| HS Code | 793599 |
| Density | 1.04 g/cm³ |
| Melt Flow Rate | 10 g/10 min |
| Tensile Strength | 25 MPa |
| Elongation At Break | 20% |
| Flexural Modulus | 1800 MPa |
| Notched Izod Impact Strength | 35 J/m |
| Heat Deflection Temperature At 0 45 Mpa | 110 °C |
| Heat Deflection Temperature At 1 82 Mpa | 75 °C |
| Rockwell Hardness | R85 |
| Mold Shrinkage | 1.0-1.4% |
| Flammability | HB |
| Water Absorption | 0.02% |
As an accredited Kingfa PP-00168A,PP Modified,Home Appliance, Mineral Filled factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-00168A is packed in 25 kg moisture-resistant bags, palletized and shrink-wrapped, with a minimum quantity of 1,000 kg. |
| Container Loading (20′ FCL) | Kingfa PP-00168A mineral-filled modified PP for home appliances loaded in a 20′ FCL container using standard palletized, secured stowage. |
| Shipping | Kingfa PP-00168A is shipped as non-hazardous, mineral-filled polypropylene pellets in moisture-barrier 25 kg bags or 500–1000 kg FIBCs on pallets. Not regulated as dangerous goods for normal transport. Transport in clean, dry vehicles/containers; avoid direct sunlight, heat, and ignition sources. Store dry and handle carefully to prevent packaging damage. |
| Storage | Store Kingfa PP-00168A in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep containers sealed and palletized to prevent contamination and dust accumulation. Avoid contact with strong oxidizers. Maintain stable ambient conditions and follow first-in, first-out stock rotation for quality and safety. |
| Shelf Life | Kingfa PP-00168A typically has a 24-month shelf life when stored dry, cool, and in original sealed packaging, away from sunlight. |
In front-loading washing machine outer tub assemblies, the mineral-filled polypropylene compound designated Kingfa PP-00168A is processed as a 100 wt% direct pellet feed on a 1,200–1,400 t clamp force injection molding machine with a 70–75 mm barrier screw and an L/D of 24. The barrel profile is set from feed to nozzle at 200 °C, 215 °C, 225 °C, 235 °C, and 235 °C, respectively, while the nozzle temperature is held at 240 °C; the tool is maintained at 35–50 °C with closed-loop water circulation. Because the material contains a mineral filler, screw back pressure is raised to 50–80 bar and screw surface speed is limited to 0.20–0.30 m/s to minimize filler-particle fragmentation and consequent melt-viscosity drift during a 5,000-cycle shift. The hold pressure is set at 60–70 MPa hydraulic equivalent for 4–6 s, followed by 12–18 s cooling for a nominal wall thickness of 2.5–3.0 mm. The processing window is narrow because under-filling causes flow lines at rib roots, while over-packing above 80 MPa creates flash at the tub rim and increases the in-plane shrinkage differential to more than 0.004 mm/mm. Pre-drying is required when bulk moisture exceeds 0.05 wt% after storage at >60% RH; a desiccant bed dryer at 80 °C for 2 h returns the material to process condition without additive degradation.
Regulatory compliance for this application is anchored to IEC 60335-1:2020 clause 15.2 spillage and clause 22.1 mechanical strength; non-enclosure structural surfaces may be specified as UL 94 HB at 1.5 mm thickness. Before production, melt mass-flow rate is verified by ISO 1133-1:2022 at 230 °C and 2.16 kg; a lot-to-lot deviation of more than ±15% from the master curve requires holding-pressure compensation. When process regrind is added, the maximum regrind proportion is limited to 10 wt%; the mineral-filled PP-00168A feed fraction therefore remains at 90 wt%. The molder must avoid blending unfilled PP homopolymer because it reduces the effective mineral content and increases post-mold shrinkage after unloading from a cooling fixture. Terminal components produced from this material in a single-cavity or two-cavity tool include front-load outer tub shells, integrated sump hose connection brackets, and detergent dispenser base plates; each part is subjected to a 1 h leak test at 0.3 bar air pressure and a 24 h creep test at 60 °C on a fixture that reproduces clamp loading.
Below -18 °C, refrigerator air distribution ducts made from Kingfa PP-00168A must absorb defrost-cycle expansion without producing cracks that could release fragments into the cold air stream. The applicational qualification uses ISO 179-1/1eA notched Charpy impact at -20 °C and ISO 6603-2 instrumented puncture at -30 °C, with the acceptance criterion that the failure mode remain ductile and that crack propagation length after 100 cycles between -30 °C and +40 °C not exceed 0.5 mm. For food-contact compliance, the material is assessed under FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011 overall migration, with total migration limited to 10 mg/dm² when tested in 10% v/v ethanol for 10 days at 40 °C; components that do not contact food are still subjected to IEC 60335-2-24:2010 clause 15.2 spillage and clause 22 mechanical strength. The compound is fed at 100 wt% as delivered because the mineral loading is fixed at a level that balances stiffness and low-temperature impact; any attempt to add more filler masterbatch or 5–10 wt% unfilled PP diluent shifts the filler-matrix interface toward brittle cracking at the junction of the duct vane and the housing wall. The molding process for large-area panels is performed on a 600–800 t two-platen press with sequential valve-gate control, using a melt temperature of 220–240 °C and a mold temperature of 25–40 °C; the tool surfaces are polished to <0.2 µm Ra because mineral-filled PP does not mask ejection drag marks on visible A-surface door-liner brackets. Terminal product types include crisper drawer rails, fixed shelf retainer brackets, top air-duct baffles, door liner pockets, and drain spout adapters.
Mineral-filled PP grades in dishwasher spray arm housings encounter a specific failure mode that is not predicted by short-term tensile testing: micro-cracking initiated at injection weld lines after exposure to heated detergent solutions at 60–75 °C for 500–1,000 h. The principal root cause is differential swelling between the PP matrix and the mineral filler at the weld-line boundary when hot alkaline detergent penetrates the skin layer; once the weld line opens, the crack propagates along filler-particle cluster boundaries and eventually creates a water jet leak that reduces spray-arm rotational speed. Kingfa PP-00168A is therefore processed with a melt temperature of 230–250 °C and a mold temperature of 30–45 °C to force fusion at the weld line, and the injection speed is set to 60–100 mm/s screw advance to maintain a short flow length before the melt fronts freeze off. The material is used at 100 wt% direct feed; regrind from sprues and runners is limited to 10 wt%, and any reclaim above 20 wt% is excluded because it lowers the hot-water burst pressure below 0.8 MPa when tested at 82 °C. Compliance testing for this application is anchored to IEC 60335-2-5:2012 clause 15.2 spillage and clause 22.6 resistance to humid heat, and to NSF/ANSI 51 where the component is located in the food zone of the wash cavity; material certification should include RoHS 2011/65/EU Annex II and REACH EC 1907/2006 SVHC declarations. Terminal products include spray arm bodies, spray-arm bearing caps, filter frames, sump bodies, and detergent dispenser clamps; each lot is checked on a 40 kN universal testing machine using ISO 527-2/1A tensile at 50 mm/min to reject lots with tensile yield below the control limit established on the master curve.
| Application area | Standard or regulation | Test method designation | Relevant acceptance condition |
|---|---|---|---|
| Washing machine outer tub | IEC 60335-1:2020 | IEC 60335-1 15.2 | Spillage does not reach live parts; 22.1 mechanical strength |
| Refrigerator air-path parts | FDA 21 CFR 177.1520; EU 10/2011 | ISO 179-1/1eA; ISO 6603-2 | Ductile failure at -20 °C; total migration ≤ 10 mg/dm² |
| Dishwasher spray arm housing | IEC 60335-2-5:2012; NSF/ANSI 51 | ISO 527-2/1A; hot-water burst at 82 °C | Tensile yield ≥ control limit; burst ≥ 0.8 MPa |
| Microwave oven door frame | IEC 60335-2-25:2020 | UL 94 HB at 1.5 mm | No ignition; door slamming without crack |
| Air conditioner drain pan | IEC 60335-2-40:2022 | ISO 175 acid immersion | No surface etching after 7 d at 60 °C |
| Vacuum cleaner chassis / cyclonic cone | IEC 60335-2-2:2019 | ISO 179-1/1eA; ISO 7784 | No brittle fracture after blocked-impeller test |
Microwave oven door frames and waveguide cover brackets made from Kingfa PP-00168A are qualified through a combination of mechanical shear tests and accelerated thermal cycling rather than through simple tensile data. Under IEC 60335-2-25:2020, the door structural assembly must withstand repeated slamming, and the material must not produce excessive smoke or ignition during abnormal operation; non-enclosure mineral-filled PP is released only when it meets UL 94 HB at a thickness of 1.5 mm or thinner, while the complete door system is evaluated with the oven test methods in IEC 60335-2-25 clause 18 abnormal operation and clause 22 mechanical strength. The pellet feed is set at 100 wt%, and a color masterbatch or slip additive package is added at 2–3 wt% as a separate gravimetrically metered stream; this addition ratio keeps the mineral-filled compound fraction at 97–98 wt% and prevents the surface-blooming defects that occur when lubricant loadings exceed 0.5 wt% of the total melt. The molding operation uses a 300–450 t hydraulic press with a cold runner and a center gate or fan gate into the frame; melt temperature is 220–240 °C and mold temperature is 30–45 °C. Because microwave door frames require zero-draft features on the visibility side, the tool is polished to <0.1 µm Ra and fitted with air-jet lifters; mineral-filled PP has higher resistance to ejection release than unfilled PP because its secant modulus at 23 °C is above 2,200 MPa and its surface hardness resists scratch damage during assembly. Terminal products include door inner frames, latch mounting brackets, waveguide cover clips, control panel stiffeners, and chassis support posts; each lot is checked for weld-line strength by ISO 179-1/1eA Charpy impact at 23 °C and for dimensional stability after 24 h annealing at 90 °C in a controlled air-circulating oven.
In a room air conditioner operating in a high-humidity coastal environment, condensed water on the evaporator can absorb carbon dioxide and trace sulfite species, causing the pH to fall into a weakly acidic range between 4.0 and 5.5. The drain pan compound is assessed by ISO 175 chemical resistance after immersion in synthetic condensate at 60 °C for 7 days; the acceptance criterion is that the mass change remains below 0.5% and the mean depth of surface whitening does not exceed 0.05 mm. Kingfa PP-00168A is fed at 100 wt% as delivered because its mineral filler is matrix-protected and inert to dilute carboxylate condensates; converters should not add secondary calcium carbonate masterbatch, because exposed CaCO₃ can react with acidic condensate and create micro-pitting that retains bio-slime in the drain channel. The production process for a 600–900 mm long drain pan uses a 700–1,000 t injection molding machine with sequential valve gates positioned at the pan base to reduce anisotropic shrinkage, and the tool is heated to 40–55 °C to minimize surface stress from the high-aspect-ratio flow path. Cycle-time management is governed by the need to hold the pan in the tool until the average wall temperature drops below 70 °C; earlier ejection causes bottom bowing that exceeds 2 mm across the long axis, which is measured on a granite surface plate after 24 h conditioning under ISO 291 23±2 °C/50±10% RH. Compliance standards are IEC 60335-2-40:2022 for electric heat pump, air conditioner and dehumidifier safety, with clause 22.7 insulation and drainage requirements, and RoHS 2011/65/EU Annex II restricted substance declarations. Terminal components include indoor split-unit drain pans, base pans, fan scroll housings, and compressor-side sound-damping brackets; each batch is subjected to a 1 m drop test at -10 °C and a 48 h condensate pooling test on the installed angle.
High-velocity dust impact against vacuum cleaner cyclonic cone walls exposes mineral-filled PP to simultaneous solid-particle erosion, vibration-induced fatigue, and low-temperature impact after storage in unheated locations. Kingfa PP-00168A is therefore introduced at 100 wt% direct feed into a 500 t hydraulic press with a 50 mm screw and a hot-runner system; the barrel temperatures are set from feed to nozzle at 200 °C, 215 °C, 225 °C, 235 °C, and 235 °C, while the mold is held at 25–40 °C. The compound fraction is not reduced below 95 wt% by any added color batch because lower apparent mineral content promotes sink marks above the screw bosses and reduces the section modulus of the cyclonic cone after the 2.2–2.8 mm wall section is molded. The downstream process includes immediate gate trimming by a 10 kN pneumatic edge-trim station, followed by 24 h post-mold conditioning before dimensional measurement; the key measured parameters are cone out-of-roundness, which must remain below 0.8 mm, and the snap-fit boss insertion force, which is controlled between 15 N and 35 N when tested with a 5 mm/s probe. Compliance is anchored to IEC 60335-2-2:2019 clause 21 mechanical strength and to UL 94 HB at 1.5 mm for non-electrical enclosures, with REACH EC 1907/2006 SVHC documentation. Published data for this specific PP-00168A configuration in erosion-corrosion service is limited; converter qualification should therefore include a lot-by-lot comparison against an approved master plaque. Terminal product types include cyclonic separation cones, brushroll housings, motor mounts, and exhaust grille frames; a production audit tests each lot by ISO 179-1/1eA Charpy impact at -10 °C and by a 500 h blocked-impeller heat-soak test at 85 °C to expose delayed brittle failure.
Competitive Kingfa PP-00168A,PP Modified,Home Appliance, Mineral Filled prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-00168A is a mineral-filled modified polypropylene compound assigned to the home appliance portfolio. The material is intended for injection-molded structural components in which dimensional stability, stiffness, and resistance to household service conditions are more important than high ultimate elongation. The designation identifies a polypropylene base resin with inorganic mineral filler; however, the exact filler chemistry, weight fraction, and additive package are disclosed only in the supplier’s certificate of analysis and technical datasheet. Published numerical values for this specific configuration are limited, and any property target must therefore be compared with the supplier’s lot-specific documentation rather than with generic PP figures.
The exact mineral filler may be talc, calcium carbonate, wollastonite, or a blended system. Talc is widely used in appliance compounds because it raises flexural modulus and reduces mold shrinkage while maintaining acceptable surface quality. Calcium carbonate may be used where stiffness requirements are moderate. Wollastonite can increase tensile strength but may produce more anisotropic behavior. The PP-00168A datasheet should state the actual filler type and loading; substitution cannot be inferred from the designation alone.
Because mineral-filled PP is selected primarily to reduce post-mold warpage and increase stiffness relative to unfilled PP, incoming resin characterisation and process control are more sensitive to filler dispersion and moisture than with unfilled grades. Production-scale lines running filled PP generally require more frequent screw and barrel inspection than unfilled PP because mineral fillers are abrasive.
Incoming resin characterisation for a mineral-filled home appliance grade typically follows the property categories defined in the supplier’s certificate of analysis. Density is measured according to ISO 1183-1 or ASTM D792; melt flow rate according to ISO 1133-1:2022 with a specified temperature and load, commonly 230 °C/2.16 kg for PP unless the supplier states otherwise. Tensile properties are tested per ISO 527-2/1A or ASTM D638, flexural modulus per ISO 178 or ASTM D790, Charpy impact per ISO 179-1/1eA, Izod impact per ASTM D256, and heat deflection temperature per ISO 75-2 or ASTM D648. Mold shrinkage is evaluated after 48 h conditioning using ISO 294-4 plaques. Ash content may be determined by ISO 3451-1 to confirm mineral loading. Each batch should be compared against the supplier’s specified range, not against generic PP values.
For injection molders, two property groups are usually controlled: melt flow rate and filler content. Melt flow rate is not a direct viscosity curve; for filled systems a capillary rheometry test is more informative when thin-wall filling is critical. However, MFR by ISO 1133-1 is sufficient for lot-to-lot consistency screening. Ash content by ISO 3451-1 can detect filler loading deviation but not filler dispersion quality. Dispersion is assessed by pressure rise during compounding or by microscopic analysis of molded plaques.
| Property | Test standard | Relevance to home appliance parts |
|---|---|---|
| Density | ISO 1183-1 | Confirms filler loading and affects part mass |
| Melt flow rate | ISO 1133-1:2022 | Verifies melt viscosity and lot consistency |
| Tensile stress at yield | ISO 527-2/1A | Short-term load-bearing capability |
| Flexural modulus | ISO 178 | Stiffness in snap-fit and ribbed housings |
| Charpy notched impact | ISO 179-1/1eA | Toughness under impact and at low temperature |
| Heat deflection temperature | ISO 75-2 | Shape retention under load at elevated temperature |
| Vicat softening temperature | ISO 306 | Softening under a defined probe load |
| Mould shrinkage | ISO 294-4 | Tool compensation and warpage prediction |
Representative appliance applications for a mineral-filled PP compound of this type include washing machine outer tubs, dishwasher lower spray arm supports, air conditioner drain pans, and refrigerator hinge covers. Each application demands a different balance of stiffness, chemical exposure, and long-term creep resistance. Drain pans require resistance to standing water and mildew; tub supports require load-bearing at elevated temperature; hinge covers require dimensional precision and controlled surface appearance. The material is not selected for transparent parts or for continuous load-bearing gears without validation.
For mineral-filled polypropylene appliance compounds, the processing window is narrower than for unfilled PP because excessive shear can cause filler attrition, while insufficient shear yields poor dispersion. General starting conditions for this class fall between 200 °C and 230 °C barrel temperature; the exact temperature profile should follow the supplier’s recommendation. Mold surface temperature is typically maintained between 20 °C and 60 °C. Higher mold temperatures reduce frozen-layer thickness and improve replication of textured surfaces, but they increase cycle time and part ejection complexity. Back pressure is commonly set between 0.5 MPa and 1.5 MPa to homogenize mineral filler distribution. Screw speed is kept low to moderate, often in the range of 50 min⁻¹ to 150 min⁻¹, because high screw speed raises melt temperature through viscous dissipation and can generate locally degraded polymer.
Shot size should fill 50% to 75% of the barrel capacity to limit residence time. On hot-runner tools, thermal soaking of filled PP at high processing temperatures can produce plate-out and black specks. Gate geometry must allow sufficient flow; direct gates or adequate fan gates minimize pressure loss in mineral-filled compounds. Gate freeze should be confirmed by increasing hold time until part mass stabilizes; the resulting gate-freeze time is used to set the hold-pressure profile. Cavity pressure sensors are recommended because they detect viscosity shifts from filler agglomeration more directly than machine position monitoring.
With mineral-filled PP, barrel temperature profiles are often set with a reverse or flat profile to minimize overheating of the filler-polymer interface. A typical rear zone is 190 °C to 210 °C, middle 200 °C to 220 °C, front 210 °C to 230 °C, and nozzle 200 °C to 220 °C; these are general starting points, not grade-specific. Mold temperature should be held uniform within ±5 °C across the cavity; larger gradients cause differential crystallisation and warpage. Injection speed is often set to fill 90% of the cavity before transfer to hold pressure; excessively fast injection can create jetting and surface defects in filled systems.
Moisture uptake in mineral-filled PP is not as high as in polyamide, but surface moisture and condensation can still produce splay, silver streaks, and surface defects. The material should be dried when sacks have been opened in ambient conditions above 60% relative humidity or when pellets have been transported in unheated containers. General drying conditions for filled PP are 80 °C to 90 °C for 2 h to 4 h in a desiccant dryer with a dew point below -30 °C. Oven drying is acceptable only if bed depth is limited and air circulation is continuous. Moisture analysis by Karl Fischer is preferred over weight-loss methods for filled PP because mineral fillers release volatile decomposition products at standard moisture-balance temperatures.
Regrind addition should be controlled because mineral-filled PP degrades on repeated processing; each heat history reduces impact toughness more than melt flow rate indicates. A conservative production limit for clean sprues and runners is 20 wt% regrind unless full part qualification demonstrates otherwise. Contamination with glass-filled PP, polyamide, or elastomer-rich TPO can produce delamination, gloss variation, and weld-line cracking. If hot-runner manifold temperatures exceed 250 °C, residence time should be reduced and purging frequency increased to limit filler degradation and carbon deposit formation. On production lines, regrind variability arises not only from heat history but from fines generated during grinding. Mineral-filled materials can generate fines that are not representative of virgin pellets. Conveying systems with long pneumatic runs can separate fines from pellets, causing local filler concentration shifts. Dust collection and fines removal should be verified when using high regrind fractions.
The mineral filler type and particle morphology control the balance between stiffness and toughness. Platy fillers such as talc increase flexural modulus and heat deflection temperature, but they create anisotropic shrinkage because platelets orient during flow. Weld-line regions in mineral-filled PP exhibit lower elongation and impact strength than the bulk material; the extent depends on filler aspect ratio. As a result, gate positions for appliance housings should place weld lines outside pressure-containing or detergent-exposed regions. On production tooling, dimensional variation is influenced by filler orientation and cooling rate; parts ejected too hot may continue to shrink asymmetrically for 24 h to 48 h after molding. Shrinkage testing according to ISO 294-4 on both edge-gated and center-gated plaques is recommended because the two flow orientations produce different shrinkage magnitudes. If a tool is designed from a single shrinkage factor without considering flow orientation, warpage can be amplified in large surfaces such as washing machine lids or dishwasher door liners.
For process monitoring, peak cavity pressure deviation above 10% at constant stroke commonly indicates viscosity drift from filler agglomeration or lot variation. Mold thermal imaging or multiple thermocouples should be used to verify uniform coolant temperature across the cavity. Cooling water temperature differentials above 3 °C between circuit inlet and outlet can create warpage gradients. Weld-line strength can be screened using a double-gate tensile bar; the weld-line to non-weld strength ratio for filled PP is typically below 1.0, and a lower ratio indicates stronger orientation effects. These thresholds are general industrial practice and must be adjusted against the actual mold and part geometry.
Comparative material selection for appliance structural parts should be based on the failure mode of the part rather than a single property. Unfilled PP offers higher elongation at break and weld-line strength, but lower flexural modulus and higher mold shrinkage. Glass-fiber PP provides higher flexural and tensile modulus but introduces surface roughness, higher mold wear, and greater anisotropic shrinkage. Mineral-filled PP is positioned between these extremes, offering moderate stiffness with improved dimensional stability and smoother surfaces than glass-reinforced grades. Compared with ABS, mineral-filled PP has lower density and generally better resistance to aqueous detergent solutions, but ABS may offer better dimensional precision at low wall thickness and a different surface gloss. The selection should include chemical resistance testing using the actual detergent, rinse aid, or oil according to ISO 175 or ASTM D543. Creep tests can be conducted under ISO 899-2 when the component is continuously loaded, such as a washing machine tub support or dishwasher base frame. If continuous stress in the finished part exceeds 20 MPa, the suitability of mineral-filled PP should be verified by finite-element analysis and component-level testing rather than material datasheet comparison.
When replacing another material, the entire wall thickness and rib design should be reviewed. Mineral-filled PP has a different shrinkage than ABS; a direct material swap without mold changes commonly produces dimensional deviation. Ribs may require a draft angle increase, and deep bosses may require ejection features because filled PP can be less forgiving at undercuts. Tool wear is higher than unfilled PP but lower than glass-fiber PP.
| Material | Density | Flexural modulus | Weld-line strength | Warpage tendency | Detergent resistance |
|---|---|---|---|---|---|
| Unfilled PP | Lower | Lower | Higher | Higher | Comparable |
| Mineral-filled PP | Reference | Reference | Reference | Reference | Reference |
| Glass-fiber PP | Higher | Higher | Lower | Higher | Comparable |
| ABS | Higher | Variable | Higher | Lower | Lower |
For regulatory compliance, the material supplier should provide evidence under REACH and the RoHS Directive 2011/65/EU for the relevant appliance market. If the part is destined for food-contact use, the finished article must be assessed under the applicable food-contact framework; the raw pellet is not automatically compliant with FDA 21 CFR or EU 10/2011. Heavy-metal migration restrictions under EN 71-3 or similar standards require verification on the finished article because colored mineral-filled PP can contain trace metals from pigments and fillers.
Kingfa PP-00168A should be qualified on production tooling with the intended regrind level, color concentrate, and processing conditions. Lot acceptance should compare not only melt flow rate and filler content but also molded plaque color and shrinkage, because minor variations in filler particle size distribution can shift appearance and dimensional behavior without changing melt flow rate.