| HS Code | 440481 |
| Density | 1.04 g/cm³ |
| Melt Flow Rate | 8 g/10 min |
| Tensile Strength | 25 MPa |
| Elongation At Break | 20% |
| Flexural Modulus | 1600 MPa |
| Notched Izod Impact Strength | 4 kJ/m² |
| Heat Deflection Temperature | 100 °C |
| Vicat Softening Temperature | 150 °C |
| Molding Shrinkage | 1.2% |
| Water Absorption | 0.02% |
| Flammability | HB |
| Filler Content | 15% |
As an accredited Kingfa PP-TC15G71,PP-TD15,Mineral Filled factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-resistant bags on pallets, clearly labeled Kingfa PP-TC15G71/PP-TD15 Mineral Filled with lot and safety data. |
| Container Loading (20′ FCL) | Kingfa PP-TC15G71/PP-TD15 mineral-filled polypropylene is loaded in a 20-foot FCL container, palletized, securely stowed, and prepared for export shipment. |
| Shipping | **Shipping Description:** Kingfa PP-TC15G71 / PP-TD15 Mineral Filled is a non-hazardous polypropylene compound shipped as solid pellets in sealed 25 kg bags or bulk totes. Not regulated for transport. Store dry, away from direct sunlight and ignition sources; handle using normal industrial hygiene practices. |
| Storage | Store Kingfa PP-TC15G71/PP-TD15 mineral-filled polypropylene in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep containers or bags tightly closed, protect from dust, contamination, and physical damage, and avoid prolonged high temperatures. Follow the manufacturer’s safety data sheet and local storage regulations. |
| Shelf Life | Shelf life is typically 12 months when stored dry, cool, and in original unopened packaging, away from direct sunlight. |
Polypropylene compounds in the 15 wt% mineral-filled class represented by Kingfa PP-TC15G71 and PP-TD15 enter automotive interior production as ready-to-mold pellets rather than let-down concentrates. The addition ratio is fixed at the compounding stage: the mineral filler is dispersed at approximately 15 wt% into a polypropylene matrix, and downstream dilution with neat PP beyond 10 wt% is not recommended because it shifts mold shrinkage and reduces the stiffening effect that the filler provides for hidden-fit parts. In low-visibility structural applications—HVAC duct shells, lower instrument panel substrates, glove box bins, cowl-side trim, and door lower trim—the filler loading is selected to raise flexural modulus while retaining sufficient low-temperature ductility for interior assembly. Under ISO 178, the 15 wt% mineral-filled compounds typically produce flexural modulus in the range of 1,800–2,400 MPa, while under ISO 294-4 mold shrinkage is normally reported between 1.0% and 1.4%, depending on flow orientation and wall stock. The reduction in mold shrinkage relative to unfilled PP is the primary reason the grades are used on tools designed for tight snap-fit clearance.
On reciprocating-screw injection molding machines with screw L/D 20:1–25:1 and compression ratio 2.5:1–3.0:1, process windows are held at melt temperature 210–230 °C, mold temperature 20–50 °C, and hydraulic back pressure 5–10 bar. Production lines with hot-runner systems frequently observe jetting when gate diameters are below 1.5 mm and gate land length exceeds 1.0 mm; cold-runner edge gates with shear-thinned laminar melt fronts are preferred where visible weld lines must be minimized. Pre-drying at 80 °C for 2–4 hours is warranted when storage humidity exceeds 60% RH because surface moisture on the mineral filler contributes to silver streaking and reduced weld-line impact strength. The material is usable in closed-loop regrind streams at up to 20 wt%; above that level, batch-to-batch shift in melt mass-flow rate can exceed ±1 g/10 min under ISO 1133-1:2022, and cavity pressure variance may reduce part dimensional consistency.
| Verification target | Standard / code | Test method / clause | Application requirement |
|---|---|---|---|
| Flammability | ISO 3795 / FMVSS 302 | Horizontal burn rate | Burn rate ≤ 100 mm/min for passenger compartment materials |
| Total VOC emissions | VDA 277 | Headspace GC/FID | OEM-specific total carbon emission limits |
| Fogging / SVOC | VDA 278 | Thermodesorption GC/MS | OEM-specific fogging condensate limits |
| ELV substances | 2000/53/EC Annex II | Material certification | Lead, cadmium, mercury, hexavalent chromium restricted |
| Mold shrinkage | ISO 294-4 | Dimensional stability | Shrinkage 1.0–1.4% after 48 h conditioning |
Compliance for these applications is supplied by ISO 3795 and FMVSS 302 burn-rate testing, with low-emission interior requirements verified via VDA 277 total VOC and VDA 278 fogging/SVOC; substances are checked against REACH and ELV 2000/53/EC Annex II. Terminal finished part types include HVAC distribution ducts, floor-level defroster nozzles, glove box bins, lower instrument panel shrouds, and cowl side trim components.
Condensate collection below evaporator coils requires the plastic to tolerate intermittent water, detergent carryover, and microbial surface films without post-mold warpage or creep. The 15 wt% mineral-filled PP grades are run at 100 wt% virgin feedstock for wet-side parts; closed-loop regrind from runners and rejected parts is held to 15 wt% because long flow-length rib fills magnify viscosity variation, and higher regrind increases the probability of non-filled ribs and sink mark formation. Injection molding is performed on large-tonnage reciprocating-screw machines with mold temperature maintained at 15–30 °C on the water circuit. Melt temperature is set between 210 and 235 °C, with screw back pressure of 4–8 bar to avoid excessive shear heating of the platy mineral filler. Sequential valve gating is standard on drain pan tooling to prevent weld lines from landing on seal surfaces; multi-cavity production requires cavity-to-cavity fill imbalance below 3% to hold seal-plane flatness within 0.5 mm over a 500 mm span. Drying at 80 °C for 2–3 hours is required when exposure to ambient RH has exceeded 65% for longer than 24 hours.
Compliance anchors to IEC 60335-1 clause 30 for heat and fire resistance, UL 94 HB for flammability classification, RoHS 2011/65/EU for restricted substances, and REACH candidate list disclosures. Terminal finished part types include condensate drain pans, evaporator tray skirts, blower scroll housings, and filter rack frames.
Appliance housing molders use mineral-filled PP to manage warpage and dimensional repeatability in covers, frames, and consoles. The feedstock is supplied fully compounded at 15 wt% mineral filler; the recommended downstream addition ratio is 95–100 wt% compound with up to 5 wt% PP-based color masterbatch added at the press throat. Incompatible masterbatch carriers reduce weld-line tensile strength under ISO 527-2 and produce visible streaks; therefore, only PP-carrier color concentrate is used. In production, melt temperature is maintained at 220–240 °C, mold temperature at 25–45 °C, and holding pressure is set to 60–80 bar hydraulic equivalent to keep gate freeze-off short while filling ribs to 2–3 mm nominal wall. Drying is required at 80 °C for 2 hours when resin has been exposed to ambient air at RH above 65% for more than 24 hours. On high-speed appliance lines, flow-line contrast at boss features appears when mold temperature falls below 20 °C, so conformal cooling near thick mounting bosses is used to maintain uniform shell temperature.
Standards are IEC 60335-1, UL 94 HB, ISO 178 for flexural modulus, ISO 75-2 for heat deflection temperature, and RoHS 2011/65/EU. Terminal finished part types include washing machine top-load door frames, dishwasher lower front panels, dryer blower housings, and lint filter bodies.
Electrical installation enclosure production demands dimensional accuracy at elevated wall-cavity temperatures and under screw torque loading. Mineral-filled polypropylene at 15 wt% filler is used in junction boxes, surface-mount back boxes, cable trunking connectors, and terminal covers where the part is not a current-carrying insulator in high-voltage systems. The formulation addition ratio is 100 wt% selected compound; no external filler or flame retardant is added downstream because the producer controls particle size distribution, and uncontrolled additive dosing can reduce the comparative tracking index and create anisotropic shrinkage across the part. Injection molding uses melt temperature 200–230 °C and mold temperature 20–40 °C; fast injection speeds above 80 mm/s screw advance are used for thin knockout membrane sections, while holding pressure is staged to counteract marked flow orientation at gate junctions. Pre-drying at 80 °C for 2–3 hours is necessary to prevent surface splay because mineral surfaces adsorb ambient moisture. Continuous operating temperature should not exceed 80 °C under sustained mechanical load unless the part has been validated for creep at higher service temperatures.
Compliance standards are IEC 60670-1 for boxes and enclosures, UL 94 HB, IEC 60695-10-2 glow-wire flammability at 650 °C or 750 °C as required by final use, and RoHS 2011/65/EU. Dielectric strength under IEC 60243-1 is commonly reported in supplier data in the range of 25–35 kV/mm, but published data for this specific PP-TD15 configuration are limited and should be verified lot-specific. Terminal finished components include surface-mounted junction boxes, concealed conduit boxes, terminal strip covers, and cable trunking couplers.
Office seating mechanisms combine repeated high-cycle loading, assembly tolerances, and cost constraints. Mineral-filled PP at 15 wt% mineral is used for armrest carriers, backrest frame inserts, lumbar support housings, and shroud covers. The downstream formulation ratio remains 100 wt% prime compound with regrind limited to 15 wt%; regrind from mineral-filled PP re-enters the feed stream without the impact modifier loss observed in short-glass fiber compounds because the platy filler does not fracture in repeated extrusion to the same degree. Injection molding uses melt temperature 210–230 °C and mold temperature 30–50 °C; the higher mold temperature improves surface appearance at the armrest interface and reduces visible flow lines but extends cycle time. Long flow distances in backrest frames require hot-drop sequential valve gates and holding pressure maintained until gates freeze; if packing is released before gate freeze-off, post-mold drift of 0.3–0.7 mm can appear at lumbar attachment holes. Drying at 80 °C for 2 hours is used after open storage in humid environments.
Compliance standards are BIFMA X5.1 for seating durability, CAL TB 117-2013 for flammability, ISO 178 for flexural modulus, and REACH. Published multi-point fatigue data for PP-TD15 at 15 wt% mineral loading in office seating are limited; first-article fatigue testing is therefore recommended before substituting unfilled or elastomer-modified grades. Terminal finished parts include armrest structural carriers, lumbar adjustment housings, backrest insert plates, and under-seat cable covers.
Industrial material handling crates and structural tote bins use mineral-filled polypropylene where high stiffness, cleanability, and dimensional repeatability are required and where living hinges are not part of the design. The 15 wt% mineral-filled grades are fed at 100 wt% for base and sidewall sections; converters may add 10–20 wt% recycled PP only if the reclaim is dry, free of incompatible polymer contamination, and does not shift melt mass-flow rate outside ±1.5 g/10 min under ISO 1133-1:2022. Production by injection molding on large-tonnage machines with accumulator-assisted injection uses melt temperature 220–240 °C and mold temperature 15–35 °C; steel-safe tooling with draft angles 1.0–1.5 degrees per side is required because mineral-filled PP has lower mold shrinkage but higher ejection friction than unfilled PP. Stack crates with reinforced base ribs require holding pressure 70–90 bar hydraulic equivalent to eliminate sink marks at rib intersections; insufficient packing produces localized shrinkage voids that reduce stack-load capacity by more than 10% in initial production trials. Incompatibilities include exposure to strong oxidizing acids and long-term outdoor UV weathering unless a UV stabilizer package is specified at compounding; standard grades are not intended for continuous outdoor service without black colorant or additional stabilizer.
Compliance for transport packaging is commonly evaluated under ISO 12048 compression testing of complete filled packages and ISO 2247 fixed-frequency vibration testing where load security is specified; no harmonized electrical or food-contact standard applies to this application. Terminal finished part types include stackable tote bins, divider boards, pallet sleeves, and dunnage trays.
Competitive Kingfa PP-TC15G71,PP-TD15,Mineral Filled prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-TC15G71 and Kingfa PP-TD15 are supplied as mineral-filled polypropylene injection-moulding compounds within the Kingfa mineral-reinforced portfolio. The numerical suffix 15 corresponds to a nominal 15 wt% mineral loading, with PP-TD15 categorised as a talc-dispersed base compound and PP-TC15G71 categorised as a compounded talc/mineral package that may include an elastomeric impact modifier. The final alphanumeric sequence G71 is an internal Kingfa grade, colour, or additive-code identifier and is not an ISO or ASTM classification. The property ranges presented in this document are class-typical published windows for mineral-filled polypropylene compounds, not a substitute for the supplier certificate of analysis.
Pre-drying is required when storage humidity exceeds 60% RH or when condensation is observed on cold granulate. A desiccant dryer set to 80 °C for 2 h to 4 h with a dew point below -30 °C removes surface moisture adsorbed on the mineral filler; moisture levels above 0.1% by weight produce splay, silver streaks, and weld-line weakness. Melt temperature measured at the nozzle should be maintained between 200 °C and 230 °C. Residence time above 5 min at these temperatures causes oxidative chain scission and release of talc-bound volatiles; if machine interruption exceeds 10 min, the barrel should be purged with unfilled PP.
Production-scale reciprocating-screw machines with clamping forces from 800 kN to 3500 kN and general-purpose polyolefin screws of L/D 20:1 to 24:1 are suitable. Screw compression ratio should remain between 2.2:1 and 2.8:1; higher compression ratios generate unnecessary shear and degrade impact-modified PP-TC15G71. Barrel zone temperatures are commonly profiled from 190 °C in the rear to 210 °C at the front, with nozzle setpoint near 220 °C. Injection speed is set at 80 mm/s to 150 mm/s in thin-wall automotive trim to stabilise talc orientation, while melt-buffer cushion is maintained at 3 mm to 6 mm.
Gate dimensions should not be less than 60% of nominal wall thickness, and land length above 1.0 mm produces premature gate freeze that interrupts packing. For wall sections of 2.0 mm to 3.0 mm, packing pressure of 60 MPa to 80 MPa and packing time of 8 s to 12 s per 2 mm of wall section are used to reduce sink and lower post-mould shrinkage. Mould temperature is held at 30 °C to 60 °C; higher mould temperature reduces frozen-in orientation but increases cycle time and may raise transverse shrinkage. Rib-to-wall ratios should remain below 0.6 to limit flow hesitation and local filler-orientation gradients.
On hot-runner tools with manifold channels below 6 mm, mineral-filled PP can generate higher pressure drop than neat PP at equivalent flow rate. Gate diameters below 1.5 mm in hot-drop systems cause shear thinning and filler-matrix separation, visible as gate blush or circumferential delamination. Measured injection pressure at transfer should be recorded because a rise of more than 10% over baseline in the same tool is an early indicator of filler agglomerate buildup on the check ring.
Specimens are conditioned under ISO 291 at 23 °C and 50% RH before destructive testing. The table below compares class-typical published property windows for unfilled PP homopolymer, mineral-filled PP near 15% talc, and 20% glass-fibre-reinforced PP. These ranges are drawn from polymer-supplier technical literature and are not release limits for any specific Kingfa lot.
| Property | Test Method | Unfilled PP Homopolymer | Mineral-Filled PP near 15% Talc | 20% Glass-Fibre PP |
|---|---|---|---|---|
| Density | ISO 1183-1 | 0.90–0.91 g/cm³ | 1.00–1.05 g/cm³ | 1.03–1.08 g/cm³ |
| Melt flow rate at 230 °C/2.16 kg | ISO 1133-1:2022 | 15–25 g/10 min | 10–25 g/10 min | 5–15 g/10 min |
| Tensile modulus | ISO 527-2 | 1,200–1,600 MPa | 2,200–3,200 MPa | 3,500–4,500 MPa |
| Flexural modulus | ISO 178 | 1,300–1,700 MPa | 2,500–3,500 MPa | 3,800–5,000 MPa |
| Notched Izod at 23 °C | ISO 180/A | 2–4 kJ/m² | 2–5 kJ/m² | 6–10 kJ/m² |
| Heat deflection temperature at 0.45 MPa | ISO 75-2 | 80–95 °C | 95–115 °C | 140–155 °C |
| Coefficient of linear thermal expansion 23 °C–80 °C | ISO 11359-2 | 100–150 ppm/K | 60–90 ppm/K | 30–50 ppm/K |
| Mould shrinkage, flow direction | ISO 294-4 | 1.2–1.8% | 0.8–1.2% | 0.2–0.5% |
Table 1 should be used only for early material-selection screening. Supplier certificates for PP-TC15G71 and PP-TD15 may list different values because molecular weight, nucleating additives, and elastomer content are grade-specific.
Mineral-filled PP grades in the 15% filler class are selected where unfilled PP parts exceed 1.2% flow-direction mould shrinkage. Under ISO 294-4, flow-direction shrinkage for 15% talc-filled PP commonly falls between 0.8% and 1.2%, while transverse shrinkage remains 1.0% to 1.4%. The differential results from talc platelets aligning with the flow front; the reduction is anisotropic and is not controlled solely by melt temperature. Mould shrinkage between 0.9% and 1.1% is achievable in flat instrument-panel components when packing pressure is held at the upper end of the processing window.
Distortion control requires uniform cavity cooling. A difference of more than 5 °C between moving and fixed halves causes asymmetric crystallisation and bowing in long parts such as pillar trims exceeding 400 mm in length. Multiple side gates or a fan gate promote a radial fill path and reduce orientation-driven shrinkage mismatch. Withdrawal from the tool is controlled by draft angles of at least 0.5°; below this, mould-release drag on talc-rich surfaces can cause stress whitening. If the drawing requires post-mould shrinkage below 1.0%, process capability studies using ISO 294-4 should be run at three packing-pressure levels to define the control band; reliance on a single laboratory value is not adequate for dimensional release.
Conversion from an unfilled PP homopolymer to PP-TD15 in a thin-wall HVAC housing increases melt pressure at transfer by approximately 5% to 15% on a single-screw moulding machine when barrel temperature settings remain unchanged. Screw recovery time rises unless back pressure is increased by 0.5 MPa to 1.0 MPa to improve compacting. The resulting housing shows lower creep under dead load at 60 °C and improved screw-boss retention, but if the same part must tolerate cold-impact tests at -20 °C, the impact-modifier content in PP-TC15G71 should be verified against the supplier datasheet rather than assumed from the mineral loading.
PP-TD15 functions as a standard talc-reinforced polypropylene with medium modulus, while PP-TC15G71 is generally a controlled-rheology or impact-modified talc compound. The TC prefix often denotes talc compounding with an adhesion promoter or elastomer package, and G71 may correspond to a specific colour or stabiliser variant. The visible distinction in moulded parts is that PP-TD15 produces harder, stiffer, lower-gloss surfaces, whereas PP-TC15G71 may retain more ductility at the expense of some flexural modulus. The exact difference is not defined by the designation alone; melt flow rate measured under ISO 1133-1:2022 and notched Izod impact under ISO 180/A must be read from the supplier datasheet.
Compared with unfilled PP homopolymer, both PP-TD15 and PP-TC15G71 raise tensile modulus from roughly 1,400 MPa to above 2,200 MPa and increase heat deflection temperature at 0.45 MPa from below 95 °C to above 100 °C. Compared with impact-copolymer PP, a mineral-filled grade provides higher stiffness and lower CLTE but lower low-temperature ductility; notched Izod values at -20 °C are typically lower than rubber-rich impact copolymers. Compared with 20% glass-fibre-reinforced PP, a 15% talc-filled compound gives less tensile strength, higher CLTE, and lower shrinkage anisotropy, but also lower density, reduced surface fibre prominence, and lower abrasion to mould surfaces. At equal filler weight fraction, platy talc increases flexural modulus more than calcium carbonate because of higher aspect-ratio reinforcement, while calcium carbonate yields more isotropic shrinkage and higher Charpy impact. Weld-line strength in talc-filled PP is typically 10% to 30% lower than in unfilled PP at the same wall thickness because mineral particles concentrate at the melt front. For parts with multiple holes, weld-line location should be moved to low-stress zones or filled with flow leaders. These substitution boundaries define where PP-TC15G71 and PP-TD15 are technically appropriate relative to other PP grades.
Compliance documentation for automotive and appliance applications should include REACH Regulation EC No 1907/2006, EU RoHS Directive 2011/65/EU Annex II with its delegated amendments, and when relevant, IATF 16949 supplier quality records for lot traceability. Flame-retardancy claims should not be inferred from mineral loading; UL 94 testing at 1.6 mm or 3.0 mm is product-specific and must be confirmed from the Kingfa certificate because filler type does not confer flammability resistance.