assembled into the instrument panel air path.
| Parameter | Method | Typical acceptance |
|---|---|---|
| Fogging condensate | VDA 275 | ≤2 mg |
| Odour | VDA 270 | ≤3 |
| VOC | VDA 278 | ≤50 µg/g |
| HDT at 0.45 MPa | ISO 75-2:2013 Method B | ≥80 °C |
| Flexural modulus | ISO 178:2019 | 1,800–2,400 MPa |
Passenger airbag door moulding from Kingfa API-2012 is the highest-risk application for fracture mechanics because the tear seam must remain invisible after laser weakening but must open at -35 °C without splintering. The compound uses 15–20 wt% talc and 8–12 wt% ethylene-octene impact modifier; the modifier content is selected so that the ductile-to-brittle transition stays below -40 °C while maintaining flexural modulus above 1,500 MPa. The gate is placed outside the airbag flap boundary; any weld line intersecting the tear seam is rejected because it changes the residual wall thickness by more than 0.05 mm. Laser scoring is performed on a three-axis galvo station after moulding; the tear seam residual thickness is held at 0.4–0.6 mm, with hole spacing of 1.0 mm and hole diameter of 0.15 mm. Mould temperature is elevated to 35–50 °C to minimize frozen-in stress at the hinge. After moulding, parts are conditioned for 48 h at 23 °C/50 % RH before laser scoring. Deployment testing follows OEM airbag system specifications at 23 °C, -35 °C, and 85 °C after heat ageing to ISO 188 at 140 °C for 500 h. Published data for this specific Kingfa compound in passenger airbag door geometry is limited; therefore lot-level Charpy impact at -35 °C is mandatory.
Indicative screening ranges for talc-filled polypropylene impact copolymer compounds are shown below; they are not a substitute for lot-specific data.
| Impact modifier content | ISO 179-1 Charpy at -35 °C | Flexural modulus |
|---|---|---|
| 0 wt% | 5–8 kJ/m² | 2,400–2,700 MPa |
| 5 wt% | 8–12 kJ/m² | 2,000–2,400 MPa |
| 8 wt% | 12–18 kJ/m² | 1,800–2,200 MPa |
| 12 wt% | 18–25 kJ/m² | 1,500–1,800 MPa |
For centre console side panels based on Kingfa API-2012, the compound is prepared with 10–15 wt% talc and 2 wt% scratch-resistant masterbatch to balance low-gloss appearance and knee-contact softness. The panels are produced with a sequential valve-gated hot runner; the first gate opens at the rear console mounting boss to orient flow toward the shifter bezel, and the second gate opens after 0.5 s to remove the hesitation line. Melt temperature is 200–220 °C, mould temperature 30–40 °C. The grained surface is specified at 60° gloss below 2.0 GU using a 20° glossmeter; gloss is checked after 100 h of ISO 105-B06 cycle 4 xenon exposure to detect surface chalking. Mounting bosses are ultrasonic welded into the floor console structure; weld joint design uses a shear joint with 0.3 mm interference and 20 kHz frequency. The terminal products are the left- and right-side centre console covers, shifter bezel substrate, and rear HVAC outlet surround.
Competitive Kingfa API-2012,PP Resin,Automotive, Interior/Dashboard prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa API-2012, PP Resin, Automotive, Interior/Dashboard, is a polypropylene-based injection-moulding grade positioned for hard dashboard substrates, instrument panel carriers, defroster grilles, and lower interior trim retainers. The material is manufactured by Kingfa Science & Technology Co., Ltd. and is described in trade literature as a controlled-rheology PP impact copolymer or mineral-modified compound; however published data for this specific configuration is limited. The exact ISO 1043-1 designation, filler content, and stabiliser package should be taken from the supplier’s technical data sheet and safety data sheet. The numerical ranges in this technical overview therefore refer to the accepted specification envelope for heat-stabilised PP interior compounds rather than to grade-certified values for API-2012.
The automotive interior positioning implies that odour, fogging, and volatile organic compound emissions are design-critical parameters. Unlike general-purpose PP injection grades, dashboard materials must be evaluated by multiple cabin-air standards, not only by mechanical property tables. Kingfa API-2012 is usually compared with unfilled impact copolymers, talc-filled PP copolymers, and occasionally ABS/PC dashboard substrates; the selection depends on part geometry, tool texture, and the OEM material approval platform.
The processing window for low-gloss PP dashboard compounds is narrower than the general PP envelope because visual-modifier domains and low-emission stabilisers show temperature sensitivity. A typical barrel profile from feed throat to nozzle is 210 °C, 220 °C, 230 °C, and 230 °C, with a permissible melt-temperature drift of ±5 °C. If the melt temperature exceeds 240 °C, surface gloss can increase at the gate and knit lines, and residual stabiliser by-products can raise VDA 277 VOC values. If the melt temperature falls below 210 °C, filling pressure rises and micro-texture replication becomes incomplete in grained dashboard surfaces.
Pre-drying is not mandatory for virgin polypropylene at routine storage conditions, but condensation-induced splay can occur when cold pellets are discharged into a warm hopper. At ambient relative humidity above 60 %, regrind should be dried at 80 °C for 2 h in a desiccant dryer with a dew point below −20 °C. The use of undried rework above 20 % by weight is not recommended unless the rework has been stored in closed silos and sampled for moisture by ISO 15512:2019.
Screw-recovery time should be matched to cooling time. If plasticising time exceeds cooling time by more than 20 %, low-gloss modifier packages can segregate in the compression zone, producing gloss bands on the part surface. A general-purpose PP screw with compression ratio 2.5:1 to 3.0:1 is adequate for most unplasticised dashboard compounds. For wall sections of 2.0–3.0 mm, screw injection speed is typically 30–100 mm/s. Filling too slowly creates hesitation lines at ribs, while excessive speed creates jetting and frictional shear heating near the gate. In multi-cavity tools, cavity pressure sensors should be mounted at the last cavity to ensure pressure at transfer remains above 30–35 MPa and the end-of-hold cavity pressure does not fall below 20–25 MPa before gate freeze.
Shrinkage anisotropy is a primary process risk in dashboard substrates because thick bosses and narrow lip features solidify at different rates. For talc-filled PP interior grades, flow-direction shrinkage on a 150 mm × 100 mm × 3 mm plaque is commonly 0.8–1.2 %, while transverse shrinkage is 1.0–1.5 % when measured according to ISO 294-4:2018. The exact values for API-2012 must be taken from the supplier’s technical data sheet. Shrinkage measurements from a single plaque are not sufficient for tool compensation; a full mould trial with optical scanning or coordinate measuring machine data is required for grained dashboard parts because surface grain depth and pattern orientation alter local shrinkage.
Weld-line strength in mineral-filled PP is reduced relative to parent material by 30–50 % on average, depending on gate position and melt temperature. Dashboard carrier designs should place knit lines away from airbag deployment paths, snap-fit hooks, and screw bosses. Where a passenger airbag flap is present, the hinge region must be evaluated by instrumented impact testing at cold and elevated temperatures, not solely by ISO 527-2 tensile data.
Commercial polypropylene compound supply chains often control melt volume-flow rate within a batch-to-batch relative deviation of ±15 %. For dashboard moulders, that variation can shift filling pressure and gate seal time enough to alter gloss and warpage on multi-cavity tools. The actual statistical process control window for API-2012 should be obtained from the supplier’s certificate of analysis, and incoming inspection should use ISO 1133-1:2022 at 230 °C/2.16 kg.
Many high-flow automotive PP grades are produced by peroxide-induced chain scission. This route lowers melt viscosity but can create a low-molecular-weight tail that increases VOC emissions unless vacuum devolatilisation and stabiliser selection are controlled. For API-2012, the polymerisation or compounding route is not disclosed in public literature, but the grade should be audited for residual peroxide decomposition products when high MVR and low VDA 277 values are simultaneously required. In production, an inadequately devolatilised grade may show high emission variability between lot numbers even when mechanical properties remain within specification.
Replacing an unfilled impact copolymer with API-2012 or a similar talc-filled dashboard grade changes the mechanical hierarchy. The mineral filler raises flexural modulus and heat deflection temperature, but reduces elongation at break and weld-line strength. The substitution should not be validated by melt flow rate alone; shrinkage anisotropy, odour, and surface gloss are more sensitive to filler geometry and additive package than to MVR.
| Property | Test method | Unfilled impact copolymer class | Mineral-filled dashboard class |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.900–0.910 g/cm³ | 0.96–1.05 g/cm³ |
| Melt volume-flow rate | ISO 1133-1:2022 | 12–30 cm³/10 min | 10–35 cm³/10 min |
| Tensile yield stress | ISO 527-2:2012 | 18–25 MPa | 20–30 MPa |
| Flexural modulus | ISO 178:2019 | 800–1200 MPa | 1500–2600 MPa |
| Notched Izod at 23 °C | ISO 180:2019 | 8.0–20.0 kJ/m² | 8.0–25.0 kJ/m² |
| Heat deflection temperature at 0.45 MPa | ISO 75-2:2013 | 70–90 °C | 90–110 °C |
The comparison above is a screening envelope only. Published data for API-2012 is limited; a grade-certified ISO 19069-2 datasheet should be requested before tool simulation. When the local OEM specification is based on ASTM D638-14 rather than ISO 527-2, measured tensile yield stress may differ by up to 5–10 % because specimen type and strain rate are not equivalent between the two standards.
Impact modification in dashboard PP compounds relies on dispersed elastomer domains, typically ethylene-propylene rubber or metallocene ethylene-octene copolymer. The structural parameters that control low-temperature ductility are the rubber particle size distribution, the rubber-phase glass transition temperature, and the interparticle distance. A notched Izod value at 23 °C of 10–25 kJ/m² may still be associated with poor −30 °C performance if the rubber phase has a high glass transition. For airbag-area validation, instrumented puncture tests on notched plaques are more relevant than Izod because dashboard loading includes bending and high-speed puncture rather than pure shear. If the OEM requires low-temperature impact, ISO 6603-2 or ASTM D3763 multi-axial impact testing at −30 °C should be performed on weld-line specimens. Published data for API-2012 is limited; a generic PP impact copolymer cannot be assumed to pass airbag-deployment cold-impact requirements.
Odour, fogging, and VOC emissions are not stable material constants for automotive interior PP compounds; they depend on stabiliser package, processing temperature, residence time, and post-mould storage. A material that passes VDA 277 after injection moulding at 220 °C can fail at 240 °C if low-molecular-weight additives are degraded into more volatile fragments. For this reason, dashboard suppliers should retain moulding parameter records alongside emission coupons.
Kingfa API-2012 is intended for interior applications; therefore the grade should be assessed against the vehicle manufacturer’s cabin-air specification, not solely against general PP toxicity or food-contact requirements. No food-contact, medical, or flame-retardant classification should be inferred from the automotive dashboard listing unless separately declared by the supplier. The material should not be combined with amine-based additive masterbatches or high-sulphur colour concentrates without compatibility testing, because acid–base interactions with low-emission stabilisers can alter long-term VOC levels.
Interior PP dashboard substrates are screened with multiple emission methods because no single test captures total cabin-air sensory impression. Total organic emissions are often screened by VDA 277, while VDA 278 separates volatile and semi-volatile fractions. Fogging is typically measured gravimetrically by DIN 75201 or ISO 6452. The table below lists common methods and typical automotive acceptance bands; these bands are not API-2012 certification values and must be replaced with the OEM-approved material specification.
| Method | Reported parameter | Typical acceptance band |
|---|---|---|
| VDA 277 | Total VOC | ≤ 50 µgC/g; some cockpit programmes allow ≤ 100 µgC/g |
| VDA 278 | VOC / SVOC | VOC ≤ 100 µg/g; SVOC ≤ 600 µg/g |
| DIN 75201 | Fogging gravimetric | ≤ 2 mg for most rigid PP substrates |
| ISO 6452 | Fogging | No universal limit; pass/fail is set per OEM |
RoHS screening of PP interior compounds typically follows IEC 62321 series for lead, mercury, cadmium, hexavalent chromium, and brominated flame retardants. The supplier should provide a REACH Regulation (EC) No 1907/2006 Article 33 declaration for candidate-list substances above 0.1 % w/w. Since dashboard PP compound is supplied as natural or pre-coloured pellet, antimony trioxide or brominated flame retardants are not usually present; however custom colour, scratch-resistant, or UV-stabiliser masterbatches should be checked against the Global Automotive Declarable Substance List.
Interior dashboard surfaces are tested for scratch and mar resistance because talc-filled PP is more prone to stress whitening than unfilled PP. Scratch testing is commonly conducted according to VW PV3952 or GMW14688, with a 10 N single-stylus load and measurement of ΔL under a defined illumination geometry. Typical acceptance is ΔL ≤ 1.5; however some textured surfaces use ΔL ≤ 2.0. The result is influenced by grain depth, not only by the material’s additive package. Therefore a flat plaque material-ranking test should be followed by a trial moulded grained plaque from the same tool texture.
UV resistance for enclosed cabin parts is usually evaluated by xenon-arc exposure according to ISO 4892-2 with a black-standard temperature of 89 °C and relative humidity 50 %. The common requirement is grey-scale rating ≥ 4 after 300–1000 h, depending on upper surface versus shaded lower panel. For API-2012, the stabiliser package should be verified against the vehicle manufacturer’s weathering specification; automotive interior listing alone does not guarantee UV stability.
In dashboard substrates containing a passenger airbag flap or break-away seam, the moulding process must produce a repeatable hinge thickness and a controlled weld-line morphology. Gate-freeze time should be measured by cavity-pressure decay, not by estimating gate seal from part weight. A typical gate-freeze time for a 2.5 mm wall at a melt temperature of 230 °C and mould temperature of 40 °C can exceed 3 s; if hold time is shorter than gate-freeze time, sink marks and internal voids can form in thick bosses. In airbag-hinge regions, a void fraction above 1–2 % by micro-CT is usually unacceptable because it reduces tear resistance under deployment speed.
Production-scale injection machines for dashboard substrates typically require clamp force from 3,500 kN to 12,000 kN, depending on projected area and hot-runner flow geometry. Hot runner systems should maintain manifold temperature at 230–240 °C; a hot runner temperature above 250 °C can increase emission by-products and gloss variability. If the tool has sequential valve-gate control, the gate-opening delay should be determined by pressure-drop studies at the knit line rather than by volumetric fill alone.
Compared with general-purpose PP homopolymer, API-2012-class dashboard material should show better low-gloss surface stability and lower cabin odour, but elongation at break and weld-line strength may be lower. Compared with talc-filled PP compounds used for under-hood parts, the interior grade should contain a low-emission stabiliser package and should be validated for cabin-air conformity. The product should not be considered a direct substitute for ABS/PC dashboard substrates without re-evaluation of shrinkage, sound transmission, and thermal ageing in the instrument panel upper surface.
Heat ageing of PP dashboard compounds is commonly evaluated at 120 °C for 500 h according to ISO 188:2011, with tensile retention and colour shift recorded. The exact ageing programme for API-2012 depends on OEM cabin temperature profiles; published data for this specific configuration is limited.