Kingfa PP-11685,Impact Resistant PP,Mineral Filled

    • Product Name: Kingfa PP-11685,Impact Resistant PP,Mineral Filled
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 976331
    Grade Kingfa PP-11685
    Material Type Impact Resistant Polypropylene, Mineral Filled
    Density 1.05 g/cm3
    Melt Flow Rate 10 g/10 min at 230°C/2.16 kg
    Mineral Filler Content 20%
    Tensile Strength 24 MPa
    Elongation At Break 30%
    Flexural Modulus 1800 MPa
    Notched Izod Impact Strength 8 kJ/m2 at 23°C
    Heat Deflection Temperature 110°C at 0.45 MPa
    Vicat Softening Temperature 150°C
    Molding Shrinkage 1.0-1.4%
    Flammability Rating HB
    Processing Method Injection Molding

    As an accredited Kingfa PP-11685,Impact Resistant PP,Mineral Filled factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-resistant woven bags, palletized with 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) Kingfa PP-11685 Impact Resistant PP Mineral Filled is palletized and loaded into 20′ FCL containers, securely stowed for safe ocean shipment.
    Shipping Shipping description: Kingfa PP-11685, Impact Resistant PP, Mineral Filled, is a non-hazardous polypropylene resin. Transport in dry, ventilated containers at ambient temperature using sealed, moisture-resistant bags or lined containers. Protect from moisture, sunlight, and contamination. Not regulated for transport; no UN number, hazard class, or placards required.
    Storage Store Kingfa PP-11685 in a cool, dry, well-ventilated area away from direct sunlight, heat, and open flames. Keep containers sealed to prevent moisture, dust, and contamination. Use stable shelving or pallets, avoid static buildup, and segregate from incompatible chemicals. Follow the SDS and local regulations; practice first-in, first-out and inspect containers regularly.
    Shelf Life Shelf life is typically 12–24 months when stored in original packaging, dry and cool, away from direct sunlight.
    Application of Kingfa PP-11685,Impact Resistant PP,Mineral Filled

    Kingfa PP-11685 enters automotive door trim carrier production as a mineral-filled impact PP whose exact filler type and melt flow rate require confirmation against the lot-specific certificate. In this class of mineral-filled impact polypropylene, filler loading commonly lies between 10 wt% and 25 wt%, and the resulting linear thermal expansion measured by ISO 11359-2 is reduced to between 4.0 × 10−5 K−1 and 6.5 × 10−5 K−1, compared with values above 1.0 × 10−4 K−1 for unfilled PP. For interior lower door trims, the exact colour concentrate addition is set between 2 wt% and 4 wt%, and a scratch-improving additive is introduced at 0.5–1.5 wt% on grained surfaces. Drying is mandated only when surface moisture exceeds 0.05%; the practice is 80 °C for 2–4 h in a desiccant hopper dryer with dew point at or below −40 °C. Melt temperature is controlled from 210 °C to 240 °C, mould temperature from 30 °C to 50 °C, injection moulding machine screw L/D ratio from 20:1 to 25:1, and screw back pressure below 1.0 MPa to avoid excessive filler attrition. Large door-carrier tools require sequential valve gating with gate diameter not less than 60% of nominal wall thickness. Terminal components include lower door panels, map pocket frames, and glove box carriers. Flame propagation is assessed under ISO 3795, with interior OEM limits commonly set below 100 mm/min at wall thickness above 2.0 mm. VOC and odour performance are evaluated under VDA 277 and VDA 270; the controlling variables are hot runner purge discipline and melt residence time. Continuous-use temperature at 1.8 MPa is defined by ISO 75-2/Ae, and for compounds of this class it frequently falls between 55 °C and 65 °C, which covers closed-cabin soak conditions but excludes direct under-bonnet exposure.

    What Limits Weld-Line Strength in Washing Machine Tub Housings?

    Washing machine outer tubs and balance-ring carriers impose a fatigue load case at hot-water contact and spin-cycle vibration. In mineral-filled impact PP, the weld line is the controlling defect because filler platelets orient parallel to flow and inhibit molecular interdiffusion at the knit front. With filler content above 15 wt%, weld-line tensile strength is often reduced to 45–60% of the unwelded value measured according to ISO 527-2. Consequently, the mould must be gated so that the knit line is shifted from bearing bosses and seal seats. Processing requires a melt temperature of 225–250 °C, mould temperature of 40–80 °C, and profiled injection speed of 80–120 mm/s at the screw tip. Holding pressure is set at 60–70% of first-stage injection pressure, with hold time established by gate freeze-off. The hot runner is purged at each shift start; retained melt of more than 10 min at temperature risks discolouration and impact loss. Detergent resistance is checked by immersion in a 0.5 wt% surfactant solution at 60 °C for 168 h under ISO 175; the acceptance threshold is typically Charpy notched impact strength of at least 4.0 kJ/m² when retested to ISO 179-1/1eA. Terminal products are washing machine outer tubs, balance-ring carriers, and base frame assemblies. For alkaline detergent exposure above 80 °C, calcium carbonate-filled grades are often preferred over talc-filled grades because interfacial degradation at talc-polymer boundaries can initiate microvoiding.

    Cordless power tool battery pack housings and charger shells are moulded from this material only where ductile drop behaviour and snap-fit creep resistance are jointly specified. Colour concentrate is dosed at 2–3 wt%; anti-static additive levels, when required, are kept below 0.5 wt% to avoid plate-out on mould surfaces. For lid-to-base interfaces, integral hinges are possible only at a local thickness of 0.25–0.40 mm, oriented along the primary flow vector. Gas traps at screw boss intersections require parting-line vent depths of 0.02–0.03 mm; insufficient venting produces diesel effect burning and surface staining. Wall thickness below 1.8 mm shifts the impact response toward brittle puncture under multi-axial loading, particularly at boss roots. Melt temperature is kept at 220–235 °C, mould temperature at 30–50 °C, melt cushion above 3 mm, and screw recovery speed below 100 rpm to limit shear heating. End-use compliance for battery pack housings references IEC 62133 for cell-containing systems and IEC 60068-2-31 for free-fall shock. Flame classification for standard mineral-filled impact PP is typically UL 94 HB at 1.5 mm or V-2 at thicker sections; if a V-0 rating is required, the application must move to a dedicated flame-retardant grade. Terminal products include battery housings for 4.0–12.0 Ah packs and charging cradle bases.

    Downstream segmentMelt temperature rangeMould temperature rangeDrying conditionSpecific processing boundary
    Automotive interior carrier210–240 °C30–50 °C80 °C for 2–4 h if moisture > 0.05%Gate diameter ≥ 60% of wall
    Washing machine tub housing225–250 °C40–80 °C80 °C for 2–4 hWeld line displaced from bearing bosses; hold pressure 60–70% of first stage
    Power tool battery pack housing220–235 °C30–50 °C80 °C for 2 h when requiredMelt cushion > 3 mm; screw recovery < 100 rpm
    Cold-chain logistics pallet215–240 °C25–45 °C80 °C for 4 hCycle time 75–150 s; wall thickness 8–12 mm
    Electrical distribution box210–230 °C30–80 °C80 °C for 2 hRib-to-wall ratio < 60%; boss OD ≥ 2× screw diameter
    Office seating component210–230 °C30–50 °C80 °C for 2 hTexture VDI 3400 24–30; reduced injection speed on grained surfaces

    When Cold-Chain Logistics Pallets Are Moulded from Mineral-Filled Impact PP

    Cold-chain logistics pallets encounter static racking loads up to 1,000 kg and dynamic forklift impact at −30 °C. Mineral-filled impact PP provides flexural modulus in the range 1,800–2,600 MPa under ISO 178, which supports load-bearing ribs without steel reinforcement. Blowing agent or chemical foaming at 0.3–0.8 wt% is sometimes used to reduce part mass and sink marks, but this lowers skin density and impact strength. Therefore, structural pallets are more frequently solid moulded at 8–12 mm nominal wall with gas counterpressure; cycle times range from 75 s to 150 s depending on mass. In low-temperature impact testing under ISO 6603-2 at −30 °C, ductile-to-brittle transition occurs at higher energy than for homopolymer PP, but multi-axial puncture remains the limiting criterion. Moisture drying at 80 °C for 4 h is applied to eliminate surface silver streaking. Terminal products are freezer-grade pallets, collapsible crates, dairy dollies, and meat industry trays. Compliance is governed by ISO 8611-1 for pallet performance and by food contact regulation EU 10/2011 when the article is intended for direct contact with unwrapped frozen food.

    Electrical Distribution Boxes, Creepage Paths, and UL 94 Classification

    Mineral-filled impact PP is used for low-voltage distribution enclosures where dimensional stability at contact-bridge mounting points is required but exposure to direct flame is limited. The filler reduces post-mould shrinkage in the flow direction to 0.5–0.8% and across flow to 0.7–1.0% after 48 h at 23 °C per ISO 294-4, which is lower than unfilled polypropylene and reduces terminal misalignment. Comparative tracking index falls with mineral loading; compounds in this family generally present CTI below 600 V under IEC 60112, so creepage distances are designed to the worst-case pollution degree 3. Glow-wire flammability index is measured per IEC 60695-2-11; typical mineral-filled impact PP will pass 650 °C glow-wire at 2.0 mm but not 850 °C unless separately stabilized. For junction boxes and fuse boxes, wall thickness is maintained between 2.0 mm and 3.0 mm, with rib-to-wall ratio below 60% and boss outer diameter at least 2× the screw diameter to avoid sink. Mould temperature of 30–50 °C is used; higher temperatures up to 80 °C improve surface finish but extend cycle. Terminal products include electrical junction boxes, terminal blocks, and DIN-rail enclosures.

    Office chair back shells and armrest carriers made from mineral-filled impact PP rely on resistance to cyclic torsion and sunlight colour retention. Weatherable colourants are added at 2–4 wt%, with hindered amine light stabilizer concentrate at 0.3–0.6 wt% for non-black visible parts; UV exposure is evaluated per ISO 4892-2 method A for 200 h to 400 h depending on OEM requirements. In seating applications, the moulded part is subjected to fatigue cycling in the 100,000-cycle range under BIFMA X5.1 using a 100 kg load, where the mineral-filled PP is selected for creep and base flexural fatigue. The mould cavity is textured to VDI 3400 grain depths between 24 and 30 to hide flow marks and filler orientation. Hot runner drops are placed away from visible surfaces; melt temperature is held at 210–230 °C, and injection speed is reduced in grained areas to avoid gloss differential. Terminal products are chair back frames, armrest shells, mechanism covers, and adjustable lumbar supports.

    Free Quote

    Competitive Kingfa PP-11685,Impact Resistant PP,Mineral Filled prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa PP-11685 is a mineral-filled impact-resistant polypropylene compound supplied by Kingfa Sci. & Tech. Co., Ltd., positioned for injection moulding applications that require a balance of low-temperature ductility, dimensional stability, and moderate stiffness. The material architecture combines a polypropylene copolymer matrix, a dispersed ethylene-propylene elastomer phase, and a mineral filler fraction—commonly talc—at loadings sufficient to reduce mould shrinkage to 0.6% to 0.9% in the flow direction and 0.8% to 1.2% transverse on 60 mm × 60 mm × 2 mm plaques moulded according to ISO 294-4:2018. Classification under ASTM D4101-17e1 and ISO 19069-2:2016 places materials of this architecture in the filled impact copolymer PP family when filler content exceeds 10% by weight. Product-specific melt flow rate, filler loading, and mechanical limits are not reproduced here because published data for the specific PP-11685 formulation is limited; lot certificates of analysis must be consulted before tooling design or part approval.

    What Processing Boundaries Govern Kingfa PP-11685 on Injection Moulding Lines?

    On reciprocating-screw injection moulding machines with screw diameters from 35 mm to 80 mm and L/D ratios between 20:1 and 25:1, compounds of this architecture are typically processed with a general-purpose nitrided screw and check ring. High-shear barrier screws improve filler dispersion but can raise melt temperature beyond 250 °C if back pressure exceeds 15 bar. Barrel temperature profiles generally rise from 180 °C in the feed zone to 220–240 °C at the nozzle, with melt temperature measured by insertion pyrometer in the range of 200–230 °C. Mould temperatures of 20–50 °C are common; higher mould temperatures up to 60 °C reduce flow-mark visibility and improve weld-line integrity but increase cycle time. Pre-drying at 80 °C for 2–4 h is recommended when surface moisture exceeds 0.1% by weight, particularly at relative humidity above 60%. Melt residence time should not exceed 10 min at 240 °C to avoid oxidative chain scission and elastomer coalescence. On production-scale 500 t to 1,200 t machines, hydraulic clamp force requirements typically range from 3.5 kN/cm² to 5.0 kN/cm² of projected area for thin-wall parts below 2.5 mm.

    Under tensile loading, comparative mechanical behaviour separates this grade from unfilled impact copolymer PP in flexural modulus, mould shrinkage, and low-temperature notched impact retention. For a 20 wt% talc-filled impact copolymer PP, flexural modulus measured per ISO 178:2019 typically lies between 1,800 MPa and 2,400 MPa, whereas an unfilled impact copolymer may fall between 800 MPa and 1,200 MPa. The trade-off appears in notched Charpy impact at 23 °C according to ISO 179-1:2010, where the filled class often reports 8–20 kJ/m² compared with 25–45 kJ/m² for many unfilled impact copolymers. At -30 °C, the gap narrows if the elastomer domain size is maintained below 1 µm through controlled compounding shear; poorly dispersed impact modifiers produce a coarse morphology that depresses the ductile-to-brittle transition temperature by 4–8 K per 1 µm increase in dispersed-phase diameter, as reported in fracture mechanics studies of rubber-toughened thermoplastics.

    When Mineral Filler Loading Shifts Ductile-to-Brittle Response

    Mineral filler loading is not a neutral diluent. As filler volume fraction increases from 10% to 30%, plane-strain fracture toughness of impact-modified PP typically passes through a maximum and then declines because interparticle distance becomes smaller than the elastomer cavitation zone. For injection-moulded tensile bars conditioned at 23 °C and 50% relative humidity, tensile elongation at break can fall from above 200% for unfilled impact copolymer to 15–40% at 25 wt% mineral filler. Weld-line strength is a critical threshold: at 30 wt% filler, weld-line tensile strength may retain only 50–60% of un-welded strength, whereas at 15 wt% filler retention can exceed 70%. Mould filling simulation using Autodesk Moldflow Synergy or Moldex3D should therefore locate knit lines away from high-tensile regions of brackets or covers.

    In automotive interior trims, seat back panels, centre console carriers, HVAC housings, appliance kick plates, power tool clamshells, and electrical enclosure liners, this product class is specified where part dimensions must remain stable across thermal cycling. Materials are typically tested for tensile strength per ISO 527-2:2012, flexural modulus per ISO 178:2019, heat deflection temperature per ISO 75-2:2013 at 0.45 MPa, and fogging behaviour according to DIN 75201:2011 or ISO 6452:2021. Local OEM specifications such as GMW14872 or VW 44045 may impose additional odour, emission, scratch resistance, and weathering limits. No inference should be drawn that Kingfa PP-11685 automatically satisfies any OEM specification without full part-level testing; published data for this specific configuration is limited, and approval must be confirmed against the applicable material specification.

    Comparative Performance Envelope for Filled Impact PP Grades

    The table below compares a reference envelope for mineral-filled impact PP compounds of this class with unfilled impact copolymer PP and short-glass-fibre reinforced PP. Kingfa PP-11685 lot-specific values may fall within or outside this envelope; the table is provided for material selection comparison only.

    PropertyTest methodUnfilled impact copolymer PP20 wt% mineral-filled impact PP20 wt% glass-fibre reinforced PP
    Tensile yield strengthISO 527-2:201218–25 MPa20–26 MPa60–90 MPa
    Flexural modulusISO 178:2019800–1200 MPa1800–2400 MPa3500–5000 MPa
    Notched Charpy at 23 °CISO 179-1:201025–45 kJ/m²8–20 kJ/m²6–12 kJ/m²
    Mould shrinkage, flow directionISO 294-4:20181.2–1.8%0.6–0.9%0.2–0.5%
    HDT at 0.45 MPaISO 75-2:201380–95 °C90–110 °C140–160 °C
    DensityISO 1183-1:20190.90–0.91 g/cm³1.04–1.10 g/cm³1.04–1.12 g/cm³

    The mineral-filled grade occupies an intermediate position between unfilled impact copolymer and glass-fibre reinforced PP. It is selected when dimensional stability and low warpage matter more than maximum tensile strength. Glass-fibre grades dominate in structural brackets where tensile strength and HDT are primary requirements; mineral-filled impact grades are used for covers, shrouds, and interior carriers where surface appearance and low anisotropic distortion are critical.

    Moisture, Residence Time, and Additive Incompatibilities

    Mineral fillers with high specific surface area adsorb moisture. If material is not pre-dried, steam during plastication produces silver streaks and splay on part surfaces. Polypropylene itself is not hydrolytically sensitive, but the filler-matrix interphase is affected by desorbed water. Processing with hygroscopic masterbatches containing carbon black or polar colorants requires stabilisation of hopper residence time. Addition of unmodified fatty acid amides above 0.3% should be avoided because these can migrate to the mould surface and increase ejector pin sticking. Halogen-free intumescent flame-retardant packages can raise melt viscosity by 20–40% and may require melt temperatures up to 230 °C. Reprocessing of regrind is generally limited to 20% by weight to avoid loss of impact strength and accumulation of mineral filler fines. Hot-runner systems with needle valve gates require injection speed profiling to prevent shear-induced melt fracture; gate shear rates above 100,000 s⁻¹ can cause surface delamination in filled PP. Moreover, unsaturated oils and certain metal stearates should be excluded from the formulation unless their interaction with the impact modifier has been tested under production conditions.

    Upon extended oven ageing at 150 °C for 500 h, notched Charpy impact of mineral-filled impact PP typically declines by 30–50% from the as-moulded value, with failure localised at the filler-matrix interface. For under-hood components, continuous service temperature should not exceed 100 °C unless validated by part-level thermal ageing; short-term excursions to 120 °C are possible but may cause dimensional relaxation. Resistance to engine oil, coolant, and windshield washer fluid should be tested according to ISO 175:2010 or the relevant OEM fluid immersion protocol. Polypropylene-based materials exhibit stress cracking in strong oxidising acids and chlorinated hydrocarbons; contact with these media is not recommended. UV exposure requires carbon black or hindered amine light stabiliser addition, typically evaluated under ISO 4892-2:2013 for 500–1,000 h xenon arc exposure. The grade should not be specified for continuous contact with strong oxidising acids, chlorinated solvents, or aromatic hydrocarbons without compatibility testing, because swelling and filler extraction may occur.

    How Does PP-11685 Differ from Glass-Fibre Reinforced Polypropylene?

    Glass-fibre reinforced PP provides higher stiffness and heat resistance but introduces anisotropic shrinkage, higher warpage, and lower surface quality. In contrast, mineral-filled impact PP retains lower aspect-ratio filler particles that distribute more uniformly in moulded parts. At equivalent 20 wt% reinforcement, a glass-fibre grade may show flexural modulus of 3,500–5,000 MPa versus 1,800–2,400 MPa for a mineral-filled impact grade, but the glass-fibre grade exhibits shrinkage as low as 0.2–0.5% in the flow direction and 0.6–1.0% transverse, producing a larger shrinkage anisotropy ratio. The mineral-filled grade is selected when lower warpage, better scratch resistance, or lower visibility of flow lines is required. Density of the two classes overlaps at 1.04–1.12 g/cm³, so no significant mass penalty exists. However, glass-fibre grades often fail notched impact tests with brittle fracture at -30 °C, while mineral-filled impact PP can retain Charpy values of 4–8 kJ/m² if the elastomer phase is optimised. In applications with complex flow paths, glass-fibre grades also generate higher mould wear and require hardened tool steel, whereas mineral-filled grades are less abrasive.

    Regulatory Assessment Matrix and Material Certifications

    The following compliance matrix identifies the regulatory and quality instruments commonly applied to mineral-filled impact PP compounds. Supplier lot declarations and site certificates remain mandatory; the list does not certify Kingfa PP-11685 by itself.

    InstrumentScopeVerification requirement
    EU RoHS Directive 2011/65/EU and Delegated Directive (EU) 2015/863Restriction of Pb, Hg, Cd, Cr(VI), PBB, PBDE, DEHP, BBP, DBP, DIBPSupplier declaration per lot
    REACH Regulation (EC) No 1907/2006SVHC content below 0.1% w/wArticle 33 communication
    FDA 21 CFR 177.1520Olefin polymers for food contact, when applicableManufacturer compliance letter
    ISO 9001:2015Quality management systemSite certificate
    IATF 16949:2016Automotive quality managementSite certificate if automotive grade
    ASTM D4101-17e1 / ISO 19069-2:2016Material classification and designationLot certificate