| HS Code | 749728 |
| Productname | Kingfa PP-UV531, PP Weather Resistant (UV Stabilized), Home Appliance |
| Materialtype | Polypropylene (PP) |
| Grade | PP-UV531 |
| Uvstabilization | Yes |
| Weatherresistance | Yes |
| Application | Home appliance |
| Density | 0.90 g/cm³ (typical) |
| Meltflowrate | 8 g/10 min (230°C/2.16 kg, typical) |
| Tensilestrength | 25 MPa (typical) |
| Elongationatbreak | 30% (typical) |
| Flexuralmodulus | 1200 MPa (typical) |
| Notchedizodimpactstrength | 5 kJ/m² (23°C, typical) |
| Heatdeflectiontemperature | 95°C at 0.45 MPa (typical) |
| Vicatsofteningtemperature | 150°C (typical) |
| Moldingshrinkage | 1.5% (typical) |
| Waterabsorption | 0.01% (typical) |
| Processingmethod | Injection molding |
As an accredited Kingfa PP-UV531,PP Weather Resistant (UV Stabilized),Home Appliance factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Kingfa PP-UV531 weather-resistant PP supplied in 25 kg moisture-proof bags, 40 bags per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Kingfa PP-UV531 weather-resistant, UV-stabilized polypropylene for home appliance use, securely packed for export. |
| Shipping | Kingfa PP-UV531 is supplied as UV-stabilized polypropylene pellets for home-appliance applications. Ship in sealed, moisture-barrier 25 kg bags or bulk FIBCs, palletized and stretch-wrapped. Keep dry, cool, and out of direct sunlight; avoid heat and contamination. Generally non-hazardous for transport; follow local regulations and the SDS. |
| Storage | Store Kingfa PP-UV531 in a cool, dry, well-ventilated indoor area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture and dust contamination. Avoid contact with strong oxidizing agents. Keep away from incompatible chemicals. Use first-in, first-out stock rotation; maintain good housekeeping, prevent static buildup, and provide spill containment. Handle pellets carefully to avoid slips. |
| Shelf Life | Typically 24 months when stored unopened in a cool, dry place, protected from sunlight and moisture. |
In split-unit air conditioner manufacturing, outdoor condensing unit parts molded from Kingfa PP-UV531 are specified where the enclosure must retain surface gloss, dimensional registration, and impact resistance after prolonged solar exposure. The formulation is supplied as a ready-to-use UV-stabilized compound; the production addition ratio is 100 wt% for components required to carry a UL 746C f1 outdoor rating, and the only accepted dilution is clean sprues and runners reground at 15–20 wt%, beyond which notched impact strength at -20 °C begins to show measurable loss. Color masterbatch is added at 2.0–3.0 wt%, and no separate benzophenone or HALS masterbatch is required because the stabilizer package is already dispersed during compounding. Industry compliance for this application is governed by IEC 60335-2-40:2022 for heat pumps and air conditioners, IEC 60335-1:2020 Clause 30.2 for resistance to heat and fire, UL 746C f1 for UV and water exposure, and UL 94 HB unless regional product standards require 5VA for internal electrical enclosures. Accelerated weathering qualification is typically run to ISO 4892-2:2013 cycle 1 at 0.51 W/(m²·nm) at 340 nm with a black-panel temperature of 65 °C ±3 °C and a minimum of 1,500 h for f1 compliance. On the production floor, large louvered condenser housings are injection molded on toggle presses of 1,200–1,600 t clamp force using a screw with an L/D ratio of 22:1–24:1, melt temperature 220–245 °C, and mold temperature 30–50 °C. Filling is completed in 2.5–4.0 s through sequential valve-gated hot runners; when the cavity flow length-to-wall-thickness ratio exceeds 250:1, short shots and hesitation lines appear unless melt temperature is raised to the upper limit and injection velocity is increased. Warpage and residual stress are controlled by maintaining a mold temperature differential below 15 °C across the core and cavity; pre-drying at 80 °C for 2 h is applied only when ambient relative humidity is above 60% or when resin has been stored in unsealed containers after ocean freight. Process limits are defined by additive volatilization: sustained melt temperatures above 260 °C produce plate-out on mold surfaces and a loss of weather resistance at the surface. Terminal finished components include the top cover, service panel, louver grille, drain pan, motor bracket shroud, and terminal block cover for outdoor condensing units.
Balcony-installed washing machine top covers and control panel bases are subjected to repeated moisture cycling, solar UV, and detergent overspray. Kingfa PP-UV531 is used at a production addition ratio of 100 wt% for injection-molded structural covers; post-industrial runner and sprue regrind is limited to 15 wt% because higher fractions lower the surface concentration of the UV absorber and reduce xenon-arc retention below the intended 1,000–1,500 h threshold. Detergent-drawer front panels and translucent control windows are not produced from this grade; opaque tinted control panels are molded with 1.5–2.5 wt% pigment masterbatch. Compliance anchors to IEC 60335-2-7:2019 for washing machines, IEC 60335-1:2020 for general household safety, and ISO 4892-2:2013 cycle 1 for accelerated weathering; for machines placed where rain can reach electrical parts, enclosure flammability is additionally evaluated under UL 94 V-0 at the specified minimum thickness. The dominant processing issue on a 600–700 mm-wide top cover is sink marks around bosses and ribs; production molds run on clamp forces of 1,000–1,600 t and use sequential valve gating to shift weld lines to non-visible edges. Melt temperature is held at 230–250 °C, mold temperature at 35–55 °C, and packing pressure is maintained at 55–70 MPa for 10–15 s; if packing pressure drops below 45 MPa, sink mark depth in boss areas becomes visible. Cycle time is normally 40–60 s depending on wall thickness. The stabilizer system is sensitive to prolonged contact with hypochlorite-based bleach and acidic descalers; direct contact with undiluted bleach in the dispenser area should be avoided because surface extraction of the stabilizer can produce local glossy patches and later micro-cracking. Finished terminal components include top cover, front panel, control panel base, detergent drawer front frame, and base frame segments.
Ultraviolet exposure in domestic kitchens is not limited to direct sunlight; south-facing glazing and high-intensity task lighting can deliver enough near-UV to cause discoloration in unpainted PP appliance shells over multi-year service. For small kitchen appliances such as electric kettle bases, toaster side panels, drip-tray covers, blender drive housings, and stand mixer head covers, the material is molded as supplied at 100 wt%, with color masterbatch added at 2.0–4.0 wt%. Post-industrial regrind is allowed up to 20 wt% for non-metallized internal brackets but is limited to 10 wt% for glossy exterior surfaces because pigment dispersion and UV absorber distribution become less uniform with repeated heat histories. Food-contact compliance is verified against FDA 21 CFR 177.1520 for olefin polymers and (EU) Regulation 10/2011 when the part contacts food under the end-use time and temperature conditions; electrical safety is governed by IEC 60335-2-15:2012 for heating liquids, IEC 60335-2-9:2008 for toasters and grills, and IEC 60335-1:2020. Thin-wall housings with nominal wall thickness 2.0–2.5 mm are molded on 200–400 t presses using hot-tip or tunnel gates, with melt temperature 230–245 °C, mold temperature 40–60 °C, injection speed 60–100 mm/s, and back pressure 4–8 MPa. Surface splay occurs when the granulate has taken up surface moisture; pre-drying at 80 °C for 2 h is recommended if ambient relative humidity exceeds 60% or after condensation during air freight. Published multi-year data for high-intensity task lighting exposure on unpainted PP is limited; accelerated xenon-arc testing remains the industrial surrogate for predicting color stability. The material is not intended for direct food contact at processing temperatures above 100 °C or for pressure-cooker components exposed to 121 °C steam sterilization; those applications exceed the continuous-use deflection temperature and accelerate additive migration. Terminal finished products include opaque lower housings, side trims, bezels, and bases that must withstand kitchen window exposure without fading.
For portable evaporative coolers and dehumidifiers used on verandas, covered patios, and laundry rooms, large flat panels and long flow paths create specific gating and packing challenges that are aggravated by intermittent UV exposure. In these components, the addition ratio of Kingfa PP-UV531 is 100 wt% for exterior casings requiring UV resistance, and clean injection sprues and runners are accepted at 15–25 wt% if the final part is not required to carry a UL 746C f1 outdoor rating. For water tank shells where contact with lime-scale removers is possible, the regrind fraction is reduced to 15 wt% because lower stabilizer concentration at the surface increases sensitivity to extraction by weak acids. Compliance is evaluated under IEC 60335-2-98:2018 for humidifiers, IEC 60335-2-40:2022 for dehumidifiers, IEC 60335-1:2020, and UL 94 HB at minimum part thickness; ultraviolet aging is assessed by ISO 4892-2:2013 cycle 1 for 800–1,200 h when the unit is specified for semi-outdoor use. Large side panels and air-outlet louvers with flow lengths above 250 mm are molded on 1,300–1,600 t hydraulic presses using multiple valve-gated hot runners. Melt temperature is set at 235–250 °C, mold temperature at 40–65 °C, and fill speed is profiled from 45 mm/s to 90 mm/s; weld-line locations are shifted toward the louver edges to preserve visible surface quality. Weld-line tensile strength as a fraction of un-welded material is commonly 60–70% when tested to ISO 527-2, so louvers are gated such that knit lines do not cross mounting bosses or snap-fit retention features. The material shows no hydrolytic degradation in standing water at 50 °C, but prolonged contact with concentrated citric or acetic descaling solutions at elevated temperature can extract the UV absorber at the surface; flushing after descaling is required to prevent localized chalking. Terminal finished components include top cover, side panel, water tank shell, air-outlet louver, base drain tray, and motor bracket cover.
Refrigerator door end caps, hinge covers, water dispenser drip trays, and drawer trims are produced from Kingfa PP-UV531 when the appliance is positioned near long-duration window exposure and visible yellowing must be controlled. The production addition ratio is 100 wt%; post-industrial regrind is typically controlled at 15–20 wt% for non-appearance internals and 10 wt% for high-gloss exterior parts. If a local molder blends this grade with non-stabilized PP homopolymer or matte metallocene PP, the blend ratio must not exceed 20 wt% of non-UV resin because the weather stabilization is diluted and surface gloss differences become visible under raking light. Food-contact and potable-water contact compliance is established under FDA 21 CFR 177.1520 and (EU) Regulation 10/2011; appliance safety is governed by IEC 60335-2-24:2010 for refrigerating appliances and IEC 60335-1:2020. These smaller parts are molded in multi-cavity tools on 120–250 t presses with hot-tip gating, melt temperature 220–240 °C, mold temperature 30–50 °C, and back pressure 3–6 MPa; cycle time is 20–35 s depending on rib thickness. Surface defects associated with additive plate-out can be managed by keeping melt temperature below 250 °C and performing a purge every 2,000 shots with a high-viscosity PP purge grade. The grade is not suitable for interior food liner thermoforming or for parts that must be post-mold electroplated, because the stabilizer package interferes with surface adhesion. Terminal finished parts include door end caps, hinge covers, dispenser drip trays, drawer fronts, and toe-kick trim strips.
Competitive Kingfa PP-UV531,PP Weather Resistant (UV Stabilized),Home Appliance prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa PP-UV531, PP Weather Resistant (UV Stabilized), Home Appliance, is a polypropylene-based injection-molding compound intended for unpainted and lightly coated exterior components that must tolerate intermittent or sustained ultraviolet exposure. The grade belongs to the home appliance segment, where part geometry, color retention, and cost per cubic centimeter govern material selection. Candidate components include air-conditioner outdoor unit top covers, side panels, louver frames, washing machine control panels mounted adjacent to windows, and refrigerator rear panels exposed to indirect UV during distribution. The resin is supplied as cylindrical or lenticular pellets and is intended for conversion on conventional single-screw or reciprocating-screw injection-molding machines. Published data for this specific configuration is limited; release values from the Kingfa certificate of analysis and technical datasheet should therefore govern incoming acceptance testing.
The stabilization chemistry relies on a UV absorber of the type commonly associated with the suffix 531—often a substituted benzophenone such as 2-hydroxy-4-n-octyloxybenzophenone—combined with hindered amine light stabilizers and phenolic antioxidants. The benzophenone absorber converts absorbed UV photons into thermal energy, while the HALS package intercepts alkyl and alkoxy radicals produced by photo-oxidation. Unstabilized polypropylene exposed to UV undergoes rapid chain scission, leading to surface crazing, gloss loss, and a sharp decline in elongation at break before deep-section embrittlement is observed. A UV-stabilized appliance compound is therefore specified when field service includes direct sunlight through glazing or intense warehouse lighting. In xenon-arc testing under ISO 4892-2, UV-stabilized PP compounds of this melt-flow class typically show extended time to 50% retention of tensile elongation relative to non-stabilized controls, but the absolute retention curve is color- and thickness-dependent.
For mold design and incoming material control, the property ranges below represent unfilled or lightly filled UV-stabilized PP appliance compounds in the same melt-flow class as PP-UV531; they are not a substitute for the grade-specific Kingfa datasheet. Melt flow rate is measured at 230 °C under 2.16 kg by ISO 1133-1:2022. A flow window of 8–15 g/10 min is typical for large-area thin-wall appliance enclosures, balancing short-shot risk against excessive drool and weld-line fragility. Tensile stress at yield and elongation at break are measured on ISO 527-2/1A specimens after standard conditioning. Flexural modulus is measured by ISO 178 at 2 mm/min. Notched Charpy impact is measured by ISO 179-1/1eA at 23 °C and -20 °C. Heat deflection temperature under 0.45 MPa is measured by ISO 75-2/B.
| Property / weathering response | Test standard | PP-UV531 typical range | Unstabilized PP control |
|---|---|---|---|
| Melt flow rate at 230 °C / 2.16 kg | ISO 1133-1:2022 | 8–15 g/10 min | 8–15 g/10 min |
| Tensile stress at yield | ISO 527-2 | 20–27 MPa | 22–29 MPa |
| Tensile elongation at break | ISO 527-2 | 200–500% | 100–300% |
| Flexural modulus | ISO 178 | 1100–1500 MPa | 1200–1600 MPa |
| Notched Charpy impact at 23 °C | ISO 179-1/1eA | 4–8 kJ/m² | 3–7 kJ/m² |
| Elongation retention after 1000 h xenon arc | ISO 4892-2 + ISO 527-2 | 70–90% | 30–50% |
The comparative weathering row is illustrative for unfilled PP appliance compounds and not a grade-specific guarantee. Pigment loading, dispersion quality, and processing thermal history shift the absolute value. The supplier should be asked for lot-specific data on the production color.
Polypropylene is not hygroscopic; moisture-induced splay is less frequent than in filled or condensation-prone resins. Condensation on cold pellets stored above 70% relative humidity can nevertheless create surface defects in high-gloss parts. Where surface appearance is critical, a desiccant dryer at 80 °C for 2 h removes surface moisture. Melt temperature measured at the nozzle normally ranges from 210 °C to 240 °C. Exceeding 260 °C or residence times above 8 min should be avoided because thermal depletion of the HALS and phenolic antioxidant package accelerates yellowing in light colors and reduces weatherability retention. Mold temperature is typically 25–50 °C; higher mold temperature improves weld-line strength and surface smoothness but lengthens cooling time.
Production-scale observations in thin-wall louver tooling indicate that short-shot defects can appear below 210 °C melt temperature when fill speed is limited by an undersized clamp system or a worn check-ring. Back pressure between 0.5 MPa and 1.5 MPa assists additive dispersion without excessive shear heating. General-purpose screws with 20:1–22:1 L/D are acceptable; low-shear barrier screws are preferred for color consistency. Screw recovery should be set so that the ratio of shot weight to barrel capacity does not create prolonged residence time; for a 1000 kN clamp machine, keeping the shot below 70% of rated capacity reduces the risk of inconsistent cushion and stabilizer depletion.
Gate location and weld-line placement influence weatherability because UV-stabilized PP parts frequently fail first at weld lines after outdoor exposure. For louver frames and grilles, direct-edge gating or multiple hot-runner drops reduce flow length and preserve impact at knit lines. Mold-flow simulation should use the measured viscosity curve for the production color because small shifts in molecular weight distribution can move weld-line position and change local orientation.
In pigmented black and dark-gray exterior formulations, the UV stabilizer package retards the development of a chalky surface layer generated by polymer chain scission and loss of pigment-to-matrix adhesion. For high-chroma colors, benzophenone-class absorbers alone are usually insufficient because photolytic scission of organic colorants continues aggressively; HALS is required. Surface gloss at 60° and ΔE should be recorded before and after accelerated weathering under ISO 4892-2. A ΔE value below 3.0 after 1000 h xenon arc exposure is a commonly used target for UV-stabilized appliance whites and grays, but it is not an automatic guarantee for all pigment packages. Published data for this specific configuration is limited.
The principal processing difference between PP-UV531 and a general-purpose PP appliance grade is usually small because the stabilizer package is added at low loading; melt viscosity, filling pressure, and cooling time may be nearly identical. The critical difference appears after service in UV-exposed locations. A non-stabilized copolymer can show surface microcracking, gloss collapse, and loss of ductility after a single outdoor season, while PP-UV531 is intended to shift the failure mode to slower surface oxidation and better retention of thin-wall flexibility.
Compared with talc-filled PP, PP-UV531 tends to exhibit lower flexural modulus and lower heat deflection temperature. Direct replacement in a dimensionally critical panel may require rib thickening, local gate relocation, or higher mold temperature to maintain flatness. Compared with ASA or PC/ASA, PP-UV531 has lower density and is generally more resistant to alkaline cleaning agents and hydrolytic degradation, but its upper continuous-use temperature and retained stiffness under load are lower. The grade is not inherently a UL 94 V-0 flame-retarded material; if the appliance enclosure standard requires a flammability rating, a flame-retarded PP or other certified grade must be selected.
| Regulatory / test area | Standard or regulation | Application to PP-UV531 |
|---|---|---|
| Restriction of hazardous substances | RoHS Directive 2011/65/EU as amended by (EU) 2015/863 | Conformance required for home appliance electrical and electronic components in the supplied color |
| SVHC communication | REACH (EC) No 1907/2006, Article 33 | Supplier declaration should list Candidate List substances above 0.1% w/w |
| Xenon arc weathering | ISO 4892-2 | Comparative UV stability and color fastness under filtered xenon radiation |
| Tensile properties | ISO 527-2 or ASTM D638-14 | Acceptance of mechanical quality on molded specimens |
| Melt flow rate | ISO 1133-1:2022 | Incoming resin viscosity check at 230 °C / 2.16 kg |
Regrind addition up to 30% is generally tolerated in appliance production, but repeated heat histories reduce the stabilizer reservoir and darken light colors. If regrind is used, UV retention should be evaluated on a blend containing the highest planned regrind fraction, not on virgin material.
Because appliance standards vary by region and end-product category, the article producer retains final responsibility for converted-part compliance. The compound supplier provides chemical and regulatory data for the pellet product, not for finished components assembled with other materials.
For high-altitude, coastal, or high-UV-albedo installations, weathering test duration should be extended or a higher-stability package should be evaluated. Avoid processing with copper-containing colorants or flame-retardant systems that release free acidity, because transition metals and acidic residues accelerate oxidative degradation of both unstabilized and UV-stabilized polypropylene. The product should not be used in continuous under-load service above 90 °C without heat-aging validation.