| HS Code | 433000 |
| Polymer Type | Polypropylene (PP) |
| Filler Type | Mineral filled |
| Density | 1.05 g/cm3 |
| Melt Flow Rate | 10 g/10 min (230°C/2.16 kg) |
| Tensile Strength | 25 MPa |
| Elongation At Break | 30% |
| Flexural Modulus | 2200 MPa |
| Notched Izod Impact Strength | 25 kJ/m2 at 23°C |
| Heat Deflection Temperature | 100°C at 0.45 MPa |
| Molding Shrinkage | 0.8-1.2% |
| Flame Rating | HB |
| Impact Modification | High impact |
| Warpage | Low warpage |
As an accredited Kingfa PP-36380 GA,PP-TD Mineral Filled High Impact Low Warpage,Home Appliance factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaging: 25 kg moisture-barrier bags, 40 bags per pallet (1,000 kg net), labeled Kingfa PP-36380 GA. |
| Container Loading (20′ FCL) | 20′ FCL container fully loaded with Kingfa PP-36380 GA PP-TD mineral-filled high-impact low-warpage home appliance compound, 25 kg bags. |
| Shipping | Shipping Description: Kingfa PP-36380 GA is supplied as non-hazardous mineral-filled polypropylene pellets in sealed 25 kg moisture-proof bags, palletized and stretch-wrapped. Transport in clean, dry vehicles or containers at ambient temperature. Store dry, away from heat, sunlight, moisture, and contamination; protect bags from punctures and damage. |
| Storage | Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat/ignition sources, moisture, and incompatible chemicals such as strong acids, alkalis, and oxidizers. Keep in original sealed packaging on pallets; avoid crushing or deformation. Maintain stable temperature and humidity, use first-in-first-out, and follow the manufacturer’s safety data sheet. |
| Shelf Life | Typical shelf life is 12 months when stored cool, dry, in original sealed packaging, protected from moisture, heat, and sunlight. |
Kingfa PP-36380 GA is a talc/mineral-filled polypropylene copolymer injection-molding compound formulated for low-warpage structural components in home appliances. The application scenarios below are restricted to the product’s demonstrated loading window in domestic and light-commercial equipment. Each scenario lists the relevant product safety standard, the recommended proportion of PP-36380 GA in the molding feedstock, the downstream injection-molding process window, and the terminal part families. No compounding step is performed by the molder; the pellet is metered as a ready-to-mold feedstock.
| Application subsegment | Primary product safety standard | Critical material test method | Recommended PP-36380 GA loading |
|---|---|---|---|
| Washing machine outer tub | IEC 60335-2-7 with IEC 60335-1:2020 Clause 30.2 | ISO 527-2, ISO 178, ISO 179-1/1eA, ISO 175 | 100 wt% as received; regrind ≤15 wt% |
| Dishwasher base frame | IEC 60335-2-5 | UL 94 HB, IEC 60695-2-11, ISO 175:2010 | 100 wt%; dilution ≥80 wt% |
| Refrigerator shelf frames | IEC 60335-2-24 | FDA 21 CFR 177.1520, EU 10/2011, ISO 179-1/1eA | 85–100 wt%; post-industrial regrind 0–15 wt% |
| Air-conditioner drain pan | IEC 60335-2-40 | UL 94 HB, ISO 175:2010 | 100 wt% |
| Microwave structural bracket | IEC 60335-2-25 | IEC 60695-10-2, ISO 179-1/1eA | 100 wt%; regrind ≤10 wt% |
| Floor-care nozzle housing | IEC 60335-2-2 | UL 94 HB | 85–100 wt%; regrind ≤15 wt% |
In horizontal-axis washing machines, the outer tub is not a simple cylindrical bucket; the door-gasket seat, bearing-boss attachment, and lower drain port create an asymmetric wall-thickness distribution from 2.8 mm to 6.5 mm. PP-36380 GA is metered at 100 wt% as supplied when the molded tub is load-bearing and must survive residual unbalance at spin speeds from 1,200 rpm to 1,600 rpm. In-house regrind of sprues, runners, and rejected tubs is permitted only up to 15 wt%; above that level, production-floor verification indicates that the reduction in melt strength of the regrind fraction and the reorientation of talc platelets during remelting increase the longitudinal-to-transverse shrinkage differential by more than 0.35%, outside the tolerance of the door-bellow seal groove. Compliance for this subassembly includes IEC 60335-2-7 for washing machines in combination with IEC 60335-1:2020 Clause 15 moisture exposure and Clause 30.2 resistance to heat and fire. The material qualification set includes ISO 527-2 tensile modulus, ISO 178 flexural strength, ISO 179-1/1eA Charpy notched impact at 23 °C and -20 °C, ISO 175 immersion in 1% anionic detergent solution at 60 °C for 72 h, and ISO 294-4 mold shrinkage on a plaque of 60 mm × 60 mm × 2 mm. On the production floor, one-cavity or two-cavity tools with clamp force between 16,000 kN and 22,000 kN are used; screw diameter is typically 70–100 mm at a 20:1 L/D ratio, with compression ratio 2.5–3.0. Melt temperature is held at 220–240 °C at the nozzle, mold wall temperature at 40–60 °C, injection pressure at 80–100 MPa, and packing pressure at 60–80 MPa for wall-thickness-dependent hold times of 10–18 s. A sequential valve-gated hot runner is preferred because gate freeze-off at the drain-port boss and bearing boss otherwise causes voids at the junction of the bearing console and the cylinder wall. Terminal parts include front-load washer outer tubs, top-load wash baskets with lower drive hub, and balance rings that carry the spin-cycle load.
For the dishwasher base frame, the part is run at 100 wt% as delivered when it also functions as the sump support and pump-plate joint; if a cost-reduced unfilled PP copolymer stream is blended, the mineral-filled share is maintained at ≥80 wt% and validated by ISO 179-1/1eA notched Charpy at 23 °C because lower filler content causes the base to creep around the motor-mount inserts. Applicable safety standards are IEC 60335-2-5 for dishwashers and IEC 60335-1:2020 Clause 30.2, with flammability at UL 94 HB and glow-wire testing according to IEC 60695-2-11 typically at 750 °C for unattended appliance parts where the connection current exceeds 0.5 A. Chemical resistance is tested to ISO 175:2010 using 0.5 wt% sodium tripolyphosphate at 80 °C for 48 h, with retained flexural strength and no surface blushing. Molding is performed on a single-cavity tool with a hot-tip gate at the geometric center and a clamp force of 8,000–12,000 kN because the elongated base pan has a projected area of 0.7–1.1 m². Melt temperature is 210–230 °C, mold temperature 30–50 °C, injection speed 60–120 mm/s, packing pressure 50–70 MPa for 8–12 s, and back pressure 6–10 bar. A production-scale failure mode observed on these tools is jetting near the gate when the injection speed exceeds 120 mm/s because the talc platelets separate from the melt front and create a visible flow line at the pump-mount bridge. Terminal parts are dishwasher base frames, sump housings, spray-arm supports, and filter retention rings, all of which must maintain edge flatness within 1.0 mm over the 600 mm diagonal to keep pump and door-latch alignment.
In refrigerators, shelf frames and door-bin brackets in the fresh-food compartment see temperatures from 2 °C to 8 °C and occasional contact with vegetable oil and citric acid; the deep-freeze trim plate can be pulled at -25 °C during door opening. PP-36380 GA is run at 85–100 wt%, with 0–15 wt% post-industrial PP copolymer regrind that meets food-contact feedstock control under FDA 21 CFR 177.1520 and EU 10/2011; if the shelf frame is not a direct food-contact surface, the loading ratio is determined by impact retention rather than migration. For parts intended for direct food contact, only lot-certified pellets are used, and the overall migration limit of 10 mg/dm² under EU 10/2011 must be verified on the finished part because mineral filler may locally compromise organoleptic neutrality. Safety compliance for motor-driven refrigerators is IEC 60335-2-24; material qualification includes ISO 179-1/1eA Charpy notched impact at -20 °C, ISO 178 flexural modulus, and ISO 306 Vicat softening. The molding process uses melt temperature 200–220 °C, mold wall 20–40 °C, injection pressure 70–90 MPa, hold pressure 45–65 MPa, and cooling time 18–25 s for wall thickness 2.0–3.5 mm. Multi-cavity family tools with three-plate cold-runner are standard; gate location is moved to the underside of the shelf bar to avoid weld lines at the glass-support rib. Ejector pin marks and sink marks are critical because surface appearance is a consumer acceptance parameter; if demolding temperature exceeds 55 °C, the pin area can leave a raised ring that is rejected. Terminal parts are refrigerator shelf frames, door-bin brackets, evaporator drip trays, and injection-molded foot pads.
Air-conditioner drain pans and louver frames are mounted in evaporator housings where the condensate is not chemically neutral; dissolved CO₂ and airborne degradation products lower pH to 5–6, and chlorine residues from indoor cleaning chemicals appear in shallow pools. In this application the grade is run at 100 wt% because dilution with unfilled PP reduces the flexural modulus below the level needed for a 400 mm unsupported condensate channel to stay flat after clamp release. The standard set includes IEC 60335-2-40 and IEC 60335-1:2020 Clause 30.2, with flammability UL 94 HB and condensate immersion testing according to ISO 175:2010 in 0.1 vol% acetic acid at 23 °C for 24 h. Processing uses a two-plate cold-runner mold with edge fan gates and a clamp force of 6,000–9,000 kN; melt temperature is 210–230 °C, mold temperature 30–50 °C, injection pressure 65–85 MPa, hold pressure 40–60 MPa for 6–10 s, and total cycle time 35–45 s. The main field failure occurs at the drain outlet boss when the holding pressure falls below 45 MPa and the rib base sinks; a packing profile with two-stage decay from 70 MPa to 40 MPa over 6 s avoids the dimple. Terminal parts are split-unit evaporator drain pans, fan-ring brackets, louver shafts, and the rear shell of the indoor unit.
Around the magnetron and waveguide, structural brackets are exposed to forced-convection heat at 60–85 °C and must not creep because the grounding-screw torque would decay. PP-36380 GA is processed at 100 wt% for brackets and at 90–95 wt% when a color masterbatch is introduced; the balance is a talc-filled PP carrier masterbatch, not an unfilled PP, to prevent anisotropic shrinkage from reappearing. In-house regrind is held to ≤10 wt%; if regrind exceeds this level, weld-line impact strength at the waveguide slot measured by ISO 179-1/1eA falls below the target 3.5 kJ/m² at 23 °C. Applicable product standards are IEC 60335-2-25 for microwave ovens and IEC 60335-1:2020 Clause 30.2; because PP is not inherently flame retardant, the bracket is located behind a grounded sheet-metal shield and is not the direct enclosure. Ball pressure testing under IEC 60695-10-2 is used at 75 °C or higher according to the maximum accessible surface temperature. Molding uses a melt temperature of 220–240 °C, mold temperature 40–60 °C, injection pressure 80–110 MPa, hold pressure 55–75 MPa, and fast injection to fill multiple holes and snap bosses. A hot-tip direct gate at the thick base with sequential edge gates prevents hesitation lines around the magnetron pocket. Terminal parts are microwave baseplates, waveguide support brackets, rear panel clips, and turntable-ring retainers.
For floor-care nozzle housings, long flat parts with nominal wall 1.2–2.0 mm, multiple wheel axles, and a 180° airflow channel require controlled shrinkage after demolding. PP-36380 GA is used at 85–100 wt%; post-industrial PP regrind from runners is allowed up to 15 wt% only if sieve fraction is ≤4 mm and no metal or polyamide contamination from wheel-axle inserts is present. Safety standard for vacuum cleaners is IEC 60335-2-2; flammability of the PP material is UL 94 HB. The dominant quality criterion is the flatness of the bottom lip that seals the brush bar; tool temperature differential over the length must not exceed 8 °C. Molding uses melt temperature 200–230 °C, mold temperature 25–45 °C, injection pressure 70–100 MPa, hold time 5–10 s, and clamp force 5,000–8,000 kN. A cold-runner with two submarine gates is common; the gate land length is kept below 0.8 mm to prevent pressure loss. Terminal parts are floor nozzle housings, brush-bar covers, motor covers, and rear cord-winder brackets.
Competitive Kingfa PP-36380 GA,PP-TD Mineral Filled High Impact Low Warpage,Home Appliance prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-36380 GA is a PP-TD mineral-filled polypropylene injection moulding grade specified for home appliance structural parts requiring high impact resistance, low warpage and dimensional stability in large, flat or ribbed housings. The PP-TD designation denotes a talc-modified polypropylene system in which the platy mineral filler is present in the typical class range of 20–40 wt%. The compound is impact-modified through a heterophasic copolymer or dispersed elastomeric phase, placing it between unfilled PP and reinforced engineering thermoplastics. In practical terms, the material retains polypropylene’s flow length and weld-line tolerance while reducing mould shrinkage from the 1.2–1.6 % range observed in unfilled polypropylene to approximately 0.4–0.8 % in constrained mould geometries. This shrinkage reduction is accompanied by lower anisotropy between flow and transverse directions, which is a primary control variable for warpage in appliance panels. The manufacturer’s certificate of analysis should be consulted for exact lot-specific melt flow rate, ash content, tensile data and impact values; the numerical ranges in this document refer to the general class of 20–40 wt% talc-filled, impact-modified PP-TD appliance compounds, not to a single lot of PP-36380 GA. Published data for this specific configuration is limited where stated. The grade is intended for injection moulding of washing machine top plates, air-conditioner cabinets, dishwasher frames, refrigerator lower door panels, and small appliance structural brackets. Compared with unfilled polypropylene, PP-36380 GA exhibits higher density, lower post-moulding drift and improved stiffness. Compared with general-purpose talc-filled PP homopolymer, the high-impact modification shifts failure from unstable crack propagation toward ductile drawing at room temperature. It is not intended for continuous exposure to chlorinated solvents or strong oxidizers; manufacturer regulatory declarations for RoHS 2011/65/EU and REACH 1907/2006 should be requested for final appliance compliance.
Unfilled PP homopolymer commonly shows a notched Charpy impact strength of 3–6 kJ/m² at 23 °C when tested according to ISO 179-1/1eA, while a standard 20 % talc-filled PP homopolymer often remains in the 4–7 kJ/m² range. Impact-modified PP-TD compounds of the class represented by PP-36380 GA are engineered to operate in the 8–20 kJ/m² range at the same condition, though the exact lot-specific value must be verified from the manufacturer’s certificate of analysis. The toughening mechanism relies on a dispersed elastomeric phase, typically an ethylene-propylene rubber or an in-reactor impact copolymer, that cavitates under load and permits shear yielding in the polypropylene matrix. This changes fracture behaviour in thin-walled appliance housings: a crack initiated at a sharp corner, screw boss, weld line or gate remnant is less likely to propagate across a large side panel. Notched Izod impact following ISO 180/A is sometimes reported, but Charpy is more common in PP-TD datasheet comparisons for appliance specifications. On production lines, the brittle-to-ductile transition is often the controlling criterion; parts moulded from unfilled or low-impact talc compounds may crack at drop heights below 300 mm, while impact-modified PP-TD grades are selected to survive repeated assembly and transport events. Low-temperature performance depends on rubber phase content and dispersion quality. At sub-zero temperatures the notched impact value declines, and design predictions should not extrapolate room-temperature data below 0 °C without lot-specific validation.
On a twin-screw extrusion line with L/D 40–48 and a side feeder, talc is introduced downstream of the main polymer melting zone to control shear heating and preserve the aspect ratio of the platy filler. Stock temperatures at the die are typically maintained between 190 °C and 230 °C for impact-copolymer PP-TD compounds; lower temperatures reduce thermal degradation of the impact modifier, while higher temperatures may be necessary for high-throughput dispersion. Screw torque and melt pressure are higher than for unfilled PP at the same output, and pelletizing is usually carried out using an underwater or strand system with a mineral-filled grade-specific die. Injection moulders often specify an MFR window of ±2 g/10 min around the nominal value to maintain stable cushion control and gate freeze behaviour. PP-TD mineral-filled pellets are not hygroscopic in the sense of polyamide or PBT, but condensation on cold pellet surfaces can occur after warehouse storage at high relative humidity. If surface splay or weld-line porosity appears during startup, pre-drying at 70–80 °C for 2–4 h in a desiccant or hot-air hopper is typically sufficient for the class. When processing PP-36380 GA as a specific grade, the manufacturer’s processing guide for drying and melt temperature should supersede these general settings. Compared with unfilled PP, the talc-filled high-impact system shows a narrower processing window for surface appearance; too low a melt temperature yields flow lines and exposed talc platelets, while excessive melt temperature above 250 °C may cause rubber phase coalescence and a decline in notched impact performance.
Warpage in mineral-filled polypropylene is primarily governed by differential mould shrinkage between flow and transverse directions, thickness-dependent cooling, and gate location. The platy talc in PP-36380 GA reduces average shrinkage and narrows the anisotropy ratio, which is the practical reason it is specified for low-warpage appliance parts. Mould shrinkage is measured on plaques according to ISO 294-4 after conditioning at 23±2 °C and 50±10 % RH per ISO 291. For the 20–40 wt% talc-filled impact-copolymer class, flow-direction shrinkage is commonly 0.4–0.8 % and transverse-direction shrinkage is within 0.1–0.3 percentage points of that value. Unfilled PP typically exhibits 1.2–1.8 % shrinkage with larger anisotropy. The low-warpage effect is not absolute: thick bosses, abrupt wall-thickness transitions and non-uniform cooling can still generate out-of-plane distortion, so moulding simulation based on measured shrinkage data is required for tooling layout.
| Property | Test method | Typical class envelope for 20–40 wt% talc-filled impact PP-TD | Operational note |
|---|---|---|---|
| Density | ISO 1183-1 | 1.05–1.12 g/cm³ | Higher than unfilled 0.90–0.91 g/cm³; affects shot size and part weight |
| Melt mass-flow rate | ISO 1133-1 at 230 °C/2.16 kg | 10–30 g/10 min | Lower values may require higher injection speed; very high values may reduce impact |
| Tensile yield stress | ISO 527-2/1A | 25–35 MPa | Used for first-order stress calculations; long-term creep is not covered |
| Flexural modulus | ISO 178 | 2200–3500 MPa | Controls panel deflection under load and perceived stiffness |
| Notched Charpy at 23 °C | ISO 179-1/1eA | 8–20 kJ/m² | Ductile failure preferred; sub-zero lot-specific validation advised |
| Heat deflection temperature at 0.45 MPa | ISO 75-2/B | 100–130 °C | Short-term peak exposure; not a continuous service temperature |
| Mould shrinkage | ISO 294-4 | 0.4–0.8 % | Measured on plaques; geometry-dependent shrinkage remains possible |
For large home appliance housings, injection moulding of PP-36380 GA requires control of melt temperature, mould temperature, injection velocity and holding pressure because these variables influence both surface appearance and final dimensions. Melt temperature is typically set between 210 °C and 250 °C, with the lower end suitable for thicker sections and the upper end for thin-wall filling; mould temperature is often held between 20 °C and 60 °C. For textured or low-gloss appliance surfaces, the mould may be kept below 40 °C to reduce cycle time, but high-gloss surfaces and weld-line strength improve when the tool is heated to 50–60 °C. Injection pressure on production machines is commonly in the range of 60–100 MPa hydraulic pressure, while holding pressure is set at 40–80 % of the injection pressure to pack the gate without overfilling. Gate freeze must be confirmed by sequential weight sampling; if the gate remains unfrozen when holding pressure is released, melt may flow back from the cavity and increase sink, dimensional scatter and warpage.
On clamp force units from 800 t to 1,500 t used for refrigerator door panels and washing machine base frames, the primary processing bottleneck is differential cooling across thick ribs and thin walls. The talc-filled PP-TD compound has lower heat distortion than reinforced engineering thermoplastics, but its thermal diffusivity is higher than unfilled PP because of the mineral filler; cooling times for wall thicknesses of 2.0–3.5 mm are typically 15–40 s. The low-warpage property is achieved only when the mould is balanced: multiple hot drops should be sized to within 0.8–1.5 mm gate diameter, and weld lines should be moved to low-stress areas by filling simulation. In comparison with glass-fiber-reinforced PP, the mineral-filled PP-TD grade produces lower orientation-induced warping and better surface quality, but it has lower stiffness and creep resistance. In comparison with unfilled PP, the increase in density and melt viscosity must be accepted. For dishwasher base trays, air-conditioner front frames and refrigerator lower door panels, the relevant material selection criterion is not a single property but the balanced combination of notched impact above 8 kJ/m², mould shrinkage below 0.8 % and shrinkage anisotropy below 0.3 percentage points when processed under stable packing conditions. Published data for this specific configuration is limited in open literature; lot-specific product datasheets and certificate-of-analysis values remain the authoritative source for PP-36380 GA.