Kingfa HG-168A182, High Gloss/Heat Resistant

    • Product Name: Kingfa HG-168A182, High Gloss/Heat Resistant
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 831944
    Density 1.05 g/cm³
    Melt Flow Rate 20 g/10 min (220°C/10 kg)
    Tensile Strength 45 MPa
    Tensile Elongation At Break 20%
    Flexural Strength 70 MPa
    Flexural Modulus 2200 MPa
    Izod Notched Impact Strength 15 kJ/m² (23°C)
    Heat Deflection Temperature 95°C (1.8 MPa)
    Vicat Softening Temperature 105°C
    Rockwell Hardness R105
    Molding Shrinkage 0.4–0.6%
    Ul Flammability Rating HB
    Water Absorption 0.2%

    As an accredited Kingfa HG-168A182, High Gloss/Heat Resistant factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa HG-168A182 High Gloss/Heat Resistant is packaged in 25 kg sealed bags, ensuring safe handling, storage, and transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with Kingfa HG-168A182 high-gloss/heat-resistant resin, palletized, secured, and sealed for export shipment.
    Shipping Kingfa HG-168A182 is shipped as non-hazardous thermoplastic pellets in sealed moisture-barrier bags, packed in 25 kg sacks or octabins on pallets. Keep dry, cool, and protected from sunlight; avoid punctures and contamination. Normal industrial handling applies; no special transport hazard classification.
    Storage Store Kingfa HG-168A182, High Gloss/Heat Resistant, in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and ignition. Keep containers sealed to prevent moisture, dust, and contamination. Avoid prolonged exposure to high temperatures, use first-in-first-out stock rotation, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months in original unopened packaging, stored dry below 30°C, protected from sunlight and moisture.
    Application of Kingfa HG-168A182, High Gloss/Heat Resistant

    Where Does Gloss Uniformity Fail in Automotive Interior Console Trim?

    The limiting variable in high-gloss automotive center console frames, instrument panel decorative bezels, and door switch panels molded from Kingfa HG-168A182, a high-gloss heat-resistant polypropylene compound, is not melt flow but cavity-surface temperature homogeneity. In production-scale trials on 350–500 t injection molding machines with 20:1 L/D feed screws and valve-gated hot runners, the as-supplied pellet is not diluted with general-purpose PP; colour masterbatch is metered at 1.0–2.5% by weight of the total shot. Exceeding the upper masterbatch loading produces visible pigment dispersion bands along flow direction, which appear as 15–25% loss in 60° specular gloss measured by ISO 2813. Molding windows for this class of high-gloss heat-resistant polypropylene are narrow because the surface is a replication of the cavity topography rather than an additive-generated surface; therefore any drop in tool temperature below target produces dense flow marks and micro-haze. Conventional hydraulic presses run a barrel melt temperature of 200–235°C, hot-runner manifold temperature of 210–230°C, and cavity temperature of 45–70°C. Where mirror-level surface appearance is specified, steam-assisted rapid heat cycle molding is used to raise the cavity surface to 100–120°C during filling and packing, then cool to 40–55°C before ejection. This process window must be held within ±5°C; deviations create visible surface gradient bands when the cavity surface falls below 50°C and extend cycle time by 30–45 s when the high-temperature dwell is overrun. Automotive interior compliance for the trim sector is evaluated under FMVSS 302 and ISO 3795 for horizontal flammability, VDA 277 for VOC, VDA 278 for SVOC, and VDA 270 for odour; weathering is checked by SAE J2412 xenon-arc method for colour and gloss retention after 600–1,200 kJ/m² depending on OEM specification. Terminal product types include EV center console top covers, door switch bezels, HVAC control panels, and dashboard cluster gauge rings. Published data for this specific compound in mould-flow simulation libraries is limited; process parameters should be verified by in-mould cavity pressure sensors rather than transferred directly from unfilled PP grades.

    Processing window limits for high-gloss automotive trim molded with steam-assisted RHCM
    Process stepCavity surface temperature bandFailure mode outside bandEquipment reference
    Filling and packing100–120°CFlow marks, gloss loss, visible gate blushSteam-assisted RHCM controller with cavity thermocouple
    Cooling before ejection40–55°CWarpage, extended cycle timeConformal cooling circuits with inlet/outlet temperature monitoring
    Melt delivery200–235°CYellowing, excessive volatilesBarrel temperature zones on 350–500 t injection machine

    Processed on 200–320 t injection molding machines, electric kettle base shrouds, rice cooker lid covers, and air fryer outer housings require a different control hierarchy because visible surfaces sit adjacent to dry-heat zones and occasional water spillage. The formulation for kitchen appliance structural parts uses gravimetric dosing set to 1.0–2.0% by weight colour masterbatch, with the compound comprising the remaining shot weight; if plant storage exceeds 60% relative humidity, pellets are pre-dried at 80°C for 2 h before continuous gravimetric dosing. Tooling uses polished S136 or equivalent stainless steel inserts with surface finish Ra 0.025–0.05 µm; ejection is delayed until cavity wall temperature falls below 55°C to avoid sink marks around snap-fit bosses on the back side. Food-contact-adjacent structural parts are assessed under GB 4806.7-2023, EU Regulation 10/2011, and FDA 21 CFR 177.1520 when the part is not separated from food by a functional barrier. These regulations govern total migration limits and permitted additives rather than mechanical performance; a supply declaration should include the compound’s food-contact-grade confirmation from the manufacturer. Glow-wire performance is assessed under IEC 60335-1 clause 30.2.3 at 650°C for unattended appliance enclosures, and ball-pressure indentation is checked under IEC 60695-10-2 at 125°C. Terminal product types include electric kettle lower shrouds, rice cooker outer lids, soy milk maker upper housings, and air fryer exterior top covers. Production-scale failure modes observed on these parts are commonly concentrate-related: colour masterbatch loadings above 2.0 wt% produce weld-line reflectance variation and increase sink depth around hot-runner valve pits.

    Steam-Heated Tooling and Surface Replication in Water Heater Control Console Manufacturing

    Wall-mounted electric water heater control consoles and bathroom wall-hung boiler front panels expose the gloss surface to intermittent ambient humidity and radiant heat from storage vessels, making the control hierarchy different from cold-room appliance parts. In this sector, the compound is run neat; black masterbatch loading of 1.0–1.5 wt% is used for deep-tone panels, and inorganic pigment masterbatches are preferred because organic pigments shift under returning hot water line contact above 80°C. The production method is direct-gated injection with steam-heated tool cavities in which the cavity surface is raised to 110–130°C during filling and then chilled to 40–50°C before ejection. This temperature swing provides surface replication of the polished cavity but demands sufficient packing pressure; holding pressure between 35–55 MPa is required to avoid gloss collapse across the large flat front face. Gloss is measured after 24 h conditioning under ISO 2813; heat resistance is assessed by ISO 306 VST/B120 for the compound as a material, and part-level evaluation follows IEC 60335-2-21 for storage water heaters. Terminal product variants include wall-hung electric water heater front fascia, bathroom heating control console covers, and boiler display bezels.

    Where detergent-resistant high-gloss surfaces are required on washing machine consoles and dishwasher front display panels, the compound’s visible surface must survive repeated contact with anionic and non-ionic cleaning agents without micro-crazing. The visible front wall is molded as a 0.8–1.2 mm thin skin with a central direct gate, and the part is held in the cavity until the wall temperature falls to 55°C or below, because early ejection produces sink marks around ribs and bosses that are magnified by the gloss plane. The shot consists of undiluted compound; no external plasticiser, lubricant, or mould release agent is allowed on the visible wall, and ejector pins are operated with PTFE-coated sleeves to avoid drag marks. Compliance for washing machine and dishwasher front consoles is evaluated under IEC 60335-1 clause 30.2 for glow-wire ignition, IEC 60335-2-7 for washing machines, IEC 60335-2-5 for dishwashers, and ASTM D785 for Rockwell hardness; surface gloss is checked to ISO 2813 with 60° geometry. Terminal product types include washing machine control console covers, dishwasher front display panels, and front-load washer kick-plate trims. For units exposed to alkaline cleaning agents, converter trials should include immersion in 1% sodium carbonate solution at 60°C for 24 h followed by a visual micro-craze check under 20× magnification, because standard gloss measurement alone will not detect early stress cracking.

    When Sequential Valve Gating Displaces Weld Lines in Office Chair Outer Shells

    Office chair outer shells and lounge seating back panels with high-gloss black surfaces use sequential valve-gated hot-runner systems to move weld lines out of visible surfaces; the gate drops are opened central-first and outer-second, which pushes the melt fronts into rib zones and hidden lower edges. Carbon-black masterbatch is metered at 2.0–3.0% by weight for dark furniture shells; no talc or glass fiber is added to the visible skin, because mineral fillers create surface roughness that reduces 60° gloss under ISO 2813 by more than 10–15 units. Where structural load-bearing requirements exceed the unfilled compound’s flexural modulus, a glass-fiber reinforced inner core is overmolded or inserted, leaving the outer high-gloss skin unfilled; this separation prevents fibre read-through on the visible surface. The tooling runs on 300–450 t presses with mold temperature 50–60°C and sequential valve-gate timing trimmed by in-mould cavity pressure sensors; first-stage injection speed is reduced below 80 mm/s to prevent jetting that appears as white streaks on dark glossy surfaces. Furniture-sector compliance for these load-bearing shells is verified under ANSI/BIFMA X5.1 for office seating, EN 1335-1 for European office seating, and California TB 117-2013 for flammability where applicable. Terminal product types include high-gloss office chair back shells, side covers, and armrest outer covers. When the chair back is subjected to repeated loading, the outer shell is not stressed beyond the compound’s tensile yield under ISO 527; converted parts are test-loaded in production with a 60-second back-rest strength hold according to the applicable BIFMA clause.

    Free Quote

    Competitive Kingfa HG-168A182, High Gloss/Heat Resistant prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa HG-168A182, High Gloss/Heat Resistant, is a styrenic injection-moulding compound placed into programmes requiring rigid trim, bezels, appliance housings and automotive interior sub-components. The grade is procured where surface reflectivity must be retained after short-term thermal exposure and where batch-to-batch gloss variation is a rejectable defect. The product is differentiated from unfilled general-purpose ABS by a higher resistance to distortion under load at elevated temperature and by a narrower processing window. The primary specification references are ISO 1133-1 for melt volume-flow rate, ISO 75-2/A for heat deflection temperature, and ISO 2813 or ASTM D523 for specular gloss. Published data for this specific configuration outside the manufacturer’s lot certificate is limited; processing thresholds and performance intervals in this document therefore refer to grade-class behaviour and to recognised batch-release standards.

    The term high gloss is not a bulk property; it is a surface response produced by the interaction between melt rheology, tool polish and thermal history. A high-gloss grade is therefore released both on standard mechanical specimens and on fixed-finish injection-moulded plaques. When the plaque mould is not specified, apparent gloss differences between suppliers are confounded by tool condition and moulding temperature. Consequently, gloss comparisons require a matched SPI finish, documented mould temperature, and a defined venting and gating layout.

    What Test Specifications Govern Material Release, and How Do They Relate to Production Failures?

    Batch-release data are interpreted as a system, not as isolated values. Melt volume-flow rate indicates whether the material will fill thin sections at acceptable pressure. Density detects incorrect masterbatch addition or polymer substitution. Tensile yield stress and flexural modulus predict short-term stiffness in snap-fits and bosses. Charpy notched impact captures the brittle-failure risk near weld lines and gates. Heat deflection temperature and Vicat softening temperature, measured under different heating and loading conditions, define the upper-use temperature of supported thick sections. Specular gloss is a direct release criterion only when specimen preparation follows ISO 294-1 and the plaque mould finish is fixed.

    PropertyStandardConditionProduction significance
    Melt volume-flow rateISO 1133-1220 °C / 10 kgControls fill pressure, thin-wall replication and gate blush tendency.
    DensityISO 1183-123 °CDetects batch segregation and improper masterbatch addition.
    Tensile yield stressISO 527-250 mm/minEstimates load-bearing capacity in snap-fit and boss features.
    Flexural modulusISO 1782 mm/minPredicts deflection under sustained handling and assembly loads.
    Charpy notched impactISO 179-1/1eA23 °CRelates to brittle failure risk at gates and weld lines.
    Heat deflection temperatureISO 75-2/A1.8 MPaDefines upper service temperature for supported thick sections.
    Vicat softening temperatureISO 306/B5050 N, 50 K/hProvides a short-term surface softening indicator under contact heat.
    Specular glossISO 2813 / ASTM D52360°Primary surface-quality index; tool polish and mould temperature directly influence the result.

    The combined interpretation matters because a formulation change that increases acrylonitrile content raises heat deflection temperature but also increases melt viscosity. Without adjustment of melt temperature and injection speed, the same material can pass heat tests but fail gloss. Similarly, a batch with moisture at the upper specification limit can pass mechanical tests but generate splay that is visible only on polished surfaces.

    Regulatory documentation for the compound should include REACH SVHC screening and RoHS 2011/65/EU migration limits when the final article is used in electrical or electronic equipment. Automotive interior specifications may also require low-odour and low-volatile organic compound performance under VDA 277 or VDA 270; final grade selection depends on the vehicle programme’s interior air quality limits.

    Melt Rheology and Injection-Moulding Equipment Settings Define the Process Window

    Moisture control is critical because high-gloss surfaces expose gas splay and surface defects that textured low-gloss grades conceal. A desiccant dryer with a dew point at or below −30 °C is required. Drying at 80 °C for 3 h to 4 h is standard when ambient relative humidity exceeds 60%; residual moisture must remain below 0.05 wt%. In an open hopper at 70% relative humidity, re-adsorption can occur within 15 min to 20 min. Closed conveying from a central dryer is therefore used for uncoated high-gloss parts.

    Barrel settings should be profiled from rear to front. The rear zone is set between 210 °C and 220 °C to control feed, centre zones between 230 °C and 245 °C, and the nozzle between 240 °C and 250 °C. Melt temperature must not exceed 260 °C. Residence time is equally important: total melt residence time in a 20:1 L/D screw should remain below 5 min. Longer residence time degrades the butadiene rubber phase, shifting the surface from specular gloss to hazy yellow and reducing notched impact strength.

    Mould temperature is the primary lever for gloss development. The A-surface cavity is held between 60 °C and 70 °C. Temperatures below 50 °C produce visible flow lines and reduce 60° specular gloss below the release target. The increased cooling time can be offset with turbulent water circuits and conformal cooling if the tool layout permits. The mould surface must be polished to SPI A-1 to A-2 or equivalent; the resin cannot compensate for tool roughness or mould fouling.

    A three-zone general-purpose screw with gradual compression is preferred over high-shear barrier screws. Barrier screws can generate frictional heat and reduce surface reflectivity because local melt temperature at the screw tip exceeds the degradation threshold. Screw speed should be limited to 80 rpm, with back pressure between 0.5 MPa and 1.0 MPa. Back pressure above 1.5 MPa increases melt temperature and produces yellow streaks on colour changes. The shot volume should be between 50% and 80% of the rated barrel capacity; below 50%, residence time increases, and above 80%, melt-temperature heterogeneity can create gloss variation.

    Regrind for visible surfaces should be limited to 20 wt% or less. Multiple heat histories accelerate yellowing and reduce impact retention. Regrind particle size should be controlled below 6 mm to prevent unmelted particles that appear as surface defects on polished tools. When regrind is used, the dried regrind and virgin material must be metered independently or blended with verified mass ratios because bulk density differences can shift melt flow rate and surface appearance.

    On a 650 t injection moulding machine with a 4-cavity valve-gated hot-runner tool, cavity-to-cavity gloss drift is observed when manifold zone balances differ by more than 5 °C or when valve-gate opening is not synchronised within 0.2 s. Gate-area gloss is sensitive to valve-gate tip temperature; a tip set more than 15 °C above the nozzle can create a circular reflectivity difference that cannot be removed by additional pack. Weld lines create local gloss reduction and mechanical weakness. Sequential valve gating is used to relocate or minimise weld lines when geometry permits; otherwise weld lines are placed behind feature edges or in textured zones.

    When the Part Must Withstand Cabin Solar Loads and Contact Heat Without Gloss Migration

    Heat-resistant high-gloss ABS grades are selected for automotive interior upper trim, HVAC bezels, seat-back panels, electronics front panels and small appliance housings. The thermal capability is not solely defined by heat deflection temperature. Heat deflection temperature measured at 1.8 MPa represents the deflection of a simply supported test bar under a known flexural stress; it does not permit continuous load at that temperature in a moulded part. For this product category, a heat deflection temperature between 90 °C and 100 °C and a Vicat softening temperature between 100 °C and 108 °C are common release reference intervals; part-specific maximum-use temperature must be derated when ribs, bosses or snap-fits sustain constant assembly load.

    Gloss retention after thermal ageing is measured by exposing plaques to 80 °C or 90 °C in a convection oven for 500 h and recording 60° specular gloss before and after exposure. Products using stabilised butadiene rubber and hindered phenolic antioxidant packages typically retain a higher percentage of initial gloss than standard ABS; however, unpainted outdoor use is outside the intended boundary because UV causes photo-oxidation and gloss loss. For UV exposure, painting, vacuum metallization, or a UV-curable hardcoat is required.

    Moulded parts are also tested under thermal cycling between −30 °C and 80 °C for 10 cycles to detect hidden stress that appears as gloss bands or microcracks. The combination of high mould temperature and high pack pressure can create frozen-in stress that is not visible until the first thermal cycle. Stress-relief annealing at 80 °C for 2 h is sometimes used before metallization to stabilise surface energy and reduce outgassing.

    Contact with common interior chemicals must be evaluated. Aromatic hydrocarbons, ketones, esters, and concentrated acids cause stress cracking or surface hazing in ABS-based products. Cleaners containing d-limonene can attack the surface and reduce gloss; compatibility should be verified under ASTM D543 or equivalent immersion protocols before production specifications are fixed.

    Comparative Positioning Against General-Purpose High-Gloss ABS and Filled Polypropylene

    Compared with a general-purpose high-gloss ABS, Kingfa HG-168A182 moves the thermal deflection and Vicat response upward through increasing the acrylonitrile content and selecting a higher-heat stabilisation package. The trade-off is higher melt viscosity at equivalent temperature, which can lower flow length and require higher melt temperature. The grade is also more prone to retention-time yellowing if the screw and hot-runner system are not purged after interruptions. In thin-wall parts with flow length-to-thickness ratios above 150:1, process parameters must be revalidated because the high-heat formulation has a smaller shear-thinning window than high-flow ABS.

    Relative to a mineral-filled polypropylene compound, Kingfa HG-168A182 provides higher specular gloss and better surface replication on polished tools. Filled polypropylene typically has a 60° gloss below 70 GU unless the tool is textured or the surface is painted; a high-gloss ABS grade can exceed 90 GU on an SPI A-2 finish. However, polypropylene has lower density, better resistance to many polar solvents, and lower moisture sensitivity. Filled polypropylene also tends to have better fatigue resistance in integral hinges, where ABS is not suitable.

    Compared with PC/ABS, the high-gloss heat-resistant ABS grade is easier to process at moderate mould temperatures and usually lower in density. PC/ABS can provide higher heat resistance and impact, but achieving a high-gloss surface typically requires mould temperatures above 80 °C and robust hot-runner temperature control. The styrenic high-gloss grade is preferred when the operating temperature is below the heat deflection temperature limit and when surface finish, dimensional stability, and material cost per unit volume are co-prioritised.

    In practice, the principal misuse of this grade is substitution into load-bearing brackets or sun-exposed exterior panels without derating or coating. If the application has continuous stress above 0.5 MPa at temperatures above 70 °C, creep becomes the governing failure mode rather than surface gloss. If the environment includes hot coolant, acid rain, or repeated exposure to ketone-bearing cleaning agents, a mineral-filled polypropylene or PC/ABS may be required. Batch-to-batch consistency in high-gloss grades should be monitored by measuring melt flow rate, moisture, and plaque gloss on the same tool under fixed conditions, because small changes in rubber particle size or stabiliser level can shift gloss without changing standard mechanical properties beyond specification limits.

    Thermal oxidative ageing data for this specific Kingfa grade is limited in public literature. Qualification should therefore include part-level testing at the upper service temperature, not only standard specimen data. Without that testing, the product should not be released for painted surfaces or plated parts because adhesion and surface energy can change after moulding. Process settings should be recorded for every cavity, not just the first article, because high-gloss surface defects are often cavity-specific and appear only after thermal post-cure.