| HS Code | 617258 |
| Polymer Type | Polypropylene Copolymer |
| Filler Type | Mineral |
| Density | 1.05-1.15 g/cm³ |
| Melt Flow Rate | 9-12 g/10 min |
| Tensile Strength | 24-30 MPa |
| Elongation At Break | 15-30% |
| Flexural Modulus | 2000-3000 MPa |
| Notched Izod Impact Strength | 3-6 kJ/m² |
| Heat Deflection Temperature | 100-120 °C |
| Vicat Softening Temperature | 145-155 °C |
| Molding Shrinkage | 0.8-1.5% |
| Ul 94 Flammability Rating | HB |
As an accredited Kingfa PP-35090,PP Copolymer, Mineral Filled factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-35090 PP Copolymer, Mineral Filled is packaged in 25 kg moisture-proof, polyethylene-lined bags, palletized and clearly labeled. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Kingfa PP-35090, PP Copolymer, Mineral Filled in 25 kg bags, palletized, shrink-wrapped and secured for ocean transport. |
| Shipping | Kingfa PP-35090, PP copolymer mineral filled, is shipped as non-hazardous polymer pellets in moisture-barrier bags or bulk containers. Keep dry and away from direct sunlight, heat, and contamination. Use normal freight; no special dangerous-goods classification applies. Store in a cool, ventilated area and handle with standard industrial precautions. |
| Storage | Store Kingfa PP-35090 (mineral-filled PP copolymer) in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and incompatible chemicals. Keep original containers sealed to prevent moisture and contamination; avoid prolonged UV exposure and physical damage. Use first-in/first-out stock rotation and follow the supplier safety data sheet and local regulations. |
| Shelf Life | Typical shelf life is 24 months when stored dry, below 30°C, away from sunlight and moisture in original packaging. |
Kingfa PP-35090 is a mineral-filled impact-copolymer polypropylene supplied as a pelletized injection-moulding compound. Compounding on a 40:1–44:1 L/D co-rotating twin-screw extruder with side-fed mineral filler and vacuum devolatilization at −0.08 MPa provides filler dispersion; strand pelletizing is preferred over underwater pelletizing because mineral-filled strand surfaces embrittle during low-temperature cutting. The material requires no drying when water content remains below 0.1 wt%, but storage at 60–75% RH beyond 30 days should be corrected by 80–85 °C forced-air drying for 2–3 h. Because the specific filler loading for this grade should be confirmed by ISO 3451-1 ash content, the following scenarios state only industrially observed windows for mineral-filled PP copolymers rather than grade-specific certificate values.
Mineral-filled PP copolymer is used in lower interior trim because the plate-like filler reduces coefficient of linear thermal expansion from approximately 100–120 µm/(m·°C) for neat PP to 55–75 µm/(m·°C) in the filled compound, depending on filler orientation and gate geometry. This reduction prevents fastener pop-out and acoustic squeak when the substrate is assembled with metal clips and adjacent glass-reinforced ABS or PC/ABS brackets. On production tools, the main failure mode is differential shrinkage between thick bosses and adjacent 2.0–2.5 mm nominal walls; boss wall thickness should not exceed 50–60% of adjacent wall thickness. Weld lines generated at gate boundaries cause notch-sensitive impact loss at cold temperatures, so sequential valve gating or cashew gates are used to reduce visible weld line depth, but they require injection velocity profiling to prevent jetting through restricted gate lands.
Compliance is anchored to vehicle interior air and fire requirements: FMVSS 302 / ISO 3795 for horizontal burning, VDA 277 for total volatile organic compounds, DIN 75201-B for fogging condensate, and REACH Annex XVII restrictions for polycyclic aromatic hydrocarbons. The compound is used at 100 wt% as supplied. In programs where the same tool also runs unfilled PP, a letdown of up to 15 wt% virgin impact copolymer is used to improve low-temperature hinge ductility, but exceeding this limit shifts CLTE and evaporative emission behaviour; recertification under VDA 277 is required. Injection moulding is performed with clamp force from 600–1200 t, a 20:1–24:1 L/D screw, 2.0:1–2.5:1 compression ratio, melt temperature 200–230 °C, mould temperature 20–50 °C, holding pressure 50–70 MPa, and cooling time 25–40 s for 2.5 mm walls. Terminal product types include lower instrument panel substrates, B-pillar lower trims, door lower carriers, seat side shields, and rear quarter trim covers.
Non-cosmetic appliance structural brackets in washing machines and refrigerators are moulded from mineral-filled PP copolymer where low water uptake and vibration damping are required; the filler reduces creep under continuous tub loading while the copolymer phase retains low-temperature ductility during shipping at -20 °C. Compliance is assessed under IEC 60335-1 clause 30.2 for resistance to fire, and IEC 60335-2-24 for refrigerating appliance electrical safety; food-contact status is available only if the specific compound formulation is listed under 21 CFR 177.1520. The compound is processed at 200–220 °C melt temperature and 45–60 MPa holding pressure; mould temperatures are kept at 30–50 °C to avoid gloss differences on visible surfaces. Addition ratio is 100 wt% as supplied, with colour masterbatch metered at 2–3 wt% at the feed throat rather than manually mixed. Terminal product types include washing machine bottom covers, dryer front air ducts, refrigerator hinge brackets, and dishwasher base frames.
| Application category | Standard / code | Clause or test method | Operational boundary |
|---|---|---|---|
| Automotive lower interior trim | FMVSS 302, ISO 3795, VDA 277, DIN 75201-B | Horizontal burn, VOC, fogging | Dilution not above 15 wt% without recertification |
| Appliance structural brackets | IEC 60335-1, IEC 60335-2-24 | Clause 30.2, refrigerating appliance safety | Melt temperature not above 220 °C to avoid odour |
| Low-voltage enclosures | IEC 60670-1, IEC 60529, UL 94 HB | Enclosure safety, ingress protection, horizontal burn | Not for live parts; impact modifier limited to 8 wt% |
| HVAC blower scrolls | EN 60335-2-40, UL 94 HB, ISO 178 | Flexural modulus, horizontal burn | Avoid amine-based antistats; plate-out risk |
| Office seating shells | ANSI/BIFMA X5.1, ISO 899-2 | Structural durability, creep after 1000 h | Recycled fraction limited to 10 wt% |
| Outdoor tool housings | ISO 4892-2, ISO 179-1/1eA, ISO 527-2 | Xenon weathering, Charpy at -20 °C, tensile | Melt temperature not above 230 °C |
Low-voltage electrical enclosure applications introduce a different set of constraints when ABS is replaced by mineral-filled PP copolymer. The unmodified mineral-filled grade is generally classified UL 94 HB and must not be used as the sole insulation of live parts. Replacement of ABS by mineral-filled PP reduces specific gravity and water absorption but introduces anisotropic mould shrinkage in the range of 0.8–1.2% in flow direction and 1.0–1.5% transverse, measured by ISO 294-4, which changes lid fit dimensionally across long gate paths. Tooling should place the gate at the thickest boss or side wall, maintain nominal wall stock at 2.3–2.8 mm, and use latch ribs with 0.25–0.4 mm interference rather than larger interference values common for ABS; otherwise latch fingers fracture during repeated opening due to lower notched impact strength.
Compliance for junction boxes is established through IEC 60670-1; enclosure ingress protection is tested under IEC 60529 when a gasket seat is moulded into the cover groove. Comparative tracking index measured by IEC 60112 should be monitored because mineral fillers may reduce surface tracking resistance relative to neat PP, and the compound is not suitable for creepage distances governed by IEC 60664-1 without verification. Formula addition for drop-test improvement is an impact-modifier masterbatch at 3–6 wt%. Additions above 8 wt% cause measurable loss in load-bearing capability and may shift comparative tracking index outside the class required for live parts; published data for this specific grade configuration is limited. Injection moulding parameters include melt temperature 210–230 °C, mould temperature 30–50 °C, holding pressure 55–75 MPa, and dimensional stabilisation at 23 °C / 50% RH for 24 h before coordinate measurement. Terminal product types are wall-mounted junction boxes, busbar support housings, DIN rail adaptor bases, and meter enclosure internal covers.
Centrifugal blower scrolls and air guide vanes in heat-recovery ventilation units are moulded from mineral-filled PP copolymer where the flatness of the inlet venturi seat is critical for backflow control. Compliance is linked to EN 60335-2-40 for motor-compressor and heating-system safety, UL 94 HB, and ISO 178 flexural modulus measurement for creep-resistant mounting flanges. The compound is injection moulded at melt temperature 200–220 °C, mould temperature 20–40 °C, holding pressure 50–65 MPa, and cycle time 40–65 s for 2.5 mm walls. If static discharge is an issue on unfilled PP parts, an antistatic masterbatch at 0.5–1.0 wt% is added; amine-based antistats should be avoided because they can cause plate-out on tool steel and odour in the air stream. Terminal product types are centrifugal blower scrolls, ventilation flaps, air guide vanes, condensate drip trays, and fan volute covers.
In cantilevered office seating applications, structural shells and ergonomic back shells use mineral-filled PP copolymer when the design requires a rigid support beneath polyurethane foam without the weight of glass-filled nylon. Compliance is driven by ANSI/BIFMA X5.1 structural durability and ISO 899-2 creep modulus after 1000 h at 23 °C; flammability testing for upholstered seating is handled by the finished article standard, not the shell alone. A closed-loop recycled mineral-filled PP fraction of 5–10 wt% is added to the virgin compound only where the recycle stream has been tested for ash content under ISO 3451-1 and melt flow under ISO 1133-1; higher addition rates produce visible flow lines at the shell rim. Injection compression moulding is preferred over straight injection because it reduces orientation-induced warpage and demoulding stress. Terminal product types are chair back shells, seat pan bases, sled chair frames, and workstation screen supports.
Outdoor power equipment shrouds and handheld tool housings specify mineral-filled PP copolymer where fuel splash resistance and low-temperature crack resistance are required without the added mass of glass-filled engineering resins. Compliance is anchored to ISO 4892-2 xenon-arc weathering, ISO 179-1/1eA Charpy notched impact at -20 °C, and ISO 527-2 tensile properties for snap-fit louvre retention. A UV stabiliser masterbatch or carbon black masterbatch is added at 1–2 wt%; the specific UV package must be matched to the OEM colour tolerance and rapid-cycling mould temperature settings. Injection moulding is performed at melt temperature 200–215 °C, mould temperature 15–35 °C, and holding pressure 45–60 MPa; excessive melt temperature above 230 °C degrades the impact copolymer phase and can raise post-mould warpage due to oriented mineral filler acting as a nucleating surface. Terminal product types include lawn mower engine shrouds, string trimmer motor housings, chainsaw covers, portable generator control panels, and brush cutter debris guards.
Competitive Kingfa PP-35090,PP Copolymer, Mineral Filled prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-35090 is a pelletised polypropylene copolymer compound modified with mineral filler. The grade designation identifies a copolymer matrix rather than a homopolymer matrix, indicating that ethylene-propylene comonomer is present to retain impact resistance after the mineral filler raises stiffness, thermal deflection temperature, and dimensional stability. The material is normally characterised by melt mass-flow rate under ISO 1133-1:2022 at 230 °C with a 2.16 kg piston load, density under ISO 1183-1:2019, tensile stress at yield under ISO 527-1:2019 / ISO 527-2:2012, flexural modulus under ISO 178:2019, heat deflection temperature under ISO 75-2:2013, notched Charpy impact under ISO 179-1:2010, and mould shrinkage under ISO 294-4:2018. The exact mineral type, filler mass fraction, particle size distribution, and surface treatment are manufacturer-controlled variables. Independent third-party data for this exact grade is limited; therefore the class-typical ranges below are derived from mineral-filled PP copolymer systems with comparable filler chemistry and are not a substitute for the lot-specific Kingfa certificate of analysis, which governs final design limits and incoming inspection.
| Property | Test method | Unfilled PP copolymer | Mineral-filled PP copolymer class | 20 wt% glass fibre-reinforced PP |
|---|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.89–0.91 g/cm³ | 1.03–1.13 g/cm³ | 1.03–1.08 g/cm³ |
| Flexural modulus | ISO 178:2019 | 900–1200 MPa | 1800–2600 MPa | 2500–3500 MPa |
| Tensile stress at yield | ISO 527-2:2012 | 20–28 MPa | 22–28 MPa | 55–75 MPa |
| Notched Charpy impact, 23 °C | ISO 179-1:2010 | 8–20 kJ/m² | 3.5–8 kJ/m² | 5–10 kJ/m² |
| Notched Charpy impact, -20 °C | ISO 179-1:2010 | 3–7 kJ/m² | 2–4 kJ/m² | 4–7 kJ/m² |
| Mould shrinkage, flow direction | ISO 294-4:2018 | 1.2–1.6% | 0.6–1.0% | 0.2–0.4% |
Drying and melt-state handling of PP-35090 follow mineral-filled PP copolymer practice. Pre-drying at 80 °C for 2–4 hours in a desiccant or hot-air hopper dryer is applied when packaging has remained open for more than 24 hours at relative humidity above 60%; residual moisture above 0.05% by mass can produce surface splay, delamination at mineral-rich surfaces, and internal porosity on large flat components. For single-stage injection moulding, melt temperature measured by nozzle pyrometer is controlled at 200–240 °C. Mould temperature is set at 30–60 °C for non-appearance structural parts and 50–70 °C where surface gloss or grain replication is specified. Screw geometry influences filler dispersion: a three-zone general-purpose screw with L/D 18:1–22:1 and a check ring is acceptable, but peripheral screw speed should be limited to 0.2–0.4 m/s to avoid excessive shear heating and premature degradation of the PP copolymer matrix. Back pressure in the range 0.5–1.0 MPa improves melt homogeneity without overworking the filler-binder interface. Injection velocity should maintain a flow-front velocity of 100–300 mm/s in wall sections between 1.5 mm and 3.0 mm; higher velocity can generate jetting, mineral-rich weld lines, and glossy surface defects. Holding pressure is commonly set at 60–80% of peak injection pressure. For a 2.0 mm-thick edge gate, gate freeze time is typically 0.8–1.2 s/mm. Dimensional metrology should be postponed 24–48 hours after demoulding because post-mould crystallisation and moisture equilibration continue after ejection.
Unfilled PP copolymer normally exhibits flexural modulus of 900–1200 MPa under ISO 178:2019, whereas the mineral-filled PP-35090 class reaches 1800–2600 MPa. This increase is accompanied by density change: unfilled PP copolymer has an ISO 1183-1:2019 density near 0.90 g/cm³, while mineral-filled grades commonly fall in the range 1.03–1.13 g/cm³. Mould shrinkage measured on 60 mm × 60 mm × 2 mm plaques to ISO 294-4:2018 is 1.2–1.6% in the flow direction for unfilled PP copolymer; the mineral filler in PP-35090 constrains post-mould chain relaxation and reduces flow-direction shrinkage to 0.6–1.0%. The trade-off appears in notched Charpy impact under ISO 179-1:2010: high-ethylene unfilled PP copolymer can exceed 10 kJ/m² at 23 °C, while mineral-filled systems often occupy 3.5–8 kJ/m². At -20 °C, the copolymer base of PP-35090 limits the sharp brittle transition observed in mineral-filled homopolymer PP because ethylene segments within the matrix provide local energy dissipation and delay crack propagation.
When glass fibre-reinforced PP is evaluated as an alternative, the selection logic changes. A 20 wt% glass fibre-reinforced PP may reach tensile stress at yield of 55–75 MPa under ISO 527-2:2012, while mineral-filled PP copolymer remains in the 22–28 MPa range. The mineral-filled PP-35090 class compensates with reduced warp and greater shrinkage isotropy. Glass fibre orientation creates flow-direction shrinkage as low as 0.2–0.4%, but transverse shrinkage is often larger and visible fibre orientation can appear on textured surfaces. Mineral-filled PP copolymer provides a more uniform shrinkage field and better surface uniformity in visible interior components. Against calcium carbonate-filled PP homopolymer, the PP-35090 copolymer matrix offers improved low-temperature impact retention; calcium carbonate-filled homopolymer grades can show notched Charpy at -20 °C below 2 kJ/m² under ISO 179-1:2010. Against talc-filled PP homopolymer, PP-35090 lowers the brittle-ductile transition temperature and improves weld-line elongation, but the homopolymer can provide higher upper heat deflection temperature at equal filler loading because of higher matrix crystallinity.
Mineral-filled PP copolymer of the PP-35090 class is used in door trim carriers, lower instrument panel supports, airbag housing components, and pillar covers. Dimensional stability after humidity cycling is commonly evaluated by conditioning specimens at 40 °C and 95% relative humidity for 48–96 hours and then measuring linear change by ISO 294-4:2018 or an OEM internal method. PP absorbs very little water; equilibrium moisture uptake at 23 °C and 50% RH is below 0.05% by mass, but the mineral filler can retain surface moisture at filler-polymer interfaces, so a properly moulded component may shift by less than 0.1% after humidity exposure. Interior odour and fogging are controlled by measuring volatile organic compounds by VDA 277 and condensate by DIN 75201:2011 or VDA 278; acceptance limits are OEM-specific, but mineral-filled grades with controlled filler surface chemistry can meet automotive interior requirements when processed inside the stated thermal window. On production-scale equipment, a 1600 kN hydraulic injection moulding machine with a 50 mm diameter screw and insulated runner system has been used for this material class at melt temperature 220 °C, mould temperature 45 °C, and holding pressure in the range 35–55 bar. This processing envelope is illustrative for mineral-filled PP copolymer and does not replace the moulding protocol supplied by Kingfa for PP-35090.
Appliance housing programmes may select PP-35090 to replace ABS where chemical resistance to alkaline cleaners, cost per unit volume, and stress-cracking resistance are constraints. Mineral-filled PP copolymer does not match the room-temperature stiffness of ABS in all wall sections; ABS flexural modulus is typically 2000–2500 MPa under ISO 178:2019, overlapping the upper range of mineral-filled PP. The difference appears in falling dart impact and deep-gloss surface: ABS can provide higher melt flow and better thin-wall stiffness, but PP-35090 resists environmental stress cracking in alkaline and grease environments better, and can be processed on standard PP screw and barrel assemblies without ABS purging procedures. Flammability is limiting: polypropylene burns readily, and a UL 94 HB yellow card may apply only at the minimum thickness tested for this grade. Any claim of V-2, V-1 or V-0 classification must be verified against the UL Product iQ certificate for PP-35090. Glow-wire testing to IEC 60695-2-11 is used for appliance enclosures; mineral fillers can increase ignition resistance and reduce dripping, but the glow-wire flammability index and ignition temperature are lot- and thickness-dependent.
Electrical enclosures produced from mineral-filled PP copolymer are specified by comparative tracking index under IEC 60112, glow-wire flammability under IEC 60695-2-11, and flammability class under UL 94. Glass-reinforced PP may show higher tensile strength and heat deflection temperature, but the mineral-filled PP-35090 class can offer lower surface conductivity, lower visible fibre orientation, and more uniform low-gloss appearance. In low-voltage switchgear enclosures, dimensioned openings must remain within assembly tolerance; mineral-filled PP copolymer reduces post-mould shrinkage relative to unfilled PP. However, PP-35090 is not a substitute for polycarbonate or polyamide in continuous service above 100 °C. Heat deflection temperature class values under ISO 75-2:2013 method B are 95–120 °C, but electrical enclosure standards may require a relative temperature index under UL 746B or an RTI value that is grade-specific and thickness-dependent. If an electrical RTI is required, the UL yellow card for PP-35090 must be consulted; class-typical mineral-filled PP may not satisfy elevated RTI electrical or mechanical claims above 85 °C without additional testing.
| Regulatory framework | Document or standard basis | Verification requirement |
|---|---|---|
| REACH SVHC declaration | EC No 1907/2006 Article 33 | Confirm supplier statement and substance concentration below 0.1% by mass if applicable |
| RoHS restricted substances | 2011/65/EU with amendment (EU) 2015/863 | Pb, Hg, Cd, Cr(VI), PBB, PBDE, DEHP, BBP, DBP, DIBP concentrations within legally specified maximum values |
| Flammability rating | UL 94 | Yellow card minimum thickness must match the moulded part wall section |
| Glow-wire performance | IEC 60695-2-11 | GWT or GWFI value reported at the tested wall thickness only |
| Food-contact suitability | 21 CFR 177.1520 and/or Regulation (EU) No 10/2011 | Explicit grade-specific regulatory letter is required; base PP compliance does not automatically extend to the filled compound |
PP-35090 is not recommended for applications requiring continuous exposure to strong oxidising acids, chlorinated solvents above 40 °C, or repeated steam sterilisation above 121 °C. Mineral filler can increase moisture uptake at the filler-matrix interface, so parts exposed to condensing humidity should be dried before painting, bonding, or foam-in-place assembly. The use of the compound in food-contact articles requires explicit grade-specific certification and must not be assumed from base polypropylene compliance alone. Lot-to-lot melt viscosity variation should be monitored by ISO 1133-1:2022; if melt mass-flow rate shifts by more than ±15% from the approved nominal value, packing time and holding pressure may require adjustment to avoid sink marks or flash in thin-walled sections.