Kingfa PP-36370(G2),Mineral Filled Toughened Modified PP (High Impact, Low Warpage)

    • Product Name: Kingfa PP-36370(G2),Mineral Filled Toughened Modified PP (High Impact, Low Warpage)
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 370974
    Density G Cm3 1.03
    Meltflowrate G 10min 8.0
    Tensilestrength Mpa 22.0
    Elongationatbreak Percent 30
    Flexuralmodulus Mpa 1600
    Notchedizodimpactstrength Kj M2 25
    Heatdeflectiontemperature 1 8mpa C 100
    Vicatsofteningtemperature C 130
    Moldshrinkage Percent 0.8-1.0
    Waterabsorption Percent 0.02
    Rockwellhardness R 85
    Ul94flammability HB
    Fillertype Mineral
    Impactmodification High impact
    Warpage Low

    As an accredited Kingfa PP-36370(G2),Mineral Filled Toughened Modified PP (High Impact, Low Warpage) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa PP-36370(G2) is packaged in 25 kg moisture-resistant bags, palletized and wrapped for secure industrial transport and storage.
    Container Loading (20′ FCL) 20′ FCL container loading: Kingfa PP-36370(G2), mineral-filled toughened modified polypropylene, high-impact and low-warpage; securely palletized and loaded for shipment.
    Shipping Kingfa PP-36370(G2) is supplied as dry pellets in sealed, moisture-proof 25 kg bags, palletized and shrink-wrapped. Ship in clean, dry containers or trucks at ambient temperature; protect from moisture, direct sunlight, and contamination. Not classified as dangerous goods. Ensure pallets remain stable during loading.
    Storage Store Kingfa PP-36370(G2) in a cool, dry, well-ventilated warehouse, protected from direct sunlight, heat sources, moisture, and contamination. Keep pellets in original sealed bags on pallets, and reseal opened bags. Avoid prolonged exposure to high humidity, oxidizing agents, and incompatible chemicals. Maintain stable conditions, prevent bag damage, practice good housekeeping, follow local safety regulations, and use first-in, first-out stock rotation.
    Shelf Life Typically 12 months in original unopened packaging, stored dry, cool, and ventilated, away from moisture, direct sunlight, and contamination.
    Application of Kingfa PP-36370(G2),Mineral Filled Toughened Modified PP (High Impact, Low Warpage)

    On a 1,200 t injection molding line with accumulator-assisted injection speed of 300 mm/s, the low-warpage requirement for a passenger vehicle door module carrier is dominated by the flatness of the sealing interface. A tolerance of 0.8 mm over a 600 mm span is commonly applied, and the material response must be validated with ISO 294-4 shrinkage plaques. For a mineral-filled toughened PP such as Kingfa PP-36370(G2), published lot-specific data may be limited; production validation should therefore include assembly-level flatness gauging and batch-to-batch shrinkage monitoring. Moulding trials typically set melt temperature between 220 °C and 235 °C, tool surface temperature between 30 °C and 50 °C, and holding pressure from 50 MPa to 70 MPa. Weld-line impact retention at clip towers and boss bases is a recognized failure mode; moving the gate to relocate the weld line away from load-bearing bosses is preferred over increasing impact modifier content alone. Multiaxial impact performance is screened using ISO 6603-2 at −30 °C, while notched Charpy values are compared under ISO 179-1. Dimensional compliance for interior trim brackets includes heat sag testing under ISO 306 Vicat softening temperature and creep under automotive OEM-specific methods. Regulatory requirements include EU 2000/53/EC ELV, REACH SVHC screening, and RoHS 2011/65/EU. The terminal component set includes a door module carrier with speaker ring, harness clip towers, armrest bracket, and window regulator mounting points.

    What Locking Boss Design Prevents Electrode Misalignment in Power Tool Housings?

    Rotor-bearing bore roundness and clamshell alignment define the critical dimensional path. In 2.5 mm nominal wall sections, mineral-filled toughened PP displays orientation-dependent shrinkage that can shift the bearing seat by 0.05 mm to 0.10 mm if filling becomes unbalanced. Tool trials on 150 t to 250 t injection machines should set melt temperature at 225 °C to 240 °C, mold temperature at 35 °C to 60 °C, and injection pressure at 80 MPa to 100 MPa. Locking bosses should use a minimum draft angle of 1° and a boss wall thickness not exceeding 60% of the adjacent nominal wall to avoid sink marks and stress concentration. Drop-impact validation follows manufacturer-specific 1.0 m drop from six faces; notched Charpy impact is compared under ISO 179-1 at 23 °C and −10 °C. Electrical insulation is assessed by IEC 62841-1 for motor-operated hand-held tools, and the housing must prevent electrode misalignment after repeated battery insertion cycles. Battery clamshells require additional chemical resistance to lithium-ion electrolyte droplets; immersion screening in 40 °C electrolyte simulant under ISO 175 can be used, but published data for this specific polypropylene formulation in electrolyte exposure is limited. The terminal application is a 18 V to 36 V cordless tool housing with injected metal inserts and sealing lip.

    Low-warpage mineral-filled impact-modified PP is evaluated for condensate drain pans where dimensional stability after hydrolytic aging matters more than short-term tensile strength. A pan with 400 mm to 600 mm longest dimension must remain flat within 1.0 mm after 1,000 h at 70 °C and 95% RH. Testing is performed according to ISO 175 for liquid chemical exposure and ASTM D638-14 for tensile property retention. Blower housing applications add a rotational balance requirement; eccentricity of the motor mounting face should be checked with a coordinate measuring machine after 24 h conditioning at 23 °C and 50% RH. Processing on hydraulic machines of 500 t to 800 t uses melt temperature 220 °C to 240 °C and mold temperature 30 °C to 50 °C. Cooling time is influenced by mineral filler thermal conductivity and typically extends from 18 s to 30 s for thick pan ribs. The material must not be combined with hygroscopic regrind unless pre-dried at 80 °C for 2 h to 4 h at dew point −20 °C, because surface moisture on filler can produce silver streaks and pressure loss. Compliance for polymeric materials in HVAC enclosures is assessed under UL 746C; plenum installations may require additional UL 2043 smoke and heat release screening if the pan is located in an air-handling plenum. The terminal component is an injection-molded condensate tray with integrated float switch bosses and a blower housing lower shell.

    When Outdoor Service Temperatures Approach −25 °C in Disconnect Switch Enclosures

    Low-temperature impact retention is the controlling material property for polypropylene junction boxes installed outdoors. Enclosures with wall thickness from 2.0 mm to 3.5 mm require notched Charpy impact under ISO 179-1 at −25 °C and multiaxial impact under ISO 6603-2. Mineral-filled toughened PP often exhibits adequate low-temperature impact if the elastomer phase is well dispersed, but screw boss torque retention and post-mould distortion remain process-dependent. Moulding trials on 350 t to 600 t machines should use melt temperature 225 °C to 250 °C, mold temperature 30 °C to 55 °C, and hold pressure 40 MPa to 60 MPa. Post-mould shrinkage is monitored with ISO 294-4 plaques for 48 h at 23 °C. Seal groove flatness after moulding should be measured before assembly; an out-of-flat condition above 0.5 mm over 300 mm can compromise IP65 gasket compression. Outdoor UV resistance is achieved by carbon-black masterbatch at 2 wt% or hindered amine stabilizer systems, with accelerated weathering checked under ISO 4892-2 for 1,000 h xenon-arc exposure. Electrical enclosure compliance is evaluated under IEC 62208 for empty enclosures and IEC 60670 for boxes and enclosures for household and similar fixed electrical installations. Flammability classification is typically UL 94 V-2 for mineral-filled polypropylene; applications requiring V-0 must use a flame-retardant package that may alter warpage and impact balance. The terminal product is a weatherproof IP65 disconnect switch enclosure with integrally moulded hinges and captive cover screws.

    Industrial feasibility screening matrix for mineral-filled toughened PP in cited downstream component classes
    Component classPrimary standardTest conditionTypical acceptance window
    Automotive door module carrierISO 6603-2−30 °C, 4 m/s strikerNo brittle failure; ductility index > 80%
    Power tool housingISO 179-123 °C notched Charpy6–15 kJ/m² grade-dependent
    HVAC condensate panASTM D638-1470 °C, 95% RH, 1,000 hTensile strength retention > 70%
    Outdoor disconnect enclosureISO 179-1−25 °C notched CharpyNo crack propagation; ≥4 kJ/m² typical screening
    Washer outer tubISO 527-223 °C, 50 mm/minModulus 1,500–2,500 MPa
    Reusable logistics toteASTM D5276-19−30 °C, 0.5 m dropNo structural fracture; corner weld intact

    Washer outer tubs made from mineral-filled toughened PP are processed on 1,600 t to 2,000 t injection machines with sequential valve gating to fill the 700 mm to 900 mm diameter part without excessive clamp pressure fluctuation. The critical process defect is out-of-roundness at the bearing insert seat; roundness is typically held within 0.20 mm after 48 h post-mould conditioning. Melt temperature is set at 230 °C to 250 °C, mold temperature at 40 °C to 60 °C, and cooling time at 25 s to 40 s. Mineral filler reduces shrink anisotropy relative to unfilled PP, but gate position and flow length can still produce differential shrinkage between the tub wall and the bearing hub. Balance ring applications use rotational imbalance frequency; post-mould warpage causes mechanical interference at spin speeds above 1,200 rpm. Material screening includes ISO 527-2 tensile modulus and ISO 179-1 notched Charpy at 23 °C. Hydrolytic aging in 60 °C water with 0.5% detergent is assessed by tensile strength retention after 500 h. Compliance follows IEC 60335-1 for household appliance safety, with specific chemical resistance to detergent and softener under manufacturer-specific methods. The terminal part is a direct-drive washer outer tub with overmoulded bearing housing and a snap-fit balance ring.

    Tote Bottom Warpage After 40 kg Corner-Drop Cycles in Cold Storage

    Reusable logistics containers require a combination of freezer-impact resistance and stack-wall dimensional stability. A tote with 600 mm × 400 mm footprint and 320 mm height is typically produced on 800 t to 1,200 t machines with two-stage injection and a film gate along the bottom rib. Mineral-filled toughened PP provides low creep under vertical stacking load of 60 kg at 23 °C for 72 h, evaluated by ISO 9967 for creep ratio. Cold storage validation includes ASTM D5276-19 drop test of filled containers at −30 °C from 0.5 m to 1.0 m. Bottom warpage after corner-drop cycles must remain below 2.0 mm across the diagonal to maintain conveyor stability. Moulding parameters generally include melt temperature 210 °C to 230 °C, mold temperature 15 °C to 35 °C, and cooling time 20 s to 35 s. Preheat of regrind to 80 °C for 2 h is required if moisture is present. Food-contact compliance is established under FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011, but migration testing must include the mineral filler and impact modifier because overall migration can shift with filler content. The terminal product is a vented dairy crate or freezer tote with interlocking stacking lugs and four-way fork entry.

    After ejection from an 800 t single-stage injection machine, a contract chair seat shell is measured for stackability flatness within 1.5 mm over the 500 mm seating plane. Mineral-filled toughened PP is selected when the design combines textured undercuts, ribbed underside grid, and metal insert bosses. Process settings include melt temperature 220 °C to 240 °C, mold temperature 30 °C to 55 °C, and holding pressure 45 MPa to 65 MPa. Warpage control depends on balanced flow through the rib grid; differential cooling between thick boss areas and thin webbing is a known source of post-demold distortion. Impact performance is evaluated by BIFMA X5.1-2021 back and seat durability cycles, which include drop loading and cyclic seat impact. Notched Charpy impact under ISO 179-1 at 23 °C and −10 °C provides comparative toughness screening. For upholstered seating components, additional fire safety is specified under NFPA 260 or BS 5852 depending on the market; however, those standards apply to the upholstered composite, not the polypropylene shell alone. Surface texturing depth of 25 µm to 30 µm is common for low-gloss appearance and scratch visibility reduction. The terminal part is a one-piece armrest body or chair seat shell with moulded-in insert receivers and concealed cable channels.

    Free Quote

    Competitive Kingfa PP-36370(G2),Mineral Filled Toughened Modified PP (High Impact, Low Warpage) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa PP-36370(G2) is a mineral-filled toughened modified polypropylene compound supplied in pellet form for injection moulding applications where high impact resistance and low warpage are simultaneous requirements. The grade is positioned within the Kingfa PP portfolio as a high-impact, low-warpage variant in which a mineral filler component is combined with an elastomeric or ethylene-propylene-based impact modifier. The “G2” suffix is a manufacturer-specific designation for the filler/toughener package and flow characteristics; the exact mineral content is controlled by ash-content testing and reported on the lot certificate of analysis rather than inferred from the grade name alone.

    Product characterisation follows standard polymer test methods. Melt mass-flow rate is measured according to ISO 1133-1:2022 at 230 °C under a 2.16 kg load. Density is determined by ISO 1183-1:2019. Tensile behaviour is evaluated according to ISO 527-2:2012, flexural modulus by ISO 178:2019, notched Izod impact by ISO 180:2000, heat deflection temperature by ISO 75-2:2013, ash content by ISO 3451-1:2019, and moulding shrinkage by ISO 294-4:2018. The following table identifies the reporting fields used on the certificate of analysis.

    Reported propertyTest methodCondition / measurement basis
    Melt mass-flow rateISO 1133-1:2022230 °C, 2.16 kg, die diameter 2.095 mm
    DensityISO 1183-1:2019Method A, immersion in water at 23 °C
    Tensile stress at yieldISO 527-2:2012Type 1A specimen, test speed 50 mm/min
    Flexural modulusISO 178:2019Span length 64 mm, test speed 2 mm/min
    Notched Izod impact strengthISO 180:200080 mm × 10 mm × 4 mm, notch Type A, 23 °C and −20 °C
    Heat deflection temperatureISO 75-2:2013Method B, 0.45 MPa, flatwise
    Ash contentISO 3451-1:2019600 °C to constant mass
    Moulding shrinkageISO 294-4:201860 mm × 60 mm × 2 mm plaque, 24 h after demoulding

    Numerical acceptance limits are controlled by the supplier’s product specification and the lot-specific certificate of analysis. Secondary values reproduced without lot traceability are not a substitute for the release test data, especially because mineral filler content and impact-modifier ratio can be adjusted within a defined window to meet melt-flow and impact requirements.

    How Does Mineral Filling and Toughening Alter PP-36370(G2) Relative to Unmodified Polypropylene?

    Unfilled PP homopolymer and conventional impact copolymer grades exhibit anisotropic mould shrinkage because of oriented crystalline domains. In PP-36370(G2), the mineral filler component reduces the difference between flow-direction and transverse-direction contraction, which lowers warpage in flat parts and large-area structural components. The filler also raises modulus and heat deflection temperature, but it creates stress concentrations at the filler-matrix interface. The toughener package in PP-36370(G2) is therefore included to recover notched Izod impact and to extend ductility below 0 °C. Compared with standard mineral-filled PP grades using little or no impact modifier, PP-36370(G2) provides higher resistance to crack propagation at the expense of a measurable reduction in stiffness. Compared with unfilled high-impact PP, the grade has lower shrinkage and better dimensional stability, but generally requires higher melt pressure during filling because of increased compound viscosity at a given melt temperature.

    Weld-line performance differs from uniform-wall sections. Mineral-filled systems typically show lower tensile strength at weld lines than unfilled systems; the presence of an impact modifier changes the failure mode from brittle fracture to controlled yielding. If a part design places a weld line in a load-bearing region, tensile specimens produced under ISO 527-2:2012 with a centre film gate can be used to measure weld-line strength retention. This verification is application-specific because published data for this specific configuration is limited.

    At the compounding scale, this class of material is produced on a co-rotating twin-screw extruder with an L/D ratio of 40:1 and gravimetric feeders. The mineral filler is introduced through a side feeder to minimise pellet breakage and to maintain distributive mixing, while the downstream vacuum vent is maintained at ≤ −0.08 MPa to remove residual moisture and low molecular weight volatiles. Screw torque and melt temperature are logged continuously because torque changes indicate filler agglomeration or feed-rate drift, which are common sources of batch-to-batch variance in melt mass-flow rate and notched impact. From a morphological standpoint, the mineral particles act as heterogeneous nucleation agents, increasing crystallisation temperature and reducing spherulite size. Finer spherulites produce more uniform shrinkage and reduce post-moulding secondary crystallisation. The impact modifier forms discrete domains in the PP matrix; if those domains are over-coarsened by prolonged high-temperature residence, low-temperature impact retention decreases.

    On the injection moulding line, pre-drying is required only when pellets have been stored at relative humidity above 60% or when condensation is visible on the pellet surface. Drying at 80 °C for 2 h to 4 h in a desiccant dryer with a dew point of ≤ −20 °C is applied to critical surface-finish parts, because free moisture can generate splay and reduce weld-line strength. The melt temperature window at the nozzle is 200 °C to 240 °C. The lower bound is set by the viscosity increase from the mineral filler, which raises injection pressure and the risk of short shots; the upper bound is set by the beginning of thermal degradation of the elastomer phase. On a 1200-kN injection moulding machine with a 25:1 L/D three-zone screw, back pressure is held between 0.5 MPa and 1.5 MPa. Injection velocity is adjusted to 100 mm/s to 300 mm/s in thin-wall sections to prevent hesitation marks and to keep the melt front continuous. Mould temperature is controlled from 20 °C to 60 °C; for parts with critical flatness, the upper half of this range is used because slower cooling reduces frozen-in orientation and post-moulding warpage. Hold pressure must be maintained beyond gate seal time; gate seal time is determined by pressure-curve analysis or by ultrasonic thickness measurement. Cumulative barrel residence time should not exceed 10 min. If melt temperature exceeds 260 °C, the impact modifier may degrade, and the melt mass-flow rate may increase through chain scission.

    Operational boundaries include avoiding combination with amine-based processing additives or unknown halogen-free flame-retardant additives that may interact with filler surface treatments. This grade should not be mixed with low-viscosity PP grades at high let-down ratios unless the resulting melt flow is verified on the production lot. For process purging after high-temperature hold-up, a general-purpose PP purge is preferred; solvents and strong oxidising agents are unsuitable for equipment cleaning where residue may remain in the feed throat or hot runner.

    Where Low Warpage and High Impact Requirements Intersect in Part Design

    PP-36370(G2) is specified for injection moulded parts that combine large flat surfaces, varying wall thickness, and assembly loads. The mineral filler reduces differential shrinkage between flow and transverse directions, while the toughener package prevents brittle failure at mounting bosses, snap fits, and screw bosses. In automotive interior applications, this material type is used in dashboard substrate carriers, door panel inserts, HVAC housings, and battery-housing brackets; in appliances, it is used for structural covers and load-bearing frames where warpage after demoulding must remain within the assembly tolerance. Actual suitability is established by part-level tests according to the relevant component standard, not solely by material data sheet values.

    For thin-wall consolidation, gate location and rib layout are more influential than material selection alone. A mineral-filled toughened PP can warp if gate placement creates asymmetric orientation. Multiple gates or an edge gate with a flow leader can reduce orientation-induced warpage. Ribs should be designed at 50% to 70% of the adjacent wall thickness to avoid sink marks and excessive packing pressure. Weld lines should be moved away from impact points; when a weld line is unavoidable, prototype moulds should use overflow wells to vent the cold front and to increase weld-line pressure.

    Compared with standard mineral-filled PP, PP-36370(G2) may be selected when low-temperature impact and low warpage are jointly specified. The trade-off is lower flexural modulus than a mineral-only grade; therefore stress analysis should verify that the modulus is adequate for the ribbed structure. When a part requires higher stiffness, a mineral-filled PP without the toughener package may be substituted, but the loss in low-temperature impact must be accepted. When a part requires maximum impact and can tolerate higher warpage, an impact copolymer PP can be used. Low-temperature impact is assessed by ISO 180:2000 at −20 °C, and warpage is assessed by moulding shrinkage according to ISO 294-4:2018 or by part flatness gauge after conditioning.

    Compliance Documentation Fields on the Certificate of Analysis

    Each lot of Kingfa PP-36370(G2) is reported with the test methods listed in the table. The certificate of analysis typically includes melt mass-flow rate, density, ash content, tensile stress at yield, flexural modulus, notched Izod impact at 23 °C and −20 °C, heat deflection temperature, and moulding shrinkage. These values carry lot-level traceability and are the controlling specifications for release. The material is accompanied by a safety data sheet prepared in accordance with CLP Regulation (EC) No 1272/2008; no dangerous-goods classification is implied for shipment. Regulatory compliance for restricted substances is verified against EU RoHS Directive 2011/65/EU Annex II and REACH SVHC commitments. If the finished part is exported or used in electrical and electronic equipment, the supplier should be requested to provide a lot-specific statement.

    Where a part is intended for food-contact or medical use, the standard mineral-filled PP designation is not sufficient. Compliance must be confirmed against Regulation (EU) 10/2011 or ISO 10993-1 with the specific lot and processing conditions, because mineral filler surface treatments and processing aids may be present. For automotive interior use, the compound should be evaluated for odour, fogging, and VOC emissions according to the vehicle manufacturer’s material specification; generic PP datasheet values do not replace those tests.

    Storage should be in a closed, dry area at 5 °C to 40 °C. If the pellets are exposed to relative humidity above 60%, pre-drying is applied before moulding to prevent splay and impact loss. The material should be kept away from direct sunlight, strong oxidising agents, and open flame during handling.