Kingfa PP-11270,PP Copolymer (Mineral Filled)

    • Product Name: Kingfa PP-11270,PP Copolymer (Mineral Filled)
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 361789
    Density 1.04 g/cm³
    Melt Flow Rate 10 g/10 min (230°C/2.16 kg)
    Tensile Strength 24 MPa
    Elongation At Break 25%
    Flexural Modulus 2000 MPa
    Notched Izod Impact Strength 35 J/m
    Heat Deflection Temperature 105 °C at 0.45 MPa
    Vicat Softening Temperature 150 °C
    Molding Shrinkage 1.1%
    Rockwell Hardness R90
    Flame Rating HB
    Water Absorption 0.02%

    As an accredited Kingfa PP-11270,PP Copolymer (Mineral Filled) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa PP-11270 mineral-filled PP copolymer is packaged in 25 kg moisture-barrier bags, palletized and shrink-wrapped for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized bags of Kingfa PP-11270 PP Copolymer (Mineral Filled), shrink-wrapped and secured for export.
    Shipping Kingfa PP-11270 mineral-filled PP copolymer is shipped as dry pellets in sealed moisture-barrier bags, octabins, or bulk containers at ambient temperature. Keep dry, clean, and protected from UV/heat; store in a cool, ventilated area per SDS. Normally non-hazardous for transport.
    Storage Store Kingfa PP-11270 in original sealed packaging in a cool, dry, well-ventilated area, protected from direct sunlight, heat, moisture, and flames. Keep away from oxidizing agents and incompatible chemicals. Avoid dust generation and contamination; keep containers closed on pallets. Maintain good housekeeping and first-in, first-out rotation; consult the SDS for specific requirements.
    Shelf Life Kingfa PP-11270 typically has a 12-month shelf life when stored unopened in a cool, dry place away from sunlight.
    Application of Kingfa PP-11270,PP Copolymer (Mineral Filled)

    Automotive interior structural carriers in PP-11270 are typically validated on long-flow, low-pressure injection moulding lines where melt-cushion stability and mineral-filler dispersion control both dimensional repeatability and grain reproduction after tool texturing. The material is processed at melt temperatures of 210–250 °C with mould temperatures maintained between 20 °C and 60 °C; for door-module carriers exceeding 900 cm² projected area, clamp force is calculated at 0.35–0.60 t/cm² and holding pressure is set between 30 MPa and 50 MPa for 6–12 s. Batch-to-batch shift is monitored by melt-flow verification to ISO 1133-1:2022 because a change of 0.5 g/10 min at 230 °C/2.16 kg can alter cushion position enough to change short-shot frequency in long ribs. Compliance for interior trim requires horizontal burning rate to ISO 3795:1989 or FMVSS 302, VOC and odour control according to VDA 277, and chemical registration under REACH Annex XVII. The formulation addition ratio at the converter typically uses 90–100 wt% PP-11270 with 0–10 wt% dry in-house regrind and 1–2 wt% colour or carbon black masterbatch; higher regrind levels reduce low-temperature notched impact and increase odour re-emission. Tooling employs valve-gated hot-runner systems with screw L/D ratios of 20:1 to 24:1, back pressure of 5–10 bar, and screw speed capped at 60–100 rpm to limit filler attrition. Terminal product types include door-module carriers, dash-panel carriers, glove-box frames, lower pillar trims and seat-back trays.

    Calculating Clamp Force and Tool Surface Temperature for Washing Machine Component Moulding

    Moulding trials on front-load washing machine base frames with PP-11270 show that tonnage calculation is controlled less by maximum melt pressure than by projected area and wall-section uniformity; floor frames above 1,200 cm² projected area are run on machines with 1,500–2,500 t clamp force to prevent perimeter flash because mineral-filled PP copolymer displays reduced melt compressibility under high packing pressure. The process window uses melt temperature of 220–245 °C, mould temperature of 30–60 °C, and holding pressure of 30–45 MPa for 8–15 s; venting depth at the parting line is limited to 0.02–0.03 mm to avoid flash while releasing filler-decomposition volatiles. Compliance for structural parts sits under IEC 60335-1:2020 and IEC 60335-2-7 for washing machines or IEC 60335-2-5 for dishwashers, with glow-wire testing to IEC 60695-2-11 at 650 °C or 750 °C depending on distance from live electrical elements; flammability is documented as UL 94 HB. The compounding ratio in production is typically 85–95 wt% PP-11270, 5–15 wt% PP impact copolymer regrind, and 1–2 wt% pre-dispersed colour; when a higher stiffness lot is specified, 2–5 wt% of a talc coupling masterbatch is added, but the resulting melt-flow shift must be confirmed against ISO 1133-1:2022. Valve-gate accumulations of mineral filler can produce gate freeze-off if screw decompression exceeds 5 mm. Terminal products include outer-tub supports, pump brackets, kick panels and dishwasher base frames.

    What Shrinkage Anisotropy Range Is Observed in Power Tool Housing and Garden Equipment Shroud Moulding?

    Mineral-filled PP copolymer is selected for power tool housings and garden equipment shrouds when the design accepts a flexural modulus below short-glass PP and requires better surface appearance than long-glass grades. Processing uses melt temperatures of 220–245 °C, mould temperatures of 25–50 °C and profiled injection velocity to prevent jetting at confined gates; because mineral platelets orient in the flow direction, shrinkage anisotropy is measured by ISO 294-4:2018 and typically falls between 1.0% and 1.6% in flow and 0.8% and 1.3% transverse, imposing a minimum tooling compensation differential of 0.5% on multi-cavity layouts. Compliance for double-insulated power tools references IEC 62841-1, with comparative tracking index to IEC 60112 at 600 V where the shell is adjacent to live parts; flammability is generally classified to UL 94 HB unless a flame-retardant package is pre-compounded. Formulation addition ratio at processing is 92–98 wt% PP-11270, 2–5 wt% impact modifier for drop impact below -10 °C, and 0.5–1.5 wt% colour masterbatch; nucleating agents at 0.1–0.3 wt% are sometimes used but can produce inconsistent shrink compensation because mineral filler already supplies heterogeneous nucleation surfaces. Terminal products include drill housings, battery-pack clamshells, angle-grinder housings, lawn-mower engine shrouds and snow-thrower cowls.

    Where low-voltage junction boxes and indoor control enclosures are specified without exposure to uninsulated live parts or arcing, PP-11270 is considered only if the application does not require a V-0 rating; the unfilled and mineral-filled PP copolymer class is normally limited to UL 94 HB unless halogenated or intumescent flame retardants are pre-compounded. Compliance for enclosure shells is anchored to IEC 60670-1:2015, IP classification testing to IEC 60529, and material restrictions to RoHS Directive 2011/65/EU; if the enclosure integrates with luminaires, thermal and glow-wire clauses of IEC 60598-1 apply. Formulation addition for this sector is kept at 100 wt% PP-11270 with uncontaminated sprue/runner regrind limited to 0–10 wt%; higher recycled content is not recommended for screw bosses below 0 °C because mineral-filled PP copolymer shows reduced notched impact after multiple heat histories. Production uses multi-cavity cold-runner moulds in P20 or H13 tool steel at mould temperatures of 30–60 °C and screw back pressure of 6–12 bar; terminal products include IP40/IP54 junction boxes, surface-mount switch boxes, terminal enclosure bases and low-voltage control box covers.

    PP-11270 downstream conformance and addition-ratio matrix
    Downstream sectorPP-11270 loadingPrimary compliance anchorSecondary validation
    Automotive interior structural trim90–100 wt% + 0–10 wt% regrindISO 3795:1989 / FMVSS 302VDA 277
    Home appliance base frames and tub supports85–95 wt%IEC 60335-1:2020IEC 60695-2-11
    Power tool housings and garden equipment shrouds92–98 wt%IEC 62841-1IEC 60112
    Low-voltage enclosures and junction boxes100 wt% + 0–10 wt% regrindIEC 60670-1:2015IEC 60529
    Reusable logistics and pallets80–90 wt%ISO 8611-1:2021EC 10/2011
    HVAC condensate handling85–95 wt%ISO 527-2ISO 179-1/1eA

    When Mineral-Filled PP Copolymer Replaces HDPE in Reusable Logistics Systems

    The substitution of HDPE by PP-11270 in reusable pallets and collapsible containers becomes technically acceptable when the payback cycle demands higher top-deck stiffness and lower creep under static load than HDPE at ambient temperature, and when the logistics operation does not expose parts to repeated impact below -20 °C without a compounded impact modifier. Compliance in this sector is defined by ISO 8611-1:2021 for pallet performance, ISO 22088-3 for environmental stress cracking in chemical contact, and EC 10/2011 migration testing where the logistics item may contact packaged food indirectly. The mixing ratio for pallet and container production usually comprises 80–90 wt% PP-11270, 10–15 wt% talc or mineral masterbatch if flexural modulus above 2,500 MPa is specified, and 0–5 wt% UV stabiliser masterbatch for outdoor storage; regrind addition up to 20 wt% is permitted only after ISO 1133-1:2022 melt-flow verification shows no shift beyond 10% of virgin value. Processing is performed on structural-foam or multi-nozzle low-pressure injection machines with melt temperatures of 245–260 °C, cooling times of 60–180 s, and wall thicknesses of 8–25 mm; terminal products include 1200×1000 mm pallets, collapsible bulk containers, automotive returnable dunnage trays and industrial tote boxes.

    Condensate Pan Creep Resistance and Chlorinated Water Contact in Air-Handling Applications

    In air-handling equipment, PP-11270 encounters a thermal-cycling environment in which condensate at 5–15 °C alternates with coil-block temperatures near 50–60 °C during defrost cycles, producing long-term flexural load on pan ribs and mount points. The relevant test set includes ISO 527-2 tensile properties, ISO 179-1/1eA Charpy notched impact at 23 °C and -20 °C, and ISO 899-2 tensile creep where long-term deformation is evaluated; published data for PP-11270 under alternating condensation and defrost temperature conditions are limited, so part-level validation is required for drain pans with unsupported spans above 60 mm. Material compliance for air-handling components is typically limited to UL 94 HB flammability and chemical resistance verification against de-chlorinated water, with system-level microbial growth managed by ASHRAE 62.1 rather than polymer formulation. The addition ratio in this zone is commonly 85–95 wt% PP-11270, 5–10 wt% barium sulfate or talc masterbatch, and 0.2–0.8 wt% hindered-amine light stabiliser/UV package for louver-exposed surfaces; pre-drying at 80 °C for 2 h is enforced when storage RH exceeds 60% to prevent splay at gates. Production tooling uses three-plate or valve-gated hot-runner moulds with parting-line vents of 0.015–0.025 mm and screw speeds limited to 50–80 rpm on a 60 mm barrel; terminal parts include HVAC condensate drain pans, blower scrolls, air guide vanes, intake louvers and condensing-furnace collector boxes.

    Free Quote

    Competitive Kingfa PP-11270,PP Copolymer (Mineral Filled) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa PP-11270 is a mineral-filled polypropylene copolymer compound supplied in pellet form for injection moulding, sheet extrusion, and blow moulding. The designation identifies a polypropylene copolymer matrix modified with an inorganic mineral filler; the filler fraction is generally in the 15–25 wt% range for this product class, but the exact mineral species and nominal loading are controlled by the supplier’s certificate of analysis. Melt volume-flow rate measured at 230 °C under 2.16 kg according to ISO 1133-1:2022 is expected in the 8–15 cm³/10 min band, and density according to ISO 1183-1:2019 is expected between 1.05 g/cm³ and 1.10 g/cm³. These values place PP-11270 in the medium-flow mineral-filled impact copolymer category used for thin-wall interior parts where flow length and dimensional stability are more critical than short-term tensile strength. Published data for this specific configuration is limited to lot-specific test records; the values presented in this document are class-typical ranges derived from mineral-filled PP copolymer datasheets and should be verified against the manufacturer’s release data before tooling is committed.

    Typical application contexts include door panel substrate, centre console carriers, lower trim, HVAC distribution housings, appliance structural covers, and industrial transport containers. In such parts, the mineral filler reduces post-moulding shrinkage variation, while the copolymer matrix retains impact behaviour after long cold-conditioning intervals. Processing is performed on single-screw injection units with general-purpose polyolefin screws; compounding for custom formulations is carried out on co-rotating twin-screw extruders with length-to-diameter ratio of 40:1 and side feeding of the mineral filler after the polymer melting section.

    Compositional and Rheological Profile

    The rheological profile is controlled primarily by the copolymer base and filler aspect ratio. The melt flow rate of PP-11270 places it above low-flow glass-filled grades and below high-flow thin-wall homopolymer grades. A mineral-filled copolymer with this MFR window typically shows pseudoplastic behaviour; apparent viscosity decreases with increasing shear rate, which permits filling of long flow paths at moderate injection pressure. The filler increases apparent melt viscosity relative to unfilled impact copolymer, so injection pressures must be higher by approximately 10–25 % for identical wall thickness and flow length. At the same time, mineral fillers improve heat conduction from the polymer melt, and the formulation reaches ejection modulus earlier in the cycle than an unfilled equivalent.

    The density after moulding is the primary lot-release indicator for filler dispersion. A variation greater than ±0.02 g/cm³ from the nominal target on a production lot suggests filler metering drift or poor distributive mixing on the compounding line. Ash content by ISO 3451-1:2019 should be used to confirm filler mass fraction. For black pigmented lots, carbon black addition is typically below 1.0 wt%, and it does not materially shift density. Moisture uptake is lower than for glass-filled PA or PBT, but drying is still recommended when regrind fractions exceed 20 % or when storage humidity has exceeded 60 % RH for prolonged periods.

    The comparative bands in the table below show where a mineral-filled PP copolymer sits relative to unfilled and glass-reinforced grades. The values are representative for a 20 wt% mineral filler level and are not a substitute for lot-specific release testing.

    Property Test method Mineral-filled PP copolymer Neat PP copolymer 20% talc-filled PP homopolymer 20% glass-reinforced PP
    Density ISO 1183-1:2019 1.05–1.10 g/cm³ 0.90–0.91 g/cm³ 1.05–1.08 g/cm³ 1.03–1.06 g/cm³
    Tensile yield strength ISO 527-2:2012 22–26 MPa 20–24 MPa 28–32 MPa 45–55 MPa
    Flexural modulus ISO 178:2019 2000–2600 MPa 900–1200 MPa 2400–3000 MPa 3200–4000 MPa
    Notched Izod impact at 23 °C ISO 180:2019 4–6 kJ/m² 8–20 kJ/m² 2–4 kJ/m² 8–12 kJ/m²
    Heat deflection temperature at 0.45 MPa ISO 75-2:2013 100–115 °C 80–90 °C 110–125 °C 130–145 °C
    Mould shrinkage ISO 294-4:2018 0.8–1.2 % 1.5–2.0 % 0.7–1.0 % 0.2–0.5 %

    Injection moulding of Kingfa PP-11270 is most reproducible when the material is dried at 80 °C for 2–4 h in a desiccant dryer if surface moisture exceeds 0.05 wt%. Barrel temperature profiles from feed to nozzle are typically 190 °C, 210 °C, 225 °C, 230 °C, and 230 °C. The maximum recommended melt temperature is 240 °C; operation above that threshold accelerates degradation of the ethylene-propylene rubber phase visible as a decline in notched impact and an increase in melt flow rate on recycled material. Mould temperature should be held between 30 °C and 50 °C for general parts. For high-gloss appearance surfaces, a mould temperature of 60 °C is permissible but increases cycle time by 10–20 %. Injection pressure at the transfer point is typically 60–100 MPa, with holding pressure set at 60–80 % of transfer pressure. A clamp force of 3–5 kN/cm² of projected area is used on production machines to prevent flash at the higher melt temperatures. Screw geometry with 20:1–24:1 L/D and a compression ratio of 2.5:1–3.0:1 provides adequate melt homogeneity without excessive shear heating. Back pressure of 0.5–1.5 MPa and screw rotation in the 30–80 rpm range are suitable starting conditions.

    During production-scale audits, the principal defects observed in mineral-filled PP copolymer are flow-line delamination at knit lines, sink marks above ribs, and post-ejection warpage caused by anisotropic filler orientation. Weld-line strength in mineral-filled PP can be 20–40 % lower than parent material tensile strength; the copolymer component in PP-11270 partially offsets this loss but does not eliminate it. Gate location should therefore place weld lines in low-stress zones. Sink marks are mitigated by holding pressure above 60 % and by rib-to-wall thickness ratios below 0.6. Post-ejection warpage is best controlled by maintaining a uniform mould temperature and by locating the gate to create radial or near-radial flow. Batch-to-batch variation in MFR should be limited to ±1.5 g/10 min to keep cushion and switchover position stable on automatic injection cycles.

    What Distinguishes a Mineral-Filled Copolymer from Glass-Reinforced Homopolymer Alternatives?

    The primary difference is failure mode. Glass-reinforced PP homopolymer provides higher tensile strength and flexural modulus, usually 45–55 MPa and 3200–4000 MPa respectively, but its cold-temperature impact retention is lower and it is more sensitive to fibre orientation at weld lines. Mineral-filled PP copolymer sacrifices some room-temperature stiffness to gain ductility retention and lower total part density. Differences with unfilled PP copolymer are equally significant: the mineral filler increases flexural modulus from approximately 900–1200 MPa to 2000–2600 MPa and reduces mould shrinkage from 1.5–2.0 % to 0.8–1.2 %, but notched impact at 23 °C decreases from 8–20 kJ/m² to 4–6 kJ/m². Against a 20 wt% talc-filled homopolymer, the copolymer matrix of PP-11270 shifts the ductile-to-brittle transition downward by approximately 10–20 °C, which is relevant for interior parts stored or installed below 0 °C.

    Surface quality also differs across these product families. Mineral-filled copolymer grades exhibit reduced floating fibre defects relative to glass-filled compounds, which allows lower post-moulding painting and grain retention in visible interior surfaces. However, mineral-filled PP is still more notch-sensitive than unfilled impact copolymer, so sharp internal radii below 0.5 mm should be avoided in load-bearing ribs and clips. The grade is also less suitable than ASA or ABS for high-heat painted exterior panels because its heat deflection temperature at 0.45 MPa is below 115 °C and unpainted black surfaces can show chalking after prolonged UV exposure unless stabilizer packages are specified at the compounding stage.

    If Barrel Residence Time Exceeds 6 Minutes, Impact Retention Declines

    The ethylene-propylene phase in PP-11270 is more susceptible to thermo-oxidative chain scission than the polypropylene homopolymer matrix. In production moulding, cumulative barrel residence time above 6 min at 230 °C is associated with measurable loss of notched impact and an increase in melt flow rate as the rubber phase undergoes viscosity reduction before matrix oxidation becomes visible. This condition appears first as a shift in switchover position and then as a drop in short-shot margin. Hot-runner drops with large dead zones, oversized barrels relative to shot weight, and long colour-change purges amplify this failure mode. The recommended shot size should be 40–70 % of barrel capacity to keep residence time below the 6 min threshold. If a line stoppage occurs, the barrel should be purged with virgin PP at low screw speed before restarting PP-11270. Oxidative stabilizers in the formulation provide protection up to roughly 230–240 °C under normal cycle conditions, but published kinetic data for this specific grade is limited and stabilizer depletion is best monitored by melt flow rate shift and notched Izod retention after multiple recycling passes.

    Thermal stability in mineral-filled PP compounds also depends on filler moisture and trace metal content. Drying at 80 °C for 2–4 h reduces hydrolysis at the filler-polymer interface and prevents surface silver streaks on visible parts. Storage in closed gaylords or silos is recommended when plant humidity exceeds 60 % RH. The use of regrind should be limited to 20 wt% for interior appearance parts and 30 wt% for hidden structural parts; higher regrind fractions reduce weld-line strength and increase variability in mould shrinkage.

    Door panel substrate applications use PP-11270 in thicknesses of 2.0–2.5 mm; the mineral filler reduces local sink over the map pocket and speaker grille supports. Flame spread performance is typically tested according to ISO 3795 or FMVSS 302, with a horizontal burn rate below 100 mm/min for automotive interiors. Appliance enclosures moulded in this material are usually evaluated for heat deflection under 0.45 MPa according to ISO 75-2:2013 and creep behaviour under continuous load at 60–80 °C. Electrical housings require surface resistivity and comparative tracking index data from the supplier; the mineral filler can increase comparative tracking index relative to neat PP, but values should not be assumed without lot-specific testing.

    High-speed filling of thin-wall parts with nominal wall thickness below 1.5 mm may require melt temperatures of 230–240 °C and injection speeds up to 300 mm/s. In such conditions, gate freeze time is short, and holding pressure must be profiled to avoid overpacking near the gate and underpacking at the end of flow. Compression moulding and blow moulding are possible but less common; blow moulding operations should select the higher-viscosity end of the MFR range to maintain parison stability. Sheet extrusion for thermoformed panels should use a melt pump after the breaker plate to attenuate pressure fluctuations caused by filler slippage on the screw.

    RoHS and REACH Verification Follow Lot-Specific Test Reports

    Compliance statements for Kingfa PP-11270 must be requested as lot-specific documents from the manufacturer, because filler suppliers and additive packages can vary by production campaign. Under EC 1907/2006, each substance of very high concern on the Candidate List is typically declared below 0.1 wt% in the finished article by supplier screening, but Article 33 communication duties must be confirmed by the downstream user. Under Directive 2011/65/EU, lead, mercury, hexavalent chromium, polybrominated biphenyls, and selected polybrominated diphenyl ethers are generally limited to 0.1 wt% of homogeneous material, while cadmium is limited to 0.01 wt%. Standard test protocols include IEC 62321-5:2013 for mercury and IEC 62321-4:2013 for lead and cadmium by AAS or ICP. Food-contact use is possible only if the specific lot is qualified under 21 CFR 177.1520 or regional equivalents, and the article’s end-use temperature and food type must remain within the conditions evaluated in the migration test.

    The compliance assessment framework is summarised below. These statements are not a substitute for lot-specific certification and do not expand the manufacturer’s warranty obligations.

    Requirement Regulatory reference Typical verification limit
    REACH SVHC communication EC 1907/2006, Article 33 <0.1 wt% per individual Candidate List substance
    RoHS restricted substances 2011/65/EU, Annex II Pb, Hg, Cr(VI), PBB, PBDE 0.1 wt%; Cd 0.01 wt%
    Food-contact olefin polymer 21 CFR 177.1520 End-use extraction conditions apply
    Automotive interior flammability ISO 3795 Horizontal burn rate <100 mm/min when specified