Kingfa API-2208,PP+EPDM-TD,Automotive, Exterior

    • Product Name: Kingfa API-2208,PP+EPDM-TD,Automotive, Exterior
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 770974
    Product Name Kingfa API-2208, PP+EPDM-TD, Automotive, Exterior
    Polymer Type Polypropylene (PP) + EPDM + Talc (TD)
    Filler Type Talc (TD)
    Application Automotive Exterior
    Processing Method Injection Molding
    Density 1.04 g/cm³
    Melt Flow Rate 18 g/10 min (230°C/2.16 kg)
    Tensile Strength At Yield 22 MPa
    Tensile Elongation At Break 30%
    Flexural Modulus 1600 MPa
    Notched Izod Impact Strength At 23 C 35 kJ/m²
    Notched Izod Impact Strength At 30 C 8 kJ/m²
    Heat Deflection Temperature 110°C (0.45 MPa, unannealed)
    Molding Shrinkage 0.8-1.2%

    As an accredited Kingfa API-2208,PP+EPDM-TD,Automotive, Exterior factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa API-2208 PP+EPDM-TD automotive exterior compound is packed in 25 kg moisture-proof bags, 40 bags (1,000 kg) per pallet.
    Container Loading (20′ FCL) 20′ FCL container loaded with Kingfa API-2208 PP+EPDM-TD automotive exterior compound in moisture-proof bags, palletized and securely stowed for export.
    Shipping Kingfa API-2208 is shipped as non-hazardous PP+EPDM-TD pellets in moisture-resistant bags or octabins on pallets. Store in a cool, dry, ventilated area away from direct sunlight and moisture. Avoid sharp impacts and temperature extremes; keep packaging sealed until use. Suitable for standard freight; no special hazardous shipping classification.
    Storage Store Kingfa API-2208 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep in original sealed, labeled packaging on pallets; prevent contamination by oils, solvents, or other chemicals. Maintain stable ambient temperature and use first-in, first-out stock rotation. Avoid prolonged UV and humid exposure to preserve material properties.
    Shelf Life Shelf life is typically 12 months when stored dry, below 30°C, away from sunlight, in original sealed packaging.
    Application of Kingfa API-2208,PP+EPDM-TD,Automotive, Exterior

    Front bumper lower air-intake grilles manufactured in API-2208 are processed as a ready-to-use compound without additional polymer blending. The compliance record for this part family is governed by OEM exterior-plastic specifications that reference ISO 4892-2:2013 xenon-arc exposure with a black-panel temperature of 65±3 °C and 1,500 kJ/m² total irradiance when specified on the drawing, with a post-exposure ΔE limit of ≤2.0 CIELAB units per ISO 11664-4; low-temperature impact acceptance is frequently evaluated on 3.0 mm notched Charpy specimens per ISO 179-1:2010 at −30±2 °C after 24 h conditioning. The recommended addition ratio at the moulding plant is 100 phr API-2208, with carbon black masterbatch let-down between 2.0 wt% and 3.5 wt% to achieve full UV opacity and prevent surface chalking of the PP matrix; regrind from sprues, runners, and start-up purgings is restricted to 15 wt% of shot weight and only when the recovered fraction has not been exposed to floor sweepings or mixed-material dust. The downstream process uses injection moulding machines with a screw L/D of 20:1 to 24:1 and a compression ratio between 2.2:1 and 2.8:1, melt temperature held at 225–240 °C, mould wall temperature 35–55 °C, and cavity filling controlled at 80–140 mm/s flow-front velocity beyond the gate to limit talc platelet fracture. Hot runner valve gates with sequential opening delays of 0.2–0.5 s are used on grille ribs to shift the weld line away from the high-strain rear face of the hexagonal mesh; cavity pressure transducers switch from speed control to pack at 30–40 % of full cavity volume, and hold pressure is maintained at 40–60 MPa until gate freeze. Pre-drying is not required for sealed packaging stored below 40 °C, but material exposed for more than 8 h at relative humidity above 60 % should be dried at 80 °C for 2 h with a desiccant dryer delivering a dew point of −20 °C. Terminal finished product types include front bumper lower grilles, lower air-dam inserts, and bumper side vent surrounds with integral snap features.

    What Limits Flow-Length-to-Wall-Thickness Ratios in Cowl Vent Grille Moulding?

    Cowl vent grille geometries carry a large projected area with wall sections between 2.0 mm and 2.8 mm and louver ribs that raise the effective flow-length-to-wall-thickness ratio above 180:1; this makes API-2208 processing sensitive to gate drool, cavity-pressure transfer timing, and gas traps at the final fill corner. The applicable standard for this part family is often the OEM exterior-plastic specification that invokes ISO 4892-2:2013 for xenon weathering with 1,000–1,500 kJ/m² total exposure and ISO 188 for forced-air ageing at 120±2 °C for 1,000 h, with tensile elongation retention of ≥70 % relative to unmoulded compound tested on ISO 527-2:2012 specimens; if the part is a plenum water deflector, the drawing may also apply a seal compression set test per ISO 815-1:2014. The recommended addition ratio is 100 phr API-2208, with in-house regrind limited to 20 wt% of shot mass and screened through a 4.0 mm off-line granulator sieve after separation of dust by cyclone; recycled material should not be used above 25 wt% unless the melt mass-flow rate measured per ISO 1133-1:2022 at 230 °C and 2.16 kg is confirmed within 15 % of the virgin compound value. The production process uses hot runner systems with 4–6 sequential valve-gate drops and cavity pressure sensors placed behind the last fill zone; melt temperature is held at 230–245 °C, mould wall temperature 40–60 °C, and holding pressure 30–50 MPa after switch at 30–40 % of full cavity volume. Fill time for a 2.5 mm nominal wall is controlled to 1.8–2.6 s to avoid vibration marks on the ribbed surface, and cooling time is set to 25–35 s depending on part thickness; ribs are capped at 0.5–0.7 times the adjacent wall thickness to prevent sink marks at the A surface. Terminal finished products include cowl vent grilles, upper plenum water deflectors, and lower windshield trim panels snap-fitted to the bulkhead.

    When High-Gloss Body Side Mouldings Are Moulded Without a Paint Primer

    Unpainted high-gloss side mouldings in API-2208 are moulded with a direct-spun colorant system and no primer or adhesion promoter. Compliance is referenced to ISO 4892-2:2013 weathering at 1,500 kJ/m² and gloss retention per ISO 2813:2014; the drawing may also require cross-cut adhesion per ISO 2409:2013 when a local hot-stamp foil is applied to the upper surface. The addition ratio is 100 phr API-2208 with 1.0–2.5 wt% of a high-dispersion black masterbatch and ≤10 wt% clean regrind. Processing demands an SPI A1 mirror-finish tool at 50–70 °C wall temperature, melt at 235–245 °C, and flow-front velocity 100–200 mm/s to avoid gloss variation. Terminal finished parts include body side mouldings, door lower appliqués, and rocker protection strips with adhesive tape slots.

    ScenarioReferenced standardMeasured characteristicTypical verification condition
    Front bumper lower grilleISO 4892-2:2013, ISO 179-1:2010Accelerated weathering; low-temperature notched Charpy1,500 kJ/m² at 65±3 °C; −30±2 °C on 3.0 mm specimen
    Cowl vent grilleISO 4892-2:2013, ISO 188Weathering; forced-air heat ageing1,000–1,500 kJ/m²; 120±2 °C, 1,000 h
    High-gloss side mouldingISO 4892-2:2013, ISO 2813:2014Weathering; gloss retention1,500 kJ/m²; 60° geometry
    Rear bumper step padSAE J2527, ISO 6603-2:2000Accelerated exterior weathering; puncture impact4.4 m/s at −30±2 °C
    Wheel arch linerISO 4892-2:2013, ISO 179-1:2010Weathering; low-temperature impact−30±2 °C after 168 h salt immersion
    Rocker panel claddingISO 11359-2:2021, ISO 4892-2:2013Linear thermal expansion; weathering−40 °C to +80 °C

    For rear bumper step pads and rear bumper top covers, API-2208 is selected because the talc-filled PP/EPDM matrix resists both low-temperature crack initiation and the high-point indentation loads imposed by footwear on sun-heated surfaces. The compliance path for this part family references SAE J2527 for accelerated Florida-equivalent exterior weathering and ISO 6603-2:2000 puncture-impact testing at −30±2 °C on 65 mm × 65 mm plaques cut from moulded pads, with no brittle failure allowed at 4.4 m/s impact velocity when required by the OEM engineering standard. The recommended addition ratio in this segment is 100 phr API-2208 with a let-down of 2.0–3.0 wt% black masterbatch and a maximum of 20 wt% same-material regrind; external slip agents are deliberately excluded because they migrate to the surface and reduce the coefficient of friction on a step pad where slip resistance is governed by the tool-knurled grain geometry. The downstream process uses injection moulding machines with a clamp force selected at 4.0–4.5 kN/cm² of projected area, a melt temperature of 220–235 °C, and a mould wall temperature of 35–50 °C; the part thickness is maintained at 3.5–4.5 mm over the standing surface, with rib-to-wall junctions thickened only on the hidden face to avoid sink. Holding pressure is profiled from 50 MPa to 30 MPa over 10–18 s, and the gate is placed in a non-visible edge region to keep flow marks outside the tactile grain area. Terminal finished products include rear bumper step pads, rear bumper top covers, and pickup-style rear sill protectors with snap-in attachments.

    Wheel Arch Liner Impact Resistance After Thermal Ageing at 90 °C and Road Salt Immersion

    Wheel arch liners produced from API-2208 are subjected to repeated stone impingement at low ambient temperature and to saturated road salt with anti-icing brine, conditions that generate pitting and stress whitening in unreinforced PP copolymers. The standard test sequence combines ISO 4892-2:2013 exposure, ISO 179-1:2010 notched Charpy impact at −30±2 °C after specimen conditioning, and immersion in 23±2 °C 5 wt% sodium chloride solution for 168 h with subsequent visual inspection for surface blistering or talc wash-out. The formulation addition ratio for this application is 100 phr API-2208 with 2.0–3.0 wt% carbon black masterbatch and up to 25 wt% clean in-house regrind passed through a 5.0 mm sieve after magnetic separation; no additional impact modifier is added at the injection moulding stage because the EPDM phase is already dispersed in the compound. The production process is performed on large injection machines in the 1,200–2,000 metric ton clamp range for wheel liners with a projected area above 0.7 m²; melt temperature is held at 225–240 °C, mould wall temperature 45–65 °C, and injection speed programmed with a slower first stage of 60–80 mm/s followed by a second stage of 120–160 mm/s to evacuate air from the deep fender lip geometry. Sequential valve gates with 0.3–0.6 s opening delays are used to prevent knit lines at the upper attachment bosses, and hold pressure is set at 45–60 MPa until gate freeze. Terminal finished products include front and rear wheel arch liners, mudguards, and rear bumper side splash shields.

    Talc Aspect Ratio Governs Post-Mould Linear Expansion in Rocker Panel Cladding

    Rocker panel cladding and lower sill extensions moulded in API-2208 require tight gap and flushness values along the body side, so post-mould linear expansion becomes the primary dimensional risk when the paint shop or field heat load exceeds the part conditioning temperature. The compliance standard for this dimensional requirement is ISO 11359-2:2021 thermomechanical analysis, with the part drawing specifying a coefficient of linear thermal expansion measured between −40 °C and +80 °C on machine-direction specimens cut from the outer surface; in addition, exterior weathering follows ISO 4892-2:2013 and stone-chip resistance is assessed according to the OEM method attached to the component specification. Published multi-month fleet durability data for this exact part and material combination is limited; validation is therefore carried out on a multicavity production tool with short-shot mapping and a minimum 200-cycle in-mould pressure study before series release. The recommended addition ratio is 100 phr API-2208 with 2.0–3.0 wt% black masterbatch and regrind capped at 15 wt%; the regrind fraction is stabilised because talc platelet orientation and EPDM phase viscosity are extremely sensitive to repeated thermal history, and adding more than 15 wt% without shear-history control produces visible tiger stripes on long flat surfaces. The downstream process uses a sequential coining or low-pressure injection-compression sequence with melt temperature at 230–245 °C, mould wall temperature 40–60 °C, and a clamping force profile that allows the mould to breathe by 0.3–0.5 mm during the filling stage before final compression at 80–110 MPa cavity pressure. Gate placement is moved to the hidden lower edge, and the rocker panel is run with a 0.4–0.6 mm vent land along the upper show surface to remove trapped volatiles without leaving witness lines. Terminal finished products include rocker panel cladding, lower sill extensions, and door lower skin mouldings with integrated stone-protection ribs.

    Free Quote

    Competitive Kingfa API-2208,PP+EPDM-TD,Automotive, Exterior prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa API-2208 is a melt-compounded polypropylene/ethylene-propylene-diene-monomer/talc PP+EPDM-TD thermoplastic polyolefin compound formulated for exterior automotive components manufactured by injection moulding. The designation indicates a continuous polypropylene matrix toughened with an EPDM elastomer dispersion and stiffened with a talc mineral filler. The grade is positioned for large thin-wall trims that require low-speed ductile fracture resistance at winter ambient temperatures and dimensional repeatability in assembly-level gap and flush conditions. Typical application areas include lower bumper inserts, rocker panels, wheel arch liners, sill cladding, and unpainted exterior trim. Published typical-property data for the grade must be read in conjunction with the batch certificate, because talc concentration, elastomer viscosity, and stabiliser package are adjusted at compounding scale. The material is not classified as a structural engineering resin; its continuous load-bearing ceiling is lower than that of polyamide or PC/ABS, but its lower density and injection pressure window allow reduced part mass on conventional polypropylene screw geometry.

    How Does the Talc/EPDM Balance Affect Low-Speed Impact and Shrinkage?

    In API-2208, the dispersed EPDM phase serves as a stress concentrator that promotes shear yielding and delays brittle crack propagation, while talc platelets reduce mould shrinkage and increase flexural modulus. The resulting property compromise is measurable through notched Izod impact and mould shrinkage. At 23 °C, the notched Izod value of 35 kJ/m² under ISO 180/A:2023 reflects ductile response, while at −30 °C the same method gives approximately 5 kJ/m², indicating that the compound retains some post-yield deformation but is no longer fully ductile. Flexural modulus of 1800 MPa under ISO 178:2019 is achieved because talc platelets orient during injection and constrain chain mobility. Mould shrinkage under ISO 294-4:2018 is controlled in the range 0.8–1.0 %, with cross-flow shrinkage typically at the upper end of the range. The talc acts as a nucleating agent, reducing spherulite size and increasing crystallisation rate, which shortens cycle time but also contributes to anisotropic shrinkage in flow and transverse directions.

    PropertyTypical ValueTest Method
    Density1.04 g/cm³ISO 1183-1:2019
    Melt volume-flow rate, 230 °C/2.16 kg20 cm³/10 minISO 1133-1:2022
    Tensile yield stress19 MPaISO 527-2:2012, specimen type 1A, 50 mm/min
    Elongation at yield6–8 %ISO 527-2:2012
    Flexural modulus1800 MPaISO 178:2019, 2 mm/min
    Notched Izod impact, 23 °C35 kJ/m²ISO 180/A:2023
    Notched Izod impact, −30 °C5 kJ/m²ISO 180/A:2023
    Heat deflection temperature, 0.45 MPa95 °CISO 75-2/B:2013
    Vicat softening temperature, B5065 °CISO 306:2022
    Linear thermal expansion coefficient9 × 10⁻⁵ K⁻¹ISO 11359-2:2021
    Mould shrinkage0.8–1.0 %ISO 294-4:2018

    Predrying is not a universal prerequisite for API-2208, but packaging ruptures or warehouse relative humidity above 60 % can introduce surface moisture that generates splay on cosmetic surfaces. A dehumidified-air hopper at 80 °C for 2–4 h is sufficient; the melt is not hydrolytically sensitive. Melt temperature measured at the nozzle should remain between 200 °C and 240 °C, with the upper limit reserved for thin-wall sections below 2.0 mm. Mould temperatures between 30 °C and 60 °C control gloss and surface skin formation. Higher mould temperatures raise gloss uniformity but extend cycle time and increase after-shrinkage. Back pressure of 0.5–1.5 MPa and screw speed of 40–80 min⁻¹ are typical for standard three-zone screws with an L/D of 18:1–22:1. Gate freezes earlier than unfilled PP because talc increases thermal conductivity, so hold-pressure time must be verified by gate-seal studies.

    Production-scale observation on multicavity tools has shown that weld-line strength in talc-filled TPO is governed more by melt-front temperature than by packing pressure. When API-2208 is injected through a single hot-runner drop into four cavities with unequal flow lengths, the shortest cavity can experience packing-induced flash at the parting line before the longest cavity seals. Sequential valve gating or flow restrictors are therefore required for balanced pressure profiles. The nucleating effect of talc produces a fine spherulitic skin and lowers post-mould warpage, but orientation of talc platelets along the flow direction creates longitudinal-transverse shrinkage anisotropy. Mould designers should use shrinkage of 0.8 % in flow and 1.0 % cross-flow for preliminary steel sizing and confirm with a first-off tool study.

    Melt viscosity, shear thinning, and gate design for exterior trim

    The melt volume-flow rate of 20 cm³/10 min under 230 °C/2.16 kg according to ISO 1133-1:2022 places API-2208 in the medium-flow range for talc-filled exterior TPO compounds. Spiral flow length depends on wall thickness, melt temperature, and mould texture, but the material is formulated to fill textured exterior skins at wall sections from 2.0 to 3.0 mm. Direct edge gates should be sized from 1.0 to 1.5 mm in thickness, while fan and tab gates are preferred for low-gloss surfaces because they reduce jetting. Venting at the parting line should be maintained at 0.02–0.04 mm because talc-filled compounds are less likely to flash at narrow vent depths but are prone to burn marks if air is trapped. Hot-runner systems should use externally heated manifolds with thermal homogeneity within ±5 °C across drops, because cold spots increase EPDM phase viscosity and produce visible flow streaks.

    Incoming-lot testing for exterior programmes should include melt volume-flow rate by ISO 1133-1:2022, ash content by ISO 3451-1:2019, notched Charpy or Izod at 23 °C and −30 °C, and flexural modulus by ISO 178:2019. Ash content is a direct check for talc loading; a drift of 2 percentage points can change CLTE and shrinkage enough to cause gap and flush deviations on a bumper assembly. Melt-flow drift above 3 cm³/10 min indicates a change in PP base resin, recycled content, or visbreaking degree and must trigger a process capability study.

    Because exterior trims are exposed to UV radiation, hydrocarbon road films, and cyclic moisture, API-2208 is supplied with a stabiliser package that can be evaluated by ISO 4892-2:2013 xenon-arc exposure or SAE J2527:2023 for automotive exterior materials. Delta E for pigmented black or grey formulations is typically kept below 2.0 after 1500 h xenon exposure when the part is not painted, but published data for this specific configuration is limited. Validation on textured plaques is necessary because talc platelets at the surface can contribute to whitening under abrasion. Scratch and mar response follows the load increments of VW PV3952 or GMW14688, where a talc-filled TPO without a clearcoat will exhibit stress whitening at lower normal force than a painted or hard-coated counterpart. Grained surfaces and darker pigments reduce visible damage. Reclaimed material co-fed above 20 % may shift gloss and odour, and process aids that migrate can impair downstream adhesion.

    When PC/ABS or ASA Is Replaced in Unpainted Lower Exteriors

    API-2208 loses to PC/ABS and ASA in continuous heat resistance and grain retention, but replaces them where total part cost, low-temperature ductility, and low density control the programme. Its flexural modulus of 1800 MPa is lower than that of many PC/ABS grades, so ribbing and wall section may require modification. Its CLTE of 9 × 10⁻⁵ K⁻¹ is higher than PC/ABS and requires larger mounting clearances. The melt temperature is 60–80 °C lower, reducing energy and allowing sequential valve gating on smaller presses. Unlike amorphous PC/ABS, PP+EPDM-TD cannot be solvent-bonded. Joining is by vibration welding, hot-plate welding, mechanical fixation, or adhesive with polyolefin primer. Paint adhesion requires power wash and flame or plasma treatment before primer, and the substrate must not exceed 120 °C bake temperature because modulus collapses near the heat deflection temperature.

    AttributeAPI-2208 PP+EPDM-TDPP+EPDM unfilledPP-TD20 mineral-filledPC/ABS or ASA
    Density1.04 g/cm³0.90 g/cm³1.05 g/cm³1.13 g/cm³
    Flexural modulus1800 MPa700–900 MPa2200–2600 MPa2200–2500 MPa
    Notched Izod, −30 °C5 kJ/m²8–12 kJ/m²2–3 kJ/m²10–15 kJ/m²
    CLTE9 × 10⁻⁵ K⁻¹12–15 × 10⁻⁵ K⁻¹7–8 × 10⁻⁵ K⁻¹6–8 × 10⁻⁵ K⁻¹
    Mould shrinkage0.8–1.0 %1.4–1.8 %0.7–0.9 %0.5–0.7 %
    Paint adhesion for exteriorRequires flame or plasma plus primerRequires primerRequires primerDirect or primer depending on grade

    For rocker panels and bumper lower inserts, impact loading is multiaxial and strain-rate dependent. Instrumented puncture testing on injection-moulded plaques following ISO 6603-2:2022 is more informative than notched Izod data alone. At −30 °C, the ductile-to-brittle transition of PP+EPDM-TD is influenced by the EPDM volume fraction, the talc particle size distribution, and the interparticle distance. A reduction in talc median particle diameter below 1 μm improves impact but raises viscosity and compound cost. No single test captures the service loading of a stone-struck wheel arch liner. Suppliers typically combine component-level gravelometer tests with plaque-level multiaxial impact.

    Painting adhesion to PP+EPDM-TD exterior parts requires surface oxidation and removal of low-molecular-weight process aids. A three-stage power wash at 60–70 °C followed by air-knife drying is common before flame or plasma treatment. Adhesion testing after a water-jet crosshatch according to ISO 2409:2020 or ASTM D3359-23 may be supplemented by stone-chip resistance. Direct bonding to polyurethane adhesives without primer is not assured. A polyolefin primer based on chlorinated polypropylene is required in most glazing or trim-bonding operations.

    Continuous use above 90 °C under mechanical load is not recommended. The grade is not a replacement for polyamide in under-hood or structural applications. Contact with concentrated acids, strong oxidising agents, and certain solvent-based masking fluids can swell or crack the EPDM phase. Parts should be validated for emission requirements using VDA 277 or PV 3341 when cabin boundary transitions are involved, because talc-filled polypropylene compounds can retain process oils and stabiliser residuals. Recycling is compatible with unpainted polypropylene streams, but painted or metalized components must be separated. Compression set and creep are not primary selection criteria; unsupported horizontal panels should be re-ribbed or formed with curvature to avoid long-term sag.