| HS Code | 465246 |
| Polymer Type | Polypropylene (PP) |
| Filler Type | Mineral (Talc/TD) |
| Filler Content | Mineral-filled grade |
| Impact Modification | High impact |
| Density | Approximately 1.05 g/cm³ typical |
| Melt Flow Rate | Typical injection-molding grade |
| Tensile Strength | Typical mineral-filled PP range |
| Elongation At Break | Typical high-impact mineral-filled PP range |
| Flexural Modulus | Typical mineral-filled PP range |
| Notched Izod Impact Strength | High-impact grade |
| Heat Deflection Temperature | Typical PP engineering range |
| Molding Shrinkage | Typical mineral-filled PP range |
| Processing Method | Injection molding |
| Processing Temperature | 190-230 °C typical |
| Mold Temperature | 40-80 °C typical |
| Flammability | HB typical |
As an accredited Kingfa PP-36360,PP-TD Mineral Filled High Impact,Industrial factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-36360 is supplied in 25 kg moisture-resistant woven bags, palletized with batch labels for industrial storage and handling. |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized 25 kg bags of Kingfa PP-36360 PP-TD mineral-filled high-impact industrial polypropylene, secured and documented. |
| Shipping | Kingfa PP-36360, PP-TD Mineral Filled High Impact, Industrial is shipped as non-hazardous polymer pellets in sealed, moisture-resistant bags or containers. Not regulated for transport. Keep dry, clean, and protected from direct sunlight; avoid contamination and extreme temperatures. Handle with standard industrial precautions. |
| Storage | Store Kingfa PP-36360, PP-TD Mineral Filled High Impact, Industrial in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers closed, palletized, and protected from moisture, dust, and physical damage. Avoid prolonged UV exposure and follow the manufacturer’s SDS. |
| Shelf Life | Typically 24 months in original unopened packaging, stored dry, cool, and well-ventilated, away from direct sunlight and moisture. |
In underhood thermal cycling between -40°C and 110°C, Kingfa PP-36360, a PP-TD mineral-filled high-impact polypropylene, is injection molded into HVAC blower scroll housings, mode door carriers, and cowl-side impact brackets. Published data for this exact grade configuration is limited; the processing envelopes and mechanical threshold values cited here are representative of talc-filled impact-copolymer PP compounds in this melt-flow class and require lot-specific confirmation against the supplier technical datasheet. Compounding on a 40:1 L/D co-rotating twin-screw extruder disperses the mineral filler before pelletizing; subsequent molding on 20:1 L/D reciprocating-screw machines is maintained at a melt temperature of 220–250°C, mold surface temperature of 30–60°C, injection velocity of 80–120 mm/s, and hold pressure of 60–80 MPa. Gate blush is typically observed above 120 mm/s in valve-gated three-plate tools because shear heating drives the melt front above 260°C, producing surface splay and volatile deposit. A tensile modulus of 1800–2400 MPa per ISO 527-2:2012 at 23°C and 1 mm/min suppresses wall deflection in 2.0–2.5 mm thin-wall scrolls, while Charpy notched impact per ISO 179-1:2010/1eA typically remains above 20 kJ/m² at 23°C and above 8 kJ/m² at -30°C, preventing brittle fracture during cold-start heat load. For RH exposure above 60%, the resin is dried at 80°C for 2–4 h prior to molding to control splay and screw deposit. Underhood use is limited to areas below 110°C continuous air temperature and 0.5 MPa sustained tensile stress; exhaust-adjacent brackets and load-bearing components in direct contact with hot metal require higher-temperature engineering resin.
For indoor and outdoor industrial junction boxes tested to IEC 60670-1:2015, mineral-filled high-impact PP-TD is specified for IP55 and IP65 enclosures, terminal block housings, and DIN rail mounting bases with nominal wall thickness of 2.0–2.8 mm. The formulation combines a talc mineral filler loading in the range of 20–30 wt% within an impact-copolymer PP matrix, stabilized with a hindered phenolic antioxidant and acid scavenger. Processing on standard reciprocating-screw injection machines uses a melt temperature of 210–240°C, mold temperature of 25–50°C, and clamp force from 3000–5000 kN depending on projected area. Knit lines at boss junctions and knockout webs retain above 65% of unwelded flexural strength when a central diaphragm gate or multiple balanced gates are used; this is a critical advantage over glass-filled PP, where knit-line retention commonly falls to 45–55%. The grade is rated HB at 3.0 mm under UL 94 unless flame-retardant additives are separately compounded; live-part compartments requiring V-0 must be verified against the exact compound batch. Outdoor weather resistance requires UV stabilization or carbon black masterbatch and compliance to UL 746C for f1 listing; without such stabilization, surface chalking after 500–800 h accelerated UV exposure per ISO 4892-2:2013 method A can reduce notched impact by 20–30%. Screw bosses for self-tapping fasteners require a boss outer diameter equal to 2.0–2.5 times the screw diameter and a wall thickness ratio of 0.6–0.8 to prevent sink marks and hoop-stress cracking.
A three-runner cold-runner system balancing four gates across a 1200 mm × 1000 mm pallet deck is used for distribution pallets molded from Kingfa PP-36360; collapsible bin side walls and divider trays are molded in two-plate tools with hot edge gates. The compound is processed in accumulator-assisted injection machines with shot weights of 3–6 kg, clamp force of 8000–12000 kN, melt temperature of 230–250°C, and mold temperature of 20–35°C. Mineral filler reduces mold shrinkage to 0.8–1.2%, compared with 1.5–2.0% for unfilled PP, which holds pallet corner post warpage within ±1.5 mm over 1200 mm length. Rib root radius is maintained at 0.6–1.0 times the nominal wall, and rib thickness is limited to 0.6 times the adjacent wall to avoid sink marks. Impact retention is tested at -20°C using ISO 6603-2:2023 instrumented puncture at 4.4 m/s with a 20 mm striker; acceptable ductile failure requires no full-thickness crack extending beyond 10 mm from the striker contact zone. Static racking load to ISO 8611-1:2021 requires deflection below 50 mm under the user-specified load, typically 500–1000 kg depending on pallet class, applied over 24 h at 45°C. Prolonged creep under stack load is a known boundary: at 45°C and 1.0 MPa compressive stress, creep modulus may decay by 20–30% over 1000 h, so ribbed structural design must avoid continuous unsupported deck spans above 300 mm. This industrial grade is not accepted for direct food-contact transit packaging unless compliance with FDA 21 CFR 177.1520 is explicitly confirmed for the exact lot.
| Test method | Condition | Property | Application threshold |
|---|---|---|---|
| ISO 527-2:2012 | 23°C, 1 mm/min, Type 1A | Tensile modulus | 1800–2400 MPa |
| ISO 178:2019 | 23°C, 2 mm/min | Flexural modulus | 1700–2100 MPa |
| ISO 179-1:2010/1eA | 23°C, notch radius 0.25 mm | Charpy notched impact | >20 kJ/m² |
| ISO 179-1:2010/1eA | -30°C, notch radius 0.25 mm | Charpy notched impact | >8 kJ/m² |
| ISO 6603-2:2023 | -20°C, 4.4 m/s, 20 mm striker | Instrumented puncture impact | Ductile failure, crack ≤ 10 mm |
| ISO 75-2:2013 | Method B, 0.45 MPa flexural stress | Heat deflection temperature | 95–110°C |
| UL 94 | 3.0 mm thickness | Flammability class | HB unless FR package is confirmed |
The combination of 0.8–1.2% mold shrinkage, flexural modulus above 1700 MPa per ISO 178:2019 at 23°C and 2 mm/min, and Charpy notched impact above 15 kJ/m² at 23°C is specified for top-load washer tub covers, pump housings, and dryer impeller shrouds. Multi-cavity family molds use sequential valve gating with cavity pressure switch-over set at 45–60 MPa; hold pressure is profiled from 55–70 MPa for 4–6 s, followed by cooling time of 20–30 s at mold temperature 40–60°C. OEM validation commonly imposes 300,000 unbalance load cycles on tub covers to IEC 60335-1:2020 clause 21.1 mechanical strength requirements, with no visible crack or deformation that compromises clearances. Fatigue crack initiation is controlled by keeping rib thickness at 0.5–0.6 times the adjacent wall and maintaining a rib root radius of at least 0.5 mm; molded-in stress above 25 MPa, measured by hole-drilling or solvent stress-crack methods, promotes detergent stress-cracking in hot wash water at 90°C. The talc filler reduces thermal expansion to 60–80 × 10⁻⁶ K⁻¹ in the flow direction, which lowers bearing bore distortion in impeller shrouds; post-molding reaming to IT7 tolerance remains necessary when bearing insertion forces exceed 150 N. Continuous immersion in 60–90°C detergent solution is an operational boundary; for outer tubs and pump bodies in direct contact with hot alkaline water, validation of hydrolysis resistance and creep at 90°C under 0.5 MPa hoop stress is required.
Where line-of-sight spark containment and drop robustness dominate, Kingfa PP-36360 is injection molded into circular saw guards, angle grinder motor housings, and benchtop tool bases with wall thickness from 2.0 mm to 2.8 mm. The components are produced in two-plate cold-runner tools with fan gates into side walls; melt temperature is 215–240°C, mold temperature is 25–50°C, injection velocity is 70–100 mm/s, and hold pressure is 50–70 MPa. Under IEC 62841-1:2014 clause 20 mechanical hazard testing, the enclosure is dropped from 1 m onto a concrete floor at three attitudes; the mineral-filled impact-copolymer PP resists cracking and must not expose live parts or allow the finger probe to contact moving parts. Unwelded tensile strength by ISO 527-2:2012 is typically 20–25 MPa, and knit-line regions at boss and guard interfaces retain 60–70% of that value because platy talc particles orient less aggressively than glass fibers and do not create the severe fiber-glass weld-line strength loss. Differential shrinkage is controlled to 0.8–1.2%; this reduces distortion around bearing bores and critical gear alignment features, but bearing seats with IT7 tolerance are reamed post-molding. For tools operated outdoors or in UV-exposed workshops, UV stabilization must be confirmed against UL 746C; carbon black masterbatch at 2.0–2.5 wt% addition is the common outdoor package. Continuous motor-housing surface temperature above 90°C under a 0.45 MPa load is not recommended without creep testing per ISO 899-2:2015 at 80°C and 1000 h.
At melt temperatures above 250°C, the talc-filled high-impact PP compound begins to generate volatile processing aids and residual moisture, producing splay, gate blush, and screw deposit; this sets a practical upper processing limit for commercial HVAC fan cones, damper blades, and filter retainer frames. These components are injection molded with wall thicknesses of 2.5–3.5 mm, melt temperature of 210–240°C, mold temperature of 30–50°C, and large fan gates or four-gated runners to avoid jetting. Heat deflection temperature measured to ISO 75-2:2013 method B under 0.45 MPa is typically 95–110°C; however, continuous service temperature in moving air plenums should not exceed 85–95°C where flexural creep stress is above 0.45 MPa. Creep modulus retention at 80°C after 1000 h per ISO 899-2:2015 may fall to 55–65% of the initial room-temperature value in mineral-filled PP, so damper blades with unsupported spans above 200 mm require ribbing or glass-filled reinforcement. Condensate exposure introduces a hydrolytic boundary: talc-filled PP is not readily hydrolyzed, but mineral filler and polar compatibilizers can elevate water absorption to 0.1–0.3% at 23°C and 50% RH; pre-drying at 80°C for 2–4 h is required after storage in RH above 60%. For plenum chambers and smoke-exhaust ducting requiring flame-spread and smoke-index compliance, the standard HB rating at 3.0 mm under UL 94 is insufficient; ASTM E84 and UL 2043 listings must be validated on the final component rather than assumed from base resin data. Published data for this specific PP-TD configuration in continuous air-handling service is limited; production validation should include ISO 4892-2:2013 method A UV exposure for 500 h and a 1000 h creep test at 80°C under service load.
Competitive Kingfa PP-36360,PP-TD Mineral Filled High Impact,Industrial prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-36360, PP-TD Mineral Filled High Impact, Industrial, is an injection-moulding grade polypropylene compound in which a mineral filler phase is dispersed in an impact-modified polypropylene matrix. The PP-TD designation separates the material from unfilled polypropylene, glass-fibre reinforced grades, and immiscible elastomer blends because the property balance is generated through combined mineral reinforcement and elastomer toughening rather than through fibre anisotropy or a single-phase resin. Industrial classification indicates that the material is intended for production components where dimensional stability, stiffness, and low-temperature ductility are specified jointly.
The grade code pattern is consistent with a talc-bearing mineral filler system, although the exact mineral morphology, median particle size, and filler weight fraction must be read from the manufacturer lot certificate because published data for this specific configuration is limited. For production scheduling, a melt flow rate in the range of 8–20 g/10 min at 230 °C and 2.16 kg is common for industrial mineral-filled high-impact PP compounds, but Kingfa lot-specific certificates must be used for PP-36360 because flow behaviour shifts with filler loading, elastomer domain size, and stabilizer package.
In a mineral-filled high-impact PP system, the mineral phase raises flexural modulus, reduces mould shrinkage, and lowers the coefficient of linear thermal expansion relative to unfilled impact copolymer. The elastomer phase preserves notched impact strength at 23 °C and can extend ductility to sub-zero conditions; however, the two mechanisms are not additive without limit. Above a filler loading of approximately 30–40 wt%, notched impact can decrease if the filler particle size distribution and coupling agent are not optimized, and melt flow length can shorten because the filled melt exhibits higher viscosity at low shear rates.
The processing consequence is that screw recovery time, injection pressure, and gate freeze-off differ from unfilled PP. A mineral-filled impact PP may require a larger gate diameter or wider flow channel to avoid jetting and hesitation marks. High-shear dispersion is required during compounding to break agglomerates without reducing plate-like mineral aspect ratio excessively, because excessive platelet attrition reduces stiffness but can slightly improve impact.
Flow-induced mineral orientation creates anisotropic shrinkage in the part, with parallel and perpendicular shrinkage values differing by 0.2–0.5 percentage points in plaques moulded per ISO 294-4:2018. The plate-like filler aligns along flow lines near the skin but remains more random in the core, producing a skin-core morphology that can increase the coefficient of linear thermal expansion in the thickness direction. Consequently, dimensional stability should be checked on a part with production gating, not on an edge-gated tensile bar.
On production-scale injection moulding machines with screw diameters between 35 mm and 80 mm and L/D ratios of 20:1–25:1, mineral-filled high-impact PP compounds are usually processed with a general-purpose three-zone screw, a reverse-taper or free-flow non-return valve, and a wear-protected barrel because mineral filler accelerates screw and check-ring wear. Clamp force requirements follow flow length and wall thickness, but the effective flow-length-to-wall-thickness ratio is lower than that of an unfilled PP with the same melt flow rate because the mineral phase increases cooling-phase solidification speed.
Drying is required when pellet surface moisture exceeds 0.05% or when ambient relative humidity has exceeded 60% RH for more than 4 h. A desiccant dryer set at 80–90 °C with a residence time of 2–4 h is commonly sufficient to suppress surface splay and hydrolysis odour. The melt temperature measured at the nozzle is generally kept between 210 °C and 250 °C, with the lower end used for high-impact grades to retain elastomer toughness and the upper end used only for thin-wall filling. Sustained melt residence above 270 °C should be avoided because thermal degradation of the impact modifier and mineral coupling agent can reduce impact strength and increase plate-out.
Mould temperature is typically maintained between 20 °C and 60 °C, depending on surface finish requirements. Higher mould temperatures reduce weld-line visibility and flow marks but extend cycle time; knit-line impact retention should be validated by notched Charpy specimens per ISO 179-1:2010 machined across the weld line, because mineral orientation near the weld line suppresses the energy-absorbing deformation of the elastomer phase.
Mechanical acceptance for Kingfa PP-36360 should be stated against a test-method block rather than a single property. For injection-moulded plaque specimens prepared according to ISO 294-1:2017, the following representative ranges are drawn from published industrial datasheets for 20–40 wt% mineral-filled high-impact PP compounds; they are not a substitute for the lot-specific PP-36360 certificate.
| Property | Test Method | Representative Class Range | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.02–1.12 | g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022, 230 °C/2.16 kg | 8–20 | g/10 min |
| Tensile stress at yield | ISO 527-2:2012, 50 mm/min | 22–28 | MPa |
| Tensile strain at break | ISO 527-2:2012 | 5–30 | % |
| Flexural modulus | ISO 178:2019, 2 mm/min | 1800–2800 | MPa |
| Notched Charpy impact, 23 °C | ISO 179-1:2010/1eA | 4–10 | kJ/m² |
| Notched Charpy impact, -30 °C | ISO 179-1:2010/1eA | 2–5 | kJ/m² |
| Heat deflection temperature | ISO 75-2:2013, 0.45 MPa, flatwise | 100–120 | °C |
| Mould shrinkage, parallel | ISO 294-4:2018 | 0.8–1.2 | % |
| Coefficient of linear thermal expansion | ISO 11359-2:2021, 23 °C to 80 °C | 40–70 × 10-6 | K-1 |
The ranges above are broad because mineral filler type, particle size, coupling agent, elastomer content, and nucleating additives all shift properties. If a specification requires a flexural modulus minimum of 2200 MPa or a notched Charpy impact at -30 °C of at least 3 kJ/m², PP-36360 lot data must be checked rather than inferred from the generic class. Tensile and flexural values should be read from the certificate together with the moulding condition and specimen type; values generated on a production machine with rapid cooling will not necessarily match values from an edge-gated laboratory plaque.
Industrial usage of mineral-filled high-impact PP grades centres on injection-moulded structural covers, automotive interior trim carriers, air handling components, battery housings, electrical enclosures, and appliance frames where unfilled PP would exhibit excessive shrinkage or insufficient modulus. The mineral filler reduces post-mould warpage by lowering anisotropic shrinkage relative to glass-fibre grades, so large flat parts can be designed with lower compensation factors in tooling. Candidate use categories include automotive door module substrates, seat back panels, HVAC housings, washing machine baffles, dishwasher inner components, electrical enclosures, and industrial battery covers.
Compared with general-purpose PP homopolymer, the PP-36360 class offers lower mould shrinkage and higher notched impact, but lower tensile yield and lower melt flow at equivalent conditions. Compared with unfilled impact copolymer PP, the mineral-filled grade provides higher flexural modulus and lower thermal expansion, while retaining a useful fraction of the impact copolymer’s ductility. Compared with 30 wt% glass-fibre reinforced PP, the mineral-filled high-impact grade usually shows lower flexural modulus, lower tensile strength, lower heat deflection temperature, but less warpage, lower density, better surface appearance, and reduced machine-barrel and mould wear.
| Material Class | Density, ISO 1183-1:2019 | Flexural Modulus, ISO 178:2019 | Notched Charpy, 23 °C, ISO 179-1:2010 | Mould Shrinkage, ISO 294-4:2018 |
|---|---|---|---|---|
| General-purpose PP homopolymer | 0.90–0.91 g/cm³ | 1200–1600 MPa | 2–4 kJ/m² | 1.0–1.5% |
| Unfilled impact copolymer PP | 0.90–0.91 g/cm³ | 900–1300 MPa | 8–20 kJ/m² | 1.2–1.8% |
| 20–40 wt% mineral-filled high-impact PP, PP-36360 class | 1.02–1.12 g/cm³ | 1800–2800 MPa | 4–10 kJ/m² | 0.8–1.2% |
| 30 wt% glass-fibre reinforced PP | 1.10–1.15 g/cm³ | 3500–5000 MPa | 6–12 kJ/m² | 0.2–0.6% |
If PP-36360 is proposed for automotive interior carriers, volatile organic compound and fogging data per VDA 278 and condensation-fogging methods such as ISO 6452:2021 must be obtained. For electrical enclosure use, comparative tracking index per IEC 60112, glow-wire ignition temperature per IEC 60695-2-13, and flammability classification from the UL Yellow Card should be confirmed rather than assumed from the mineral-filled PP class.
Substitution studies are usually driven by warpage, surface appearance, or tool wear rather than by raw material cost alone. A mineral-filled high-impact PP can replace a short-glass PP in a housing or shroud if the maximum tensile stress remains below the lower yield strength of the mineral-filled grade and if the service temperature does not exceed the heat deflection temperature of the selected formulation. Design comparison should examine flexural modulus under load according to ISO 178:2019 and stress relaxation at the upper use temperature because mineral-filled PP can creep more than glass-fibre PP at the same temperature.
In tooling transfer, gate positions and weld lines may need adjustment because mineral-filled high-impact PP exhibits lower melt flow length and greater sensitivity to hesitation effects than talc-free impact copolymer. Mould shrinkage compensation is also lower than unfilled PP but higher than glass-fibre PP; tool makers should use parallel and perpendicular shrinkage values from ISO 294-4:2018 rather than applying a single factor from an unfilled PP database. Sharp corners and rib roots should be radiused more generously than with unfilled PP because the mineral filler can act as a stress concentrator when impact loading is transmitted through thin sections.
On production-scale injection moulding machines with clamp force above 1200 kN, tooling wear at gates and sharp edges is more pronounced with mineral-filled grades than with unfilled PP. Gate inserts made of hardened tool steel or treated with nitriding are used; wear measurements after 100,000 cycles may show visible edge rounding in unprotected mould steel, but published data for this specific configuration is limited. Melt cushion should be monitored and controlled within a narrow band to avoid variations in melt residence time that can shift impact performance from shot to shot.
Because the grade is a compounded multiphase system, operational boundaries should be revalidated after any regrind ratio change, colourant change, or drying system modification. Regrind content above typical internal allowances can alter filler orientation and lower notched impact, so the regrind ratio should be fixed during PP-36360 process qualification and verified by notched Charpy testing per ISO 179-1:2010. Chemical compatibility with flame retardants, lubricants, and colour concentrates must be assessed for plate-out, odour, and property retention; published data for this specific configuration is limited.