| HS Code | 566377 |
| Grade | API-3015 |
| Materialtype | PP+EPDM-TD30 |
| Fillercontent | 30% talc |
| Elastomertype | EPDM |
| Uvstabilization | Yes |
| Rigidtoughbalance | Yes |
| Automotiveexteriorsuitability | Yes |
| Density | 1.05-1.10 g/cm3 |
| Meltflowrate 230c 2 16kg | 12-20 g/10 min |
| Tensilestrength | 20-25 MPa |
| Elongationatbreak | 30-80% |
| Flexuralmodulus | 1900-2500 MPa |
| Notchedizodimpactstrength 23c | 25-45 kJ/m2 |
| Notchedizodimpactstrength Minus30c | 6-10 kJ/m2 |
| Heatdeflectiontemperature 0 45mpa | 105-120°C |
| Vicatsofteningtemperature | 135-150°C |
| Moldingshrinkage | 0.9-1.5% |
As an accredited Kingfa API-3015,PP+EPDM-TD30 (Rigid-Tough Balance, UV),Automotive, Exterior factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg moisture-barrier bags, palletized at 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | 20′ FCL container loading of Kingfa API-3015 PP+EPDM-TD30, UV-stabilized, rigid-tough balanced automotive exterior compound in export packaging. |
| Shipping | Kingfa API-3015 is supplied as dry, non-hazardous thermoplastic pellets in sealed moisture-barrier bags or FIBCs, palletized and labeled. Ship in clean, dry, ventilated conditions, protected from moisture, heat, sunlight, and ignition sources. Avoid punctures or bag rupture; store away from incompatible chemicals. |
| Storage | Store Kingfa API-3015 PP+EPDM-TD30 in original sealed packaging in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat sources, flames, moisture, and strong oxidizers. Keep pallets off the floor and avoid excessive stacking to prevent deformation. Maintain stable temperature and humidity, follow first-in, first-out rotation, and inspect containers for damage before use. |
| Shelf Life | Shelf life: typically 24 months in original unopened packaging, stored cool, dry, and protected from direct sunlight. |
Front lower fascia close-out panels and bumper lower grilles manufactured from Kingfa API-3015 are specified for exterior positions where the part must retain stiffness after exposure to road de-icing salts, stone impact, and repeated thermal shock without exhibiting brittle failure below -30 °C. The downstream formulation addition ratio for this application is 100 parts API-3015 as the ready-to-mold compound, with clean same-grade regrind limited to 10–15 wt% on visible textured surfaces and 20 wt% in hidden rib or boss areas. If non-black coloring is required, a UV-stabilized PP/EPDM-carrier color concentrate is metered at 1–2 wt%. Industry compliance is anchored to the EU ELV directive 2000/53/EC heavy-metal limits, EU REACH SVHC screening, and, where OEM fire safety review applies, ISO 3795 burning-rate classification. The production process is injection molding on a reciprocating-screw machine with an L/D ratio of 20:1 to 24:1, a shut-off nozzle, barrel zone settings of 180–220 °C rear-to-nozzle, and a melt temperature of 200–230 °C. Mold temperature is held at 20–50 °C, and a profiled injection velocity fills 85–95% of the cavity before the pack-and-hold transition. The main processing conflict in this part family is weld-line formation at apertures for tow hooks, parking sensors, and license plate cutouts, where talc platelets orient along the advancing flow front and reduce weld-line strength. Sequential valve-gate control is used to move weld lines to low-stress regions. When the melt exceeds 230 °C, EPDM phase degradation can produce silver streaks and acrid volatiles. Drying is not required for sealed hopper storage below 60% relative humidity; open-bin or condensation-exposed material is desiccant-dried at 80 °C for 4–6 h. Terminal finished product types include lower bumper spoilers, skid plate garnishes, and license plate close-out panels.
Wheel arch extensions and fender flares produced from API-3015 rely on the biphasic PP/EPDM matrix and 30 wt% talc filler to provide dimensional stability for clip-tower retention while maintaining multiaxial impact energy absorption at sub-zero temperatures. The applicable addition ratio is 100 parts API-3015; clean same-grade regrind is allowed at 10–15 wt% for visible parts and up to 20 wt% for concealed mounting ribs, with regrind particle size screened to ≤5 mm and moisture content to ≤0.05 wt%. Industry compliance is verified under ISO 6603-2 for instrumented puncture impact at -20 °C, SAE J2527 for xenon arc weathering of exterior plastic components, and ISO 179-1/1eU for unnotched Charpy impact. In the downstream injection molding process, the part is normally produced with a hot runner mold using one to four valve gates, melt temperature 200–220 °C, mold temperature 25–45 °C, and clamp force of 2.5–4.5 kN/cm² projected area. The critical production-scale failure mode is clip-tower cracking after cold-impact loading or after improper regrind addition; because the 30 wt% talc content increases local stiffness, regrind that introduces degraded EPDM phase or moisture reduces the crack-initiation resistance of the clip towers. Cavity pressure sensors are set to switch to packing at 80–90% of peak cavity pressure, and the pack time is extended until the gate freezes to control sink marks around clip towers. Terminal finished products include wheel arch extensions, fender flares, and gravel-guard liners.
Side sill covers, rocker panel moldings, and lower door claddings molded from API-3015 are placed along the vehicle’s lower body line, where the part is exposed to direct stone impact, galvanic corrosion from metal fasteners, and thermal expansion mismatch along body panels exceeding 1.2 m. The downstream addition ratio is 100 parts API-3015; return material from the same part line is allowed at 15–20 wt% for non-visible ribs and bosses, while visible rocker surfaces are restricted to 10 wt% regrind. Compliance in this section is anchored to ISO 179-1/1eU for unnotched Charpy impact at -20 °C, ISO 4892-2 for artificial weathering with a daylight filter, and the EU ELV directive 2000/53/EC restrictions on lead, cadmium, mercury, and hexavalent chromium. The downstream production process is injection molding on large-platen machines with clamp force calculated at 3.0–5.0 kN/cm², a melt cushion of 3–6 mm, and a screw L/D ratio of 22:1 to 25:1. The dominant process conflict is warpage caused by anisotropic talc orientation along the flow axis after ejection. To limit bowing, the mold uses sequential valve gating and a cavity pressure switch-over at 80–90% of peak pressure, followed by cooling in fixed contour jigs for 40–60 s before free-air storage. Material incompatibility must be controlled: polyamide- or PBT-contaminated regrind creates separate phases that reduce weld-line strength and visible surface consistency. Published data for this specific warpage-control configuration is limited; part-level dimensional audits are required against the OEM checking fixture. Terminal finished products include rocker panel covers, side sill extensions, and lower door cladding inserts.
Tailgate garnish panels and liftgate lower trims fabricated from API-3015 are specified when the exterior surface is either molded in a low-gloss black finish or painted as a Class A component, because the 30 wt% talc filler can otherwise generate visible bloom on sharp edges after humidity cycling. The application-level addition ratio is 100 parts API-3015 for the visible Class A surface; regrind is excluded from visible surfaces and restricted to 15 wt% in hidden reinforcement ribs or screw bosses. Industry compliance is verified through ISO 2409 cross-cut adhesion after paint, ISO 6270-2 condensation exposure for 240 h without blistering, SAE J2527 exterior weathering, and EU REACH SVHC screening. In the downstream production process, the part is first injection molded at melt temperature 200–220 °C and mold temperature 25–40 °C, then subjected to a surface preparation step before painting because talc-filled PP/EPDM surfaces have low inherent polarity. Flame treatment or atmospheric plasma is used to raise surface energy to 38–42 mN/m; a chlorinated polyolefin adhesion promoter is then applied before a basecoat and clearcoat system. The main production conflict is talc bloom on sharp radii and edge areas, which is controlled by reducing regrind uptake on visible material, avoiding direct gate vestige on visible edges, and maintaining mold temperature uniformity. External mold release agents containing silicone or zinc stearate are excluded because they interfere with paint adhesion. Published data for this specific API-3015 paint system configuration is limited; OEM paint adhesion tests should be run on the actual part geometry. Terminal finished products include tailgate center garnish, liftgate lower trim, and tailgate latch cover panels.
Cowl vent grilles and plenum chamber covers produced from API-3015 must maintain dimensional stability while water drains continuously along the lower windshield edge, and the part must resist UV degradation because it is one of the highest solar exposure positions on the exterior. The addition ratio is 100 parts API-3015; clean same-grade regrind is allowed at 15–20 wt% because the visible surface is not a painted Class A finish, but it must be free of windshield washer fluid residues and silicone lubricants. Industry compliance is anchored to ISO 4892-2 for xenon arc weathering, ISO 1133-1 for melt flow-rate verification, and ISO 180/A notched Izod impact at 23 °C and -20 °C. The production process is injection molding with thin-wall sections typically 2.2–2.8 mm thick; because the 30 wt% talc content reduces melt flow length, the mold is filled through multiple edge gates or a valve-gated manifold rather than a single central sprue. Melt temperature is held at 200–230 °C, mold temperature at 20–50 °C, and injection speed is profiled to avoid surface hesitation marks. A process conflict arises from long, thin drain slots and small louvers, where gas venting must be placed at the end-of-fill locations to prevent burn marks and short shots. Terminal finished products include cowl top covers, plenum chamber grilles, and windshield water deflector panels.
Exterior mirror housings and A-pillar exterior appliqués molded from API-3015 require high dimensional accuracy at small part mass, typically below 300 g, along with a balance of low-temperature impact resistance and UV stability. The downstream addition ratio is 100 parts API-3015; cold-runner sprues and runners are reground and returned at 10 wt% for visible housing surfaces and up to 20 wt% for internal stiffening ribs, provided the regrind is free of paint overspray and glass-filled residues. Compliance is anchored to ISO 180/A notched Izod impact, SAE J2527 exterior weathering, ISO 3795 burning-rate classification where required, and EU ELV 2000/53/EC heavy-metal limits. The downstream process is injection molding in a cold-runner, two-cavity or four-cavity tool with a heated sprue bushing rather than a hot manifold, because the small shot size would increase residence time in a hot-runner system and expose the EPDM phase to thermal degradation. Melt temperature is controlled at 190–220 °C, mold temperature at 25–40 °C, and back pressure at 4–8 bar. The critical production conflict is premature gate freeze caused by the high thermal diffusivity of talc-filled PP/EPDM; gate diameter is therefore maintained at ≥1.2 mm, and the machine is equipped with a screw tip check ring to prevent melt cushion fluctuation. Cavity surface texturing is used to reduce visible sink marks over screw bosses and rib intersections. Terminal finished products include exterior mirror housing shells, mirror base brackets, and A-pillar exterior appliqués.
Competitive Kingfa API-3015,PP+EPDM-TD30 (Rigid-Tough Balance, UV),Automotive, Exterior prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa API-3015, designated PP+EPDM-TD30 (Rigid-Tough Balance, UV), Automotive, Exterior, is a talc-filled polypropylene impact copolymer modified with an ethylene-propylene-diene monomer elastomer and a UV stabilization package for automotive exterior components. The material is formulated around a 30 wt% talc loading in a continuous PP matrix, with EPDM dispersed as a discrete impact-modifying phase. Injection molding process guidance supplied with the grade indicates barrel temperatures of 200–230 °C, mold surface temperatures of 30–60 °C, and hydraulic back pressure of 0.5–1.5 MPa. Under ISO 1183 a representative density for this class of 30 wt% talc-filled impact-modified PP is 1.11–1.13 g/cm³; the melt flow rate determined under ISO 1133-1:2022 at 230 °C with a 2.16 kg load typically falls within 8–18 g/10 min, depending on pigment package and lot. Published data for this specific configuration is limited to supplier technical data sheets and application-specific Kingfa documentation; independent peer-reviewed values for exact batch-to-batch variation are not widely available.
Typical exterior components for which the material is evaluated include lower bumper stiffeners, wheel arch liners, rocker panel covers, cowl grilles, and exterior trim brackets. The rigid-tough balance is achieved by combining talc-induced stiffness with EPDM-induced low-temperature ductility, allowing thin-wall sections of 2.0–3.5 mm to meet both flexural modulus requirements under ISO 178 and multiaxial impact requirements under ASTM D3763 or ISO 6603-2. Unlike conventional PP-TD30 compounds without elastomer modification, the EPDM phase lowers the ductile-to-brittle transition temperature and reduces notch sensitivity at gate and weld-line regions.
The presence of 30 wt% talc raises flexural modulus and lowers mold shrinkage, but unmodified PP-TD30 suffers from low crack-initiation energy because talc platelets act as stress concentrators. In API-3015, the dispersed EPDM phase improves impact toughness without entirely sacrificing stiffness. The comparative values in Table 1 are representative ranges derived from industrial compounder technical literature for equivalent talc-filled polypropylene classes; they are not guaranteed lot-specific values for Kingfa API-3015.
| Property | Test method | PP homopolymer | Unmodified PP-TD30 | PP+EPDM-TD30 class |
|---|---|---|---|---|
| Density | ISO 1183 | 0.90 g/cm³ | 1.12 g/cm³ | 1.11–1.13 g/cm³ |
| Melt flow rate, 230 °C/2.16 kg | ISO 1133-1 | 8–15 g/10 min | 8–15 g/10 min | 8–18 g/10 min |
| Tensile strength at yield | ISO 527-2 | 32 MPa | 28 MPa | 22–25 MPa |
| Flexural modulus | ISO 178 | 1450 MPa | 2800 MPa | 2200–2600 MPa |
| Charpy notched impact, 23 °C | ISO 179-1/1eA | 5 kJ/m² | 6 kJ/m² | 20–35 kJ/m² |
| Charpy notched impact, -30 °C | ISO 179-1/1eA | 2 kJ/m² | 3 kJ/m² | 8–12 kJ/m² |
| Heat deflection temperature, 0.45 MPa | ISO 75-2/B | 90 °C | 125 °C | 110–120 °C |
| Linear mold shrinkage, flow direction | ISO 294-4 | 1.4–1.8% | 0.8–1.2% | 0.8–1.2% |
Mechanistically, unmodified PP-TD30 derives stiffness from talc but fails at low energy because talc particles concentrate stress. In the EPDM-modified grade, dispersed elastomer domains of 0.5–2.5 µm diameter cavitate under impact, leading to shear yielding in the matrix and higher energy absorption. This shift is most visible at subambient temperatures, where unmodified PP-TD30 exhibits brittle fracture and the EPDM-modified system retains ductile tearing. Compared to a long-glass-fibre PP exterior structural bracket compound, API-3015 sacrifices short-term modulus but provides lower anisotropy, better surface quality, and higher low-temperature notched impact. Glass fibre reinforced PP of 30 wt% fibre content can show flexural modulus above 4500 MPa, but notched impact at -30 °C is often below 10 kJ/m² and exposed fibre can produce poor Class A surfaces. Compared to a reactor TPO with similar EPDM content but no talc, API-3015 provides higher flexural modulus and lower mold shrinkage, at the expense of room-temperature impact and melt flow.
In production-scale twin-screw compounding, downstream feeding of talc is preferred to limit platelet attrition and to reduce peak torque in the primary feed zone. For API-3015, pre-drying at 80 °C for 2–4 h in a desiccant dryer with a dew point below -30 °C is required when storage humidity has exceeded 60% RH or when visible surface condensation is present. Residual moisture above 0.08–0.10 wt% can generate silver streaking, splay, and gloss loss on large exterior panels. The melt should not be held above 240 °C for more than 10 min; extended residence degrades EPDM by chain scission or crosslinking, causing viscosity drift and surface delamination. A screw L/D ratio of 20:1–24:1 with compression ratio 2.5:1–3.0:1 and a mid-shear mixing section is typical for talc-filled TPO pellet processing. Hot-runner systems for thin-wall tooling should use open-pipe runners with gate diameters of at least 1.2 mm, and valve-gated nozzles should maintain tip temperature within 10 °C of the setpoint to avoid premature freeze-off at the gate. Under ISO 294-4, linear post-mold shrinkage on a 60 mm × 60 mm × 2 mm plaque is typically 0.8–1.2% in the flow direction and 0.9–1.3% transverse to flow, with greater anisotropy in highly oriented edge-gated parts.
Flow simulation for this material class is sensitive to filler orientation and EPDM domain deformation. Moldflow analyses for injection-tool validation usually require a Cross-WLF viscosity model fit to capillary rheometry data obtained under ISO 11443 at shear rates from 10 s⁻¹ to 10,000 s⁻¹. At 230 °C, shear viscosity of a 30 wt% talc-filled PP/EPDM typically ranges from 150 Pa·s at 1000 s⁻¹ to 35 Pa·s at 10,000 s⁻¹; the shear-thinning index between these rates is around 0.4–0.5. Pressure-volume-temperature behavior measured under ISO 17744 is required for accurate packing and shrink prediction because talc reduces compressibility relative to unfilled PP by approximately 20–30%. Weld lines in talc-filled EPDM-modified PP typically retain 40–60% of the base material tensile strength; placement of gates in walk-weld areas should be optimized using short-shot studies on production tooling.
On production-scale injection molding lines with clamp forces of 800–1600 t, common defects for talc-filled EPDM exterior trims include tiger stripes in high-flow areas, gate blush, and delamination at EPDM-rich weld lines. Reducing injection speed to 20–40 mm/s and raising mold temperature to 50–60 °C reduces tiger stripe severity; however, mold temperatures above 60 °C prolong cycle time and may increase gloss variance on grained surfaces. Short-shot trials on comparable tools have indicated that flow-front temperature drops of more than 15 °C before weld lines produce visible delamination. Setting the screw decompression to 2–3 mm prevents drool without causing air entrapment at the check ring. Mold design for talc-filled PP/EPDM requires venting of 0.02–0.03 mm depth along the parting line and at flow-front intersections to prevent gas burn and short shots. Ejector pins and ribs should use draft angles of 1.0–1.5° for textured surfaces because talc increases scratch sensitivity but does not increase release friction as much as glass fibre.
Exterior automotive parts are validated under accelerated weathering because the primary failure mode is surface chalking, gloss loss, and impact retention reduction after photo-oxidation. Unstabilized PP-based TPOs can lose more than 50% of initial elongation at break within 1000 h of xenon-arc exposure; the HALS/UV absorber combination in API-3015 is intended to suppress this degradation pathway. The test methods most often cited in OEM specifications are ISO 4892-2 cycle 1 with xenon-arc daylight filters at 0.51 W/m² @ 340 nm, black standard temperature 65 °C, and water spray, and SAE J2527 with borosilicate inner and outer filters at 0.55 W/m² @ 340 nm, black panel temperature 70 °C. Acceptance thresholds commonly require ΔE* ≤ 3.0 and grayscale rating ≥ 4 after 1500–2500 h, with retained Charpy notched impact of at least 50% of the unweathered value. Because talc-filled surfaces are inherently matte, UV-induced microcracking may appear earlier on white or light gray TiO₂-pigmented parts than on carbon black grades. The stabilizer package should not be combined with amine-based antiozonants or copper-based pigments that can antagonize HALS performance in long-humid UV cycles. The exact accelerated weathering performance must be confirmed against the specific OEM color approval because pigments and UV package interactions vary.
Post-molding decoration for API-3015 exterior parts requires surface treatment because the talc-filled PP/EPDM surface is nonpolar. Without treatment, cross-hatch adhesion under ISO 2409 on injection-molded PP/EPDM is typically class 4–5; after flame treatment to a surface energy of 38–45 mN/m or application of a chlorinated polypropylene adhesion promoter, class 0–1 is achievable for two-component polyurethane or acrylic coatings on equivalent TPO substrates. For adhesive bonding to metal or thermoset frameworks, polyurethane or acrylic structural adhesives are preferred over cyanoacrylate or anaerobic chemistries because EPDM-rich surfaces exhibit exudation and low polar functionality. If noise-reducing felt or scrim is applied, adhesion should be qualified after heat aging at 90 °C for 168 h and after 10 cycles of thermal shock from -40 °C to 80 °C under OEM test specifications.
Chemical exposure on exterior parts includes windshield washer fluid, road salt, diesel splash, and car wash detergents. The polypropylene/talc/EPDM system has good resistance to aqueous acid and alkali solutions but limited resistance to aromatic and halogenated solvents. Under ISO 175, a 7-day immersion in 10 wt% sodium chloride solution at 23 °C produces negligible mass change, while xylene or toluene causes swelling of the EPDM phase and surface tack. Contact with biodiesel and long-term fuel splash should be avoided unless validated under OEM exterior exposure protocols; EPDM-rich phases can extract plasticizer from adjacent sealing materials. Continuous contact with strong oxidizing acids, aromatic hydrocarbon solvents, or hot oil above 100 °C is not recommended.
Continuous heat exposure affects exterior dark-colored parts even though peak air temperatures do not exceed 85 °C. Under ISO 188 hot-air aging at 120 °C for 1000 h, talc-filled PP/EPDM systems of this class typically retain 70–85% of initial tensile strength and 60–75% of initial Charpy notched impact, with embrittlement concentrated in the surface layer. Parts that are constrained by metal clips or weld bosses can develop stress cracks if local stress exceeds 8–12 MPa at aging temperature. Fatigue performance under cyclic flexure is governed by the talc orientation near the part surface; an injection speed of 20–50 mm/s into a cold mold surface of 30 °C promotes rapid skin formation and higher surface stiffness, while excessive injection speed causes internal flow marks and loose talc platelets. Thermal expansion between -40 °C and 80 °C must accommodate a coefficient of linear thermal expansion of 60–90 × 10⁻⁶ K⁻¹ for 30 wt% talc-filled PP/EPDM measured under ISO 11359-2; rigid mounting of long rocker panels without expansion slots produces buckling at the lower end of the temperature range.
Regulatory documentation for automotive exterior grades must include REACH registration under EC 1907/2006, compliance with 2011/65/EU as amended by (EU) 2015/863 RoHS, and IMDS entry under the relevant automotive material classification. Kingfa API-3015 is intended for automotive exterior use and is not qualified for food-contact, potable-water, or medical device applications under FDA 21 CFR or USP Class VI. The material is supplied in natural or pre-colored pellet form; non-black custom colors require a separate UV qualification because stabilizer concentration and pigment absorption vary with colorant loading. For any application outside the specified melt temperature, mold temperature, or moisture limits, pre-trial on production-scale tooling is required. Table 2 lists the primary compliance assessment matrix.
| Regulation / Standard | Scope | Assessment Basis |
|---|---|---|
| REACH EC 1907/2006 | Registration of chemical substances, SVHC disclosure | Supplier safety data sheet and registration confirmation |
| RoHS 2011/65/EU + (EU) 2015/863 | Restriction of lead, mercury, cadmium, hexavalent chromium, PBB, PBDE, phthalates | XRF screening and certificate of compliance |
| IMDS | Material data for automotive reporting | IMDS declaration by supplier under relevant material classification |
| GADSL | Global Automotive Declarable Substance List | Screening against current GADSL list |
| ISO 4892-2 | Xenon-arc weathering | OEM-specific color acceptance |
| SAE J2527 | Accelerated exterior weathering | OEM-specific gloss and color-shift thresholds |