| HS Code | 928367 |
| Density | 1.04 g/cm³ |
| Meltflowrate | 12 g/10 min at 230 °C/2.16 kg |
| Tensilestrength | 22 MPa |
| Elongationatbreak | 30% |
| Flexuralmodulus | 1800 MPa |
| Notchedizodimpactstrength | 25 kJ/m² at 23 °C |
| Heatdeflectiontemperature | 105 °C at 0.45 MPa |
| Vicatsofteningtemperature | 145 °C |
| Moldingshrinkage | 1.0-1.4% |
| Waterabsorption | 0.01-0.02% |
| Mineralfillercontent | 20% |
As an accredited Kingfa PP-11680,Impact Resistant PP, Mineral Filled factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-11680 Impact Resistant PP, Mineral Filled is supplied in 25 kg moisture-resistant bags, palletized for safe transport and storage. |
| Container Loading (20′ FCL) | Kingfa PP-11680 impact-resistant, mineral-filled PP loaded in 20′ FCL containers, palletized and securely stowed for safe transport. |
| Shipping | Kingfa PP-11680 is shipped as mineral-filled, impact-resistant polypropylene pellets in sealed moisture-barrier bags or octabins. Transport in clean, dry, covered containers at ambient temperature, avoiding direct sunlight, moisture, and contamination. Protect packaging from damage; no special hazardous-goods classification is normally required. |
| Storage | Store Kingfa PP-11680 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizers and incompatible chemicals. Maintain good housekeeping to control dust, and follow the manufacturer’s SDS and local regulations for safe storage and handling. |
| Shelf Life | Shelf life is typically 24 months when stored dry and cool in original unopened packaging, away from direct sunlight. |
Kingfa PP-11680 is specified where a mineral-filled impact-modified polypropylene is required to control post-mould shrinkage, stabilise ribbed geometry, and preserve low-temperature ductility without the weight penalty of engineering thermoplastics. The application descriptions that follow are organised by downstream sector and include compliance criteria, formulation loading windows, process equipment types, and finished-part categories. Published datasheet values for this specific grade should be verified against the production lot certificate; processing parameters are representative industrial starting points and must be established through mould trials on the intended tool.
In automotive interior component production, mineral-filled impact-modified polypropylene compounds are specified for substrates that require a balance of low warpage, dimensional stability, and ductile failure under knee-load and hand-pressure loads. A starting formulation for lower door panel substrates is 100% PP-11680 with 2–3 wt% PP-based colour masterbatch; if regrind is introduced, the in-plant recycle fraction should not exceed 15 wt% unless the blend melt flow rate is re-verified after reprocessing per ISO 1133-1:2022 at 230 °C/2.16 kg and held within ±2 g/10 min of the virgin lot value. Flammability of finished interior trim is evaluated under ISO 3795:2010, with a commonly applied maximum burn rate of 100 mm/min; where vehicle OEM specifications require emissions screening, thermodesorption testing per VDA 278:2011 is used to quantify VOC and SVOC content, and REACH Annex XVII restrictions on PAH and heavy metals remain applicable. Injection moulding is performed on a reciprocating-screw machine with L/D 22:1–25:1, compression ratio 2.2:1–2.8:1, melt pool temperature 210–230 °C, and mould wall 30–50 °C. Cavity pressure is held at 30–40 MPa during packing, with packing time 6–10 s for nominal wall stock of 2.0–2.5 mm; pre-drying at 80 °C for 2–4 h is applied when storage relative humidity exceeds 60% to suppress surface silver streaks caused by mineral filler moisture. Finished component types include door panel lower substrates, seat side shields, centre console side covers, cowl side trim, and pedal covers.
Large-format appliance structural parts that combine high stiffness, low creep, and sound damping are typically produced from mineral-filled impact PP rather than unfilled PP to control thermal expansion and reduce cycle-time warpage. For a top-load washer tub support or an outer tub cover, a dry-blend formulation containing 80–90 wt% PP-11680 and 10–20 wt% clean in-house regrind is common; the regrind fraction is constrained by the need to maintain flexural modulus within ±5% of the virgin lot value under ISO 178, because repeated granulation lowers filler aspect ratio and can create sink marks at gate pads and rib intersections. Batch-to-batch differences in mineral filler content produce measurable melt-pressure shifts on the injection unit; if hydraulic pressure fluctuates more than ±7% at constant screw position, fill control is switched to pressure-limited fill and the regrind content is reduced to 10 wt% until dosing stabilises. For unattended appliances exceeding 0.5 A, the moulded part is evaluated according to IEC 60335-1:2020 Clause 30.2 glow-wire and needle-flame requirements; non-flame-retardant mineral-filled PP is not inherently glow-wire ignition resistant, so components located within 3 mm of live connections require either a dedicated flame-retardant grade or an internal barrier. Injection moulding on vertical clamp machines in the 800–1,600 kN range uses melt temperature 215–235 °C, mould temperature 40–60 °C, sequential valve gating for flat structural ribs above 300 mm flow length, and hold pressure 35–45 MPa with switchover at 95–98% of filled volume. Terminal production parts include washer tub covers, dishwasher lower frame brackets, dryer motor mounts, and vibration-sensitive motor seating rings.
Across corded and cordless portable tool platforms, the housing shell must survive repeated drop impacts, solvent contact, and thermal loads from the gearbox without stress whitening that signals ductile failure. For this application, PP-11680 is used either at 100% or blended with 10–15 wt% of a higher-flow PP homopolymer to fill ribs with wall thickness down to 1.0 mm; the blend is checked by ISO 1133-1:2022 at 230 °C/2.16 kg, and the resulting melt flow is held within the moulder’s validated thin-wall fill window. Mechanical safety under IEC 62841-1:2020 Clause 21 requires that the housing withstand impact and drop tests appropriate to the tool category; UL 94 HB is often acceptable for the main housing shell, but battery encapsulation components and terminal shields must be evaluated separately. Moulding is performed on 1,000–1,800 kN hydraulic or hybrid presses with accumulator-assisted injection; melt temperature is 210–240 °C, mould temperature 25–50 °C, fill speed 80–120 mm/s, and cooling time 15–25 s for a nominal 2.0 mm wall. Pre-drying at 80 °C for 2–4 h is applied if storage RH exceeds 60% to prevent surface splay; exposure to aromatic solvents and continuous service above 100 °C should be avoided in motor-proximate zones. Terminal products include angle grinder gear housings, circular saw blade guards, hammer drill side handles, and battery tool body shells in non-flame-critical platforms.
Thin-wall electrical enclosures and cable management channels produced from mineral-filled PP capitalise on the material’s low warpage and fatigue resistance, but the maximum service voltage and proximity to live parts determine whether the grade can be used without flame-retardant modification. For low-voltage trunking and junction-box bases, a starting formulation is 95–100 wt% PP-11680 with 0–5 wt% UV or colour masterbatch; the use of regrind is limited to 20 wt% and should not appear on exposed surfaces or wire-contact ribs. Compliance under IEC 60670-1:2015 for boxes and enclosures for electrical accessories requires the finished part to pass ball-pressure testing at 125 °C or the declared service temperature, and glow-wire testing per IEC 60695-2-11 if the part is within 3 mm of a live terminal. PP-11680 without additional flame-retardant masterbatch should not be specified for enclosures requiring UL 94 V-0, UL 94 V-1, or glow-wire ignition temperature above 750 °C. Injection moulding uses a heated sprue bushing and cold runner, melt temperature 215–235 °C, mould temperature 30–50 °C, and rib-to-wall ratio 0.5:1–0.6:1 to reduce sink and maintain flatness; cycle time for a 2.0 mm wall enclosure is typically 25–40 s. For cable trough extrusions, a single-screw extruder with L/D 30:1 and a vacuum vent at −0.06 MPa removes moisture and volatile residuals before the die. Finished part types include low-voltage junction box bases, cable trunking, terminal block housings, and DIN rail enclosures not requiring V-0 classification.
Returnable logistics assets operating in multi-shift distribution environments require impact toughness at low temperature, creep resistance under stacked load, and washdown tolerance; mineral-filled impact PP is introduced where HDPE pallets exhibit excessive sag under sustained static load. A typical moulding formulation for a closed-loop returnable crate uses 85–100 wt% PP-11680 with 0.5–1.5 wt% UV masterbatch and up to 30 wt% external regrind; the regrind fraction is not increased beyond this point because Charpy notched impact under ISO 179-1:2010 at −20 °C declines rapidly when the filler-to-matrix interface is degraded by repeated extrusion and prolonged washdown cycles. For pallets, performance testing follows ISO 8611-1:2021 for bending, compression, and forklift tine loading; food-contact crate interiors may need verification under 21 CFR 177.1520 olefin polymer clearance, and REACH Annex XVII applies for heavy metals and restricted plasticisers. Large-platen injection presses of 2,000–3,500 t clamp force with accumulator assist are used; melt temperature is 200–220 °C, mould temperature 20–40 °C, and cycle time 60–90 s for pallet decks up to 1,200 mm × 1,000 mm. Weld lines at tine entry ribs require an overflow well 10–15 mm from the rib root to avoid low-strength seams. Terminal products include returnable pallets, collapsible bulk crates, divider trays, dunnage boards, and washable dairy or beverage transport bases.
Because underbody and air management components are subjected to simultaneous moisture, stone impingement, and thermal load from engine soak, the specification is not satisfied by impact resistance alone; dimensional stability after hot-wet ageing and melt-flow stability for thin-wall air ducts are equally decisive. In this application, PP-11680 is blended with 5–15 wt% high-crystallinity PP to raise heat distortion temperature and reduce creep in wheel arch liners; the high-crystallinity fraction is introduced by gravimetric dosing at the machine throat, and the blend is checked under ISO 75-2 at 0.45 MPa for heat deflection and ISO 6603-2 for multiaxial impact at −30 °C. For wheel arch liners and underbody shields, stone-chip resistance is evaluated according to ISO 20567-1 using a common starting condition of 500 g chilled steel shot at 2 bar; the assessment scale and acceptance limit are fixed by the relevant OEM material specification because published data for this specific grade in stone-chip configurations is limited. Interior HVAC ducts require flammability evaluation under ISO 3795:2010 and total VOC emission testing when specified. Sheet extrusion for thermoformed underbody shields uses a single-screw extruder with L/D 30:1–34:1 and melt pump, melt temperature 220–240 °C, and sheet surface temperature 160–180 °C before forming. Injection-moulded air ducts use melt temperature 210–230 °C, mould temperature 30–50 °C, and gas-assisted or water-assisted hollow-wall production for duct diameters 25–40 mm. Continuous service above 110 °C is not recommended for PP-11680-based parts located in direct exhaust proximity. Terminal products include wheel arch liners, underbody engine shields, HVAC distribution ducts, and cowl drain channels.
Competitive Kingfa PP-11680,Impact Resistant PP, Mineral Filled prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-11680 is a mineral-filled impact-resistant polypropylene compound classified under the manufacturer’s specification as an injection-moulding grade. The product code is entered in production control systems as Kingfa PP-11680 Impact Resistant PP, Mineral Filled. The compound consists of a polypropylene matrix, a mineral filler phase, and an elastomeric impact modifier; the exact composition is proprietary and not disclosed in the public datasheet. Downstream processors should therefore request the lot-level certificate of analysis and the current technical datasheet revision before tooling cut-off. Release testing for a mineral-filled impact PP of this class commonly includes melt mass-flow rate under ISO 1133-1 at 230°C with a 2.16 kg piston load, density under ISO 1183-1 at 23°C, tensile properties under ISO 527-2, flexural properties under ISO 178, and Charpy notched impact under ISO 179-1/1eA. Published data for this specific configuration is limited, so class-typical ranges are identified as such in this document.
The following test method matrix identifies the normative references most frequently used for release testing of mineral-filled impact polypropylene. It is not a substitute for lot-specific datasheet values.
| Property | Standard code | Specimen or condition | Purpose |
|---|---|---|---|
| Density | ISO 1183-1 | immersion in water, 23°C | mineral loading screening |
| Melt mass-flow rate | ISO 1133-1 | 230°C, 2.16 kg | flow-length estimate |
| Tensile stress at yield | ISO 527-2 | Type 1A, 50 mm/min | short-term load resistance |
| Tensile strain at break | ISO 527-2 | Type 1A, 50 mm/min | ductility |
| Flexural modulus | ISO 178 | 80×10×4 mm, 2 mm/min | part stiffness |
| Charpy notched impact | ISO 179-1/1eA | 80×10×4 mm, 23°C and -30°C | impact toughness |
| Heat deflection temperature | ISO 75-2 method B | 0.45 MPa, flatwise | low-load thermal resistance |
| Moulding shrinkage | ISO 294-4 | 60×60×2 mm plaque, 23°C | tooling compensation |
Comparative positioning between PP-11680 and other polypropylene grades is controlled by the ternary balance of filler loading, elastomer content, and matrix melt viscosity. Unfilled impact copolymers typically show higher notched Charpy impact at 23°C and -30°C than mineral-filled grades, but their flexural modulus under ISO 178 is commonly below 1,300 MPa. A mineral-filled impact grade in the class of PP-11680 is usually selected when a part requires flexural modulus above 1,500 MPa and still needs a notched Charpy impact above 8 kJ/m² at 23°C. The elastomeric modifier also shifts the brittle-to-ductile transition toward lower temperatures. A filler-only homopolymer can exhibit notched Charpy values below 3 kJ/m² at -20°C, whereas an impact-modified mineral grade may remain above 4 kJ/m² depending on formulation. These ranges are class-typical, not lot-specific values for PP-11680. Glass-fiber-filled PP differs from mineral-filled PP by producing higher tensile strength and higher heat deflection temperature at 1.8 MPa, but also higher flow-direction anisotropy and higher warpage in flat parts. A mineral-filled impact PP is therefore selected when shape stability and impact retention are more important than maximum tensile strength.
Thermal endurance of mineral-filled PP is limited by oxidation rather than melting. Short-term heat deflection temperature under ISO 75-2 method B at 0.45 MPa for mineral-filled PP is generally above 100°C; method A at 1.8 MPa is lower, often between 55°C and 70°C. Continuous service in air is typically below 110°C, and antioxidant level determines long-term retention of elongation at break. In under-hood components, external heat sources above 120°C can consume the stabilizer package and cause brittle failure weeks before visible discoloration. The datasheet should therefore be checked for long-term heat ageing data if the application environment exceeds 80°C continuously.
Rheological characterisation of mineral-filled PP should use a capillary rheometer rather than relying on MFR alone because the filler increases shear thinning. At shear rates between 100 s⁻¹ and 1,000 s⁻¹, the viscosity of filled PP is lower than that of an unfilled grade at the same MFR, but at near-zero shear the filled grade can be higher. This means MFR alone underestimates thin-wall filling resistance in very thin sections where shear rates exceed 1,000 s⁻¹. Injection-moulding simulation software should use Cross-WLF viscosity coefficients fitted from capillary data at 200°C, 220°C, and 240°C.
The specification boundaries are set by the interaction of mineral filler, impact modifier, and polypropylene matrix molecular weight. Mineral filler raises flexural modulus and reduces mould shrinkage, but each increase in filler loading generally lowers notched Charpy impact under ISO 179-1/1eA unless impact modification compensates. The melt mass-flow rate under ISO 1133-1 at 230°C and 2.16 kg is the primary process control for flow length. A medium-flow grade is usually selected for thin-wall parts below 2.5 mm nominal wall thickness; a low-flow grade may provide higher melt strength for thick sections but can generate higher shear heating at the gate land. For PP-11680, the manufacturer's datasheet should be used to identify the nominal MFR, because independent public values are limited.
Density cannot be used alone to verify mineral loading unless the filler type and matrix density are known. A density above 1.10 g/cm³ typically indicates mineral loading above 20 wt% for talc-filled polypropylene, while calcium carbonate-filled grades may exceed 1.10 g/cm³ at similar loadings because of higher filler density. Density is therefore a screening tool rather than a full compositional verification. Lot-level compositional verification may require thermogravimetric analysis under ISO 11358-1 or ash content under ISO 3451-1, depending on the mineral type. Tensile stress at yield under ISO 527-2 for mineral-filled impact PP commonly falls between 18 MPa and 25 MPa, while tensile strain at break is often above 20% at 23°C for impact-modified grades. Flexural modulus under ISO 178 is more sensitive to filler aspect ratio than to filler loading alone. Talc with median particle size near 5 µm and high platelet aspect ratio increases modulus more than calcium carbonate of similar median size, but reduces impact more aggressively if dispersion is poor. These relationships are well documented for filled polypropylene systems and provide the context for interpreting the PP-11680 datasheet.
Processing of mineral-filled impact PP demands attention to melt temperature because the filler increases thermal conductivity and shear heating. A melt-temperature range of 200°C to 240°C is typical for this compound class. Below 200°C, the viscosity of the mineral-filled melt rises sufficiently to create hesitation lines in thin sections, to increase injection hydraulic pressure, and to reduce replication of grained or textured surfaces. Above 250°C, thermo-oxidative degradation of the polypropylene backbone accelerates, and an ethylene-based impact modifier can undergo chain scission that reduces notched Charpy impact at -30°C. Screw speed and back pressure should be limited to keep residence time under 5 min at full melt temperature. Twin-screw compounding lines with length-to-diameter ratio 40:1 to 48:1 are used to disperse the mineral filler. For injection moulding, a general-purpose screw with compression ratio 2.5:1 to 3.0:1 and a free-flow non-return valve is appropriate; high-shear barrier screws are not required and can cause filler attrition at excessive screw speeds.
Moisture-related defects in polypropylene are less severe than in hygroscopic resins, but surface moisture can create splay and reduce weld-line strength. If ambient relative humidity exceeds 60% or packaging has been open for more than 24 h, pre-drying at 80°C for 2 h to 3 h in a desiccant dryer is recommended. Hopper-magnet and throat temperature should be kept below 80°C to prevent pellet softening and bridging. The mould temperature should be held at 20°C to 60°C for most applications; when high weld-line strength or low weld-line visibility is required, the mould temperature can be raised to 80°C, but cycle time increases and cooling-channel pressure drop must be reviewed. Hot-runner systems should use fully round flow channels with generous radii; dead spots increase residence time and create black specks. Hot-runner tip temperature should not exceed 280°C. Before introducing PP-11680 into a barrel that previously processed polycarbonate, polyamide, or polyoxymethylene, the barrel should be purged with a low-MFR polypropylene purge material or a commercial purge compound. Residual engineering resins can form layered interfaces that delaminate in mineral-filled PP parts. A purge volume of at least 3 barrel capacities is a production-floor baseline, but the purge should be continued until visual inspection shows no streaks or off-colour matter.
Mineral-filled impact PP exhibits anisotropic mould shrinkage because filler platelets align with the flow direction. Under ISO 294-4, parallel shrinkage of a 60×60×2 mm plaque is typically lower than transverse shrinkage. Published studies on talc-filled PP report parallel shrinkage values between 0.6% and 1.0% and transverse values between 0.8% and 1.2%, depending on filler content and mould temperature. Tooling compensation must account for gate location and flow orientation. Weld-line retention factor, defined as the tensile strength of the weld relative to unwelded bulk strength under ISO 527-2, is typically 0.55 to 0.75 for mineral-filled PP. This reduction is operationally significant in multi-gate parts and in components with insert-induced flow division. Mineral filler reduces interdiffusion across the weld interface; the impact modifier can improve weld-line tensile retention slightly, but high mould temperature improves weld appearance more reliably than it improves weld strength. Cooling fixtures should control post-mould warpage because differential shrinkage between parallel and transverse flow directions is a primary cause of out-of-flatness in filled PP parts.
Compared with an unfilled impact copolymer PP, the PP-11680 class is expected to show lower notched Charpy impact under ISO 179-1/1eA but higher flexural modulus and lower mould shrinkage. Compared with a 20% glass-fiber-filled PP, mineral-filled PP offers lower warpage and lower anisotropy in flow and cross-flow directions; however, tensile strength and heat deflection temperature at 1.8 MPa are lower. Compared with a standard talc-filled homopolymer without impact modification, PP-11680 is expected to retain ductile behaviour at lower temperatures. These comparisons are based on general class behaviour; specific differences must be confirmed from the Kingfa datasheet or physical testing on injection-moulded specimens.
Components that require a combination of stiffness and impact resistance include automotive interior trim substrates, fan shrouds, battery housings, appliance structural brackets, and electrical enclosures. Candidate part designs for PP-11680 are those in which an unfilled impact copolymer would exceed deflection limits under flexural load and a 20% talc-filled homopolymer would fail ductility tests at -20°C or -30°C. The material should not be specified for continuous exposure above 100°C under load without validating long-term thermal ageing to the relevant OEM standard. Flammability classification under UL 94 is thickness-dependent; mineral fillers can reduce dripping, but the final classification must be tested on the production part at the minimum wall-thickness section. Electrical enclosure applications may require glow-wire testing to IEC 60695-2-12 at 650°C or 750°C, depending on the product standard. The material is not recommended for solvent welding; joining should use vibration welding, hot-plate welding, mechanical fastening, or adhesive bonding after corona or plasma surface activation. Adhesive shear strength under ISO 4587 varies with surface preparation and adhesive chemistry. Avoid contact with strong oxidising acids and chlorinated hydrocarbons; polypropylene swells or degrades in contact with aromatic and halogenated solvents at elevated temperatures. If UV exposure is required, a UV-stabilized lot or a protective coating is necessary because polypropylene chain scission under UV reduces elongation at break under ISO 527-2 and creates surface chalking.