| HS Code | 534425 |
| Manufacturer | Kingfa |
| Grade Name | PP-116 |
| Material Type | Polypropylene (PP) |
| Filler Type | Talc |
| Filler Content | 30% |
| Density | 1.13 g/cm3 |
| Melt Flow Rate | 8 g/10 min |
| Tensile Strength | 35 MPa |
| Flexural Modulus | 3000 MPa |
| Notched Izod Impact Strength | 4 kJ/m2 |
| Heat Deflection Temperature | 125 °C |
| Vicat Softening Temperature | 145 °C |
| Molding Shrinkage | 0.8-1.2% |
| Flammability Rating | HB |
| Typical Application | Home appliance components |
As an accredited Kingfa PP-116,PP-TD30 High Heat High Rigidity,Home Appliance factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-proof bags, 40 bags per pallet, stretch-wrapped, clearly labeled, for safe industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL loaded with Kingfa PP-116 PP-TD30 high-heat, high-rigidity home appliance polypropylene, palletized and secured for export shipment. |
| Shipping | Kingfa PP-116 (PP-TD30) is shipped as non-hazardous, talc-filled polypropylene pellets in 25 kg bags or 1000 kg jumbo bags, palletized and shrink-wrapped. Transport in dry, covered vehicles/containers; avoid moisture, direct sunlight, and excessive heat. No special dangerous-goods classification or handling required. |
| Storage | Store Kingfa PP-116/PP-TD30 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep in original sealed bags/containers on pallets to prevent moisture, dust, and contamination. Avoid high humidity and static buildup. Use first-in, first-out; reseal opened packages. Store below 40 °C where possible, away from food, drink, and incompatible materials. |
| Shelf Life | Shelf life: 2 years from production date under dry, cool, ventilated storage in original sealed packaging, away from sunlight. |
Substitution of unfilled polypropylene homopolymer with Kingfa PP-116 series PP-TD30 in top-load washing machine tub assemblies is driven by the need to maintain hoop stiffness and dimensional stability when residual water temperature reaches 95°C during sanitizing cycles. The compound is a 30 wt% talc-reinforced PP with the filler pre-dispersed at source; downstream addition ratio is therefore 100% as supplied, or 85–95 wt% PP-TD30 with 5–15 wt% in-house regrind from identical tub sprues and runners. On a 1,200 t multi-platen injection moulding machine equipped with a 22:1 L/D barrier screw and 2.3:1 compression ratio, the barrel profile is maintained between 190°C and 230°C, nozzle temperature at 225°C, and mould steel at 35°C to 55°C to promote talc platelet wetting without creating skin-layer delamination at the flow front. Sequential valve-gated hot-runner drops are preferred because simultaneous edge gating creates weld lines at the intersection of tub ribs and bosses, where talc platelets align parallel to the weld plane and reduce weld-line tensile strength by approximately 30–50% compared with the bulk matrix when measured on ISO 527-2 weld-line specimens. Finished component categories include vertical-axis spinner baskets and outer tubs for 7–16 kg washing machines, balance-ring supports, and pulsator-hub stiffeners. Mandatory compliance references include IEC 60335-2-7, IEC 60335-1 Clause 21 for mechanical strength, ISO 75-2/A at 1.8 MPa for heat deflection, ISO 1133-1 for melt flow rate verification, and UL 94 HB minimum flammability classification. Export compliance additionally requires REACH Regulation (EC) No 1907/2006 SVHC screening and RoHS Directive 2011/65/EU restricted substance verification.
Alkaline detergent exposure at 65°C to 75°C in dishwasher sump assemblies imposes simultaneous requirements for hydrolytic stability, creep stiffness, and dimensional stability around rotating spray-arm shafts and pump seal seats. PP-TD30 enters the production line at 100% as furnished; when drop-impact testing reveals brittle boss cracking in thin-walled filter-cup regions, moulders dry-blend up to 10 wt% of a compatible PP impact copolymer, but addition above 15 wt% causes the heat deflection temperature of the pump-housing flange to fall below the specified ISO 75-2/B limit. Moulding is performed on 600–1,000 t hydraulic clamp units with sequential valve-gated hot runners, melt temperature controlled between 215°C and 235°C, and mould coolant held at 35–50°C to maintain a crystalline skin; mould temperatures below 30°C produce surface delamination around talc agglomerates in spray-arm water channels. Terminal finished parts include lower and upper spray-arm bodies, filter-cup sumps, circulation-pump covers, breather fittings, and salt-container brackets. Compliance references are IEC 60335-2-5, IEC 60335-1 Clause 30.2 for glow-wire ignition resistance, ISO 180/A notched Izod impact, ISO 75-2/B for low-load thermal stability, and UL 94 HB. Continuous exposure to free chlorine sanitizer above 200 ppm is outside the validated operating boundary; published data for long-term PP-TD30 behaviour in this specific chlorinated water configuration is limited.
| Component category | Appliance safety standard | Primary mechanical/thermal test methods | Flammability/chemical reference |
|---|---|---|---|
| Top-load washer tub assembly | IEC 60335-2-7 | ISO 75-2/A, ISO 527-2, ISO 178 | UL 94 HB; IEC 60335-1 Clause 21 |
| Dishwasher sump/spray-arm parts | IEC 60335-2-5 | ISO 180/A, ISO 75-2/B | IEC 60335-1 Clause 30.2 |
| Refrigerator structural brackets | IEC 60335-2-24 | ISO 527-2, ISO 75-2/A | UL 94 HB |
| Microwave door frame/base plate | IEC 60335-2-25 | ISO 75-2/A, IEC 60335-1 Clause 30.1 | UL 94 HB |
| Rice cooker shell/lid frame | IEC 60335-2-15 | ISO 75-2/A, ISO 527-2 | EU 10/2011 where direct food contact applies |
| Air purifier fan scroll/motor mount | IEC 60335-2-65 | ISO 527-2, ISO 178 | UL 94 HB |
Refrigerator machine-compartment structural components produced from PP-TD30 are generally confined to non-food-contact zones where compressor-zone ambient temperature cycles between −10°C and 65°C and where low-temperature impact after freezer exposure is not the governing requirement. The material is used at 100% as supplied; if narrow rail ribs exhibit high ejection friction, moulders introduce no more than 10 wt% clean in-house regrind from the same grade, but external process aids are avoided because they reduce stiffness under load. Injection moulding is performed on 350–600 t machines with wall thicknesses of 1.8–2.5 mm; the higher thermal conductivity of talc-filled PP relative to unfilled PP permits cooling-time reductions of 10–20% on drawer-rail and door-bin geometries, provided ejection temperature remains below the compound's Vicat softening threshold. Terminal finished components include crisper drawer rail supports, door-bin bracketing, rear compressor-cover frames, drain-trough hangers, and evaporator-cover mounting flanges. Standards applicable to this segment are IEC 60335-2-24, ISO 527-2 for tensile yield, ISO 75-2/A for heat deflection, ISO 306 Vicat softening temperature, and UL 94 HB flammability class.
In microwave oven door-frame applications, the specification for PP-TD30 is driven by the requirement to maintain door flatness and hinge-pad dimensional stability under intermittent radiant heat from the cavity while avoiding metal-shield distortion at the door periphery. The compound is used at 100% as the base resin with no further talc addition; textured low-gloss surfaces are produced with 2–4 wt% mineral-filled colour masterbatch only after the selected pigment system has been verified as non-arc-prone in the microwave field, because conductive carbon-rich masterbatches can concentrate field strength in high-voltage regions. Processing on 250–450 t two-platen electric injection machines uses melt temperatures between 220°C and 240°C, mould surface temperatures of 30–50°C, and valve-gated drops positioned to avoid knit lines at the door-latch bosses and hinge mounting pads. Terminal finished part types include door frames, control-panel support brackets, cavity base plates, and magnetron mounting frames. Mandatory compliance references are IEC 60335-2-25, IEC 60335-1 Clause 30.1 for ball-pressure test class assigned to the part zone, ISO 75-2/A at 1.8 MPa, and UL 94 HB; published data for PP-TD30 in partly metal-film-coated microwave door assemblies is limited, so OEM-specific thermal-cycle and door-slam validation remains mandatory.
At the upper shell and lid-hinge region of rice cookers and electric pressure cookers, repeated exposure to steam condensate at approximately 100°C and occasional oil mist requires a compound that does not soften at the hinge boss under clamp load or lose dimensional stability during extended keep-warm cycles. PP-TD30 is processed at 85–90 wt% with 10–15 wt% of a PP impact-copolymer dilution when hinged lid bosses show brittle cracking in cold-drop tests; this ratio must not exceed 15 wt% because heat deflection under keep-warm holding conditions may decline below the OEM limit. Moulding is carried out on 300–500 t injection machines with a melt profile of 200°C to 230°C and mould temperature of 30–50°C; the process is configured for two-plate tools with outer-shell wall thicknesses of 2.0–2.8 mm to avoid sink marks at snap-fit notches and hinge reinforcement ribs. Terminal finished products include outer body shells, base support rings, hinge covers, lid frames, and steam-valve mounting plates. Compliance references include IEC 60335-2-15, ISO 75-2/A, ISO 527-2, and EU 10/2011 only where the part is in direct food contact and the final compound has been migration-tested under the intended food simulants; FDA 21 CFR 177.1520 may apply to the PP base polymer portion but does not automatically clear talc-filled compounds for direct food-contact use.
Centrifugal fan scrolls in air purifiers require a flexural modulus high enough to hold rotor-blade clearance below 0.5 mm under maximum backpressure; PP-TD30 is used at 100% as supplied because talc reduces the thermal expansion differential between the scroll housing and the rotor end plates. The injection moulding process runs on 200–350 t machines with a two-cavity balanced runner system, melt temperature of 210°C to 230°C, and mould temperature of 25–45°C; the outer scroll is gated at the volute tangent rather than the hub to prevent jetting and to preserve smooth airflow surfaces on the pressure side of the volute. Terminal component types include scroll housings, motor-mount flanges, filter-frame stiffener ribs, and inlet grille support rings. Applicable standards are IEC 60335-2-65, ISO 527-2 tensile modulus, ISO 178 flexural modulus, and UL 94 HB; long-term ozone exposure data for this specific talc-filled PP grade in high-output ionizer models has not been published, so activation for ozonating air purifiers requires OEM-specific validation.
Competitive Kingfa PP-116,PP-TD30 High Heat High Rigidity,Home Appliance prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-116 and Kingfa PP-TD30 are polypropylene-based injection moulding compounds supplied for structural and thermally stressed components in home appliances. PP-116 is an unfilled high-flow polypropylene grade intended for thin-wall mouldings where demoulding stability and balanced impact–stiffness response are required; PP-TD30 is a talc-reinforced polypropylene compound containing nominally 30 wt% talc, designed for high heat and high rigidity applications. The distinction between the two products is not limited to filler loading. PP-116 provides lower density and easier filling of multi-cavity tools, whereas PP-TD30 raises the heat deflection temperature under ISO 75-2:2013 by 20 °C to 30 °C at 0.45 MPa and increases flexural modulus under ISO 178:2019 by approximately 80% to 110% relative to unfilled PP. Both grades are supplied in natural and black variants, and lot-specific certificates should be consulted for exact melt flow rate and ash content because compound manufacturers adjust formulations within controlled ranges.
Thermal resistance in unfilled polypropylene is determined primarily by spherulite size, crystallinity and nucleating agent content. In PP-116, thermal stability in appliance service is adequate for intermittent contact with warm surfaces but less suited to continuous hot-water immersion. PP-TD30 shifts the service boundary by introducing a percolating talc network that restrains amorphous chain mobility and reduces creep under load. Heat deflection temperature at 0.45 MPa per ISO 75-2:2013 for PP-TD30 is typically 125 °C to 135 °C, compared with 95 °C to 110 °C for PP-116. At 1.80 MPa, the gap narrows because polypropylene retains only a small fraction of room-temperature modulus at elevated temperature; published values for PP-TD30 at 1.80 MPa are generally 70 °C to 85 °C, whereas PP-116 typically falls between 50 °C and 65 °C. These thresholds determine whether a dishwasher pump housing or washing machine outer tub bracket can survive long-term exposure to 60 °C to 90 °C aqueous detergent without creep deformation.
| Property | Test method | PP-116 typical range | PP-TD30 typical range |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.90–0.91 g/cm³ | 1.12–1.14 g/cm³ |
| Melt flow rate, 230 °C/2.16 kg | ISO 1133-1:2022 | 8–15 g/10 min | 5–12 g/10 min |
| Tensile stress at yield | ISO 527-2:2012 | 24–30 MPa | 28–34 MPa |
| Flexural modulus | ISO 178:2019 | 1300–1600 MPa | 2300–2800 MPa |
| Heat deflection temperature at 0.45 MPa | ISO 75-2:2013 | 95–110 °C | 125–135 °C |
| Notched Charpy impact, 23 °C | ISO 179-1:2023 | 3–6 kJ/m² | 2–4 kJ/m² |
The values in the table are representative ranges for unfilled high-flow PP and 30 wt% talc-filled PP; published data for PP-116 and PP-TD30 specific batches may vary, so certification against the manufacturer’s datasheet is required. For PP-TD30, ash content determined by ISO 3451-1:2019 normally falls between 28 mass% and 32 mass%, and the talc top-size distribution influences both the flexural modulus and the notched impact retention.
Shrinkage in PP-116 follows a relatively uniform pattern, with mould shrinkage measured per ISO 294-4:2018 typically ranging from 1.2% to 1.8%. PP-TD30 produces anisotropic shrinkage because talc platelets orient parallel to the flow front during filling; longitudinal shrinkage may be 0.7% to 1.0% and transverse shrinkage 0.9% to 1.3%. The non-uniformity is increased by high-velocity injection, by lower melt temperatures, and by abrupt wall-thickness transitions. Tooling for PP-TD30 should therefore use larger gates, direct gates where possible, and flow leaders that reduce shear-induced platelet alignment. Unfilled PP-116 tends to warp from differential cooling and thickness transitions; PP-TD30 tends to warp from orientation gradients across the part, so corrective mould modifications differ. For a 2.0 mm nominal wall-thickness appliance bracket, gate placement in PP-TD30 can shift maximum flatness deviation by 0.3 mm to 0.8 mm across a 300 mm length, which is often the difference between acceptable and rejected assembly.
On production-scale injection moulding lines with clamp forces from 1200 kN to 2600 kN, PP-116 and PP-TD30 are not interchangeable without adjusting screw speed, back pressure and mould breathing. PP-TD30 accelerates screw and barrel wear because talc is abrasive; barrel assemblies with bimetallic liners and screw tips hardened to HRC 50 or above are recommended for campaigns exceeding 50 t of compound. Back pressure is held at 0.5 MPa to 1.5 MPa for PP-TD30 to homogenise filler distribution, compared with 0.2 MPa to 0.5 MPa for PP-116. Melt temperature at the nozzle, measured by infrared pyrometer, is maintained at 210 °C to 230 °C for PP-TD30 and 200 °C to 220 °C for PP-116. Mould surface temperature is controlled from 20 °C to 40 °C for both; however, for parts with weld lines or long flow paths, increasing mould temperature to 60 °C for PP-TD30 can improve weld line tensile strength by 15% to 25% relative to cold tooling, at the cost of longer cycle time. Drying at 80 °C for 2 h to 4 h is required when the material has been exposed to relative humidity above 60%; moisture contents above 0.1 wt% produce splay and surface defects in both grades.
| Parameter | PP-116 setting | PP-TD30 setting | Monitoring equipment |
|---|---|---|---|
| Melt temperature at nozzle | 200–220 °C | 210–230 °C | Infrared melt pyrometer |
| Mould surface temperature | 20–40 °C | 20–60 °C | Water-channel thermocouples |
| Back pressure | 0.2–0.5 MPa | 0.5–1.5 MPa | Injection unit pressure transducer |
| Pre-drying | 80 °C, 2–4 h | 80 °C, 2–4 h | Vacuum hopper dryer or desiccant dryer |
| Screw L/D ratio | 20:1–24:1 | 20:1–24:1 with wear-resistant coating | Reciprocating screw injection moulding machine |
Rheological behaviour differs substantially between the two products. The talc network in PP-TD30 increases low-shear viscosity and reduces melt elasticity. Spiral flow length in a 2 mm cavity at 230 °C is typically 20% to 30% shorter for PP-TD30 than for PP-116 at the same injection pressure. This flow restriction requires gates located nearer thick walls and may prohibit wall thickness below 1.5 mm for PP-TD30 unless high-speed injection is available. Capillary rheometry fitted with a Carreau-Yasuda model gives power-law index values of approximately 0.30 to 0.40 for PP-TD30 at shear rates between 100 s⁻¹ and 1000 s⁻¹, while PP-116 typically remains at 0.35 to 0.45 under the same conditions. Gate freeze-off time is shortened in PP-116 by its higher melt flow rate, which permits shorter packing time but increases the risk of sink marks at bosses. PP-TD30 has a longer packing window because the filler particles nucleate crystallization; however, excessive packing pressure above 70 MPa can fracture talc platelets and reduce local modulus near the gate. Published data for this specific configuration is limited at shear rates above 10 000 s⁻¹; high-speed thin-wall moulding therefore requires instrumented nozzle pressure validation.
Batch-to-batch variation in PP-TD30 ash content may be controlled within ±1 wt% from nominal; shifts in talc particle top-size can alter flexural modulus by ±150 MPa and notched Charpy by ±0.5 kJ/m² at constant loading. Injection moulding processors should monitor melt flow rate at incoming inspection per ISO 1133-1:2022 and record ash content per ISO 3451-1:2019 when changing lots. Surface streaks in PP-TD30 around hot runner gates have been traced to talc agglomerates formed when conveying occurs at temperatures above 60 °C; hopper dryer temperature should not exceed 80 °C to avoid pellet softening.
Creep behaviour at 80 °C and 10 MPa tensile stress differentiates PP-116 from PP-TD30 in assemblies that rely on clamped joints. PP-TD30 may show creep strain of 0.8% to 1.2% after 1000 h, while PP-116 can exceed 2.0% at the same condition. This difference defines the selection boundary for dishwasher base frames that must maintain assembly torque over a 10-year service life. Under cyclic vibration typical of washing machine spin cycles at 1000 rpm to 1400 rpm, PP-TD30 components retain clamped joint integrity when designed with adequate rib radii and boss reinforcement. However, talc-filled PP is notch-sensitive; ribs should not terminate at high-stress bosses without a 0.5 mm minimum fillet radius and generous flow leaders. Fatigue endurance at 10⁶ cycles is reduced by weld lines and sharp transitions; prototype parts should be tested on an electrodynamic shaker using the appliance manufacturer’s power spectral density profile rather than relying on static tensile properties alone.
Exposure to alkaline detergent at pH 10 to 12 and 80 °C can cause extraction of low-molecular-weight polypropylene additives and surface microcracking. PP-TD30 generally retains a higher fraction of flexural modulus after 500 h of immersion than PP-116 because the talc phase restricts swelling; published data for this specific configuration is limited, so immersion testing in the target detergent solution is required. Unfilled PP-116 is more susceptible to environmental stress cracking at grease-contaminated stress concentrations, whereas PP-TD30 shows better dimensional stability but lower notched impact after chemical ageing. Avoid combination with strong oxidising sanitizers containing hypochlorite at elevated temperature because polypropylene undergoes chain scission and embrittlement; if oxidising contact is required, part validation per ISO 175:2024 or the appliance OEM chemical-resistance schedule should be performed.
PP-TD30 differs from PP-T20 in talc loading by approximately 10 wt%, producing a step increase in flexural modulus of roughly 500 MPa to 800 MPa and a reduction in notched impact energy that must be accepted in design. Against 20 wt% glass-fiber reinforced PP, PP-TD30 offers lower warpage and smoother surfaces; glass-fiber PP can exceed 4000 MPa flexural modulus, whereas PP-TD30 remains in the 2300 MPa to 2800 MPa range under ISO 178:2019. The notched Charpy impact of PP-TD30 at 23 °C is typically 2 kJ/m² to 4 kJ/m², which is below the 8 kJ/m² to 15 kJ/m² common for medium-impact ABS at the same temperature. Against ABS, PP-TD30 provides comparable HDT at low load, lower cost per volume, better resistance to alkaline detergents, but lower gloss and lower notched impact. PP-116 is selected over high-flow PP copolymers when higher crystallinity and better elevated-temperature modulus retention are needed without the density increase of mineral-filled grades. When chemical resistance to pH 12 detergent at 80 °C dominates, PP-TD30 is usually preferred over ABS; when cosmetic gloss and impact are decisive, ABS or PC/ABS remains the benchmark.
Appliance components specified in PP-TD30 include washing machine outer tub rear brackets, dishwasher base frames, dryer impeller covers, and microwave oven waveguide covers. In these parts, the material is required to survive contact with water at 60 °C to 90 °C, detergent solutions, and cyclic vibration. PP-116 is used in refrigerator crisper supports, internal air duct grilles, and small appliance motor housings where high flow and colour stability are more important than extreme HDT. For food-contact or skin-contact appliance parts, no automatic compliance applies. Migration testing is carried out under EU 10/2011 using test condition OM2 or OM3 per EN 1186:2022; mineral-filled PP-TD30 should be tested for total migration and specific migration of talc-related elements only after colour concentrate addition, because antioxidant packages and pigments shift compliance. In the United States, FDA 21 CFR 177.1520 covers olefin polymers under specified extractables limits, but the compounded article must be tested. RoHS compliance is documented against IEC 62321 for lead, mercury, cadmium, hexavalent chromium and PBDE/PBB; REACH SVHC declarations are issued per shipment and should be archived with lot numbers.