Kingfa PP-91905,PP Copolymer, Mineral Filled

    • Product Name: Kingfa PP-91905,PP Copolymer, Mineral Filled
    • Factroy Site: Guangzhou Science City, Guangdong Province, China
    • Price Inquiry: sales3@ascent-chem.com
    • Manufacturer: Kingfa Sci. & Tech. Co., Ltd.
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 733530
    Product Kingfa PP-91905
    Polymer Type PP Copolymer
    Filler Type Mineral Filled
    Density 1.05 g/cm³
    Melt Flow Rate 10 g/10 min (230°C/2.16 kg)
    Tensile Strength 25 MPa
    Elongation At Break 20%
    Flexural Modulus 2200 MPa
    Notched Izod Impact Strength 5 kJ/m²
    Heat Deflection Temperature 110°C (0.45 MPa)
    Vicat Softening Temperature 140°C
    Molding Shrinkage 1.2%
    Water Absorption 0.02%
    Flame Rating HB

    As an accredited Kingfa PP-91905,PP Copolymer, Mineral Filled factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Kingfa PP-91905 is packaged in 25 kg moisture-resistant bags, 40 bags per pallet (1,000 kg total), with batch labels.
    Container Loading (20′ FCL) Kingfa PP-91905 PP Copolymer Mineral Filled, packed in 25 kg bags on pallets, loaded securely in one 20-foot FCL container.
    Shipping Kingfa PP-91905, PP Copolymer, Mineral Filled is a non-hazardous polymer resin shipped in moisture-resistant 25 kg bags or bulk containers. Keep dry and ventilated, away from direct sunlight, heat, and contamination during transit and storage. No special dangerous-goods transport requirements apply; follow standard handling practices.
    Storage Store Kingfa PP-91905 in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original packaging sealed to prevent moisture absorption and contamination. Place pallets on a clean, dry surface and avoid prolonged UV exposure. Follow first-in, first-out stock rotation; avoid storage near strong oxidizers or incompatible chemicals.
    Shelf Life Typically 24 months from manufacture when stored sealed in a cool, dry place, protected from moisture and direct sunlight.
    Application of Kingfa PP-91905,PP Copolymer, Mineral Filled

    Kingfa PP-91905 is a mineral-filled polypropylene copolymer supplied as a ready-to-mold pellet. The application set below is limited to established downstream conversion routes for mineral-filled PP copolymers in structural, non-food-contact, and non-implantable components. Grade-specific data sheet values are not reproduced because they are controlled under commercial revision limits; where numerical process boundaries appear, they refer to the material class and must be verified against the current supplier specification. The document does not constitute a purchase or design warranty.

    Automotive Lower Trim Carriers and Dimensional Tolerance Budgets

    Door panel lower carriers, glove box trays, and center console side panels combine low-temperature hinge impact with post-mold flatness requirements. The regulatory basis for interior trim includes FMVSS 302 and ISO 3795 for horizontal burning rate, with OEM-specific VOC screening under VDA 277 when the part is installed below the beltline. Compliance with ELV Directive 2000/53/EC Annex II is required for lead, cadmium, mercury, and hexavalent chromium, and REACH SVHC declarations are standard in EU export documentation. The addition ratio at the injection floor is normally 100 wt% neat resin; if a thin-wall glove box tray tool requires reduced fill pressure, a 10–20 wt% let-down with virgin PP copolymer is used, but this lowers the mineral-filler skeleton and may increase flow-direction shrinkage. The downstream production process is multi-nozzle injection molding on 1,800–2,500 t clamp force machines with sequenced valve gates. Melt temperature for the mineral-filled PP copolymer class is held between 220 °C and 250 °C; mold temperature is maintained at 30–60 °C. On large single-cavity door carrier tools, melt-front velocity above approximately 350 mm/s at the gate is associated with gate blush and filler orientation streaks; reducing fill velocity stabilizes the frozen skin layer but can extend fill time and reduce production output. Post-mold dimensional tolerance budgets are governed by anisotropic shrinkage; published data for this specific PP-91905 configuration is limited, but mineral-filled PP copolymers of this class typically show cross-flow shrinkage larger than flow-direction shrinkage. Terminal part families include door module lower carriers, instrument panel lower trim, glove box outer trays, center console side supports, and seat side shields.

    In top-loading washing machine outer tub carriers and base frame supports, the resin is evaluated under repeated exposure to alkaline detergent solution at 60 °C and intermittent drum out-of-balance loading. Compliance screening is tied to IEC 60335-1:2020 clause 30.2.2 for resistance to heat and fire, with appliance-specific requirements under IEC 60335-2-7 for washing machines, and material declarations under RoHS Directive 2011/65/EU and REACH. The addition ratio is 100 wt% neat PP-91905 in the tub carrier; converters that re-introduce post-industrial runner regrind from the same production cell cap regrind at 15–25 wt% after moisture-checked storage, and impact-modified lot blending with POE is not standard for this application. The downstream production process is large-shot single-cavity injection molding with sequenced hot runners and hydraulic core pulls for undercut brackets. Melt temperature is held in the 220–240 °C band, and the mold is run at 40–60 °C to reduce sink over deep ribs. The main process boundary is cooling time: wall sections up to 6 mm at the tub bearing collar require pack-and-hold pressure beyond 700 bar hydraulic pressure, and premature screw pullback produces voids on the rear face. Terminal part types include top-loading tub carriers, front-loading base frame rails, balance ring mounting brackets, and detergent dispenser housings.

    What Limits Glass-Free Mineral Reinforcement in Hand-Held Tool Housings?

    Hedge trimmer guard housings, blower fan shrouds, and string trimmer deck covers do not require the full stiffness of short-glass fiber systems, and glass-free mineral reinforcement avoids tool wear and surface fiber prominence. The compliance basis includes IEC 62841-1 for hand-held motor-operated electric tools, EN 60335-2-91 for walk-behind and hand-held lawn trimmers, and ultraviolet weathering validation under ISO 4892-2 cycle A when the part is used in outdoor service. The formulation addition ratio is 100 wt% PP-91905; external color masterbatch is metered at 2–4 wt% at the throat, and secondary mineral filler or glass fiber should not be added because the pellet already contains a dispersed mineral phase. The downstream process is conventional injection molding on 350–1,200 t machines with general-purpose polyolefin screws having compression ratios around 2.2:1. Melt temperature is kept at 210–235 °C, and mold temperature at 30–50 °C. A known production floor failure mode is screw recovery instability when backpressure is set below 10 bar; this causes filler segregation in the melt cushion and visible gloss variation on curved guard surfaces. Terminal part types include hedge trimmer guard housings, blower fan scroll housings, string trimmer motor decks, and electric pruner gear covers.

    Because wall-mounted electrical installation boxes must resist installation torque at ambient temperature while meeting glow-wire ignition criteria, the grade is used in enclosures that do not carry live current during normal use. The regulatory framework is IEC 60670-1:2015 for boxes and enclosures for electrical accessories, with glow-wire testing according to IEC 60695-2-11:2021; North American converters also verify relative thermal index and tracking resistance under UL 746A and UL 746C when UL listing is required. The addition ratio is 100 wt% PP-91905 for standard non-flame-retardant wall boxes. If a distributor or converter modifies the resin with a flame-retardant masterbatch to achieve a 850 °C glow-wire pass on 2.0 mm wall thickness, masterbatch addition levels typically fall between 12 wt% and 20 wt%, but the final melt flow and Izod impact must be requalified because published data for PP-91905 modified with flame-retardant concentrates is limited. The downstream production process is pin-point gated cold-runner molding on 250–700 t machines. Melt temperature is set between 200 °C and 230 °C; mold temperature is held at 30–45 °C to reduce flash on thin break-out webs. The primary process defect is sink around brass-threaded inserts; slow injection velocity below 60 mm/s is used to pack the insert boss before the gate freezes. Terminal part types include flush-mount installation boxes, ceiling rose mounting plates, junction box covers, and consumer-unit blanking plates.

    If Reusable Logistics Assets Require Impact Strength Without Solid-Glass Fill

    Reusable logistics assets such as folding crate side panels and pallet top decks are not selected for continuous heat resistance; they are selected for fork-tine puncture resilience after outdoor cold storage and consistent demolding from low-cost steel tools. The compliance basis includes ISO 8611-1:2021 for flat pallet performance and ISO 8611-2:2021 for rated load testing; where the crate is intended for repeated direct contact with dry, unpackaged food, migration limits under Regulation (EU) 10/2011 are assessed on the finished monolayer wall. The addition ratio in monolayer crate panels is 100 wt% PP-91905. In pallet decks with post-industrial regrind, the grade is maintained at 70–85 wt% and regrind is introduced at 15–30 wt% after lot-level melt flow verification; regenerated material from unknown origins is excluded to preserve low-temperature impact. The downstream production process is either direct injection molding for small totes or structural foam injection molding for thick pallet decks above 25 mm nominal wall. Melt temperature is held between 220 °C and 250 °C; mold temperature is run cool at 20–40 °C to shorten cycle. The critical processing boundary is sub-zero service: fork-tine impacts at below –10 °C require instrumented impact validation under ISO 6603-2; general-purpose PP copolymer toughness should not be assumed without this test. Terminal part types include collapsible crate side panels, distribution tote bases, warehouse pallet top decks, and agricultural propagation tray frames.

    Contract Furniture Shells Demand Gas-Assist Ribbing to Avoid Sink Marks

    In contract seating, gas-assist injection converts uniform wall sections into hollow rib networks; the mineral filler contributes to the stiffness required to resist the bending moment generated by a seated occupant leaning across an armrest. The compliance framework is ANSI/BIFMA X5.1-2020 for office seating performance, EN 12520:2015 for domestic seating mechanical safety, and EN 1728:2012 for test methods. The addition ratio is 100 wt% PP-91905, with color masterbatch metered at 2–3 wt%; impact modifier packages are not required for indoor armrest and seat shell applications. The downstream process is gas-assisted injection molding on 500–1,500 t presses with nitrogen gas delay controlled between 0.5 s and 1.5 s after fill initiation. Melt temperature is held between 215 °C and 235 °C; mold temperature is 30–50 °C. The primary process defect is void formation at the gas-channel ends when gas pressure is ramped too late; this appears as soft spots in the finished part and reduces screw boss pull-out strength. Terminal part types include conference chair armrest shells, task chair seat pans, reception sofa side panels, and table base support covers.

    Underhood, air cleaner lower housings subject the resin to continuous low-amplitude vibration at 85–95 °C, with intermittent exposure to hot air and limited contact with oil mist. The compliance basis for this automotive functional segment includes ISO 16750-5 for chemical loading resistance, ISO 3795 for burning rate where the housing is near the passenger compartment boundary, and REACH Annex XVII restrictions for polycyclic aromatic hydrocarbons in extender oils used in the PP compound. The addition ratio is 100 wt% PP-91905 for air cleaner housings; thin-wall air resonator ducts may be let down with 10–15 wt% virgin PP copolymer to improve melt front balance without losing heat sag resistance. The downstream process is hot-runner injection molding with multi-point valve gates, and weld-line coalescence at the housing perimeter is managed by sequential valve gate opening rather than by raising melt temperature. Melt temperature is kept between 220 °C and 245 °C; mold temperature is set at 40–60 °C to minimize post-mold warpage. A processing boundary is the maximum continuous-use temperature: the mineral-filled PP copolymer class should not be used above 110 °C continuous under load, and published PP-91905-specific thermal aging data is limited. Terminal part types include air cleaner lower housings, HVAC inlet ducts, intake resonator boxes, and windshield cowl side covers.

    Free Quote

    Competitive Kingfa PP-91905,PP Copolymer, Mineral Filled prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8615365186327

    Email: sales3@ascent-chem.com

    Inquiry

    Get Free Quote of Kingfa Sci. & Tech. Co., Ltd.

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Kingfa PP-91905 is supplied under the compound descriptor “PP Copolymer, Mineral Filled.” The material is a melt-compounded heterophasic polypropylene impact copolymer in which a mineral filler is dispersed into a matrix that also contains an ethylene-propylene rubber-like copolymer phase. The mineral component raises flexural modulus, reduces post-mold shrinkage, and lowers linear thermal expansion; the copolymer component improves notched impact and reduces the brittle-failure tendency found in mineral-filled homopolymer grades. Filler identity, loading, particle-size distribution, and surface treatment are controlled by lot-specific documentation. Because the current lot certificate is not reproduced here and published data for this specific configuration is limited, the property envelope in Table 1 is offered as a class-typical control range for mineral-filled PP impact-copolymer compounds, not as a grade-specific release specification.

    The following benchmark envelope is derived from publicly available data for mineral-filled PP impact-copolymer classes and is to be verified against the current Kingfa certificate of analysis.

    PropertyClass-Typical Control EnvelopeTest Method
    Mineral filler loading10–30 wt%ISO 3451-1 method A
    Density1.03–1.06 g/cm³ISO 1183-1 / ASTM D792
    Melt mass-flow rate, 230°C, 2.16 kg8–20 g/10 minISO 1133-1:2022 / ASTM D1238
    Tensile stress at yield18–25 MPaISO 527-2 / ASTM D638
    Tensile strain at break20–60%ISO 527-2 / ASTM D638
    Flexural modulus1500–2200 MPaISO 178 / ASTM D790
    Notched Izod impact, 23°C5–20 kJ/m²ISO 180 / ASTM D256
    Notched Charpy impact, 23°C8–25 kJ/m²ISO 179-1
    Heat deflection temperature, 0.45 MPa80–105°CISO 75-2 method B / ASTM D648
    Mold shrinkage, 24 h, 2 mm plaque0.8–1.1%ISO 294-4 / ASTM D955
    Rockwell hardness, R scale70–90ISO 2039-2 / ASTM D785

    When High-Shear Compounding Meets Low-Temperature Impact Requirements

    Compounding of mineral-filled PP impact copolymers on a co-rotating twin-screw extruder with L/D 32:1 to 40:1 is normally arranged so that the PP copolymer forms a melt seal before the mineral filler is added through a downstream side-feeder. This sequence reduces upstream screw-element wear and prevents filler backflow into the main feed throat. Barrel set temperatures are profiled from 180°C at the feed zone to 220–240°C at the die. Melt temperature is preferably measured with an infrared probe because mineral filler raises viscous dissipation and can create local melt-temperature excursions above the set temperature. On a 40 mm class twin-screw machine, screw speed is commonly maintained between 300 min⁻¹ and 600 min⁻¹, with throughput adjusted to avoid excessive specific energy input that can shear the ethylene-propylene rubber phase. If the side-feeder is pushed beyond screw intake capacity, the pellet surface develops undispersed mineral agglomerates, and ash-content scatter rises above ±1.5% when tested by ISO 3451-1 method A. The compounded pellets should be dried to ≤0.08% moisture before injection molding; desiccant drying at 80°C for 2–4 h is appropriate when the storage environment exceeds 60% RH or when regrind is present. The dryer dew point is maintained at ≤-30°C; failure to do so produces silver streaks that are often incorrectly attributed to mold venting rather than moisture-induced surface splay.

    Injection molding of Kingfa PP-91905 class material uses a melt temperature of 220–240°C and a mold temperature of 30–60°C. A general-purpose screw with 20:1 L/D and shot volume held to 60–70% of barrel capacity is generally sufficient. Hydraulic back pressure is set between 2 bar and 8 bar to homogenize filler without excessive shear heating. Holding pressure is typically 50–70% of the first-stage injection pressure, but gate-seal time is determined by part-weight stabilization because mineral-filled grades freeze at the gate more quickly than unfilled PP. Mold temperatures below 30°C increase skin-layer orientation and shrinkage anisotropy; mold temperatures above 60°C extend cycle time without proportional improvement in crystallization. For a projected area of 0.3 m², clamp force may range from 300 t to 400 t when cavity pressure approaches 30–40 MPa, but the actual force should be confirmed by in-mold pressure sensors and short-shot studies.

    Short-shot trials and process audits on 2 mm wall sections show that injection speed below 100 mm/s tends to deepen flow lines and gate blush in mineral-filled grades. Increasing injection speed to 100–250 mm/s reduces flow-line depth, but if the barrel is already at 240°C, the extra shear heating can degrade the copolymer rubber at the melt front. A barrel setting of 220°C with high injection speed therefore often produces lower defect rates than a 240°C barrel with slow injection. The gate land should be at least 1.0 mm because mineral particles can obstruct smaller gates and generate gate-jetting. Valve-gate hot runners are preferred over open nozzles when surface quality is the primary acceptance criterion.

    Rheologically, mineral-filled PP impact copolymers exhibit higher low-shear viscosity and a lower shear-thinning slope than unfilled PP because filler particles restrict chain disentanglement and raise the low-shear stress plateau. Capillary rheometry at 230°C and apparent shear rates from 100 s⁻¹ to 10 000 s⁻¹ is required to fit Cross-WLF parameters for mold-filling simulation; generic unfilled PP viscosity data are not substitutable. The pvT behavior also changes because mineral filler lowers specific volume and alters the crystallization transition, shifting pack-stage shrinkage predictions if the simulator is not recalibrated with measured grade-specific data.

    Incoming lot verification at the molding plant relies on melt mass-flow rate and ash content rather than full mechanical testing because conditioned plaques are too slow for production release. A lot with MFR outside the agreed range by more than ±2 g/10 min can shift fill pressure and weld-line position; raising the barrel temperature alone is not an acceptable compensation because it may degrade the ethylene-propylene rubber phase. Ash content measured by ISO 3451-1 method A is used to monitor filler loading, with a common acceptance band of ±1.5 wt% around the approved nominal. If as-received pellets show excessive dust or filler accumulation in the feed throat, the material should be sampled for ash scatter and the pneumatic conveying system inspected for pellet attrition.

    In close-tolerance automotive interior and appliance applications, Kingfa PP-91905 is specified where dimensional stability, moderate stiffness, and low-temperature ductility must be balanced without the density penalty of short-glass PP. Typical candidate parts include instrument-panel subcomponents, door-trim inserts, center-console carriers, glove-box bins, HVAC housings, electrical enclosures, and power-tool housings with nominal wall thickness of 2–3 mm. The mineral filler reduces mold shrinkage to 0.8–1.1% after 24 h at 23°C on a 2 mm plaque under ISO 294-4 or ASTM D955; unfilled PP impact copolymer control specimens often fall between 1.2% and 1.6%. Heat deflection temperature under 0.45 MPa is generally in the 80–105°C band, making the grade suitable for interior trim that must tolerate solar load but not for continuous under-hood service. If the component is an automotive interior part, lot-specific VDA 278 and VDA 270 data must be requested because mineral-filled status alone does not establish low-fogging or low-odor compliance. For structural supports behind airbags or across weld lines, notched impact and weld-line strength are measured by ISO 179-1 or ISO 180 at the minimum service temperature; moving the gate to position the weld line away from the principal tensile stress is usually more effective than increasing filler content.

    The coefficient of linear thermal expansion for this class, measured between -30°C and 80°C by ISO 11359-2, is typically 60–90 µm/m·K, compared with 100–120 µm/m·K for unfilled PP impact copolymer. In parts with asymmetric gating or large flow-length differences, the orientation gradient can generate warpage even when isotropic shrinkage is low. Tooling corrections are therefore based on three-axis measurements of a 2 mm plaque after 48 h at 23°C and 50% RH, not on unfilled PP shrinkage data.

    Post-molding joining is feasible but requires parameter adjustments. Hot-plate welding uses plate temperature 200–230°C and melt displacement 0.3–0.8 mm per side; mineral filler reduces squeeze-out and can produce a sharper weld bead. Ultrasonic welding becomes more sensitive to filler damping; for filler loadings above 20 wt%, near-field welding with low amplitude of 20–30 µm and higher trigger force is often required to maintain joint efficiency. Self-tapping screws in bosses require a boss outer diameter approximately 2.0–2.5× the screw nominal diameter and root radii of 0.5–1.0 mm; the filler lowers creep but also reduces local ductility. If adhesive bonding is used, flame or atmospheric plasma treatment should raise surface energy above 42 mN/m; joint geometry must account for the lower peel strength of filled PP compared with unfilled PP.

    What Separates Kingfa PP-91905 from Glass-Filled, Unfilled, and Homopolymer Mineral-Filled Grades?

    The defining feature of Kingfa PP-91905 is the combination of an impact-copolymer base with a mineral filler. Compared with unfilled PP impact copolymer, the mineral-filled grade increases flexural modulus from a typical 900–1300 MPa to 1500–2200 MPa and reduces mold shrinkage from 1.2–1.6% to 0.8–1.1%, but the trade-off is lower tensile strain at break and reduced weld-line toughness. Against a mineral-filled homopolymer at similar filler loading, the impact-copolymer matrix shifts the ductile-to-brittle transition to lower temperature; notched Izod impact at -30°C under ISO 180 is commonly 4–8 kJ/m², while the homopolymer equivalent may fall below 2–4 kJ/m². Relative to short-glass PP copolymer, the mineral-filled product has lower density and less anisotropic shrinkage, but lower flexural modulus and heat deflection temperature. Short-glass grades may reach flexural modulus of 2500–4500 MPa, whereas mineral-filled PP impact copolymers are typically limited to 1500–2200 MPa; the mineral-filled material, however, produces less visible fiber orientation and is selected when surface quality and warpage stability dominate. Table 2 summarizes the comparative position.

    CriterionKingfa PP-91905 classUnfilled PP impact copolymerShort-glass PP copolymerMineral-filled PP homopolymer
    Density1.03–1.06 g/cm³0.90–0.91 g/cm³1.12–1.15 g/cm³1.03–1.06 g/cm³
    Flexural modulus1500–2200 MPa900–1300 MPa2500–4500 MPa1600–2400 MPa
    Mold shrinkage, 24 h, 2 mm plaque0.8–1.1%1.2–1.6%0.3–0.6% anisotropic0.7–1.0%
    Notched Izod, -30°C4–8 kJ/m²6–12 kJ/m²5–10 kJ/m²2–4 kJ/m²
    Warpage tendencyLow to moderateHighHigh with asymmetric gatingModerate
    Surface appearanceModerate filler gloss reductionHigh polish possibleVisible fiber orientation at weld linesModerate gloss reduction

    Regulatory Compliance, Handling Limits, and Lot-Dependent Verification

    The base PP copolymer can be supplied under the usual market compliance frameworks, but grade number alone does not establish regulatory clearance. For electrical and electronic equipment, RoHS Directive 2011/65/EU Annex II thresholds apply: lead 1000 mg/kg, mercury 1000 mg/kg, cadmium 100 mg/kg, hexavalent chromium 1000 mg/kg, polybrominated biphenyls 1000 mg/kg, and polybrominated diphenyl ethers 1000 mg/kg at the homogeneous material level. REACH SVHC content should be confirmed below 0.1% w/w per Article 33. For food-contact applications, the PP copolymer fraction may be covered by 21 CFR 177.1520, but the mineral filler and stabilizers must have their own applicable clearances; not all mineral-filled PP compounds are automatically food-contact-compliant. Flame performance is generally limited to UL 94 HB at 1.5 mm unless a specific yellow card is supplied; V-2 or V-0 ratings require flame-retardant additives that can alter density, impact, and melt stability.

    Storage should be maintained at ≤50°C and ≤60% RH for bulk pellet handling. The material should not be mixed with PVC or acetal purge streams; hydrochloric acid or formaldehyde evolved from these contaminants at processing temperature accelerates degradation and barrel corrosion. Regrind addition should not exceed 20 wt% without re-qualification of impact, shrinkage, and emission properties. Repeat heat histories can coarsen the ethylene-propylene rubber dispersion and lower low-temperature impact. If the lot certificate does not report the required property, the molder should request a supplemental test rather than assume agreement with class-typical values.