| HS Code | 961484 |
| Polymer Type | PP/PS Alloy |
| Density | 1.04 g/cm³ |
| Mold Shrinkage | 0.4–0.6 % |
| Melt Flow Rate | 10 g/10 min |
| Tensile Strength | 25 MPa |
| Elongation At Break | 30 % |
| Flexural Modulus | 1800 MPa |
| Notched Izod Impact Strength | 5 kJ/m² |
| Heat Deflection Temperature At 1 8 Mpa | 85 °C |
| Vicat Softening Temperature | 100 °C |
| Flammability | HB |
| Painting Performance | Easy |
| Shrinkage Characteristic | Low |
As an accredited Kingfa Propalloy-1(F),PP/PS Alloy (Low Shrinkage, Easy Painting) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg moisture-proof paper sacks, palletized, with clear product labels for Kingfa Propalloy-1(F), PP/PS Alloy (Low Shrinkage, Easy Painting). |
| Container Loading (20′ FCL) | Kingfa Propalloy-1(F) PP/PS alloy (low shrinkage, easy painting) securely loaded into a 20′ FCL container for export shipment. |
| Shipping | Kingfa Propalloy-1(F) PP/PS alloy ships as non-hazardous polymer pellets in moisture-barrier bags or sealed containers. Protect from moisture, heat, sunlight, contamination, and mechanical damage during transport. Use standard freight and follow local transport and environmental regulations. |
| Storage | Store Kingfa Propalloy-1(F), PP/PS Alloy in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flame. Keep containers tightly closed and palletized; prevent moisture, dust, and contamination. Avoid strong oxidizers and solvents. Maintain stable temperature and follow the SDS and local regulations. |
| Shelf Life | Shelf life is typically 24 months from date of manufacture when stored cool, dry, and in original sealed packaging. |
Injection molding of visible automotive interior trim from PP/PS alloy compels simultaneous control of after-mould shrinkage and paint adhesion on surfaces that are touched, wiped, and subjected to cabin heat. On a 1,200 t hydraulic injection molding machine with accumulator-assisted injection, door panel lower inserts are filled through a valve-gated hot runner at a melt temperature of 215 °C to 235 °C and a tool surface temperature of 30 °C to 50 °C. The low mould shrinkage class of unfilled PP/PS alloy—reported under ISO 294-4 after 48 h at 23 °C in a 0.5–0.8 % range for comparable alloy grades—permits boss and rib features to be formed without severe sink marks. Hold pressure is staged in three steps, beginning at 65 % of peak injection pressure and decaying to 35 % over 6 s; gate freeze is verified by part weight stability of ±0.15 % across 20 consecutive cycles. Missing this hold-pressure profile produces visible sink adjacent to rib intersections after topcoat application, which is a known failure mode on interior Class A surfaces.
Painting follows with an adhesion-promoting primer based on chlorinated polyolefin; target dry film thickness 3–5 µm is applied with a 1.0–1.2 mm fluid nozzle after isopropanol/DI water wiping and ionized air blow-off. A two-component polyurethane topcoat is then deposited at 15–25 µm DFT and cured for 30 min at 80 °C. Cross-cut adhesion is assessed to ISO 2409 with acceptance at Class 0–1; methyl ethyl ketone double rubs under ASTM D5402 are limited to 100 cycles without substrate exposure. Compliance for interior components includes ISO 3795 horizontal burn behavior with a flame spread rate not exceeding 100 mm/min, DIN 75201 fogging with a condensate reflectometric value exceeding 60 %, and VDA 278 volatile/semi-volatile emission screening with class-typical TVOC below 100 µg/g for polyolefin-based interior stock. Published data for Propalloy-1(F) under specific OEM weathering cycles is limited; accelerated weathering under SAE J2527 should not be extrapolated beyond 1,500 kJ/m² without validation. Formulation for a production lot retains 100 parts of Propalloy-1(F) with 2.0 wt% color masterbatch, 0.3 wt% hindered amine light stabilizer, and 0.2 wt% antioxidant. No external release agent is permitted; mould deposit from internal lubricant is controlled by limiting stearate to 0.15 wt%. Terminal products include door lower inserts, HVAC outlet vanes, seat side shields, and speaker grille rings.
Decorative fascias for washing machines and refrigerator control consoles require a paint film that withstands alkaline cleaning agents, condensation, and repeated finger contact. The PP/PS alloy is pre-dried at 80 °C for 2 h with a desiccant dryer dew point below -40 °C, reducing residual moisture below 0.03 % before moulding. Melt temperature is held at 220 °C ± 10 °C with a screw recovery speed of 50–80 rpm, and the tool surface is maintained at 25 °C to 45 °C. Low molecular weight styrenic oligomers can bloom to the surface and function as adhesion-breakers; plasma pretreatment at 200–400 W for 5–10 s raises surface energy from 34 mN/m to 44–52 mN/m measured under DIN 55660-3. A waterborne 1K acrylic-polyurethane topcoat is then applied at 20 µm DFT. Resistance to 1 % aqueous sodium hydroxide for 24 h is evaluated under ISO 2812-1 with no blistering and no creep from scribe; cross-cut adhesion after 24 h condensation exposure is Class 0 under ISO 2409. Avoid steam autoclave exposure above 121 °C and prolonged contact with ketone-based solvents; both conditions degrade the styrenic phase and lift the paint film. Formulation for appliance fascias combines 100 parts of Propalloy-1(F) with 3.0 wt% white masterbatch, 0.1 wt% antioxidant, and 0.1 wt% nucleating agent; silicone-based processing aids are excluded because they compromise wetting before topcoat application. Terminal products include washing machine program selector bezels, refrigerator display frames, and dishwasher console panels.
| Requirement | Test method | Acceptance metric |
|---|---|---|
| Paint adhesion after water soak | ISO 2409 | Class 0–1 |
| Chemical resistance to household cleaner | ISO 2812-1 | No blistering, gloss retention > 80 % |
| Condensation resistance | ISO 6270-2 | 240 h, no creep from scribe |
| Glow-wire ignition for unattended appliance | IEC 60695-2-11 | Pass GWIT as specified by subassembly standard |
| Surface energy pre-paint | DIN 55660-3 | ≥ 44 mN/m |
Thin-wall enclosures for routers, remote controls, and smart-home sensors benefit from low shrinkage because sink marks adjacent to snap-fit undercuts and ejector pins become visible after high-gloss coating. Moulding uses melt temperatures of 230 °C to 240 °C, tool surface temperatures of 25 °C to 40 °C, and injection velocities of 180–250 mm/s for wall thicknesses of 1.5–2.0 mm. Hold pressure is set at 40–60 MPa with cooling time controlled between 8 s and 12 s; ejection is delayed until part surface temperature drops below 55 °C to reduce white stress marks around ejector pads. The unfilled alloy is not inherently flame-retardant; if a UL 94 rating is required, published data for Propalloy-1(F) with FR masterbatch systems is limited, and any formulated variant must be re-qualified for paint adhesion and low-temperature impact. Conductive coatings or EMI shielding are outside this grade unless a copper conductive primer is validated on the exact tool texture.
Painting for high-gloss consumer electronics uses a UV-curable hardcoat after low-pressure plasma activation; the adhesion promoter is applied at 5 µm and the hardcoat at 15 µm. Cross-cut adhesion is Class 0 under ISO 2409, and Taber abrasion under ASTM D4060 with CS-10 wheels at 500 g for 100 cycles produces haze below 5 % on the topcoat-only configuration. Compliance centers on RoHS 2011/65/EU, REACH SVHC screening, and halogen-free requirements per IEC 61249-2-21 where specified by electronics purchasers. Formulation for electronics enclosures retains 100 parts of Propalloy-1(F), 2.5 wt% custom colorant, 0.15 wt% antioxidant, and 0.3 wt% acid scavenger; no silicone slip additive is used because it prevents uniform hardcoat wetting. Terminal products include router upper covers, remote control shells, IoT sensor enclosures, and access-point housings.
Concealed cistern control frames and toilet seat hinge covers moulded from PP/PS alloy serve as non-water-contact aesthetic shrouds in sanitary installations where dimensional stability prevents binding of moving hinges after seasonal humidity excursions. The application is limited to exterior shrouds; potable water contact is not established for this grade and should not be specified. Moulding uses a sequential valve-gated hot runner at melt temperature 215 °C to 225 °C and tool surface 40 °C to 60 °C to suppress visible weld lines along the perimeter. Hold pressure is maintained at 35–45 MPa, and the part is dried at 80 °C for 2 h before painting. A two-component polyurethane topcoat at 20–30 µm DFT is applied after a 70 % isopropanol wipe and a chlorinated polyolefin primer at 5 µm. Chemical resistance under ISO 175 to 5 % acetic acid for 24 h is required because sanitary cleaners introduce acidic species; no cracking or spotting is permitted. Formulation combines 100 parts of Propalloy-1(F) with 10 wt% precipitated barium sulfate masterbatch for mass and sound damping, 0.1 wt% acid scavenger, and 0.2 wt% antioxidant; phthalates are excluded. Terminal products include cistern control frames, flush plate spacers, and toilet seat hinge covers.
Large-area point-of-sale panels and display headers demand low warpage after ejection because printed graphics and lacquered surfaces magnify out-of-plane distortion. For wall thicknesses of 3.0–4.0 mm and flow lengths beyond 300 mm, a cold runner with full round gates of 2.0 mm diameter is used at melt temperature 225 °C and tool surface 50 °C to reduce visible flow marks. Clamp force of 1,500–2,000 t is typical for multi-cavity display header tools. Flatness after 72 h is controlled within 1.5 mm/m using corner-to-corner measurement rather than relying solely on cavity pressure; warpage outside this window creates visible edge lift after coating. Direct-to-plastic solvent-based 2K polyurethane is applied at 20–30 µm DFT after flame treatment at 250 mm/s. Pot life is set at 45 min and forced curing at 60 °C for 30 min stabilizes crosslink density. Adhesion is Class 0–1 under ISO 2409 and pencil hardness is HB–F under ASTM D3363. UV stability for indoor display use is normally sufficient; outdoor exposure exceeding 1,000 h QUV requires an additional UV-blocking topcoat. Formulation includes 100 parts of Propalloy-1(F), 4 wt% brand-matched masterbatch, and 0.2 wt% UV stabilizer; external lubricants are excluded due to post-mould painting. Terminal products include retail display headers, shelf trays, kiosk backpanels, and exhibition wall panels.
Educational model parts, science kit housings, and architectural study models require snap-fit assembly and water-based enamel compatibility; PP/PS alloy is selected when ABS is excluded by a purchasing specification or when low paint after-cure distortion is decisive. Moulding on a small-shot injection molding machine of 80–120 t clamp force uses melt temperature 210 °C to 225 °C and tool surface 25 °C to 35 °C. Hold pressure is set at 25–35 MPa, and cushion is held at 3–5 mm to avoid short shots in multi-cavity educational component tools. The grade is not suitable for food contact or for children under 36 months without additional testing; published data for this specific configuration is limited. Compliance centers on EN 71-3 migration of heavy metals and REACH Annex XVII restrictions; no heavy-metal pigments or phthalates are added. Formulation retains 100 parts of Propalloy-1(F) with 2 wt% white masterbatch and 0.05 wt% nucleating agent. Painting uses water-based acrylic enamel at 10–15 µm DFT, air-dried for 24 h or force-dried at 50 °C for 20 min; cross-cut adhesion is Class 0 after drying. Terminal products include anatomical model parts, building block connectors, science kit housings, and educational display components.
Competitive Kingfa Propalloy-1(F),PP/PS Alloy (Low Shrinkage, Easy Painting) prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Kingfa Propalloy-1(F) is a polypropylene/polystyrene alloy engineered for injection moulded parts requiring low mould shrinkage and reduced paint-adhesion burden relative to polypropylene homopolymer. The grade designation identifies a low-shrinkage, easy-painting member of the Propalloy series, in which a dispersed polystyrene phase modifies the crystallisation shrinkage of the PP matrix and increases the surface polarity of the moulded skin. Melt processing is typically performed at barrel set temperatures from 200 °C to 230 °C and mould temperatures from 20 °C to 50 °C; these are class-typical values for PP/PS injection moulding grades, not lot-specific recommendations from the manufacturer. Class-typical mould shrinkage determined on 60 mm × 60 mm × 2 mm plaques under ISO 294-4 falls within 0.5–0.7%, whereas unfilled polypropylene homopolymer values under the same method commonly range from 1.2% to 1.8%. The styrenic domain also permits painted systems to reach ISO 2409 cross-cut class 0 or 1 when a chlorinated polyolefin adhesion promoter is applied; without such primer, wetting and adhesion are improved over PP homopolymer but may remain insufficient for automotive interior durability requirements. Published lot-specific mechanical data for Kingfa Propalloy-1(F) are limited in public databases, so the following class-typical ranges should be used for material screening and replaced with certificate-of-analysis values during production qualification.
The paintability advantage of a PP/PS alloy is primarily interfacial. The polystyrene phase exhibits a surface free energy commonly reported in the 38–42 mN/m range at 20 °C, while polypropylene homopolymer surfaces are typically 29–31 mN/m. The higher surface energy reduces the wetting angle of chlorinated polyolefin primers and two-component polyurethane topcoats, improving film formation and mechanical interlock. In practice, a system comprising a chlorinated polyolefin adhesion promoter, a two-component polyurethane or acrylic-melamine topcoat, and a 60–80 °C forced-air cure is commonly evaluated according to ISO 2409 and ASTM D3359-23. Cross-cut class 0 or 1 after 24 h at 23 °C and 50% relative humidity is typical for moulded plaques with cleaned surfaces. Pull-off adhesion measured under ISO 4624 on such systems commonly falls in the 2–4 MPa range; failures are frequently cohesive within the alloy rather than interfacial, but this depends on coating chemistry and surface contamination.
Surface preparation remains necessary. Mold release agents, waxes, and hydrocarbon residues from the moulding environment reduce adhesion repeatability. Cleaning with 50:50 isopropanol/deionised water, abbreviated plasma treatment at 0.5–1.0 kW for a 0.5–1.0 s cycle, or flame treatment can raise surface energy further; however, the PS phase can be degraded by excessive thermal exposure, causing yellowing and microcracking. For parts to be painted, the use of silicone-based mould release is contraindicated because traces of silicone alter the wetting envelope and may require additional solvent wiping.
The dispersed PS domain also introduces a chemical-resistance boundary. Aromatic hydrocarbons, chlorinated solvents, and terpene-based cleaners can swell or stress-crack the styrenic phase. Chemical compatibility testing under ISO 2812-1 or ASTM D543-20 should include the specific cleaning agents and sunscreens used in service. Unpainted parts exposed to sustained aromatic solvent contact may exhibit microcracking earlier than unfilled polypropylene homopolymer.
During injection moulding, the PP/PS melt exhibits non-Newtonian viscosity that requires sufficient fill velocity to avoid flow marks at the gate transition. Class-typical processing conditions for medium-flow PP/PS grades include melt temperatures of 210–230 °C, nozzle temperatures of 210–230 °C, and mould temperatures of 30–50 °C for dimensional stability. Back pressure is commonly set between 5 bar and 10 bar hydraulic; screw rotation should be adjusted to produce a short recovery time without introducing excessive shear heating. Because the styrenic phase is thermally sensitive at high residence times, melt residence time above 230 °C should be kept below 8 min to avoid colour drift and molecular weight reduction. These values are class-typical and must be verified against Kingfa’s lot-specific processing guideline.
For thin-wall parts below 1.5 mm, high injection speed with profiled pack is used to prevent premature gate freeze. When sink marks occur opposite bosses and ribs, hold pressure should be raised stepwise from 60% to 80% of peak injection pressure while verifying gate seal time. Because the alloy has a narrower volumetric shrinkage window than PP homopolymer, pack-pressure errors appear as sink or warpage rather than simple shrinkage. Pre-drying at 70–80 °C for 2–4 h in a desiccant dryer with dew point below −30 °C is recommended only when surface splay is observed after humid storage; at typical storage below 60% relative humidity, drying may be unnecessary.
The low-shrinkage behaviour of Propalloy-1(F) originates in part from the glassy polystyrene domains, which resist the volumetric contraction of the crystallising PP matrix. Under ISO 294-4, flow-direction and cross-flow shrinkage values are typically closer than in PP homopolymer; an anisotropy ratio of 1.1–1.3 is common for PP/PS alloys, compared with 1.4–1.8 for unfilled PP homopolymer. Post-mould shrinkage after 48 h at 80 °C is generally below 0.10% for class-typical unfilled PP/PS grades, although part geometry, gate location, and pack pressure dominate the total dimensional result.
Weld lines are a documented limitation. Microstructural examinations show that polystyrene domains can coalesce at the melt interface during flow-front convergence, producing a sharp brittle boundary if the flow fronts are cold or if gas is trapped. Weld-line tensile strength may be 20–40% lower than the parent tensile strength in unfilled PP/PS alloys; this is measured on double-gate tensile bars per ISO 527-2. For structural bosses and hole features, replacing a single weld line with an intentional stagnation-free flow path or relocating the gate improves performance. The design review should not treat weld-line strength as equivalent to PP homopolymer, which may be more forgiving due to its higher ductility.
| Property | Test standard | Class-typical unfilled PP/PS alloy | Unfilled PP homopolymer reference | Mineral-filled PP reference |
|---|---|---|---|---|
| Density | ISO 1183-1 | 0.98–1.02 g/cm³ | 0.90–0.91 g/cm³ | 1.05–1.25 g/cm³ |
| Melt flow rate, 230 °C/2.16 kg | ISO 1133-1:2022 | 10–20 g/10 min | 10–30 g/10 min | 5–15 g/10 min |
| Tensile stress at yield | ISO 527-2 | 24–28 MPa | 25–35 MPa | 22–30 MPa |
| Flexural modulus | ISO 178 | 1800–2200 MPa | 1200–1800 MPa | 2500–4500 MPa |
| Notched Izod impact, 23 °C | ISO 180/A | 4–7 kJ/m² | 3–6 kJ/m² | 3–8 kJ/m² |
| Heat deflection temperature, 0.45 MPa | ISO 75-2/B | 95–105 °C | 90–105 °C | 110–130 °C |
| Mould shrinkage | ISO 294-4 | 0.5–0.7% | 1.2–1.8% | 0.6–1.0% |
| Water absorption, 24 h, 23 °C | ISO 62 | 0.05–0.10% | 0.01–0.03% | 0.03–0.08% |
The table presents class-typical ranges for injection moulding grades drawn from ISO and ASTM methodological data, not a certificate of analysis for any specific Kingfa lot. Lot-specific data should be requested from the supplier.
Compared with unfilled PP homopolymer, Kingfa Propalloy-1(F) offers lower mould shrinkage and a more favourable adhesion surface, but the trade-off includes reduced cold-temperature impact and lower elongation at yield. It should not be selected for living hinges, high-displacement snap fits, or subzero drop-impact service unless impact modification is specified and validated. Compared with talc-filled PP, the PP/PS alloy avoids mineral filler-related density increase and surface roughness that can appear through thin paint films; however, talc-filled PP may provide greater flexural modulus and lower linear thermal expansion at equivalent wall thickness. Compared with ABS, the PP/PS alloy has lower density and a different solvent-resistance profile, but ABS generally retains better flow-front surface quality and higher notched impact across a broad temperature range. The material-choice decision for painted exteriors and interiors thus centres on whether the combination of shrinkage, paintability, density, and stiffness matches the part function.
Low-gloss painted interior trim in automotive and appliance service combines abrasive contact, occasional sunscreen or hand-cream transfer, and cleaning with dilute solvent blends. PP/PS alloy components are considered in these applications because lower shrinkage reduces gap variation and because the PS phase allows paint systems to meet adhesion requirements without plasma or flame treatment. Painted parts should still be validated by treating the finished surface with sunscreen simulant and common cleaner formulations, then repeating cross-cut and tape pull tests under ISO 2409 or ASTM D3359-23. Chemical spot testing under ISO 2812-3 or ASTM D1308-20 should cover N,N-diethyl-meta-toluamide-containing insect repellents, fatty hand-cream residues, and 10% aqueous isopropanol. Published data for Propalloy-1(F) under specific OEM cleaner specifications are limited; qualification therefore requires part-level testing with the intended paint system.
The low-gloss painted surface is less tolerant of substrate read-through than mineral-filled PP. Because Propalloy-1(F) contains no rigid mineral filler, short-term thermal expansion response under dashboard heating can produce visible stress whitening if the paint film is too rigid. Paint selection should match substrate elongation; polyurethane systems with elongation at break of at least 50% reduce mismatch cracking compared with highly cross-linked melamine systems. For parts with deep grained textures, a surface roughness of 2–5 µm Ra may be required to improve mechanical keying of the primer; moulds must be maintained to avoid gloss variation after painting.
Regulatory documentation for PP/PS alloys supplied into durable goods commonly includes REACH and RoHS declarations. The following matrix identifies the control framework; lot-specific certificates of compliance from Kingfa should be used for final article qualification.
| Regulatory domain | Control parameter | Typical compliance threshold |
|---|---|---|
| EU Regulation (EC) No 1907/2006, Article 33 | Substances of very high concern, candidate list | 0.1% by weight per article unless separately declared |
| EU Directive 2011/65/EU, Annex II | Pb, Hg, Cd, Cr6+, PBB, PBDE | Cd ≤ 0.01% per homogeneous material; others ≤ 0.1% |
| ISO 11469 | Plastics identification marking | >PP+PS< marking applicable |
| EU Directive 2012/19/EU | WEEE recoverability and information requirements | Depends on final article category and producer obligations |
Food-contact and medical use are outside the standard specification unless separately declared and supported by appropriate migration testing under the relevant national or regional framework.