| HS Code | 221887 |
| Density | 0.90 g/cm³ |
| Melt Flow Rate | 8.0 g/10 min |
| Tensile Strength | 25.0 MPa |
| Elongation At Break | 30% |
| Flexural Modulus | 1,200 MPa |
| Notched Izod Impact Strength | 50 J/m |
| Heat Deflection Temperature | 100 °C |
| Vicat Softening Temperature | 150 °C |
| Rockwell Hardness | R80 |
| Molding Shrinkage | 1.4% |
| Flammability Rating | UL94 HB |
| Processing Method | Injection Molding |
As an accredited Kingfa PP-1105,PP Copolymer,Home Appliance factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-1105 PP Copolymer for home appliances is packaged in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL loaded with Kingfa PP-1105 PP copolymer for home appliance applications, palletized 25 kg bags, securely stowed and shrink-wrapped. |
| Shipping | Kingfa PP-1105 is a non-hazardous polypropylene copolymer supplied as pellets in moisture-proof 25 kg bags, palletized and shrink-wrapped. Ship in clean, dry, covered containers at ambient temperature, avoiding direct sunlight, excessive heat, and humidity; no special hazardous-materials handling is required. |
| Storage | Store Kingfa PP-1105 PP copolymer in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep in original, closed containers or bags on pallets; protect from moisture, dust, and contamination. Avoid prolonged UV exposure and physical damage. Maintain ambient warehouse temperatures, use good housekeeping and spill control, and follow local regulations. |
| Shelf Life | Typically 24 months when stored unopened in a cool, dry place, protected from direct sunlight and moisture. |
Publicly available multi-site data for Kingfa PP-1105 in horizontal-axis washing machine outer tubs is limited; the following parameters reflect the appliance-grade heterophasic PP copolymer class and should be verified against the current supplier certificate of analysis. The outer tub is processed on hydraulic or toggle injection units rated from 900 t to 1,400 t, with shot weights between 3.2 kg and 4.8 kg. Melt temperature is maintained at 220 °C to 235 °C, and mold surface temperature is held at 35 °C to 55 °C to control post-molding shrinkage without excessive cycle-time loss. The critical process conflict is the metallic bearing insert: local wall section changes from 2.5 mm to 6.5 mm produce differential cooling that causes sink marks, voids, or elevated crystallinity in the transition zone. Plant-scale observations show that cooling-phase variation between 18 s and 28 s before core pull shifts notched Charpy impact energy measured per ISO 179-1:2010 by more than 10% at 23 °C; published data for the exact insert geometry is limited, so mold-flow simulation and short-shot studies are mandatory. The tub must withstand prolonged contact with anionic and non-ionic detergent solutions at 60 °C and occasional bleach carryover at 200 ppm active chlorine. Environmental stress-cracking resistance is screened according to ISO 22088-2:2006 with a notch technique or according to ASTM D543-21 with the specific detergent formulation used by the appliance maker. Creep under unbalanced spin loads at 1,200 rpm is evaluated by a 24 h cyclic test at 0.35 MPa to 0.70 MPa hoop stress; the exact stress depends on drum volume and load distribution. Vibration or laser welding of the balance ring adds a second thermal history. In laser welded areas, near-infrared absorber masterbatch must be dosed by the welding partner on 980 nm or 1064 nm diode laser systems, not by generic dilution, otherwise transmission drops below the minimum energy threshold. The grade is dried at 80 °C for 2 h when ambient relative humidity exceeds 60%; pre-drying below this level is normally unnecessary because excessively dried material can reduce melt pressure stability. The combination with amine-based acid scavengers in color concentrates is not recommended because of redox interference with peroxide-initiated modification residues.
Dishwasher spray arms are not simple pipes; they are thin-wall pressure chambers with internal channels of 1.5 mm to 3.0 mm wall section that must survive repeated hydrostatic pulses from the circulation pump and chemical attack from alkaline detergent formulations. The PP copolymer is injection molded with melt temperature 230 °C to 245 °C, holding pressure 60 MPa to 80 MPa, and back pressure 2 MPa to 4 MPa on valve-gated hot runner systems. The limiting reject mode on production lines is weld-line cracking at the central hub, where the flow front meets after filling the radial spray arrays. In that zone, molecular orientation is transverse to hoop stress, reducing short-term strength by up to 40% relative to a straight-flow tensile bar; the relative reduction is geometry-dependent and cannot be inferred from the data sheet alone. Long-term chemical resistance is assessed using ISO 175:2010 with the actual dishwasher detergent at end-use concentration, typically 0.5% by mass and 70 °C, for 168 h. Additional ASTM D543-21 exposure to 200 ppm active chlorine at 23 °C for 24 h is used to detect surface micro-crazing. Polypropylene homopolymer grades fail these tests by rapid crack propagation from oxidized surfaces; heterophasic PP copolymer shows higher resistance because the ethylene-propylene rubber phase arrests crack growth, but the rubber phase also raises swell in aggressive rinse aids containing citric acid above 2%. Detergent resistance is therefore not a data-sheet property but a formulation-specific result that must be re-evaluated when the appliance maker changes detergent partner or rinse aid chemistry. The table below lists a qualification matrix used on industrial PP copolymer spray arms; pass/fail limits are set by the OEM because no universal ISO visual rating applies to all geometries.
| Exposure medium | Concentration | Temperature | Duration | Test standard |
|---|---|---|---|---|
| Alkaline machine detergent | 0.5% by mass | 70 °C | 168 h | ISO 175:2010 |
| Citric acid rinse aid solution | 2.0% by mass | 60 °C | 96 h | ISO 175:2010 |
| Sodium hypochlorite solution | 200 ppm active chlorine | 23 °C | 24 h | ASTM D543-21 |
| Deionized water | blank | 70 °C | 168 h | ISO 175:2010 |
At -20 °C, the controlling failure mode in an in-freezer ice-maker housing is not motor torque during normal harvesting but the sudden resistance when the ejector shaft encounters an ice bridge. Heterophasic PP copolymers shift toward brittle behavior at this temperature, and notch sensitivity becomes the controlling design input. Molded bosses and bearing seats with wall thickness 2.0 mm to 2.6 mm concentrate stress at transitions to the main housing; failure originates at the intersection of the ejector bearing bore and the rear wall, not at the gear teeth. Qualification therefore requires instrumented Charpy impact testing at -20 °C according to ISO 179-1:2010/1eA, with acceptance values typically set at or above 4 kJ/m² to 6 kJ/m² for unfilled impact copolymer, depending on OEM safety margin. No public qualification dataset exists for Kingfa PP-1105 in this exact geometry, so notched impact is re-tested after gate vestige and flow weld lines are introduced by the production tool. Melt temperature below 210 °C can produce silvery streaks at the flow front and agglomeration of the ethylene-propylene rubber phase, reducing low-temperature ductility; melt temperature above 245 °C may generate oxidation products that migrate to the surface and produce an opaque frost layer in service. The ice-machine environment also imposes oscillatory loads at 1 Hz to 3 Hz from the ejector motor; fatigue crack growth in PP is not linear under these conditions, and stress intensity factor changes at a given crack length can accelerate sharply as the glass transition of the matrix is approached. Optical clarity is not required for the housing but dimensional stability is critical after mold shrinkage; post-molding warpage in the bearing span must be held below 0.3 mm across 150 mm to prevent shaft misalignment and subsequent gear wear. Compliance with food-contact requirements for the ice storage zone falls under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 when no functional barrier is present; specific migration testing is required for the finished molded part because processing aids and colorants alter the extractable fraction.
Microwave oven stirrer covers and door frame sub-assemblies impose a combined requirement of short-term heat resistance, microwave transparency, and food-contact migration control. The PP copolymer is exposed to surface temperatures of 85 °C during normal operation and may reach 100 °C to 110 °C in a no-load safety test cycle under IEC 60335-2-25. The part is usually molded with wall thickness 2.0 mm to 3.0 mm; overly thin walls produce sink marks around stiffening ribs, while thicker sections increase dielectric heating and cycle time. Polypropylene impact copolymer grades have low dissipation factors at 2.45 GHz, but filler packages containing carbon black or some mineral fillers can absorb microwave energy and create local hot spots; the selected grade must be checked with the actual color masterbatch and antioxidant package, not just the natural resin. Long melt residence times above 5 min at 230 °C can leave yellowed residue on hot runner valve pins and generate volatile degradation products that re-deposit on the mold cavity; these deposits are often misdiagnosed as gas marks but correlate with poor venting at thin rib intersections. Because the stirrer cover may contact airborne food aerosols, FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 establish the relevant compliance baseline for this non-fatty, low-temperature contact. Direct contact with liquid oils above 100 °C is outside the normal operating window of unfilled PP copolymer and would require separate migration testing, especially for total fat simulant D2 under Regulation (EU) No 10/2011. The material is not recommended for direct exposure to sustained steam sterilization above 121 °C because long-term hydrolysis of stabilizer residues can accelerate surface oxidation, and unsaturated components in some PP copolymer formulations can undergo further chain scission at elevated temperature. This segment favors lower viscosity PP copolymer grades that maintain impact strength after regrind; regrind content up to 20% is often evaluated using internal standards, provided melt flow rate does not shift by more than 15% from the virgin value measured by ISO 1133-1:2022.
In unitary and split air conditioners, condensate drain pans are exposed to standing water with pH ranging from 4.5 to 7.5, intermittent compressor oil carryover, and thermal cycling from 5 °C to 70 °C. Unfilled PP copolymer is selected for chemical resistance and weldability, but it must be compounded with a medium-term UV stabilization package if the pan edge is visible through the cabinet opening. Outdoor exposure is screened with ISO 4892-2:2013 method A, typically for 500 h to 1,000 h, with retained tensile elongation evaluated by ISO 527-2:2012. Water absorption of PP copolymer mouldings is normally below 0.03% by mass after 24 h immersion according to ISO 62:2008, which is not a concern; the more serious degradation mechanism is microbial film formation on the surface that retains acidic condensate against the polymer. The part therefore requires a high-gloss or fine-grained surface finish with arithmetic mean roughness below 0.8 µm to reduce biofilm anchoring, and the mold should not use chemical blowing agents that create open pores. Welded or heat-staked fittings for the drain outlet create a second thermal history that can locally increase high-melt-flow material degradation; weld strength is validated by a burst test at 0.1 MPa water pressure for 30 s, not by tensile bar data alone. The grade should not be compared directly with mineral-filled PP in this application because mineral filler increases stiffness but can release fine particles into the condensate stream; published comparative hydrolysis data for specific filler systems is limited. Published durability data for the exact Kingfa PP-1105 outdoor stabilizer system is limited; the appliance maker must confirm whether the developed formulation contains sufficient UV stabilizer for open-edge exposure or whether the design encloses the pan fully.
Cyclone cones in bagless vacuum cleaners are pressure-vacuum components that operate at 12 kPa to 25 kPa negative pressure and particle velocities above 30 m/s. Wall thickness in PP copolymer cones is typically 1.8 mm to 2.4 mm, with a single direct gate at the cone apex. The gate vestige is a critical production defect because high-velocity dust and pet hair concentrate at the apex and can tear the polymer from the vestige point; the gate diameter must be limited to 0.8 mm to 1.2 mm and the vestige height below 0.1 mm using protrusion-controlled sprue designs or a valve gate with delayed opening. The impact copolymer is preferred over homopolymer PP because the ethylene-propylene rubber phase absorbs particle impact without immediate crack formation; instrumented falling weight impact at -10 °C and 23 °C according to ISO 6603-2:2000 provides more relevant sorting data than notched flexural impact tests. Abrasion resistance is evaluated by the OEM through end-use dust tests rather than generic Taber abrasion because PP abrasion performance depends on filler size, wall thickness, and air velocity; ASTM D4060-19 data for unfilled PP can under-predict field wear. Melt temperature for thin-wall filling is held at 225 °C to 240 °C, but injection speed is more important; a filling time above 0.6 s for the cone can produce flow hesitation marks near the transition to the outlet barrel. Packing pressure is set to 60% of injection pressure for 1.5 s to 2.0 s, after which gate freeze must occur before plastication begins to avoid gate strings. Polypropylene copolymer in this application is susceptible to static dust accumulation, but antistatic additives must be selected for compatibility with the resin system; some surfactants increase mold plate-out and are not acceptable in high-gloss cones. The component is stress-tested on the production line by alternating vacuum and atmospheric pressure for 50,000 cycles at 23 °C, with pressure drop losses below 5% from initial, and by a drop test of 0.5 J impact at the apex at -5 °C. These values are OEM-specific and are not substitutes for the standard data-sheet comparison.
Competitive Kingfa PP-1105,PP Copolymer,Home Appliance prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-1105 is a pelletised heterophasic propylene-ethylene copolymer supplied for injection moulding of structural home appliance components. The supplier designation PP Copolymer, Home Appliance is a market classification rather than a compound specification; the underlying resin is an unfilled impact-modified polypropylene with controlled ethylene comonomer distribution. Melt mass-flow rate is measured under ISO 1133-1:2022 at 230 °C with a 2.16 kg piston load, and the supplier-controlled lot range is 12–18 g/10 min. Density under ISO 1183-1:2019 is held within 0.90–0.91 g/cm³, which distinguishes this grade from mineral-filled appliance compounds whose density commonly exceeds 1.05 g/cm³. The ethylene comonomer resides predominantly in a dispersed rubbery phase; xylene-soluble fraction under ISO 16152:2005 is typically 10–14 wt%, contributing to notched impact retention at sub-zero temperature. The grade is used in washing machine tubs, spin tub sleeves, dishwasher door liners, refrigerator air-channel brackets, and structural console components. In these applications the melt-viscosity profile permits filling of wall thickness down to 1.2 mm on servo-electric injection moulding machines with clamp force from 2,500 kN to 8,000 kN, provided gate geometry and venting are sized for apparent viscosity at shear rates of 10³–10⁴ s⁻¹.
Relative to a general-purpose impact copolymer, PP-1105 is differentiated by a narrower flow-control window and by lot-level verification of xylene solubles; relative to a homopolymer PP, it trades flexural modulus for higher Izod impact at -20 °C. Published multi-lot data for this specific grade outside supplier documentation is limited; the values quoted here are representative supplier datasheet ranges and must be confirmed against the lot certificate of analysis.
The principal boundary condition is not the melting point but the competition between melt-flow length and impact retention. PP-1105 melts over a crystalline melting range of 160–170 °C; the recommended melt temperature is 220–250 °C. Below 220 °C, viscosity under processing shear rates rises sufficiently to produce short-shot defects in walls below 1.5 mm when filling from a single side gate. Above 250 °C, mean residence time must be held below 10 min because thermo-oxidative chain scission begins to reduce molecular weight and notched impact properties. Barrel zones are usually set at rear 180–200 °C, central 210–230 °C, front 230–250 °C, and nozzle 240 °C. Screw geometry with L/D 20:1–24:1 and compression ratio 2.5:1–3.0:1 is standard; screws with aggressive high-shear mixing sections should be evaluated because excessive shear heating can raise melt temperature by 5–10 °C at screw speeds above 120 rpm.
In production-scale injection moulding of this resin class, the most relevant bottleneck is not melt temperature alone but mould surface temperature. When mould temperature falls below 40 °C, fast-cooled skins develop frozen-in orientation and visible stress whitening around screw bosses; raising cooling water to 40–60 °C produces a more uniform skin layer and reduces notch sensitivity at weld lines. The hold pressure profile is typically set at 50–70% of peak cavity pressure, with total hold time between 0.5 s and 2 s per millimetre of nominal wall. Pre-drying is not generally required because polypropylene moisture uptake at 23 °C and 50% RH is below 0.03 wt%; however, if bags are opened at relative humidity above 60% or stored longer than 24 h without sealed containers, desiccant drying at 80 °C for 2–4 h with dew point below -20 °C is recommended to prevent surface splay. Gate and runner design also influence the practical lower wall thickness. For multi-cavity washing machine console tools, hot runner valve gates with diameter 1.0–1.5 mm are used; edge gates for flat panels are generally 0.8–1.2 mm thick and 2–4 mm wide. Vent grooves of 0.02–0.03 mm depth at the fill end are required to prevent gas burn marks at fast injection speeds.
The grade is positioned between low-flow appliance copolymers with MFR below 8 g/10 min and high-flow thin-wall packaging copolymers with MFR above 30 g/10 min. The following table summarises the property envelope reported for PP-1105 and the corresponding test method; users should validate each line against the current certificate of analysis because property ranges may shift slightly with compounding and colorant load.
| Characteristic | Unit | Standard or condition | Typical supplier range |
| Melt mass-flow rate | g/10 min | ISO 1133-1:2022, 230 °C, 2.16 kg | 12–18 |
| Density | g/cm³ | ISO 1183-1:2019 | 0.90–0.91 |
| Tensile stress at yield | MPa | ISO 527-2:2012, type 1A, 50 mm/min | 24–28 |
| Elongation at yield | % | ISO 527-2:2012, type 1A, 50 mm/min | 6–8 |
| Flexural modulus | MPa | ISO 178:2019, 2 mm/min | 1250–1500 |
| Notched Izod impact at 23 °C | kJ/m² | ISO 180/A | 8–12 |
| Notched Izod impact at -20 °C | kJ/m² | ISO 180/A | 3–5 |
| Deflection temperature under load, method B, 0.45 MPa | °C | ISO 75-2:2013 | 85–95 |
| Xylene-soluble fraction | wt% | ISO 16152:2005 | 10–14 |
Compared with polypropylene homopolymer grades used in appliance interior trim, PP-1105 carries lower stiffness but higher cold-temperature impact. A standard homopolymer may show tensile stress at yield of 32–36 MPa but notched Izod impact at -20 °C frequently below 2 kJ/m²; the PP-1105 range of 3–5 kJ/m² at the same temperature is significant for parts subjected to transport shock and misalignment loads. A random propylene-ethylene copolymer developed for transparent refrigerator baskets typically has haze below 10% and lower room-temperature stiffness; PP-1105 is not selected for optical clarity because the dispersed rubber phase creates opacity. For appliance structural parts, opacity is not a processing limitation, and the combination of flexural modulus between 1250 MPa and 1500 MPa with notched Izod impact at 23 °C between 8 kJ/m² and 12 kJ/m² provides the primary technical rationale. Compared with glass-reinforced polypropylene compounds used for washing machine drum pulleys, PP-1105 has lower density, more uniform shrinkage, and reduced tool wear, but its flexural modulus is insufficient for high-load gear systems.
Operational boundaries become process-critical at the upper end of the melt-temperature window. At 250 °C, residence times above 10 min can produce a measurable drop in notched Izod impact and an increase in melt-flow rate because chain scission dominates over crosslinking in propylene-ethylene copolymers under oxygen-containing conditions. Production-scale equipment behaviour common to this material class includes melt-flow drift after unplanned delays on reciprocating screw machines with 60 mm screw diameter and 2200 kN clamp force; a melt temperature overshoot of 15 °C during a 12 min hold may raise the melt-flow rate from approximately 15 g/10 min to 19 g/10 min, with visible loss of drop-weight impact around the gate. Published multi-lot data for this specific configuration is limited, but the mechanism is consistent with autoxidative degradation of the polypropylene backbone. The practical controls include reducing barrel temperature during stoppages to 180 °C, retracting the screw where the controller permits, and purging with a fractional-melt purge material after delays longer than 5 min. Additive incompatibilities should not be ignored: PP-1105 should not be blended with hygroscopic engineering scrap such as polyamide or PET unless separate drying and a vented barrel are used; residual polyamide domains remain unmelted at PP processing temperatures and form notch-initiating inclusions. For colour masterbatches, carrier resins should be selected from the same PP copolymer family; a masterbatch based on low-melt-index homopolymer can leave visible flow lines at wall thickness below 1.2 mm.
Compliance verification for home appliance use is governed by Regulation (EC) No 1907/2006 and Directive 2011/65/EU as amended. The supplier’s safety data sheet and product declaration should carry lot- or grade-level statements for SVHC content; Annex II safety data sheet sections 15.1 and 15.2 are relevant for hazard and regulatory information. The unfilled PP-1105 grade is not inherently classified as hazardous under CLP, but downstream components may require glow-wire ignition temperature assessment under IEC 60695-2-12 for unattended appliance enclosures. A typical unfilled PP copolymer of this viscosity class can achieve a glow-wire flammability index at 750 °C at a wall thickness of 2 mm only if stabilised; the unmodified grade should not be specified for V-0 enclosure requirements without flame-retardant modification. The supplier’s compliance matrix should be obtained for each batch, and when colour masterbatches or processing aids are added, the finished-part regulatory status must be re-evaluated under the same standards.
| Regulatory requirement | Standard or method | Typical check |
| REACH SVHC | Regulation (EC) No 1907/2006, Article 33 | No SVHC above 0.1 wt% in supplier declaration |
| RoHS recast | Directive 2011/65/EU, Annex II | Pb, Hg, Cr(VI) < 1000 ppm; Cd < 100 ppm; PBB/PBDE < 1000 ppm |
| Glow-wire ignition | IEC 60695-2-12 | 750 °C at specified wall thickness |
| UL 94 | UL 94 | HB or V-2 for unfilled natural; V-0 requires flame-retardant modification |
| Food contact if applicable | EU Regulation 10/2011 | Migration testing dependent on layer, additives, and final use |
In injection moulding simulation work, the grade is frequently evaluated with pressure-volume-temperature data and shear-viscosity curves generated under ISO 11443:2021 or equivalent capillary rheometry. Before production release, the combined effect of the selected masterbatch on melt-flow rate, xylene solubles, and shrinkage anisotropy should be measured; some organic pigments shift nucleation behaviour and alter post-mould shrinkage by 0.1–0.3% across the flow direction. This effect is more pronounced in flat appliance panels with wall thickness below 1.5 mm and should be controlled by fixing the masterbatch lot, dosage, and gate location during validation.