Kingfa PP-36385,Mineral Filled PP (High Impact, Heat Resistant, Low Warpage)

    • Product Name: Kingfa PP-36385,Mineral Filled PP (High Impact, Heat Resistant, Low Warpage)
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 183249
    Filler Type Mineral
    Density 1.05 g/cm³ (typical)
    Melt Flow Rate 8 g/10 min (230°C/2.16 kg, typical)
    Tensile Strength 25 MPa (typical)
    Tensile Elongation At Break 30% (typical)
    Flexural Modulus 1800 MPa (typical)
    Flexural Strength 35 MPa (typical)
    Notched Izod Impact Strength At 23 C 25 kJ/m² (typical)
    Notched Izod Impact Strength At 20 C 8 kJ/m² (typical)
    Heat Deflection Temperature At 1 82 Mpa 105°C (typical)
    Heat Deflection Temperature At 0 45 Mpa 130°C (typical)
    Vicat Softening Temperature 145°C (typical)
    Molding Shrinkage 0.8% (typical)
    Water Absorption 0.02% (typical)

    As an accredited Kingfa PP-36385,Mineral Filled PP (High Impact, Heat Resistant, Low Warpage) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa PP-36385 mineral-filled PP is packaged in 25 kg moisture-proof paper-plastic bags, palletized and wrapped for secure transport and storage.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Kingfa PP-36385 mineral-filled polypropylene, high impact, heat resistant, low warpage, securely loaded in a 20′ FCL container.
    Shipping Kingfa PP-36385 is supplied as mineral-filled polypropylene pellets in moisture-barrier bags or bulk containers. It is non-hazardous and not regulated for transport. Ship in dry, ventilated conditions, protected from moisture, sunlight, and contamination; handle with standard industrial PPE.
    Storage Store Kingfa PP-36385 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags sealed and palletized off the floor to prevent moisture pickup and contamination. Avoid excessive stacking, follow the supplier’s SDS and local regulations, and use first-in, first-out stock rotation. Do not store near food or drink.
    Shelf Life Shelf life is typically 12 months in original sealed packaging, stored dry, below 30°C, protected from moisture and direct sunlight.
    Application of Kingfa PP-36385,Mineral Filled PP (High Impact, Heat Resistant, Low Warpage)

    What Limits Post-Mould Warpage in Automotive Instrument Panel Substrates?

    Mineral-filled polypropylene with a nominal talc or calcium carbonate filler content of 20–30 wt% is processed into large-area interior substrates where dimensional flatness and low volatile output are jointly specified. The formulation addition ratio of the base mineral-filled PP compound occupies 85–95 wt% of the final moulding blend, with the remaining mass split among colour masterbatch (2–4 wt%), UV and hindered amine stabiliser packages (0.3–0.8 wt%), zinc stearate processing lubricant (0.2–0.5 wt%), and, where low-VOC requirements are stringent, a compatibilised scavenger masterbatch (0.5–1.5 wt%). Compliance for interior automotive applications is anchored to ISO 3795 (burn rate ≤ 100 mm/min for materials in the passenger compartment), VDA 277 (total VOC emissions typically ≤ 100 µg C/g for visible interior parts), VDA 270 (odour rating ≤ 3 after 24 h at 80°C), DIN 75201-B (fogging gravimetric ≤ 5 mg), and the End-of-Life Vehicles Directive 2000/53/EC. The production route is injection moulding on presses with clamp force from 8,000 to 30,000 kN, a barrel temperature profile of 210–240°C, and a mould temperature of 30–60°C. Screw back pressure is maintained at 0.8–1.5 MPa, and the injection velocity profile is tuned to keep the shear rate below 50,000 s⁻¹ in thin ribs. Holding pressure is set between 50–70 MPa for a gate-seal time of 8–15 s. Sequential valve gate control is applied to substrata exceeding 600 mm flow length to prevent weld-line sinking and to keep warpage below 0.3% across the diagonal dimension. On production-scale lines, a recurring failure mode is sink mark formation at the intersection of mounting bosses and back-surface ribs when the core cooling channel spacing exceeds 40 mm; this is mitigated by conformal cooling inserts or by reducing the rib-to-wall thickness ratio to below 0.6. Terminal components include instrument panel carriers, door trim panels, centre console frames, and seat back boards. Published data for the specific Kingfa PP-36385 grade may vary from these general mineral-filled PP processing envelopes; end users are advised to validate against the supplier’s latest technical data sheet.

    In front-loading washing machine outer tubs, the mineral-filled PP compound is injected in a multi-nozzle hot runner system with shot weights from 4 to 9 kg and a clamp force of 12,000–25,000 kN. The resin addition ratio in the formulation is 98–100 wt% unless a hydrolysis-resistant additive package is specified; in that case a 0.2–0.5 wt% carbodiimide-based anti-hydrolysis masterbatch is introduced and the base resin fraction is reduced to 97.5–99.8 wt%. Compliance is evaluated under IEC 60335-2-7 for household washing machines, including the 15-day door seal integrity test and insulation resistance checks after water spillage; material-level evidence typically includes IEC 60112 comparative tracking index ≥ 600 V, UL 94 HB at 1.5 mm, and REACH SVHC screening under 1907/2006/EC. The production process requires a barrel temperature profile of 220–250°C, mould temperature 40–70°C to reduce post-mould dimensional drift, screw back pressure 0.5–1.0 MPa, and an injection speed of 80–150 mm/s for the filling phase. Terminal parts include outer tub assemblies, dishwasher sump housings, and top-loading washer bases. On full-scale lines, the largest source of batch-to-batch variability is filler dispersion during compounding; a melt flow rate swing of ±15% shifts the tub bottom flatness by 0.4–0.8 mm, which exceeds the 0.3 mm sealing surface tolerance required by OEM specifications. This application space is not suitable for long-term exposure to aggressive alkaline detergents at concentrations above 5% sodium hydroxide at 90°C; such conditions require a shift to a chemically coupled PP grade or a separate thermoset liner.

    Power Tool Housing: Impact Mechanics and UL 60745 Compliance

    Mineral-filled PP grades used for double-insulated power tool housings are typically processed into thin-wall sections of 1.8–2.5 mm nominal thickness, where the filler content contributes to low warpage but reduces ductile failure resistance if the matrix is not impact-modified. The resin addition ratio in the hard component of a two-shot moulding is 80–95 wt% of the total shot, with the remaining 5–20 wt% consisting of a soft TPE overmould for grip zones, colour masterbatch, and antistatic additives. Compliance for corded and battery-powered hand-held tools is assessed under EN 62841-1:2015, including the drop test in clause 20.3 (typically 1.2 m onto a concrete surface) and the mechanical hazard evaluation in clause 19; material-level evidence includes ISO 179-1/1eA notched Charpy impact strength, which for general-purpose mineral-filled PP typically lies in the range 6–12 kJ/m² at 23°C and 3–5 kJ/m² at -20°C, and UL 94 HB at 1.5 mm. The injection moulding process uses presses with clamp force of 3,000–8,000 kN, a melt temperature of 210–235°C, mould temperature 35–55°C, and gas-assisted injection for hollow handle sections to prevent sink marks and reduce part mass. Screw recovery speed is reduced to 80–120 RPM to limit filler attrition and maintain impact retention. Terminal components include angle grinder housings, drill/driver housings, hammer drill bodies, and battery pack shells. A known production-scale failure mode is cold weld-line fracture at the intersection of the gearbox mounting boss and the side wall when the mould temperature drops below 30°C; raising the mould setpoint to 45°C and relocating the gate away from the high-stress boss base improves weld-line strength by approximately 15–20% in Charpy tests. Published data for the specific Kingfa PP-36385 grade may differ from these general mineral-filled PP impact ranges; end users should validate against the supplier’s latest technical data sheet.

    When Low-Voltage Electrical Enclosures Must Survive a 3 mm Glow-Wire End-Product Test

    In low-voltage switchgear and installation boxes, a mineral-filled PP compound with low warpage characteristics is processed into four-wall housings with wall thickness from 2.0 to 3.5 mm to minimise post-mould deflection. The resin addition ratio is 100 wt% when no flame-retardant or track-resistant modification is required; formulations requiring improved arc resistance may incorporate 1–3 wt% of a modified silicone additive to raise surface resistivity, with the base mineral-filled PP fraction reduced to 97–99 wt%. End-product compliance is tested under IEC 60695-2-11 glow-wire flammability at 750°C with no ignition or self-extinguishing within 2 s, IEC 60695-2-12 for finished products, UL 94 V-2 at 1.5 mm for material classification, IEC 60112 comparative tracking index ≥ 250 V for pollution degree 2 environments, and ASTM D495 arc resistance > 180 s at 420 V. The production process uses multi-cavity moulds with 8–32 cavities, a melt temperature of 215–240°C, mould temperature of 50–65°C, and an extended holding pressure of 60–80 MPa for 10–20 s to compensate for filler-induced shrinkage anisotropy. Post-mould annealing at 100°C for 2 h is applied to reduce residual stress in snap-fit latching features. Terminal components include distribution box housings, terminal block enclosures, wall switch plates, and circuit breaker bases. On production lines, the dominant defect is out-of-roundness in cylindrical boss features caused by non-uniform cooling between the core and cavity; this is addressed by beryllium-copper core pins or by reducing the boss diameter-to-wall thickness ratio to 2.5 or lower.

    For office chair five-star bases and structural leg components, the mineral-filled PP compound is used at 100 wt% with a colour masterbatch addition of 1–2 wt% in single-cavity or two-cavity cold-runner moulds. Compliance is limited to mechanical durability testing under ANSI/BIFMA X5.1-2017, EN 1335-3:2009, and REACH Annex XVII restrictions. The injection process operates at a melt temperature of 190–220°C and an aluminium mould temperature of 20–40°C; insufficient cooling time below 45 s leads to hub shrinkage and audible creaking under cyclic load. Terminal parts include five-star bases, armrest frames, and table leg inserts.

    HVAC Condensate Drain Pans and the Role of Low-Warpage Geometry Under Hygrothermal Cycling

    In HVAC condensate management, mineral-filled PP with low warpage is specified for large flat drain pans where accumulated water weight and temperature cycling cause sagging in unfilled thermoplastics. The resin addition ratio is 98–99.5 wt% of the final moulding formulation, with a silver-glass antimicrobial masterbatch at 0.5–1.5 wt% to suppress biofilm formation on wet surfaces and a hindered phenolic thermal stabiliser at 0.2–0.3 wt% for long-term hot air exposure. Compliance is assessed under UL 94 HB at 1.5 mm, ASTM D648 heat deflection temperature at 1.82 MPa typically ≥ 110°C for mineral-filled PP, UL 746B relative thermal index ≥ 65°C for mechanical properties, ISO 4892-2 accelerated weathering (cycle 1) requiring ΔE ≤ 3 after 1,000 h, and REACH 1907/2006/EC. Production is injection moulding with clamp force from 5,000 to 15,000 kN, a melt temperature of 220–245°C, mould temperature 50–70°C, and cooling circuit layout designed to maintain a maximum inter-circuit temperature difference of 5°C across the pan floor to prevent differential shrinkage. Terminal components include condensate drain pans, blower housings, and indoor unit water trays. A recurrent production bottleneck is core-side vacuum venting during mould opening, which distorts the pan floor when the core has been textured to VDI 24; applying a 0.5–1.0 mm mould opening pause reduces the vacuum load and preserves floor flatness within 0.5 mm across a 900 mm span.

    Free Quote

    Competitive Kingfa PP-36385,Mineral Filled PP (High Impact, Heat Resistant, Low Warpage) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa PP-36385 is classified as a mineral-filled polypropylene compound within the high-impact, heat-resistant, low-warpage product family. The grade designation PP-36385 identifies an injection-molding compound in which a mineral filler system is dispersed in an impact-modified polypropylene matrix. Published multi-lot data for this exact configuration are limited to supplier documentation; the information below therefore uses class-typical property ranges and processing limits for mineral-filled high-impact PP and is not a substitute for a lot-specific certificate of analysis.

    Incoming inspection for this class of material is normally conducted by melt flow rate measurement under ISO 1133-1:2022 at 230 °C with a 2.16 kg load. Injection-molding grades in the mineral-filled high-impact PP class commonly fall between 8 g/10 min and 20 g/10 min. Density measured by ISO 1183-1:2019 is generally between 1.03 g/cm³ and 1.10 g/cm³, depending on filler loading. Lot-to-lot variation in melt flow rate outside ±5 % of the supplier nominal can alter fill pressure and shrink compensation in thin-wall tools and should be controlled at incoming inspection.

    How Does PP-36385 Shift the Mechanical and Thermal Envelope Compared with Unfilled Impact Copolymer PP?

    The mineral filler system raises flexural modulus and heat deflection temperature while reducing mold shrinkage anisotropy. In public technical literature for mineral-filled impact-modified PP, flexural modulus measured by ISO 178:2019 is reported between 1800 MPa and 2600 MPa; unfilled impact copolymer PP typically lies between 1000 MPa and 1400 MPa. Tensile yield strength by ISO 527-2:2012 is commonly 22 MPa to 28 MPa. Notched Charpy impact at 23 °C under ISO 179-1/1eA is retained at 5 kJ/m² to 10 kJ/m² in high-impact mineral-filled formulations; low-temperature impact at -20 °C depends on the impact modifier and must be confirmed for PP-36385.

    Table 1 summarizes representative property ranges reported for the two material classes. The table is not PP-36385 lot data and is provided for comparative orientation only.

    PropertyTest methodUnfilled impact copolymer PPMineral-filled high-impact PP class
    DensityISO 1183-1:20190.900–0.915 g/cm³1.03–1.10 g/cm³
    Melt flow rateISO 1133-1:2022, 230 °C, 2.16 kg8–20 g/10 min8–20 g/10 min
    Tensile yield strengthISO 527-2:201220–26 MPa22–28 MPa
    Flexural modulusISO 178:20191000–1400 MPa1800–2600 MPa
    Notched Charpy impact, 23 °CISO 179-1/1eA20–35 kJ/m²5–10 kJ/m²
    Heat deflection temperature, 0.45 MPaISO 75-2/B:201385–100 °C100–120 °C
    Mold shrinkageISO 294-4:20181.0 %–1.4 %0.8 %–1.1 %

    Compared with standard talc-filled PP, the high-impact designation for PP-36385 implies an elastomer-modified matrix that improves notched impact retention, particularly at low temperature. A standard talc-filled PP at equivalent filler loading can show notched Charpy at -20 °C below 2 kJ/m², whereas impact-modified grades are designed to retain higher values; the exact value for PP-36385 must be read from the supplier datasheet. Compared with glass-fiber-reinforced PP, the mineral-filled system offers lower density, lower flow/cross-flow shrinkage differential, and reduced surface fiber prominence, but lower tensile strength and flexural modulus. Glass-fiber PP can exceed 3500 MPa in flexural modulus and 70 MPa in tensile strength, with the trade-off of greater anisotropy and warpage.

    The low-warpage characteristic is governed by filler aspect ratio, particle size distribution, coupling agent efficiency, and processing-induced orientation. A low-warpage mineral-filled PP typically contains surface-treated mineral that reduces differential orientation during mold filling. Under ISO 294-4:2018, the ratio of flow-direction to cross-flow mold shrinkage in a low-warpage filled grade is often below 1.1, while unfilled impact PP can exceed 1.2.

    Processing Boundaries for Mineral-Filled High-Impact PP on Injection Molding Lines

    Mineral-filled PP compounds of this class are produced on co-rotating twin-screw extruders with L/D ratios between 40:1 and 52:1 to achieve dispersive mixing of filler and impact modifier. The downstream feeding of the mineral filler limits attrition and protects screw elements. PP-36385 is supplied as pellets; incoming pellet size should be uniform to prevent bridging in the feed throat.

    Before injection molding, the granulate should be protected from moisture. Although polypropylene is not hygroscopic, mineral fillers can adsorb surface moisture. If storage relative humidity exceeds 60 %, predrying at 80 °C to 90 °C for 2 h to 4 h in a desiccant dryer is a processing boundary for this class. Drying above 90 °C or for more than 6 h can cause granule blocking and should be avoided. Barrel temperatures from feed throat to nozzle are typically set at 190 °C, 210 °C, 220 °C, 225 °C, and 225 °C. The measured melt temperature should not exceed 240 °C; above this limit, oxidative degradation and coupling agent decomposition can reduce impact and generate surface defects. A general-purpose screw with an L/D ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.0:1 is suitable. Back pressure between 0.3 MPa and 0.7 MPa maintains melt density without excessive filler attrition.

    Mold surface temperature is a central control for low-warpage behavior. A range of 20 °C to 50 °C is used in production; the lower portion reduces cycle time, while the upper portion improves surface appearance and reduces flow-induced orientation. For nominal wall stock of 2.0 mm to 2.5 mm, injection velocity should be set to achieve a fill time of 1.0 s to 2.0 s. Excessively fast fill causes shear heating at the gate and can produce flow lines. Multi-cavity tools with naturally balanced runners are preferred because mineral-filled PP is sensitive to thermal imbalance; mold-filling simulation should be used to verify shear-rate distribution before tool steel is cut.

    Warpage on production equipment is often caused by differential packing rather than material shrinkage alone. On a 1200 kN clamping force machine, transfer pressure should be set so that cavity pressure at the gate reaches 35 MPa to 55 MPa before switchover to holding pressure. Holding pressure is then maintained at 60 % to 80 % of peak injection pressure for a time equal to gate seal time plus 0.5 s. Gate seal can be verified by weighing parts at increasing hold times; part weight plateaus when the gate freezes. Inadequate hold time produces sink marks and higher flow-direction shrinkage, which can override the low-warpage benefit of the filler.

    PP-36385 should not be blended with high-melt-flow homopolymer PP unless a reduction in notched impact is acceptable. Avoid contact with strong oxidizing acids, halogens, and certain transition-metal salts at elevated temperature because these accelerate thermo-oxidative degradation. Color masterbatches based on unsaturated carrier resins can reduce long-term heat aging resistance; a polyolefin-based carrier should be specified.

    The addition of mineral filler raises thermal conductivity, which can reduce cooling time but increases abrasion on screw and barrel surfaces. For production runs above 500,000 cycles, a bimetallic barrel and hardened screw are recommended to avoid clearance from filler abrasion. Weld-line strength in mineral-filled PP can be 20 % to 30 % lower than bulk unnotched strength measured by ISO 527-2:2012; gate locations should therefore be shifted away from load paths or the part should be redesigned to move weld lines into low-stress regions.

    Regulatory submissions for PP-36385 require lot-specific declarations. The supplier should be requested to provide compliance information against EU REACH Regulation EC 1907/2006, EU RoHS Directive 2011/65/EU as amended, and, where relevant, EU 10/2011 or FDA 21 CFR food-contact requirements. This paragraph is not a compliance statement for PP-36385.

    Heat resistance in PP-36385 is not equivalent to a continuous-use temperature rating. The mineral filler raises heat deflection temperature, but long-term oxidative resistance is controlled by the stabilizer system. A relative thermal index by UL 746B or an automotive heat aging specification should be obtained before continuous service above 90 °C.

    Among production-scale application scenarios, automotive HVAC housings and fan shrouds use this class because design service temperatures can reach 105 °C and the parts must maintain flatness after repeated heating. Heat deflection temperature at 0.45 MPa by ISO 75-2/B:2013 for this class is typically 100 °C to 120 °C, permitting short-term exposure at that service temperature. Long-term heat aging for PP-36385 must be obtained from the supplier; the oxidative stabilizer package and filler surface treatment control impact retention after 1000 h at 120 °C.

    Electrical enclosure frames and appliance structural parts use the low-warpage characteristic to maintain flatness over a gasket sealing face. A flatness tolerance of 0.3 mm over 300 mm length can be exceeded by unfilled impact PP due to differential shrinkage. The mineral filler reduces mold shrinkage to 0.8 %–1.1 % under ISO 294-4:2018 and lowers the difference between flow and cross-flow shrinkage. Parts should be measured after conditioning for 24 h at 23 °C and 50 % relative humidity because post-mold crystallization can change dimensions by 0.05 % to 0.15 %.

    Cold-climate under-hood parts require a validated notched impact at -30 °C; this value must be measured using ISO 179-1/1eA on the actual molded part because thickness and gate freeze conditions change the orientation of the impact modifier. Published general data for PP-36385 should not replace application-specific testing.

    At tool qualification, a 25-point shrinkage grid is measured after 24 h conditioning using ISO 294-4:2018, and the difference between maximum and minimum shrinkage should be less than 0.15 % for low-warpage acceptance. Parts that fail this criterion are usually corrected by moving the gate, adjusting fill time, or raising mold surface temperature to reduce orientation.