| HS Code | 831488 |
| Density | 1.04 g/cm³ |
| Melt Flow Rate | 10 g/10 min |
| Tensile Strength | 20 MPa |
| Tensile Elongation At Break | 50% |
| Flexural Modulus | 1200 MPa |
| Notched Izod Impact Strength | 35 kJ/m² |
| Heat Deflection Temperature At 1 8 Mpa | 105 °C |
| Vicat Softening Temperature | 145 °C |
| Molding Shrinkage | 1.3% |
| Flammability Rating | HB |
| Heat Resistance | High |
| Impact Resistance | High |
As an accredited Kingfa PP-350,High Heat Resistance, High Impact Resistance factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-350 High Heat Resistance, High Impact Resistance is supplied in 25 kg moisture-proof bags, palletized for industrial use. |
| Container Loading (20′ FCL) | Kingfa PP-350 high heat and impact resistant polypropylene resin, securely loaded and stowed in a 20-foot FCL container for export. |
| Shipping | Kingfa PP-350, High Heat Resistance, High Impact Resistance, is shipped as a non-hazardous polypropylene compound in sealed moisture-barrier bags, octabins, or bulk containers. Keep dry, cool, and away from direct sunlight/ignition. Follow the SDS and local regulations; generally not regulated for transport. |
| Storage | Store Kingfa PP-350 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep containers closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged storage near ignition sources, and follow the manufacturer’s SDS and local regulations for safe handling and emergency procedures. |
| Shelf Life | Shelf Life: Approximately 24 months when stored dry, cool, and protected from direct sunlight in sealed original packaging. |
Kingfa PP-350 is fed as-supplied into automotive under-hood air intake programs when the part is shielded from the exhaust manifold radiation envelope and the service temperature ceiling is 115 °C. Converter qualification follows ISO 16750-4:2010 thermal shock cycling from −40 °C to 115 °C with a 30 s transfer time and 2 h dwell. Processing on a 450-tonne hydraulic injection molding machine running a 4-cavity tool sets barrel temperatures at 230 °C rear, 235 °C middle, 240 °C front, and 245 °C nozzle. Mold temperature is maintained at 35–50 °C to balance surface gloss and crystallization; a mold surface temperature below 20 °C reduces impact through rapid quench and increases orientation at gate restrictions. Injection pressure between 70–95 MPa is adjusted to achieve 95% fill before holding pressure of 45–55 MPa is applied for 4–7 s. Back pressure is kept at 0.5–1.5 MPa to avoid screw slip without over-shearing the impact modifier phase. Drying at 80 °C for 2–4 h is applied only when silo storage RH exceeds 60%; otherwise moisture content below 0.03% by Karl Fischer permits direct melt processing. Regrind from sprues and runners is allowed at a maximum ratio of 15 wt% because higher recyclate fractions reduce Charpy impact at −30 °C. Terminal components include air cleaner housings, resonator brackets, horn brackets, and engine cover standoffs. Impact acceptance is evaluated by ISO 179-1/1eA Charpy notch tests at 23 °C and −30 °C, with converter-specific acceptance commonly set between 6–10 kJ/m² at −30 °C for ductile failure after 500 h heat aging at 120 °C, although published data for this specific grade under OEM-specific cycles is limited.
In battery pack structural components, Kingfa PP-350 is confined to non-current-carrying parts such as busbar support rails, module end plates, and cell holder frames. Direct contact with cell tabs or busbars is not permitted because the unfilled impact copolymer is not classified for live-part insulation at pack voltage. Thermal cycling qualification typically references ISO 16750-4:2010 from −40 °C to 115 °C with 2 h soaks and 30 s transfer, while mechanical shock screening follows IEC 62660-2:2018 or converter-specific acceleration pulses. Processing on 250–350 tonne electric injection molding machines uses a hot runner with sequential valve gates to shift weld lines away from snap-fit retention features. Melt temperature is held at 230–245 °C, mold temperature at 30–50 °C, and cooling time at 12–18 s for a 3 mm nominal wall. A carbon black masterbatch is added at 0.5 wt% for laser marking; higher loadings above 1.0 wt% degrade the low-temperature impact response. Clean runner regrind is limited to 5–10 wt% and requires lot-by-lot ISO 179-1/1eA verification at −30 °C after thermal aging. Terminal products include retention bars, end plates, and busbar support rails that must carry mechanical compression loads without creep to the electrical stack.
| Test method | Standard / clause | Condition | Screening acceptance |
|---|---|---|---|
| Charpy notched impact | ISO 179-1/1eA | −30 °C, single-edge notch | ≥ 6 kJ/m² |
| Tensile modulus | ISO 527-2:2012 | 23 °C, 1 mm/min | ≥ 1200 MPa |
| Heat deflection temperature | ISO 75-2:2013 method B | 0.45 MPa, edgewise | ≥ 95 °C |
| Flammability | UL 94 | 1.5 mm thickness | HB minimum for non-live structural parts |
Circulating pump volutes expose Kingfa PP-350 to continuous coolant contact only after a 1,000 h extractables and volume swell screen in 50:50 ethylene glycol–water at 105 °C per ISO 1817:2022. The fluid boundary condition is a hot coolant loop at 95–105 °C with intermittent excursions to 115 °C during stagnation. A converter adds 15 wt% high-purity talc masterbatch to the virgin pellets by gravimetric feeder; deviation beyond ±0.5 wt% shifts heat deflection and cycle time. The melt is processed at 235–245 °C with a cold runner gate diameter at least 60% of the part wall thickness to avoid shear-induced degradation at the entry. Mold temperature is set at 40–60 °C to grow sufficient crystalline fraction for coolant resistance. Hot runner residence time is limited to 5 min and hot runner temperature to 250 °C because longer residence time creates molecular weight loss that shows as a fall in ISO 179-1/1eA Charpy impact after 168 h coolant immersion. Terminal components are circulating pump volutes, impeller housings, drain plugs, and expansion tank shrouds. The grade is not recommended for potable water contact unless the converter certifies the finished part to NSF/ANSI 61 or KTW; published data for this specific grade under potable water migration protocols is limited.
For indoor electrical enclosure frames molded from Kingfa PP-350, a UL 746B relative thermal index with impact governs. The grade does not carry an unconditional yellow card for all colors and thicknesses; each color concentrate and wall thickness must be tested by the compounder or converter to establish the RTI Mechanical with Impact. Components such as smart meter internal structural frames, terminal junction box bases, and low-voltage connector housings are processed with melt temperatures of 220–235 °C and mold temperatures of 20–40 °C. Fast injection speeds of 80–120 mm/s are used to preserve impact through long flow paths. An antistatic masterbatch is added at 0.5–1.0 wt% where dust attraction and static discharge on sealed meter enclosures require surface resistivity below 10^12 Ω per IEC 62631-3-2. The material is not suitable for enclosures requiring UL 94 V-0 at 1.5 mm or glow-wire ignition above 650 °C per IEC 60695-2-11 unless an FR barrier or cover is specified. Long-term thermal aging data for heat-stabilized impact copolymer PP is shown in the screening matrix below; values are representative not lot-specific certification.
| Property | Method | Aging condition | Retention range |
|---|---|---|---|
| Tensile strength | ISO 527-2 | 1000 h at 120 °C in air | 88–93% |
| Charpy notched impact | ISO 179-1/1eA | 1000 h at 120 °C in air | 65–72% |
| Flexural modulus | ISO 178:2019 | 1000 h at 120 °C in air | +8% to +14% |
Gas-assisted injection molding of power tool housings shifts the limiting variable from melt temperature to solidification rate in thick boss-to-wall transitions. Kingfa PP-350 is run unfilled to retain impact, with melt temperature at 230–240 °C and mold temperature at 25–40 °C. Gas injection pressure is set at 10–15 MPa with a delay of 0.3–0.5 s after filling, and gas channel diameter is maintained above 4 mm to prevent premature freezing. In closed-loop material handling, sprues and runners are recycled up to 20 wt%; if drop-weight impact after conditioning at 70 °C for 4 h falls below the converter-specific criterion, regrind is reduced to 10 wt% and the part is retested. Terminal products include angle grinder gearcase covers, drill motor housings, and circular saw blade guards. Compliance testing follows IEC 62841-1 mechanical strength requirements for power tool housings, but the material itself is qualified by the tool manufacturer because the final overmold and screw boss design control the failure mode.
Under hot alkaline detergent splash and vibration in washing machines, Kingfa PP-350 is qualified in base frame brackets and dryer bearing housing supports where dimensional stability after hot-wet cycling is critical. The converter dry-blends 20 wt% talc masterbatch into the press feed to reduce creep and increase heat deflection; the letdown is controlled by gravimetric dosing within ±0.5 wt%. Melt temperature is set at 220–240 °C and mold temperature at 30–50 °C. Because the talc-filled melt is more viscous than the unfilled grade, holding pressure is raised to 45–55 MPa and packing time extended to 8–12 s for a 3 mm wall. Creep modulus is measured per ISO 899-2:2020 at 60 °C and 100 h; acceptance requires a creep modulus above 1500 MPa but published data for this specific grade in detergent solution is limited. Internal non-current-carrying parts are tested to IEC 60335-1 clause 30.2 glow-wire; if the end-use standard requires glow-wire ignition above 650 °C, the material is not selected without a flame-retardant barrier. Terminal components include base frame brackets, counterweight supports, and pump mounting plates.
Geothermal heat pump condensate drain pans expose Kingfa PP-350 to continuous neutral-pH water at 55–70 °C without hydrolytic degradation of the polypropylene backbone. A 2 wt% carbon black UV stabilization package is added for outdoor access covers exposed to indirect sunlight; unblended natural or light-colored grades are not suitable for long-term outdoor exposure without a UV stabilizer masterbatch. Injection molding uses melt temperature 220–235 °C and mold temperature 20–45 °C; wall thickness is kept between 3–5 mm to provide screw boss stiffness and impact resistance. Dimensional stability is evaluated per ISO 294-4:2018 post-molding shrinkage; values above 1.8% in the transverse direction indicate excessive orientation at the gate. Terminal products are drain pans, condensate trays, access covers, and isolated mounting brackets. Compliance relies on RoHS 2011/65/EU and REACH SVHC screening; no food-contact or potable-water claim is made for this grade.
Competitive Kingfa PP-350,High Heat Resistance, High Impact Resistance prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-350 is a high-heat-resistant, high-impact-resistant polypropylene compound supplied as a pelletized injection-moulding grade. The designation is associated with a controlled-rheology nucleated impact copolymer in which a discrete ethylene-propylene elastomer phase is dispersed in a high-crystallinity polypropylene matrix. The grade is specified for semi-structural components requiring continuous heat resistance above 100 °C and impact resistance below -20 °C. Published data for this specific configuration is limited; representative values in this document are drawn from publicly available industrial data for unfilled high-heat high-impact polypropylene impact copolymers and are not a substitute for Kingfa lot certification data.
Because the grade is an impact copolymer, its melt viscosity is regulated during compounding by controlled-rheology chain scission in a co-rotating twin-screw extruder. The screw profile typically includes two dispersion zones with kneading blocks and a downstream distributive mixing section. This is normally carried out on a co-rotating twin-screw extruder with an L/D ratio of 40:1 to 48:1 and a die plate strand pelletizer. Insufficient dispersion leaves elastomer domains above 2–5 µm, which reduces low-temperature notched impact and increases lot-to-lot variance. This morphology requirement is more decisive than melt flow rate alone in determining field performance of the moulded part.
Property windows for the class are summarized in Table 1. These are representative values, not certified lot specifications.
| Property | Test method | Representative range |
|---|---|---|
| Density | ISO 1183-1:2019 | 0.90–0.91 g/cm³ |
| Melt mass-flow rate at 230 °C/2.16 kg | ISO 1133-1:2022 | 10–30 g/10 min |
| Tensile stress at yield | ISO 527-2:2012, 50 mm/min | 25–30 MPa |
| Tensile strain at yield | ISO 527-2:2012, 50 mm/min | 4–7 % |
| Flexural modulus | ISO 178:2019, 2 mm/min | 1500–2500 MPa |
| Notched Charpy impact at 23 °C | ISO 179-1:2010, type 1 edgewise notch A | 15–40 kJ/m² |
| Notched Charpy impact at -20 °C | ISO 179-1:2010, type 1 edgewise notch A | 5–10 kJ/m² |
| Heat deflection temperature at 0.45 MPa | ISO 75-2:2013, method B flatwise | 110–130 °C |
| Heat deflection temperature at 1.8 MPa | ISO 75-2:2013, method A flatwise | 60–75 °C |
| Vicat softening temperature | ISO 306:2022, method A50 | 140–155 °C |
These class-representative values indicate that Kingfa PP-350 is positioned above a standard impact copolymer in thermal resistance while retaining sufficient impact strength for cold start conditions. A direct property comparison against mineral-filled grades is provided in Table 2.
In production-scale injection moulding of Kingfa PP-350, a barrel temperature profile from feed throat to nozzle of 200 °C, 210 °C, 220 °C, 230 °C, 230 °C, 235 °C is a typical starting point. The mould temperature should be maintained at 30–60 °C for cycle-time stability; higher mould temperatures up to 80 °C improve surface gloss and weld-line crystallization but reduce the notched impact contribution of the elastomer phase if the cooling rate is too low. Screw rotation speed of 80–120 rpm and back pressure of 0.5–1.0 MPa are commonly used for dispersion and melt homogeneity. Desiccant drying at 80–90 °C for 2–4 h is recommended only if pellet moisture exceeds 0.05 %; storage in unopened bags below 60 % relative humidity normally does not require pre-drying.
Capillary rheometry of comparable impact copolymers at 230 °C gives a shear viscosity of 150–250 Pa·s at 1000 s⁻¹ and 800–1200 Pa·s at 100 s⁻¹. The shear-thinning index between 100 s⁻¹ and 1000 s⁻¹ is approximately 3–5, supporting thin-wall filling but requiring adequate gate size to avoid excessive pressure drop. At the low-shear flow front, viscosity increases rapidly; this causes difficulty in moulding ribs with thickness below 0.8 mm unless flow length is restricted. Weld-line strength is controlled primarily by melt-front temperature. For parts with multiple gates, the melt front should remain above 180 °C for effective elastomer bridging; below that threshold, notched Charpy impact at the weld line can fall to less than 40 % of the base material value.
Hot runner systems should use externally heated manifolds with independently controlled nozzle temperatures. Internal hot runner geometries with dead spots can cause localized degradation of the peroxide-tuned molecular weight distribution, generating black specks and reducing impact strength. Gate size below 0.8 mm may cause shear heating above the recommended melt temperature and produce gate blush; enlarging the gate to 1.2 mm or reducing injection velocity usually corrects the defect. Production-scale moulding in wall thicknesses of 2.5–3.5 mm requires a clamp force of 4–6 kN/cm² of projected area because cavity pressures may reach 50–80 MPa.
At 30 °C mould temperature, the surface layer freezes before the core, producing a thicker oriented skin with reduced elastomer deformation in the outer layer. At 80 °C, the skin is thinner and the core spherulite size increases, which raises stiffness slightly but may reduce low-temperature impact if the spherulites exceed 8–12 µm. Therefore, mould temperature for Kingfa PP-350 is often constrained to 40–60 °C when both dimensional stability and low-temperature impact are required. On a production line, batch-to-batch variance in melt flow rate should be monitored by laboratory MFR per ISO 1133-1:2022; a shift of more than 5 g/10 min from the qualification lot indicates a change in the controlled-rheology ratio or elastomer content and should trigger a moulding trial before release.
Regrind can be used up to 30 % in non-appearance parts if the regrind is dry, not contaminated with oil, and not exposed to 240 °C for extended residence. Repeated recycling beyond three passes tends to reduce notched impact at -20 °C because the elastomer phase may crosslink or coalesce; published data for this specific configuration is limited.
To achieve high heat resistance, the polypropylene matrix is nucleated with a sorbitol-based clarifying/nucleating agent or a phosphate ester nucleant. Nucleation increases the crystallization temperature from approximately 110 °C for non-nucleated PP to 120–130 °C for the nucleated grade, allowing parts to be demoulded earlier and increasing stiffness above 100 °C. The trade-off is a reduction in spherulite size and an increase in crystalline fraction; the matrix alone becomes less tough, and a fine elastomer dispersion with domain sizes below 1 µm is required to restore impact strength. If the elastomer domains exceed 2–5 µm, the notched Charpy impact at -20 °C falls sharply because rubber cavitation sites are insufficient.
Long-term heat ageing of Kingfa PP-350 is governed by the consumption of hindered phenolic antioxidants and phosphite processing stabilizers. In forced-air oven ageing per ISO 188 at 135 °C for 500 h, comparable nucleated impact copolymers may retain more than 80 % of the initial tensile stress at yield, provided the stabilizer package contains adequate high-temperature antioxidants and acid scavengers. For continuous exposure above 120 °C, a heat-stabilized lot is mandatory. Without heat stabilization, polypropylene undergoes oxidative chain scission, surface cracking, and loss of notched impact after as little as 100–200 h at 135 °C, depending on part thickness and airflow. The oxidative induction time measured by differential scanning calorimetry per ISO 11357-6 should be above 20 min for heat-resistant grades; lower values indicate inadequate stabilizer loading or contamination.
Thermomechanical behaviour of PP compounds is evaluated by dynamic mechanical analysis. The elastomer phase contributes a secondary relaxation below -30 °C, while the polypropylene matrix glass transition appears near 0–10 °C. This means the notched impact transition from ductile to brittle depends on the elastomer domain size and interparticle distance. For a high-heat high-impact grade such as Kingfa PP-350, the ductile-to-brittle temperature is typically below -20 °C, but this value is sensitive to mould cooling rate and weld-line orientation.
Automotive air intake ducts and resonator assemblies moulded from Kingfa PP-350 are subjected to engine-bay heat soak at 110–120 °C and cold-impact loading at -30 °C. In this application, the material is specified because it avoids the brittleness of unfilled PP homopolymer and the density penalty of talc-filled PP. To achieve acceptable burst strength at operating temperature, part design should use a minimum wall thickness of 2.5 mm and avoid sharp internal radii below 0.5 mm at the junction of the duct and the mounting bracket. Appliance structural brackets and washing machine balance rings require dimensional stability under cyclic humidity and exposure to alkaline detergent solution at 60–90 °C. Resistance to stress cracking in this environment should be verified according to ISO 22088-2 or a bespoke constant-strain immersion test; published data for this specific configuration is limited.
In automotive cooling fan shrouds, the grade must survive hot airflow at 105 °C and stone impact at -20 °C. Parts are often moulded in two-cavity hot runner tools with direct edge gates; hot runner nozzle temperature should not exceed the melt injection temperature by more than 10 °C to avoid premature degradation. For vibration-welded appliance housings, a weld amplitude of 0.8–1.2 mm, a weld pressure of 2–4 MPa, and a holding time of 3–5 s are typical starting points for PP copolymers, but component-level validation is required because published data for this specific configuration is limited.
Compared with a conventional impact copolymer of similar melt flow rate, the high-heat package of Kingfa PP-350 shifts the heat deflection temperature at 0.45 MPa upward by approximately 10–20 °C, while retaining notched Charpy values above 15 kJ/m² at 23 °C. A 20 % talc-filled PP raises flexural modulus to 2500–4000 MPa but reduces notched Charpy at -20 °C to 3–5 kJ/m² and increases density to 1.05–1.10 g/cm³. The comparative profile is shown in Table 2.
| PP type | Flexural modulus | Notched Charpy impact at 23 °C | Heat deflection temperature at 0.45 MPa | Density |
|---|---|---|---|---|
| Kingfa PP-350 class | 1500–2500 MPa | 15–40 kJ/m² | 110–130 °C | 0.90–0.91 g/cm³ |
| PP homopolymer | 1200–1800 MPa | 3–6 kJ/m² | 90–105 °C | 0.90–0.91 g/cm³ |
| Standard impact copolymer | 900–1400 MPa | 10–30 kJ/m² | 95–110 °C | 0.90–0.91 g/cm³ |
| 20 % talc-filled PP | 2500–4000 MPa | 5–15 kJ/m² | 125–140 °C | 1.05–1.10 g/cm³ |
Substituting Kingfa PP-350 into an existing tool designed for standard PP impact copolymer may require changes to gate size and venting. The moulding compound should be processed at the same or slightly higher melt temperature because the nucleated high-crystallinity matrix freezes at a higher temperature. If the tool has thin-wall sections below 1.5 mm, injection speed should be increased to 150–300 mm/s depending on cavity geometry to prevent short shots and flow hesitation lines. In an existing tool with undersized gates below 1.0 mm, the expected pressure drop can exceed 80 MPa, causing gate bloom and degradation. A pressure drop study using cavity pressure sensors near the gate is recommended before series production.
Shrinkage behaviour differs from standard impact copolymer. Mould shrinkage for this class typically lies in the range 1.2–1.6 % parallel to flow and 1.4–1.8 % perpendicular to flow. The difference between parallel and perpendicular shrinkage produces warpage in large flat parts; design validation should follow ISO 294-4 after 24 h conditioning at 23 ± 2 °C and 50 ± 5 % relative humidity. A short shot study and a moulding area diagram are required to establish a robust process window. For parts with weld lines, the minimum process window is often no wider than ±5 °C in melt temperature because the impact strength at the weld line falls rapidly when the melt front temperature falls below 180 °C.
Regulatory compliance documentation for Kingfa PP-350 is expected to address RoHS Directive 2011/65/EU Annex II restricted substances and REACH Regulation 1907/2006 SVHC candidate list disclosure. For applications involving food contact, compliance with FDA 21 CFR 177.1520 for olefin polymers must be confirmed for the specific grade and lot; not all high-heat PP compounds are acceptable for direct food contact because of their additive formulations. The unmodified grade is not inherently flame retardant; if the application requires a UL 94 V-0 or V-2 rating, a flame-retardant variant is required, as unmodified PP typically meets only UL 94 HB.
Kingfa PP-350 should not be combined with copper-based colorants or certain metal deactivators without verifying thermal stabilizer compatibility, because transition metals can catalyze oxidative degradation of polypropylene. Contact with strong oxidizing acids, long-chain hydrocarbons, and aromatic solvents should be avoided unless chemical resistance testing per ISO 175 shows acceptable property retention. For powertrain fluids at elevated temperature, component validation should include volume swell and tensile property retention after immersion in the specific fluid, because polypropylene may swell in synthetic engine oil and transmission fluid. For applications comparing against polyamide 66 or PBT, the PP compound offers lower density and lower moisture absorption but has lower continuous use temperature; it is not a direct substitute for underhood parts requiring oil resistance above 120 °C or peak temperatures above 150 °C.
In exterior rearview mirror brackets and under-shield mounting brackets, prolonged exposure to calcium chloride road de-icing salts can accelerate stress cracking of PP copolymers. Parts should be conditioned and subjected to a constant-strain test in 10 % calcium chloride solution at 60 °C for 500 h; the acceptance criterion should be no visible surface cracks at 10× magnification and retention of at least 70 % of the initial notched Charpy impact. Published data for this specific configuration is limited; therefore, component-level validation is necessary before release.